LAMMPS data file via write_data, version 29 Sep 2021, timestep = 8000 5236 atoms 3 atom types -0.10428333 28.59108333 xlo xhi -0.10428333 28.59108333 ylo yhi -5 160 zlo zhi Masses 1 183.84 2 15.99 3 15.99 Atoms # charge 41 1 0.0006410665022661948 5.778193590772208 2.806708391778409 2.209284964489161 0 0 0 48 1 0.0001447969087999205 2.616240534671408 6.0197301094151605 2.19853122344538 0 0 0 50 1 -0.00250457077449631 5.9600433059424205 6.1298270108324076 1.9959040708615146 0 0 0 39 1 0.0010818460089754693 2.635957763383669 2.9669773829326345 2.0860361064097566 0 0 0 11 1 0.015939005722334698 1.0253829455400152 4.554416922283105 0.5769337210039627 0 0 0 13 1 0.01099894868807292 4.218836053952564 4.448658028211047 0.5454576796279819 0 0 0 4 1 0.0150737241894415 4.171371850787904 1.2579111006535546 0.6892376611765149 0 0 0 2 1 0.00957510436796085 1.0355076315064853 1.4001197011578506 0.6370312700837889 0 0 0 23 1 0.02260225338482516 6.005636071268019 6.068472924563187 -0.7939734961845051 0 0 0 45 1 0.0003986714969856133 12.21167799740617 2.857528334128401 2.0817145588815347 0 0 0 54 1 -2.3009748716789084e-05 12.147900073605076 6.000680254045733 2.160445193299098 0 0 0 52 1 -0.0027355820512129144 8.880675057786183 6.070322019949895 1.942541776930737 0 0 0 43 1 0.0003162307789352671 9.03067283698417 2.8066310370546814 2.151486766630467 0 0 0 2188 1 0.01720804436152539 13.888771098496658 1.2932651679595089 0.6177911514832835 0 0 0 8 1 0.016200531952391774 10.545359059879239 1.1935664058530904 0.7132706043961377 0 0 0 2197 1 0.01633653629150049 13.82738795083218 4.525568470250588 0.644154264643694 0 0 0 6 1 0.014633109121950323 7.350291946633721 1.1374485838136559 0.7703585204627191 0 0 0 17 1 0.010858953810188334 10.628541092470423 4.473662017778959 0.5709127294135636 0 0 0 15 1 0.006765528727332973 7.450366158091113 4.064406181942907 0.41392416072519495 0 0 0 25 1 0.02189392120223456 8.867447029773631 6.079857499724159 -0.754571490346161 0 0 0 761 1 0.00076100859823262 5.890537840306981 9.310897198691945 2.055623926464024 0 0 0 759 1 8.052039150055709e-06 2.739454613574678 9.315079663505623 2.1953710495191654 0 0 0 770 1 -8.536980036418851e-05 5.787375287853847 12.47895330725801 2.2020428765066278 0 0 0 768 1 -0.001068477941422012 2.53764724997114 12.466062668088844 2.0349226087190364 0 0 0 20 1 0.016050047932362393 1.054445033873097 7.663833002202134 0.5728721492432519 0 0 0 733 1 0.016718814165013307 4.137088748893898 10.966060183627619 0.5779452636746859 0 0 0 731 1 0.016935747923088065 1.0548245616118526 10.84902028348659 0.5197684590133219 0 0 0 22 1 0.009825723121647523 4.181993391689302 7.604140051319446 0.6021675102342878 0 0 0 742 1 0.016565464946328802 4.225295211848713 14.18817695917803 0.6394880547417897 0 0 0 740 1 0.01577279847402415 0.8893579919321335 13.964168021522282 0.6866239582696466 0 0 0 765 1 0.00011539458248390199 12.135057331822775 9.248528263681393 2.178459260565192 0 0 0 772 1 -0.0007440957018102577 9.026585560305218 12.59918592886272 2.2423573709503124 0 0 0 763 1 0.00040331698509623096 9.079332100793495 9.313999121685685 2.1094516783232793 0 0 0 774 1 -0.001022446717299709 12.252778882856097 12.471624077033598 2.226319996448431 0 0 0 2926 1 0.015321086263439997 13.854950057697204 13.973257335062181 0.7254939577476901 0 0 0 735 1 0.014897286054863013 7.493649675276066 11.047221508254914 0.6739234739091575 0 0 0 737 1 0.01584428593393255 10.712129889619167 10.939128974656109 0.6980737302957837 0 0 0 24 1 0.007367274166673703 7.468559525851023 8.139319319407281 0.3441131231298179 0 0 0 2917 1 0.015929223104982237 13.86653771778656 10.843241495780921 0.7133031335397939 0 0 0 26 1 0.010973646591792403 10.644386738350514 7.702938147471706 0.5593300737957327 0 0 0 2206 1 0.015660931986002116 13.833863600191716 7.6329372928216825 0.7081778573220413 0 0 0 746 1 0.015260292989093698 10.730474810604472 14.045186517560197 0.7373828562393097 0 0 0 744 1 0.016620798174868237 7.582938114579235 14.049145725570755 0.6377927804194712 0 0 0 94 1 0.004647713265735622 4.267740367837792 4.4802546912524805 10.107212378747139 0 0 0 83 1 0.004700776317328265 1.0087276459288288 1.3129077540888705 10.020175818757885 0 0 0 85 1 0.00470481888551328 4.157640148123654 1.3134231325993462 10.035305224662327 0 0 0 92 1 0.004612851786314114 1.108666327478928 4.497158373358001 10.09456790049894 0 0 0 102 1 0.004470765107105925 2.6700990508603017 6.134573784907104 8.510056317873369 0 0 0 95 1 0.0043956602248907874 5.761295243768747 2.858860893786911 8.541088360418621 0 0 0 93 1 0.004393535198545255 2.6171362392098256 2.9582197249831257 8.573128407332389 0 0 0 104 1 0.004241967847788904 5.8535196748394815 6.045243084545079 8.516961946349067 0 0 0 56 1 0.005122194322901322 1.038414671916624 1.4146570525941513 6.933130654085558 0 0 0 58 1 0.004884091775877546 4.248701073149276 1.307931986241 6.960159148830232 0 0 0 67 1 0.0051305076575070795 4.219331417842433 4.473722790209378 6.857227023442911 0 0 0 65 1 0.0049592476436611695 0.9818620098243708 4.508012681103697 7.009522267153425 0 0 0 75 1 0.005666091339182175 2.590944721103042 6.0861692483274235 5.3323321851121275 0 0 0 66 1 0.005557270459961558 2.5496290443629936 2.9568323996625625 5.268258900738418 0 0 0 68 1 0.00548289565034794 5.813641524761698 2.826918926009743 5.310757653374483 0 0 0 77 1 0.005886304251561461 5.8045559772135356 5.988478972265812 5.304610042508615 0 0 0 31 1 0.004408016457607716 4.146734860624084 1.2101748100709657 3.6701944461907363 0 0 0 29 1 0.004788353253786447 0.9346752007503428 1.3079371772596013 3.721506627029672 0 0 0 40 1 0.004744500958601131 4.278260410151785 4.394992688448447 3.6280689746127623 0 0 0 38 1 0.004250927603836947 1.016398078137311 4.547455838681306 3.7451854930025106 0 0 0 2278 1 0.00472480455888169 13.840882225306688 4.479726935722756 10.041738788331877 0 0 0 96 1 0.004626488417148501 7.4123093018065385 4.502481043070157 10.126906993285237 0 0 0 98 1 0.0046223025136453225 10.58348080973772 4.457416723669929 10.07186828585241 0 0 0 89 1 0.004669676725319946 10.582849948086865 1.354354408158743 10.022429964889183 0 0 0 2269 1 0.004664004488698029 13.737627702554358 1.304574298020181 10.133120603455582 0 0 0 87 1 0.004774427237515857 7.396684629494149 1.2767346257289613 10.111516731177513 0 0 0 108 1 0.0044252269520823565 12.131413664430166 6.04618107450358 8.587708372026013 0 0 0 106 1 0.0042731715627470895 8.9477267745309 5.987924083264224 8.518073692338922 0 0 0 97 1 0.0043652148859904295 8.966328350820811 2.881138157346901 8.479005195708279 0 0 0 99 1 0.004522605721492238 12.179896703692592 2.912322812891999 8.36908566599172 0 0 0 2251 1 0.004998256609340723 13.679377949621394 4.46668465671259 6.8863188077349164 0 0 0 69 1 0.005085538786164195 7.370579067678416 4.458189449375957 6.934815821408065 0 0 0 62 1 0.00508556575597219 10.611089611498107 1.210898436665611 6.82769059093677 0 0 0 71 1 0.005027965313048565 10.554100498002999 4.397529367234601 6.8733203703956285 0 0 0 2242 1 0.005250112703246721 13.808015213282115 1.1849207025272803 6.823776479267579 0 0 0 60 1 0.004814726010034482 7.38686055802701 1.2390631738482398 6.9826045131635475 0 0 0 81 1 0.005637081859575966 12.137765538491633 6.054953265688222 5.292840409482374 0 0 0 72 1 0.005341338491311118 12.224698458681802 2.9227716388872214 5.2671974278272415 0 0 0 79 1 0.006098555726095531 8.894843246585362 6.056808550682427 5.311646707920132 0 0 0 70 1 0.005756349291771802 9.018507301305247 2.853036707834214 5.387135554432381 0 0 0 35 1 0.004169857747208034 10.550773547880558 1.2511709208373782 3.71735217889516 0 0 0 2224 1 0.003914154102828521 13.730683749349428 4.438922705367682 3.706170327301159 0 0 0 42 1 0.005180779668524675 7.409964597130416 4.417877591304425 3.6832105609467574 0 0 0 2215 1 0.003793959754528774 13.770654690740566 1.277516885820997 3.7227655483750532 0 0 0 44 1 0.004877435903955131 10.514947920106122 4.5171101746182964 3.671532835400001 0 0 0 33 1 0.004230723267819987 7.30295575865153 1.3035472802811703 