Greetings, this is my first post so forgive me if misplaced. I am trying to figure out the temperature at which this computed ternary phase diagram was plotted.

https://materialsproject.org/#apps/phasediagram/{"chemsys"%3A["Al"%2C"C"%2C"Cr"]%2C"projel"%3A""}

I have had trouble determining this value for various ternary systems.


#2

Hi Tarek,

In general, all of the phase diagrams on the Materials Project are generated using DFT simulations of 0 K, 0 atm systems. Corrections could be made to the data retrieved by the API to approximate them at finite temperature and pressure, but they are not implemented in the current version of the web interface. You can read more here.