3.7267443571608414 0 0 0 769 1 0.003773401187713415 4.216152008129003 14.081124638863958 3.7389113506568052 0 0 0 103 1 0.004691110947472739 4.274947388705607 7.620702971364741 10.11602832339809 0 0 0 814 1 0.004747591341153979 4.243244254094473 10.851541058002283 10.127533247782067 0 0 0 812 1 0.00458913507304054 1.0422054264737628 10.8219036671778 10.108993641736507 0 0 0 101 1 0.004567114282130016 1.0222082299648103 7.671691490728537 10.196508686196077 0 0 0 823 1 0.004551455932442491 4.271029639678864 13.948101340709723 10.082871187562649 0 0 0 813 1 0.004564484883811438 2.6062712528211742 9.265311300305362 8.51526273910033 0 0 0 815 1 0.004290138219041166 5.812263588211268 9.26115341510842 8.49196560519663 0 0 0 824 1 0.004376628209633884 5.814192114474005 12.457067535796039 8.525855715781569 0 0 0 822 1 0.004541390135342814 2.577914495279081 12.451156270167052 8.453874966842346 0 0 0 74 1 0.005111098141581515 1.0834748970126853 7.674400759003975 6.863889988442777 0 0 0 796 1 0.0051701384098315675 4.262807703209468 14.073796173911793 6.90217034254324 0 0 0 76 1 0.00518810769111187 4.236463239643906 7.749592977505586 6.937783044645682 0 0 0 794 1 0.005167650938487331 1.0591505531661574 14.02783497124056 6.984432557306771 0 0 0 785 1 0.005156764000208749 1.005748628408586 10.806862925555283 6.849190317332918 0 0 0 787 1 0.00508267527395672 4.232061089335373 10.903260706135503 6.891024613543143 0 0 0 795 1 0.005449072552482283 2.648014441612698 12.470253541950761 5.338567442448312 0 0 0 786 1 0.0056404186200849915 2.6794703329240153 9.29239515969714 5.252192759775297 0 0 0 797 1 0.00528523943436017 5.770531366977092 12.529588912486355 5.3109383984337395 0 0 0 788 1 0.005521476214869472 5.853734968976259 9.276384278379563 5.30478066463527 0 0 0 47 1 0.004076863734578412 1.129986667072629 7.643265538771114 3.634229842308769 0 0 0 758 1 0.004113272666888703 1.0837194184437118 10.886721777912218 3.668178812414171 0 0 0 767 1 0.004153398635345024 0.9800297321469598 14.107461579264175 3.755680540629581 0 0 0 760 1 0.004255090221304809 4.234211266442373 10.910764479807833 3.6824451717097273 0 0 0 49 1 0.004995701878993305 4.356811205537917 7.63560500633026 3.673202352177311 0 0 0 821 1 0.0044465860111794035 1.0589636334685 14.002061481478979 10.149991471835198 0 0 0 771 1 0.003884303809056879 7.36587498568775 14.06345216748307 3.7126697231822354 0 0 0 762 1 0.004420035504343259 7.433048429314405 10.832797589180977 3.8182793546739116 0 0 0 2953 1 0.004233204563481108 13.775000439936367 13.941446973420316 3.8477668243054746 0 0 0 51 1 0.005366725869720748 7.297220482362457 7.689382361412523 3.639032350374955 0 0 0 2287 1 0.004616910215052518 13.89604588527416 7.680815956224898 10.140987945373025 0 0 0 105 1 0.00462425854978459 7.390940359648149 7.664550900483771 10.053558533663297 0 0 0 818 1 0.004649486473847898 10.601197095821767 10.810450389143462 10.11594443097007 0 0 0 107 1 0.004605561410730581 10.610430407519297 7.629160901674728 10.070628450404982 0 0 0 2998 1 0.004661449671544554 13.79859373943033 10.876805013785704 10.246980190785695 0 0 0 3007 1 0.00446775417593006 13.818521693523719 14.103582784471676 10.14776096547197 0 0 0 825 1 0.004575730607942835 7.431139269120185 14.00177128047421 10.138352282899536 0 0 0 816 1 0.004622335650899142 7.461652322749755 10.886991382769763 10.090876406305922 0 0 0 827 1 0.004733089244294152 10.631807788225066 14.011984056261348 10.176350203564127 0 0 0 817 1 0.004359481367992133 9.015717159017907 9.146557741487001 8.473355433034559 0 0 0 828 1 0.004717842215550903 12.302173476198272 12.415205519181939 8.54726838012684 0 0 0 819 1 0.004434533879366506 12.158099843427214 9.159528967206644 8.574263524667495 0 0 0 826 1 0.004661625881963456 9.009627500502155 12.418292145642214 8.539432915714471 0 0 0 80 1 0.0051495510342858 10.635558875827003 7.63435669693242 6.848395300720619 0 0 0 2260 1 0.005209255539797961 13.79389651359276 7.64235698575989 6.935985824820224 0 0 0 791 1 0.005017145399620315 10.558841468833316 10.734199276479737 6.982518708927576 0 0 0 2971 1 0.005352159727267292 13.745269770722704 10.824763402618787 7.015484829707944 0 0 0 2980 1 0.005182217477080224 13.778184989195307 13.948074036882662 6.899972788022235 0 0 0 789 1 0.004907056448323581 7.356544346143234 10.846888042905707 6.930998443138442 0 0 0 800 1 0.00541770618342838 10.62903291290491 14.178612776749764 6.9611912640616325 0 0 0 78 1 0.005154343352050001 7.3462904479729865 7.6842086645223 6.79040073253486 0 0 0 798 1 0.005268330898684873 7.419799219868163 13.944579297162681 6.949481803626844 0 0 0 792 1 0.005536837794545779 12.15016095028023 9.215726233039101 5.310709916770072 0 0 0 790 1 0.00557939002337025 8.977165497713772 9.263480198756994 5.316939629460533 0 0 0 801 1 0.005502135076290892 12.159607128307195 12.355359053107296 5.439993779631875 0 0 0 799 1 0.005471412743618178 9.032258490696423 12.386128781373786 5.379092321712207 0 0 0 2233 1 0.003968173063694548 13.798129174256545 7.692344953749164 3.69313998286621 0 0 0 773 1 0.004182304781512514 10.66823932377213 14.04359894040433 3.812849840832456 0 0 0 2944 1 0.00392338565427626 13.776133550148248 10.765710206640975 3.66616223105706 0 0 0 764 1 0.004238136095993552 10.55291053500049 10.867141696309202 3.7721033510464874 0 0 0 53 1 0.0048728602026529635 10.609721811304299 7.578094403240302 3.6265258516441983 0 0 0 174 1 0.004694965753955848 2.684783654081901 2.825793443530533 18.132987211706688 0 0 0 185 1 0.004737413927416228 5.942478538194943 6.069008868799467 18.211128196232355 0 0 0 176 1 0.0047410665109527406 5.8629611588573916 2.881397291501109 18.104763738995878 0 0 0 183 1 0.004734946639603709 2.7469786578940867 6.065530708736787 18.131106520667004 0 0 0 151 1 0.00469859569939363 1.0573162498610238 1.267643080845149 16.530660778255193 0 0 0 155 1 0.004755777625951798 1.1363603110428084 4.486578006547107 16.515779827729798 0 0 0 152 1 0.004848788597734816 4.177500816690687 1.317712205652078 16.52701022332288 0 0 0 156 1 0.0048117149476794175 4.227218905466528 4.4797267947116435 16.555919731673516 0 0 0 142 1 0.004690286290118129 2.5824675461006064 2.8697026924588616 14.958095199526788 0 0 0 148 1 0.004723821411730979 5.8852882794692984 6.12283331695256 14.950324739669577 0 0 0 143 1 0.004816272185587335 5.807256749828311 2.9276727791346673 14.974265144404441 0 0 0 147 1 0.004874410074611675 2.687185725654462 6.1673456394146235 14.908827635332864 0 0 0 110 1 0.004728938881567403 1.0802947109599594 1.2592920374393142 13.290920681090846 0 0 0 121 1 0.004937191634863773 4.197515107967043 4.401435966222047 13.316256064067618 0 0 0 119 1 0.004851357408748638 1.0232138180052428 4.410917151145355 13.364374039116962 0 0 0 112 1 0.004804900458799078 4.264505655967747 1.2930975280819417 13.271804067584293 0 0 0 122 1 0.005001184176381811 5.742078806581607 2.87175547691631 11.730649452402327 0 0 0 131 1 0.00500279648797845 5.882884807752249 6.044182553446056 11.746707466028726 0 0 0 129 1 0.005048695592674766 2.727853171426289 6.054683250176783 11.677321271088767 0 0 0 120 1 0.004858854471420957 2.558468547928518 2.8213686495773387 11.748749362178396 0 0 0 166 1 0.004802370263678305 4.312499435317458 1.2800955703767274 19.782193093852953 0 0 0 175 1 0.00471132398466372 4.29619761659079 4.422982417369882 19.641678272053852 0 0 0 173 1 0.0047761062252189256 1.1716496987947311 4.527077171411193 19.712033155910987 0 0 0 189 1 0.004774934179669749 12.301510393928739 6.068192810234719 18.072279008105358 0 0 0 180 1 0.004925675414688312 12.23733448610781 2.8668428309177436 18.17402904600162 0 0 0 187 1 0.004795981743907461 9.117517311923443 6.094760223524153 18.06555321921429 0 0 0 178 1 0.004787876184497769 9.047099000031192 2.9038924503317634 18.106670547425942 0 0 0 2340 1 0.004662084032179426 13.92365883698239 4.517284203582329 16.546415118166454 0 0 0 153 1 0.004746492982735533 7.444030063450727 1.327343066590497 16.49158459127986 0 0 0 158 1 0.004824663142747572 10.651397862078262 4.492541779335721 16.494096130781042 0 0 0 154 1 0.0048085400700836715 10.561709306930215 1.3427934321683979 16.496792256517406 0 0 0 157 1 0.0048278743413820695 7.46862357836128 4.512599611743411 16.490010787070013 0 0 0 2335 1 0.004793938424641786 13.793091415766954 1.3085434108868756 16.539332264729943 0 0 0 145 1 0.004828596917411566 12.249352653691865 2.810721081048886 14.981438790621272 0 0 0 150 1 0.0046595930475761375 12.253960803571886 6.03483619214948 14.943289777955156 0 0 0 149 1 0.004565243240024011 9.122004925695578 6.162625754234592 14.892449922008133 0 0 0 144 1 0.004581083553546335 9.036113357579438 2.9749556504247052 14.88722707173701 0 0 0 123 1 0.004818017465932521 7.498186268228661 4.501100114419092 13.321409012805946 0 0 0 2305 1 0.004841795983396046 13.846232957645016 4.520664417471286 13.30614553953023 0 0 0 114 1 0.004809241905788849 7.440616676111907 1.3424032293321237 13.347290727570295 0 0 0 116 1 0.004808725857055496 10.556418296898352 1.3627451897436855 13.26656861627504 0 0 0 125 1 0.0047983646262080345 10.647874348616607 4.476001907188214 13.267743786990936 0 0 0 2296 1 0.0048841247219184765 13.835527162794495 1.3719892679961763 13.319535528313994 0 0 0 135 1 0.005111317950768832 12.17697942807653 6.085996777659869 11.745650114627939 0 0 0 133 1 0.005003460313201721 9.022980703881736 6.150432168854516 11.679384702546686 0 0 0 126 1 0.005047590468975587 12.149781213220534 2.8777914282895662 11.681939463659733 0 0 0 124 1 0.004925441494138885 8.981640342744416 2.9350399142935824 11.763696877260413 0 0 0 2350 1 0.004589987838420436 13.809080171545702 1.342621721082794 19.70203567107917 0 0 0 177 1 0.004643443455254104 7.447544845208562 4.427805439451146 19.63795320582415 0 0 0 2359 1 0.0046465147362963095 13.827385498366548 4.473618656017943 19.656017277908532 0 0 0 179 1 0.004893972109504444 10.560666259925439 4.583296501489913 19.71213577191284 0 0 0 168 1 0.00469549397550403 7.476042994606655 1.3305790739079173 19.797715371436905 0 0 0 184 1 0.004721030521587481 4.315446064897892 7.591066749067578 19.710465664926023 0 0 0 903 1 0.004884435259336382 2.7147716589263227 12.402153700841914 18.043355910672823 0 0 0 894 1 0.004989808644208142 2.743026222307863 9.200941221627044 18.12899441614571 0 0 0 896 1 0.0047225529305075144 5.997719744416827 9.206402345460182 18.145594943873295 0 0 0 905 1 0.0047997790741717405 5.874920821957673 12.533980020540557 18.017799555196216 0 0 0 880 1 0.004873426903097359 1.0366086250253888 10.856271431646014 16.453353538484382 0 0 0 884 1 0.004767704901607049 1.054394540292001 14.088991489038264 16.49539586558023 0 0 0 885 1 0.004704339277406461 4.272699778190206 14.073143846995562 16.524490479407103 0 0 0 881 1 0.0049350993033607255 4.333705302341164 10.838707780781885 16.563856076756792 0 0 0 159 1 0.0049374994868798434 1.0379431057267205 7.7390222795147245 16.532776871561953 0 0 0 160 1 0.004878990650473846 4.369793271410956 7.6465121611693805 16.5027868233263 0 0 0 872 1 0.00473621096218025 5.888206495243055 12.534948530468924 14.906881810706155 0 0 0 871 1 0.004900907748089808 2.6890772649070986 12.510174395889923 14.90979705180626 0 0 0 867 1 0.004747646305864618 6.009111055345899 9.301265137820156 14.932859632404265 0 0 0 866 1 0.004800750222027408 2.680373933599485 9.362660117680326 14.93141313383939 0 0 0 850 1 0.0049286966372520565 4.25621700183641 14.11388051331745 13.309715988525737 0 0 0 839 1 0.004878202383998444 1.0714914764063141 10.86349827821489 13.271046154544882 0 0 0 848 1 0.004811982206968549 1.0291258576060025 14.076335843890943 13.295002111087124 0 0 0 841 1 0.004896140517530723 4.316418753322946 10.864105620899155 13.35079662522431 0 0 0 130 1 0.004902998649281964 4.237111402868638 7.670626097652271 13.328410388581064 0 0 0 128 1 0.004875717844381441 1.093225110457506 7.661326603777431 13.32510278795754 0 0 0 842 1 0.005016041459397063 5.838634495134579 9.306572846361972 11.672683097962732 0 0 0 849 1 0.005052205218282174 2.6020950758323202 12.53421751060093 11.658007285264732 0 0 0 840 1 0.00503290502840111 2.675973777363174 9.303160187433745 11.766193446165323 0 0 0 851 1 0.004883697579583549 5.868478986796749 12.423457563030032 11.732308041355926 0 0 0 904 1 0.004793231456273032 4.319102248339782 14.064035987556162 19.684979641329566 0 0 0 902 1 0.004977046190523891 1.0794586513362783 14.020292514981055 19.634501982924384 0 0 0 893 1 0.004947197764475586 1.1044400266424326 10.935055319094834 19.721116159794335 0 0 0 895 1 0.0048208305421734675 4.26400334422254 10.877363637519148 19.738191437775036 0 0 0 182 1 0.0048478298497242195 1.1432086944608615 7.643631169888501 19.700380326817726 0 0 0 3088 1 0.004756580647301618 13.804915219007606 14.027121006055973 19.61428409001303 0 0 0 900 1 0.004763181202763351 12.239317608084129 9.18894940233316 18.063299765098773 0 0 0 909 1 0.004698374419642763 12.226475109825747 12.346935681322579 18.157838567007172 0 0 0 907 1 0.004821292188055668 9.101298435279494 12.441670544051176 18.11826644865511 0 0 0 898 1 0.00483325520484475 8.951698102699169 9.251200658127487 18.091809079661957 0 0 0 3064 1 0.004749930191234184 13.841234171485151 10.835352932305824 16.50011936732917 0 0 0 2345 1 0.004572744379405672 13.817031603187722 7.669334587121888 16.52389832402067 0 0 0 3069 1 0.004929300076540466 13.735645715178554 14.023335795435687 16.464527178420326 0 0 0 882 1 0.004712696070666544 7.545595519103847 10.877609065125064 16.581570375553113 0 0 0 887 1 0.004792051878873001 10.644952676770288 14.086607140036444 16.565908026322248 0 0 0 883 1 0.004835257444084598 10.681785345991797 10.841644217685555 16.492958988475998 0 0 0 162 1 0.004644480963715591 10.638013855987557 7.680610719888425 16.42754241361071 0 0 0 161 1 0.004608687516002775 7.452617800807716 7.650257071656274 16.433676378851157 0 0 0 886 1 0.004764925668565505 7.51646710859852 14.038202338501517 16.446813037242038 0 0 0 869 1 0.00462053050995638 12.269747659672305 9.209797053693974 14.855849331502117 0 0 0 874 1 0.004757048121987368 12.180911342937954 12.362611042264463 14.924373099932922 0 0 0 873 1 0.00474487818250976 9.001351193073798 12.429343503919945 14.870504875549429 0 0 0 868 1 0.004723160595698321 9.092449884323239 9.27202263211135 14.858490550642674 0 0 0 3025 1 0.004867815666592366 13.789953268885466 10.694653069912265 13.366907837445135 0 0 0 2314 1 0.004708111705648678 13.884739269584562 7.587645342626766 13.349569338625223 0 0 0 132 1 0.004768691823311225 7.415601791123075 7.626817512711729 13.287661171190987 0 0 0 3034 1 0.004848702419007353 13.781863333431314 14.042189015608571 13.334227780337924 0 0 0 134 1 0.004790452192968756 10.671824023541001 7.654255361351146 13.349952855840597 0 0 0 845 1 0.004670854137187467 10.584741057371579 10.916140800177843 13.289079356665308 0 0 0 843 1 0.004633038034137251 7.37806822926705 10.865345924264595 13.287015401566675 0 0 0 854 1 0.0047509990299376085 10.718350439852275 14.136297590871749 13.45545244821879 0 0 0 853 1 0.004911571115206776 9.0421347956224 12.463597522153977 11.779885752564214 0 0 0 846 1 0.005043253750633065 12.237132715327624 9.307464745776297 11.661244509693862 0 0 0 855 1 0.004980690127246381 12.151735433060525 12.480050321610374 11.799461609066203 0 0 0 844 1 0.005143065878197867 8.992118130822847 9.309293152406468 11.686342287423448 0 0 0 2368 1 0.0047311720224578625 13.83041608694314 7.680285512023247 19.742176042543242 0 0 0 188 1 0.00492464665047208 10.631109005971341 7.712303713540464 19.59434352060116 0 0 0 908 1 0.004749586108065612 10.662763485275418 14.117971429812028 19.635134591523613 0 0 0 852 1 0.004716916264297209 7.44784349215437 14.11744855348452 13.30667013956759 0 0 0 3079 1 0.004751245046864701 13.808270896810747 10.841628466668556 19.714601521983916 0 0 0 906 1 0.0049350769078730285 7.479176635936715 13.949711861877931 19.74511004856388 0 0 0 164 1 0.004717657135436915 1.0952560950243364 1.394796935674143 19.755624853748756 0 0 0 266 1 0.004730453889714796 5.933189899085493 6.0791639201304335 27.744799939453774 0 0 0 255 1 0.00475426460786311 2.5642498176215285 2.87299788391403 27.710926492049303 0 0 0 264 1 0.004762389396535276 2.6172675272346586 6.1147860984333935 27.743122635133123 0 0 0 257 1 0.004758322339635326 5.765484528515232 2.829419197699022 27.73783648350097 0 0 0 232 1 0.004873709262246818 1.0964857943818611 1.3576227862363333 26.157517857567303 0 0 0 236 1 0.004789639648892259 1.0583494731892495 4.504144505901741 26.03536499233467 0 0 0 233 1 0.0048360503486942555 4.300520070178955 1.3452041428951345 26.08424448304812 0 0 0 237 1 0.0049113229663239645 4.307389958402701 4.522583883224807 26.137896804935465 0 0 0 223 1 0.00471267117051841 2.756720154171767 2.8762163057053214 24.5017051643913 0 0 0 224 1 0.004708701347931089 5.881736288717481 2.971137088021581 24.561720573856988 0 0 0 229 1 0.004710867544288165 5.836782396872427 6.135531234598545 24.522875003903746 0 0 0 228 1 0.004771294153438268 2.6113366759874714 6.075852455055051 24.51143800726906 0 0 0 200 1 0.004625458144516124 1.0229622189982264 4.440092091961973 22.906121464320755 0 0 0 193 1 0.00468170857971628 4.274290721431201 1.3247772132775988 22.86388490121624 0 0 0 202 1 0.00478598089792903 4.253528260888388 4.429299386783722 22.97939448607881 0 0 0 191 1 0.00467845719248988 1.0856663287823278 1.2547772799931307 22.933094850058275 0 0 0 201 1 0.004726758128469257 2.703979107352244 2.849410578802302 21.3336465438305 0 0 0 212 1 0.0048036481941148585 5.851930704820687 5.991251214700624 21.278236409168006 0 0 0 210 1 0.004884417258552896 2.6175883621262144 6.008608635849957 21.39901082480077 0 0 0 203 1 0.004706654250722206 5.940319803619511 2.9119272507179836 21.339197643816938 0 0 0 170 1 0.004646832894778586 10.590328986304195 1.1807064324428174 19.70896663828292 0 0 0 261 1 0.004681067878619792 12.183739196110864 2.86969444041374 27.669095069361628 0 0 0 259 1 0.004923598482797616 9.008444537747284 2.967323681428504 27.73701618780977 0 0 0 270 1 0.004898511708582102 12.136971673678111 6.170678141023732 27.710989686125114 0 0 0 268 1 0.00482901451646155 9.055912071931163 6.1495209084376 27.677213258356304 0 0 0 2421 1 0.004712574088925234 13.738418205524274 4.460868610327792 26.032812233093036 0 0 0 2416 1 0.004859185162656283 13.777639928979358 1.3506254464531002 26.10617087467176 0 0 0 235 1 0.004736048419246661 10.59215729407073 1.340247228902201 26.140095641372547 0 0 0 234 1 0.004878560052737185 7.473600168345998 1.259786227361641 26.18445716594763 0 0 0 238 1 0.004776034363697702 7.420382227280849 4.556709869872229 26.089346416137918 0 0 0 239 1 0.004680499685379501 10.66198904735001 4.4734522545480315 26.17036769539515 0 0 0 231 1 0.004846255150240175 12.244835150293602 6.030486883741176 24.529684315631396 0 0 0 230 1 0.004769867571239924 9.014686722693988 6.068660212679065 24.423719034862412 0 0 0 226 1 0.004731940668054796 12.063083313656692 2.9240073006171805 24.474575246436903 0 0 0 225 1 0.004856110174378326 9.035982739006508 2.994878552146953 24.447702436598224 0 0 0 2386 1 0.004721069921545685 13.873307178329537 4.480104215236615 22.90648920038625 0 0 0 2377 1 0.004957242972324076 13.8249320283487 1.3105316926397026 22.87371575194751 0 0 0 197 1 0.0047559963040135055 10.607443359577788 1.310101975494113 22.95593560608658 0 0 0 204 1 0.004632183178172187 7.386179042920109 4.550427561387689 22.893710324344333 0 0 0 195 1 0.004838787280289157 7.416841186460256 1.3294170298530685 23.030630592949503 0 0 0 206 1 0.00475795734788536 10.656511197005313 4.60833018570992 22.880955687761414 0 0 0 207 1 0.004951867590635241 12.228398145844318 2.8762168259976852 21.297770042508102 0 0 0 205 1 0.004884144950043665 9.083641796114422 2.93137718424605 21.318755127048956 0 0 0 216 1 0.00491395975447566 12.279223307150014 6.105279034638101 21.267398475364505 0 0 0 214 1 0.004850810272964114 8.974726153882587 6.146444212655505 21.288430709386752 0 0 0 984 1 0.004620637769923332 2.6163824705886674 12.389998987367619 27.623818133958892 0 0 0 977 1 0.004749118273644045 5.839144091874364 9.24453834013779 27.684863976668666 0 0 0 975 1 0.004780439457340186 2.6661315434653514 9.260648712574401 27.7185271429961 0 0 0 986 1 0.004664525440858347 5.733157028354416 12.517951911342504 27.62645024953145 0 0 0 240 1 0.004639982478208566 1.0894190546837776 7.596273564624361 26.096063101105234 0 0 0 965 1 0.004681212010075438 1.0923346585775875 14.048867247465571 26.05382576403979 0 0 0 961 1 0.0048188008112460545 1.0297297029090815 10.815878003125544 26.11057358954818 0 0 0 966 1 0.004607400925719651 4.135244568821893 14.081968365893719 26.172562692797705 0 0 0 241 1 0.004913108040500021 4.24404844721723 7.7253144208366615 26.0965148119264 0 0 0 962 1 0.004720026917263611 4.269441783099237 10.93051354509577 26.087229912803032 0 0 0 952 1 0.004689085224927281 2.685950605140787 12.456449271193824 24.49948472251479 0 0 0 953 1 0.004924611998912859 5.807214720786771 12.555765754508181 24.465987206124662 0 0 0 948 1 0.004866266133849061 5.909196832968433 9.26167714765509 24.508854226580215 0 0 0 947 1 0.004844142778505946 2.6532962961660655 9.300786434743708 24.479938376940332 0 0 0 920 1 0.004820349876934638 1.1156676492387438 10.874846417322617 22.830324285489702 0 0 0 929 1 0.004773869342674748 1.0933648855889844 14.017601187708832 22.84144333415949 0 0 0 931 1 0.004744156576449443 4.179982584288089 14.072196480273407 22.9011227037479 0 0 0 209 1 0.004691679686485279 1.0597856327403898 7.729725988893725 22.936341345000436 0 0 0 922 1 0.0047909059699546945 4.19317664944074 10.836822845229568 22.869307176349512 0 0 0 211 1 0.004892407068261313 4.268179785251634 7.678172193620582 22.852189596340178 0 0 0 930 1 0.004576844701945002 2.7273932737064683 12.499895259574949 21.264275332518256 0 0 0 932 1 0.004719069565008643 5.750415032990275 12.533822251124905 21.299223082331697 0 0 0 921 1 0.004698650409629392 2.694948981503084 9.229488712428466 21.276698996859896 0 0 0 923 1 0.004717809399390939 5.827474167058675 9.237551366909226 21.296250611794015 0 0 0 899 1 0.004881484821885277 10.709248385428989 10.891749085059574 19.733233812011964 0 0 0 897 1 0.004906985744742165 7.384380967295237 10.863065165623285 19.736675593067595 0 0 0 186 1 0.004673373123544666 7.464470630450935 7.739128608447732 19.75897762839697 0 0 0 925 1 0.004844535716496262 9.087719981978708 9.334261643802291 21.3944511002348 0 0 0 935 1 0.004692363828935885 10.746612946841488 14.002419588627488 22.837187472315538 0 0 0 990 1 0.004837198201652213 12.199104512131724 12.532593398890285 27.683602583975652 0 0 0 988 1 0.004870460330176298 9.063585583998753 12.409544540806255 27.706000746988195 0 0 0 979 1 0.004776946524540306 8.99833904179926 9.288268093043403 27.716756059491725 0 0 0 981 1 0.004714722664411735 12.122096214448705 9.322392230201674 27.64140984487421 0 0 0 3150 1 0.004701387091680654 13.902101371205747 14.081764957811869 26.084936834573373 0 0 0 968 1 0.004816022168245908 10.571368086488725 14.048239024995016 26.172515550283375 0 0 0 964 1 0.004775196121271044 10.677122688887245 10.850319343804848 26.052328096402395 0 0 0 242 1 0.004640422802165933 7.42607862024461 7.641874478537192 26.081179784474024 0 0 0 967 1 0.00481749819929601 7.397069990645878 14.063920448646554 26.186738860861425 0 0 0 243 1 0.004749681320593188 10.592774965209891 7.688273040852765 26.027101813473244 0 0 0 2426 1 0.004753523493801898 13.822662791190464 7.72358096469636 26.08134567197094 0 0 0 963 1 0.0049547297610133025 7.3462436940814415 10.932538275257206 26.16471625022849 0 0 0 3145 1 0.004752765876512967 13.866446601138225 10.851542089140287 26.07370831546218 0 0 0 949 1 0.004792417429855181 9.066458623344195 9.25656047987125 24.53657992129657 0 0 0 954 1 0.0050542070494305445 9.086810522935146 12.505102738770292 24.53462649225971 0 0 0 950 1 0.004652387371640325 12.268592527184138 9.2760609783081 24.485016002804056 0 0 0 955 1 0.00485936903301371 12.336695866988922 12.503974024806931 24.486077973405582 0 0 0 926 1 0.00475373030371317 10.691210257160078 10.900803376383466 22.957916122948106 0 0 0 3115 1 0.004711455897015115 13.823310575109051 14.06457748498295 22.8343641834321 0 0 0 2395 1 0.0047581866881100995 13.812094536053099 7.788625917448963 22.88159158995752 0 0 0 924 1 0.005029031101032581 7.445200466480501 10.87515980870659 22.91678861869219 0 0 0 3106 1 0.004681370594485389 13.900282395207789 10.900891750930485 22.903090579770613 0 0 0 215 1 0.004817139236945099 10.681871763210019 7.741243179408758 22.883606115570036 0 0 0 213 1 0.004704782294051281 7.461341288682663 7.718352864169742 22.911050313414712 0 0 0 933 1 0.004805593916301764 7.343042093896209 14.15208317386636 22.886930470333454 0 0 0 936 1 0.004602073944222757 12.237643627833531 12.536194197887113 21.27828392703039 0 0 0 927 1 0.004713775513057732 12.22318462977887 9.340996996304323 21.31077822815864 0 0 0 934 1 0.0049039574511545395 9.040496061219473 12.519760936834617 21.36539752751063 0 0 0 299 1 0.004641811120199421 1.0775314301817724 1.37093777782586 35.6836972478977 0 0 0 310 1 0.004971824769546416 4.339712072213763 4.5393641456726375 35.64468708665685 0 0 0 308 1 0.004680141007922583 1.0664105832709716 4.4340308838137155 35.66410578462888 0 0 0 301 1 0.004763593307171202 4.334121507916174 1.3903986610262318 35.62686734955916 0 0 0 318 1 0.00466100160782537 2.6378907385281023 6.183089283662575 34.05897931170645 0 0 0 309 1 0.00479536258464767 2.614074682455108 2.9257237354218018 34.104330857935516 0 0 0 311 1 0.00466152797607834 5.915037125776954 2.925713093299575 33.969974142443974 0 0 0 320 1 0.00473712424935872 5.943107496744397 6.101597402513963 34.11525687020891 0 0 0 281 1 0.004870053650099446 1.0870772298142248 4.577064106073806 32.541512865086936 0 0 0 272 1 0.0046712827641624734 1.0741050881468956 1.2878423821860037 32.44225660829681 0 0 0 274 1 0.004772047157977532 4.277310713943311 1.4052855014164836 32.5375667371496 0 0 0 283 1 0.004839903134012918 4.214114452463162 4.631097831957424 32.52382586638331 0 0 0 291 1 0.004661927152822275 2.6381470809096292 6.194533857165118 30.876162721185516 0 0 0 293 1 0.0047709886039502165 5.875529684446717 6.172553959509347 30.92697185087221 0 0 0 282 1 0.004832175525335337 2.7653169415525825 2.941528048609887 30.902022047966575 0 0 0 284 1 0.004675299951040206 5.867712579679979 2.9924750400864237 30.911151332738637 0 0 0 245 1 0.004670205337254121 1.0527481828229552 1.3185226159342613 29.308186261211688 0 0 0 254 1 0.00486530417200659 1.1261880246143068 4.517078506680614 29.2819893217718 0 0 0 256 1 0.004814200992159862 4.204088998271043 4.551483161706489 29.323861109855528 0 0 0 247 1 0.004716585581556791 4.269748267961997 1.3763218285646686 29.30259301994468 0 0 0 2485 1 0.004843053417512155 13.850994046350657 1.310219610061137 35.64225786309745 0 0 0 305 1 0.004812059933144177 10.632709121856312 1.2509371491982728 35.6792899155311 0 0 0 314 1 0.004817370129391716 10.611650802597591 4.460268913068528 35.61509319730459 0 0 0 303 1 0.004682706420162306 7.45685975304327 1.2969544172933385 35.62090085654341 0 0 0 2494 1 0.004973197275406181 13.800459980752477 4.470416854187378 35.630945477853885 0 0 0 312 1 0.004898535471986027 7.438676924804485 4.458663735515422 35.667353314435616 0 0 0 315 1 0.004710773112392654 12.20733399685701 2.8604646200778046 34.04872219918033 0 0 0 324 1 0.0048570594700607615 12.227922822651282 6.179742150610774 34.06443004638348 0 0 0 322 1 0.004689157749664002 9.121700982113023 6.078842317747276 34.07348173621316 0 0 0 313 1 0.004672871417299008 9.129194284251055 2.8118520121556165 34.046496732822774 0 0 0 276 1 0.0046221990293252874 7.492160606994984 1.3870554728702758 32.46760640422767 0 0 0 285 1 0.004687943476353481 7.469186264380778 4.500274404328403 32.45660620576626 0 0 0 2458 1 0.004690646876019316 13.821841850109404 1.4166177782063267 32.44714290373659 0 0 0 2467 1 0.005013216897617518 13.80654772751816 4.5559910113991915 32.459288959936295 0 0 0 287 1 0.0047825996502212885 10.641620138676616 4.479869313222294 32.51476527049731 0 0 0 278 1 0.004730833333417634 10.64833628909745 1.337754947677559 32.38841715562826 0 0 0 297 1 0.0048826867908168155 12.206128611776654 6.172032074614893 30.870546194756393 0 0 0 295 1 0.004969548271616582 8.999784616989261 6.112598086972353 30.918610892437222 0 0 0 286 1 0.0047697366315374665 9.030115811508189 2.9022448979700646 30.878979310598538 0 0 0 288 1 0.004830905473068527 12.234871782309483 2.899449233482136 30.812539912135595 0 0 0 2431 1 0.004766562831390217 13.877951842674232 1.239992107344892 29.28356649521748 0 0 0 2440 1 0.004997736086144693 13.827953001696358 4.4548459762481585 29.204958903339307 0 0 0 251 1 0.004760609163477741 10.656542931359134 1.2300452805913666 29.24635880410949 0 0 0 260 1 0.004881273943146157 10.611148679207755 4.510980418324707 29.332961778031326 0 0 0 249 1 0.004723819620802977 7.4126913805493 1.2768968335697557 29.346951788573133 0 0 0 258 1 0.00477860045792286 7.354357080946749 4.493280458526862 29.27829314936461 0 0 0 1039 1 0.004794455063328847 4.2595299352698754 14.010879101824086 35.708076524216004 0 0 0 1028 1 0.004792528049000565 1.0788764671080937 10.893898503781116 35.63361739137668 0 0 0 319 1 0.004642543911698998 4.2773403939259325 7.681544103727698 35.726855514224205 0 0 0 1030 1 0.0047830829061679524 4.322661751359611 10.80871035588787 35.65217687828927 0 0 0 317 1 0.004614034910949876 1.099515600962059 7.589032609867864 35.64853837300718 0 0 0 1037 1 0.004880001398432336 0.9908446886977078 14.00562109054408 35.61181684870725 0 0 0 1029 1 0.0047172882842962584 2.730077860450822 9.25795307676428 34.09463980758625 0 0 0 1031 1 0.00478442739940174 5.8366427091885855 9.289482409890038 34.096567633137006 0 0 0 1040 1 0.004848390336869434 5.825820808132927 12.499348084401761 34.0424219326227 0 0 0 1038 1 0.004828674123981271 2.6664756572217843 12.468473172455573 34.04327813225149 0 0 0 1012 1 0.004842023548116466 4.2107983105716285 14.083746916355988 32.3774147683702 0 0 0 292 1 0.0046604541415953705 4.271440563724201 7.7159687514953665 32.42300381165359 0 0 0 290 1 0.004758856723654668 1.1249008763137098 7.702208250595639 32.48933918395329 0 0 0 1003 1 0.00480051200556408 4.186798530210364 10.877278446594604 32.47195108776272 0 0 0 1001 1 0.004893434673006264 1.0904967189335448 10.841999781779375 32.427676004176895 0 0 0 1010 1 0.004863039525165045 1.0377197001476257 13.991054615718143 32.42941279928034 0 0 0 1004 1 0.004782761222818208 5.8625208274114184 9.229739283828042 30.84431803415338 0 0 0 1002 1 0.00468874686438522 2.67300367672021 9.272949279383615 30.883569671387917 0 0 0 1011 1 0.0047087228107836766 2.642476956676766 12.500702198522768 30.765332600762378 0 0 0 1013 1 0.004839699216595892 5.777417202998167 12.456750099768193 30.857051880143345 0 0 0 983 1 0.004700310761731958 0.9911598261881404 14.03406814388483 29.24492398997021 0 0 0 985 1 0.004702735439246689 4.196234559140459 14.011423838852144 29.21537932843802 0 0 0 974 1 0.004836868506787615 0.9698267585474014 10.865547481281219 29.323620997789455 0 0 0 976 1 0.00476746703431063 4.203140887660851 10.84380837760458 29.24677000504651 0 0 0 265 1 0.004680686538281707 4.238446545279699 7.714806401131843 29.273640332213187 0 0 0 263 1 0.004733391484884046 0.963217528864682 7.707893735357339 29.229588969800144 0 0 0 1043 1 0.00473472899819205 10.696520598986451 14.143769184813308 35.624127956267785 0 0 0 1041 1 0.004792609895275765 7.441432064100717 14.073133078060037 35.636112343134684 0 0 0 2503 1 0.004706661901458976 13.852645341295892 7.632618689798698 35.666929761636 0 0 0 323 1 0.004820556871794968 10.573327635012872 7.6426443371741 35.69728387063181 0 0 0 3223 1 0.004978828515564818 13.824441998093702 14.036771063299607 35.666519701532685 0 0 0 321 1 0.004755744776501895 7.456777645133583 7.64680987096474 35.70763169908974 0 0 0 1032 1 0.004761226387063805 7.4814447427268345 10.889213314141754 35.68002194418963 0 0 0 3214 1 0.004793061279473789 13.77310141761193 10.932578400665129 35.661327497569964 0 0 0 1034 1 0.004897665761133742 10.675356508958023 10.990014961937884 35.650567879559986 0 0 0 1035 1 0.0049514588434744974 12.28381221760635 9.337087716424026 34.038302262764255 0 0 0 1033 1 0.004954121392059087 9.038893380648124 9.308001028041124 34.115011493698155 0 0 0 1044 1 0.004811657034091752 12.276266841976842 12.489115474757739 34.01391595179147 0 0 0 1042 1 0.0047660671501061555 9.017855149103829 12.527679119358671 34.01214518678878 0 0 0 294 1 0.004764249136552547 7.439472494118395 7.678722420530938 32.57693267279371 0 0 0 3187 1 0.004764532481252807 13.83887975242219 10.893884798763262 32.4124755005696 0 0 0 2476 1 0.004788243408320642 13.88437618834882 7.784026077992419 32.42383615336539 0 0 0 1005 1 0.004829451384591829 7.403792387854879 10.89729131890826 32.47546834652056 0 0 0 3196 1 0.004926796145957774 13.810797209765214 14.205996266027398 32.438589639697206 0 0 0 1014 1 0.004851524545396588 7.440793701138899 14.089949393369006 32.43182919634058 0 0 0 1007 1 0.0048009081891593735 10.53213711445397 10.916616613051962 32.37861402342387 0 0 0 296 1 0.004783509998717274 10.66590382373672 7.736900576144572 32.51087918722309 0 0 0 1016 1 0.004768378199955764 10.64747071618167 14.113818433419903 32.4821818493435 0 0 0 1008 1 0.004583726351170851 12.207689616015962 9.25829481731332 30.842409203409463 0 0 0 1006 1 0.004697934439948519 8.981906499932991 9.300028189198377 30.887775384616706 0 0 0 1017 1 0.004808099529971591 12.163696011602102 12.427170773911632 30.889085910599015 0 0 0 1015 1 0.004755978112294395 9.049410023128914 12.539142496248973 30.86398365299503 0 0 0 267 1 0.004655258140650816 7.481669554604769 7.714339044606664 29.219073708917076 0 0 0 978 1 0.004871698347697007 7.44078647118045 10.88387324365865 29.385416247236478 0 0 0 987 1 0.004890127946644569 7.350960442114251 14.107350048161997 29.267236638006004 0 0 0 3160 1 0.0048674541431243615 13.816916341144042 10.844263482897178 29.305822598717306 0 0 0 269 1 0.004626642562889896 10.665348499915654 7.789392731039654 29.348026681327504 0 0 0 989 1 0.0047239652604823355 10.63397110907321 14.10666416307867 29.256275691885925 0 0 0 2449 1 0.004795187519078535 13.813416816264253 7.719973117031344 29.22242632581852 0 0 0 980 1 0.0046339439634825765 10.644658754814936 10.819772373472096 29.289692931375377 0 0 0 3169 1 0.0048998874698119275 13.807175292246308 13.95390873103373 29.321491506139697 0 0 0 392 1 0.004697908288576627 5.8405251667288125 2.8939847253562245 43.63784145090814 0 0 0 399 1 0.004854370351041679 2.683009667915783 6.155217667643634 43.59321868481607 0 0 0 401 1 0.004795006034345399 5.848241097405228 6.082868405423073 43.698186807266254 0 0 0 390 1 0.0047687810690625575 2.5916087220099704 2.812204391208448 43.5358979717433 0 0 0 372 1 0.004780678599567399 4.298233560999131 4.557739482806243 42.002845718004274 0 0 0 371 1 0.004739229231274313 1.0581739075043897 4.546891982183758 42.01994740133882 0 0 0 367 1 0.004845544751624279 1.0646601218093688 1.256745135592985 41.98718440491016 0 0 0 368 1 0.0047866247188855255 4.258634967928719 1.2553167840475052 42.038942792229264 0 0 0 364 1 0.004913481060138426 5.865714275061623 6.057524926814051 40.42001908140495 0 0 0 359 1 0.004682840141499762 5.851697211255299 2.9438643590244955 40.486286423482994 0 0 0 363 1 0.004820857634940725 2.649465972855142 6.109857876725515 40.37646059181459 0 0 0 358 1 0.004685698732726003 2.662878362547337 2.9762688551536836 40.47103827504666 0 0 0 337 1 0.0046779198614747795 4.203842288320196 4.369861170403969 38.915547764944364 0 0 0 328 1 0.004760123945318441 4.223730514627924 1.3803650657728697 38.84302268919857 0 0 0 335 1 0.00464165327012713 1.1025366532385443 4.432035998485307 38.88383490854168 0 0 0 326 1 0.004830204389630031 1.0851313846303565 1.2855603532625604 38.80347753808472 0 0 0 338 1 0.004690380924496038 5.89978415507525 2.825531689082168 37.23431934617166 0 0 0 336 1 0.004633903873776733 2.6947727906510175 2.936467044250188 37.27282893887695 0 0 0 345 1 0.004763019989033933 2.63748312610441 6.081786091756726 37.20302080995973 0 0 0 347 1 0.004795859256961311 5.846315101101728 6.0975718729974675 37.335971092670064 0 0 0 403 1 0.004745083669287269 9.063775598829823 6.137025858389663 43.69337112416416 0 0 0 396 1 0.00486492923400521 12.197692887292268 2.749364767136478 43.604502602073794 0 0 0 405 1 0.004929916669925989 12.289178355038835 6.031774593474627 43.71985039181166 0 0 0 394 1 0.004760569984248342 9.008127364172813 2.8993351657400486 43.7950209369494 0 0 0 2556 1 0.004785527704136908 13.788863702214405 4.415166554958145 41.95848966858641 0 0 0 370 1 0.004766516522137122 10.544659709550741 1.2961227823833557 42.003382713239 0 0 0 369 1 0.004867598277003272 7.4510674211519055 1.2653790790968995 42.03161075925531 0 0 0 2551 1 0.004785531451907925 13.848799693233167 1.224056556528707 42.05399440060344 0 0 0 373 1 0.004851258055494226 7.433884883237021 4.476024711281298 42.160755939394534 0 0 0 374 1 0.00486761662949234 10.545090323122473 4.416794444049432 42.09098135834414 0 0 0 360 1 0.004818495101795479 8.970739340748064 2.8350808645341647 40.40752997850275 0 0 0 361 1 0.0047019438296150295 12.13518441814025 2.8211248280972523 40.46335337372853 0 0 0 366 1 0.004684560913086463 12.238607150704507 6.016700115447576 40.4921674915733 0 0 0 365 1 0.004864214712472063 9.08720038198882 5.947060782190653 40.429595086127286 0 0 0 2521 1 0.004680253377796489 13.8505250981914 4.502599480424718 38.776375549654624 0 0 0 341 1 0.004694335981732191 10.78547678061118 4.448487567416505 38.929403522825005 0 0 0 339 1 0.004800318632676931 7.414865793556028 4.471329943826329 38.892651036752085 0 0 0 330 1 0.004709040467889378 7.344253861081826 1.3098385407686932 38.82194039260752 0 0 0 332 1 0.004685544214680612 10.575452380964753 1.1839745576297254 38.85490650967157 0 0 0 2512 1 0.004724714208303473 13.758758637526903 1.3062433197578696 38.83013877748946 0 0 0 340 1 0.004947287759213832 9.087793500685958 2.821809949812535 37.27359722038707 0 0 0 349 1 0.004889883150917514 9.040779013082995 6.022999466082466 37.26969391691847 0 0 0 342 1 0.004777383159248574 12.217153790931357 2.867806343238234 37.28540654025748 0 0 0 351 1 0.004827533100162703 12.228578698429555 6.045805191404174 37.29029018764373 0 0 0 1112 1 0.004679569370405201 5.854578578210663 9.341244777296858 43.67143593912106 0 0 0 1121 1 0.004783242409803339 5.850577407092799 12.464880293822763 43.665676549385125 0 0 0 1110 1 0.00469845075743172 2.595303698641513 9.174062831782782 43.58114649468655 0 0 0 1119 1 0.004723661488748719 2.6935055301319113 12.501220578929818 43.5927595799972 0 0 0 1096 1 0.004808907113234546 1.0120028014241114 10.91714868509047 42.04436727059671 0 0 0 376 1 0.004817681545388398 4.270067918631887 7.758806132026376 42.08370787301176 0 0 0 1100 1 0.0049198703207081525 1.0782078023853034 14.07374490265755 42.02529163153873 0 0 0 1097 1 0.004788733864113166 4.210439418883576 10.88652716380179 42.086893275407704 0 0 0 375 1 0.004834175014397396 0.9735845007478112 7.635529344411342 41.957468587537555 0 0 0 1101 1 0.0047480842105659185 4.328548562630886 14.064513698956235 42.059467070889184 0 0 0 1083 1 0.004816715006348907 5.8083168790068385 9.18440830617014 40.44264917011895 0 0 0 1088 1 0.004886324665063488 5.872153713435192 12.472964938540047 40.4269247972535 0 0 0 1082 1 0.0047457680681346395 2.634199963352902 9.323484350761564 40.46009574568732 0 0 0 1087 1 0.004654280843985101 2.6921706897115256 12.450813239314407 40.42272028386746 0 0 0 1057 1 0.004853316762959192 4.273254866990246 10.82287964359044 38.928897577087454 0 0 0 1066 1 0.00476334556982788 4.239752171564394 14.083998472974697 38.918144981410514 0 0 0 346 1 0.004720872512588358 4.205933469531203 7.677736254945593 38.804294255939475 0 0 0 1064 1 0.004606601350842022 1.0686212292880237 14.02726260299123 38.806380320307 0 0 0 1055 1 0.004626011526960223 1.1164200522291141 10.99574462819305 38.91087264387349 0 0 0 344 1 0.004712347465074792 1.0904115517405946 7.749184061137642 38.806121272037785 0 0 0 1058 1 0.004666564823229647 5.880767018092327 9.233292760213077 37.23932580614254 0 0 0 1065 1 0.004874580318788128 2.627581382524507 12.39857879786956 37.25752122266122 0 0 0 1067 1 0.004864691151503545 5.838684312997826 12.484529648039828 37.236398039497004 0 0 0 1056 1 0.004780553751999938 2.6630049802133966 9.235730631973663 37.24974264088485 0 0 0 1071 1 0.0048253927738833875 12.201424563591527 12.538640207336263 37.345450077647584 0 0 0 1116 1 0.00478223834138833 12.205460775148245 9.203795144176576 43.57462498236627 0 0 0 1114 1 0.00478080266778136 8.986443577062317 9.256445834152334 43.68716656001762 0 0 0 1123 1 0.004807347464219647 9.052421230398846 12.431622577440837 43.591820178515036 0 0 0 1125 1 0.004654098115167432 12.122790769363204 12.444561135633093 43.582095658313804 0 0 0 1098 1 0.004965710733262036 7.4232711867714976 10.866887399138811 41.95263182851692 0 0 0 2561 1 0.004848101864519018 13.848849121000836 7.613611221776884 42.039911071190886 0 0 0 377 1 0.00493549396777704 7.437468586341781 7.71658306698999 42.13973523889464 0 0 0 1102 1 0.00482147554008832 7.446086219857534 14.116442928421652 42.07806786724925 0 0 0 378 1 0.004802748014994538 10.613768776255833 7.5587394202251215 42.04815638065848 0 0 0 1099 1 0.00475976695956574 10.640871449596071 10.813401109007968 42.03897324081775 0 0 0 3280 1 0.004703869415145738 13.807371021607944 10.877972274131508 42.00322297385773 0 0 0 3285 1 0.004614012171464869 13.740603461879589 13.99936787550365 42.03287112054481 0 0 0 1103 1 0.004658699793094271 10.649108773080295 14.036631534131384 42.0127422965669 0 0 0 1084 1 0.004806287166357842 9.158138140283528 9.220461162054612 40.503253023565456 0 0 0 1085 1 0.00482760945846545 12.240394103494653 9.305195534852576 40.44083376858413 0 0 0 1089 1 0.004963408029633406 9.05716011267611 12.477617458229709 40.38977966344908 0 0 0 1090 1 0.004665134177590364 12.276175335690649 12.510491311894013 40.39182522582657 0 0 0 2530 1 0.004722507907700959 13.843371720087433 7.701150666376245 38.80834156342036 0 0 0 348 1 0.004843508675796648 7.480210620534318 7.691369643278282 38.85171120924465 0 0 0 3241 1 0.00473416295719269 13.898514604752936 10.817586181030101 38.86787870973952 0 0 0 350 1 0.004738109102480853 10.672768744241525 7.601435043880844 38.91429783775584 0 0 0 1068 1 0.004860124409457234 7.395538414265069 14.050118093120986 38.78717674484016 0 0 0 1059 1 0.004942603295578879 7.477311638344199 10.735789616827534 38.79377335814953 0 0 0 3250 1 0.004761845513330091 13.79224548479589 14.118454272571897 38.884137619593794 0 0 0 1061 1 0.004741991307903095 10.648899960093178 10.897683042251728 38.880539077312235 0 0 0 1070 1 0.0046860993602449025 10.603685756995038 14.094570705296254 38.85385638850633 0 0 0 1060 1 0.004746665113148134 9.136680511737158 9.26562061772712 37.33197815799824 0 0 0 1069 1 0.004822966098666668 9.022142592417412 12.46558283745858 37.12793264124033 0 0 0 1062 1 0.004905264915950213 12.156938684538352 9.268319358625321 37.26576461181159 0 0 0 449 1 0.004822366005827108 4.183908232776666 1.198339910058679 51.5222770396498 0 0 0 453 1 0.004854184400357701 4.125849576524882 4.594993145338914 51.57523365581958 0 0 0 452 1 0.004804577370058842 1.0069248771533044 4.395826771522738 51.57176130787507 0 0 0 448 1 0.004616468430432475 1.082635084163367 1.2270054190683628 51.584529254885965 0 0 0 445 1 0.0046420340244483025 5.815717521966586 6.201053724995399 49.98638445697934 0 0 0 439 1 0.004824830243692398 2.576425326086013 2.8959962983723346 49.98377636816593 0 0 0 440 1 0.004932725102975953 5.715758632504445 2.9589375398595483 50.016617756016146 0 0 0 444 1 0.0048482551972423744 2.5396586909941044 6.1032199810045995 49.85012477964551 0 0 0 416 1 0.004862139229171409 0.9070437580872137 4.452343540166093 48.4118825157906 0 0 0 407 1 0.004888064052443143 0.9738637313879824 1.298151549127394 48.425550848358604 0 0 0 409 1 0.004955392965137187 4.2102611920650155 1.342057649443702 48.40603862020162 0 0 0 418 1 0.004831813639559725 4.1901704649345675 4.451597306039475 48.29013889988232 0 0 0 417 1 0.004830453509284325 2.590067663187173 2.9851950674951757 46.69412429467883 0 0 0 428 1 0.004836708625969572 5.786835108317673 6.040043405552951 46.8974066354109 0 0 0 419 1 0.0047336888325625204 5.828316949620973 2.9171523905490027 46.738823614623385 0 0 0 426 1 0.004894252766417664 2.5757974872855334 6.05855107987949 46.75713242820583 0 0 0 380 1 0.004650333900458678 1.0530028468886723 1.225489970293036 45.161002744809196 0 0 0 382 1 0.004714257459844067 4.270970325740686 1.3422372070716992 45.209996015761796 0 0 0 389 1 0.004730032224632887 1.0573595204991002 4.392865826332451 45.12097572608196 0 0 0 391 1 0.004679421269108327 4.121516990559283 4.529870154177928 45.1317900418216 0 0 0 2637 1 0.004872706889329396 13.799577727279848 4.484486349539767 51.565274271532616 0 0 0 455 1 0.004640336545043339 10.59722692789181 4.549946696615187 51.60645224147528 0 0 0 450 1 0.0048779103455572 7.328772385374969 1.2208052290755582 51.58431872557131 0 0 0 454 1 0.004790580676617712 7.283390097689689 4.525939452968822 51.5631737189192 0 0 0 451 1 0.004813364917365151 10.564175956700876 1.2505493934811787 51.48831980937047 0 0 0 2632 1 0.004788369227442529 13.808742467987864 1.3273113344862726 51.512735831205745 0 0 0 447 1 0.004687179280550796 12.142350113458242 6.06734896164673 50.02413123389973 0 0 0 442 1 0.004657907460926329 12.141774642239788 2.9281082083467993 49.99126742718747 0 0 0 441 1 0.004844066618970248 8.963851445013447 3.0007271068656345 49.999254457056566 0 0 0 446 1 0.00467151189643133 9.01041092497271 6.184476839803099 49.93005211169743 0 0 0 2602 1 0.004685100364337991 13.706773598045293 4.5074560135340525 48.3310229803162 0 0 0 2593 1 0.004656981488334995 13.73185473931058 1.3543461066864853 48.4151318674275 0 0 0 420 1 0.004766268363125128 7.444479971850809 4.4848621907319774 48.454519732190164 0 0 0 422 1 0.004585478027825135 10.592379652487967 4.41601114656016 48.41749271497013 0 0 0 413 1 0.004815596262498148 10.562831764486699 1.3408235495475955 48.412051849262994 0 0 0 411 1 0.004859680291219956 7.345866886530175 1.2507115851192836 48.36756436945198 0 0 0 432 1 0.004684962715165901 12.123205905570304 6.04927041809021 46.89037019203336 0 0 0 430 1 0.0048022168309726585 9.061654910903265 6.014535908601095 46.8001786082655 0 0 0 423 1 0.004688290282871205 12.21768479682713 2.8472564383072823 46.794669953364576 0 0 0 421 1 0.00470656586156596 8.929709690672368 2.831575726709974 46.84629282623927 0 0 0 2566 1 0.004661191895636888 13.749800256128822 1.220589166674345 45.23186967673423 0 0 0 386 1 0.004791643529105652 10.584425551608819 1.301644185086805 45.213623046385244 0 0 0 393 1 0.0046917579924790846 7.376298151703259 4.480847610213166 45.29583545670339 0 0 0 2575 1 0.00478035094137551 13.867271927026634 4.3699736528242115 45.149420523668475 0 0 0 395 1 0.004770428919199647 10.62590078121394 4.489324146649053 45.301315643275295 0 0 0 384 1 0.004654926220853502 7.328616599811477 1.2167609922537164 45.14291705221104 0 0 0 1181 1 0.0048312165681746 0.9515153305714817 14.025051396221759 51.60196757056586 0 0 0 1182 1 0.004761141778588452 4.127545009467442 14.019326160737492 51.702345729087504 0 0 0 456 1 0.004777179606924777 1.0610318871334417 7.687395338489078 51.50405875749793 0 0 0 1177 1 0.004802856006362679 0.9433058129325572 10.848241682917891 51.54474243806382 0 0 0 457 1 0.004662242813731836 4.270600776903434 7.729747758403995 51.528937924852784 0 0 0 1178 1 0.004791025164193738 4.07758751055014 10.87719298380893 51.631780338486784 0 0 0 1169 1 0.004860175889382338 5.807581753099654 12.485776041047593 50.01076582387016 0 0 0 1164 1 0.004662866869114048 5.851561421300013 9.36745911652939 49.91554344274928 0 0 0 1168 1 0.0048207365804928334 2.552686859170243 12.429251402080927 49.9873202501438 0 0 0 1163 1 0.004591645197361853 2.6069137097509447 9.168976314693646 50.01937074624471 0 0 0 1138 1 0.004825222324241266 4.157457932570361 10.80643744494109 48.37028760224735 0 0 0 427 1 0.004610735588777622 4.2020085759026005 7.6824340701128335 48.49831668020572 0 0 0 1145 1 0.004831665101346258 1.0221945530754217 14.061896156947789 48.40961484803966 0 0 0 1136 1 0.0049259146800908135 0.9657861797809139 10.870581031863066 48.41331665284881 0 0 0 425 1 0.004634436537365259 0.9896212907356434 7.759549743376456 48.425074819190215 0 0 0 1147 1 0.004879341649275891 4.161922291118831 13.974636916953102 48.38292655537261 0 0 0 1146 1 0.004881477213449689 2.5963719639091134 12.463916960532115 46.78041600990161 0 0 0 1139 1 0.004627325170905361 5.8316203329572875 9.198389131433464 46.82764771813474 0 0 0 1137 1 0.004779893953732179 2.6616494448264194 9.258277269933641 46.787161401843775 0 0 0 1148 1 0.0048888505403231405 5.841911936150015 12.355068501495355 46.900989440501405 0 0 0 1109 1 0.004843124328532886 1.004293785339029 10.850061066414812 45.06810948726624 0 0 0 1111 1 0.004817729532656455 4.21762959475141 10.784232756450669 45.23295407795488 0 0 0 398 1 0.004886984908278021 0.9862391169516839 7.773896638944585 45.23959143561486 0 0 0 400 1 0.004726623252988867 4.236329379399507 7.712851994257498 45.27909884421489 0 0 0 1120 1 0.004901693166121953 4.205369255335627 14.043952626232958 45.151728978040246 0 0 0 1118 1 0.004805816882115278 1.0247573591253496 14.048217994037945 45.23331047261485 0 0 0 2642 1 0.0049036490145833375 13.800498782714744 7.693961670631779 51.56552675770273 0 0 0 458 1 0.0046844063411491475 7.4223665472378615 7.727131481283077 51.56619636739464 0 0 0 1180 1 0.004752271836512733 10.559011042788308 10.875892338350868 51.585982345292216 0 0 0 459 1 0.004701579999319165 10.607400170405644 7.661088313269378 51.58606298279671 0 0 0 1179 1 0.0047333958796980935 7.333628998708504 10.878819121886197 51.64995319930969 0 0 0 3366 1 0.004784283946978472 13.73011052969196 14.079375834085711 51.63516642145422 0 0 0 1183 1 0.004817467013343908 7.330137254860379 14.070665418202017 51.59649412980434 0 0 0 1184 1 0.004816026633199548 10.457743402139707 14.059165699194628 51.560350038417305 0 0 0 3361 1 0.004745360250412759 13.71612579332542 10.892550401601177 51.570327345778836 0 0 0 1165 1 0.004734192295786838 8.970248451513672 9.239830515259186 50.0420554766267 0 0 0 1171 1 0.00464458854458033 12.070283638968036 12.41029757788138 49.946393442479355 0 0 0 1170 1 0.004799401228603992 8.87717270297657 12.497600089889945 49.983584332373155 0 0 0 1166 1 0.00474546799568896 12.121193127835955 9.275446378373829 49.94106896958605 0 0 0 2611 1 0.004676743825689901 13.736370795379333 7.698197481488691 48.40233674573377 0 0 0 429 1 0.004590645963313392 7.331143436477396 7.669439898712081 48.458185424397925 0 0 0 3331 1 0.004744327608209347 13.686485452091684 14.10587144224024 48.40288762494259 0 0 0 1142 1 0.004823416486244191 10.552323285230681 10.976843708457563 48.39372860096725 0 0 0 431 1 0.004758596055198773 10.590010032709175 7.683386624587766 48.45455342265134 0 0 0 1140 1 0.004632737340224747 7.442192881715027 10.865307084224913 48.42583799200593 0 0 0 3322 1 0.004810614648846474 13.720826409253155 10.914841667744021 48.452958122745976 0 0 0 1149 1 0.004915083973121985 7.3651318095030875 14.136318224445677 48.337861462840074 0 0 0 1151 1 0.004764825564382624 10.566166988314466 14.040627000432329 48.346281316273924 0 0 0 1141 1 0.004956909043199641 8.939083656972404 9.272361086363782 46.81022058368869 0 0 0 1143 1 0.004803227472746209 12.25229563500839 9.319356785346221 46.83860397620058 0 0 0 1150 1 0.004732657905153044 8.948938904627235 12.482663390592979 46.722652353316406 0 0 0 1152 1 0.004685689064838586 12.220979531840847 12.54365808167538 46.821538847435484 0 0 0 2584 1 0.004684108788733229 13.782207267679997 7.640486298909817 45.288985821804395 0 0 0 1115 1 0.0048495593707403965 10.700049540402148 10.87955713302808 45.23680490068213 0 0 0 3295 1 0.004860402976737229 13.736118386579985 10.822815965435565 45.130170564493916 0 0 0 402 1 0.0047008567002666465 7.4328587079335975 7.659399800131763 45.250446396486126 0 0 0 1122 1 0.0047910218072933705 7.391382013910417 14.039923867094183 45.192557570200904 0 0 0 1124 1 0.004642131866069784 10.540579808967044 14.033708031951399 45.172930618423514 0 0 0 1113 1 0.004651416170669902 7.4325515841342575 10.836034417839176 45.24706884035422 0 0 0 3304 1 0.004874930433217101 13.74654217970037 14.062081572192287 45.18668265351703 0 0 0 404 1 0.004813142622497811 10.665902068901097 7.6839954303376246 45.26151530105909 0 0 0 527 1 0.005024780118744932 5.747621604717156 2.8994426177824124 59.54547970415025 0 0 0 534 1 0.004850758539751686 2.539266372205394 6.096844029125879 59.54835121492007 0 0 0 536 1 0.004951679331874853 5.76321717525226 6.05585933548466 59.54709037090098 0 0 0 525 1 0.00495345490625804 2.6586136853858995 2.9414611013301073 59.599588046309904 0 0 0 488 1 0.004817207224866567 1.082148316341074 1.2515535992192965 57.9459757669689 0 0 0 490 1 0.004685708667204318 4.270222056972451 1.2699779851359083 58.0239220381002 0 0 0 499 1 0.004745019550655797 4.17763576405282 4.466481982363302 57.9800651672141 0 0 0 497 1 0.004815081008749025 0.9822816598219193 4.444632249342356 58.04613668330394 0 0 0 509 1 0.004640966626907559 5.819242961893036 6.020611872976939 56.3423815856483 0 0 0 500 1 0.0047694055442588455 5.857182015980228 2.827570578508803 56.29162043198812 0 0 0 498 1 0.004724644720237738 2.5847661264555946 2.937547018826097 56.27277699503725 0 0 0 507 1 0.0047341851148208595 2.5833302878330096 6.008069566928085 56.382904859512145 0 0 0 463 1 0.004890773105475459 4.199064937270383 1.324075661845428 54.845425592546775 0 0 0 461 1 0.004772542007172819 1.008912702186598 1.3114002602280193 54.74173086510893 0 0 0 472 1 0.004803067300301746 4.229526520729172 4.521098272808697 54.761469413482295 0 0 0 470 1 0.004644834248641507 1.0634979171684629 4.483076229862323 54.77765088159441 0 0 0 473 1 0.004948598102681407 5.835388949651439 2.8685122537864034 53.12355597497629 0 0 0 482 1 0.004760681751867748 5.769518352841716 6.1149351034239725 53.151218923288745 0 0 0 471 1 0.0048019432583218565 2.6950784397416414 2.989896493235037 53.17110500883224 0 0 0 480 1 0.004847260210616348 2.577942970745189 6.1917401475524265 53.11221070723541 0 0 0 529 1 0.005053653649211178 8.907366023102059 2.9276008419849284 59.571730454347744 0 0 0 531 1 0.0049356096312022125 12.15012796276513 2.918261823496527 59.52490515406566 0 0 0 540 1 0.0049868621216216415 12.088146863343548 6.1310668373993105 59.62236009448839 0 0 0 538 1 0.004915538007243866 8.954803740390508 5.987444949634479 59.497457157714415 0 0 0 494 1 0.0047866251240997314 10.598607323488267 1.200654553461591 57.95921224491111 0 0 0 492 1 0.004667711608175171 7.471851483879697 1.2287052803268166 57.91850713200816 0 0 0 503 1 0.004781496556324701 10.608717987223121 4.4593011281753405 57.91533901585451 0 0 0 2674 1 0.004819197362621383 13.763768918319132 1.233026825480922 58.06128923254761 0 0 0 501 1 0.004622230099217079 7.411654624287262 4.427226426962712 57.837615574701104 0 0 0 2683 1 0.004812572244037463 13.693138100610634 4.508756563840539 57.92167868089974 0 0 0 504 1 0.0047134547799301905 12.114137689999316 2.8362624644069503 56.300162466540506 0 0 0 502 1 0.004757458059646967 9.021361693075063 2.818808767104819 56.319896576769885 0 0 0 513 1 0.004711170164725793 12.059020086139729 6.0648308064790335 56.288757701403476 0 0 0 511 1 0.004566837145720844 8.931151422525195 6.01205626198738 56.32240800706016 0 0 0 2647 1 0.00487419112805604 13.706968022799273 1.2246465790717285 54.670682562215156 0 0 0 2656 1 0.004645839723363845 13.771915365532765 4.466343777491021 54.778339126348094 0 0 0 467 1 0.004664696215006311 10.57230517769693 1.2037710497428662 54.75558273203598 0 0 0 476 1 0.004682463351569601 10.708839779852765 4.436085718484175 54.72300431715253 0 0 0 474 1 0.004811538667506441 7.420662804135274 4.509342815050462 54.78452502014798 0 0 0 465 1 0.004892407922785407 7.427393582212285 1.2903440741347338 54.691172806981484 0 0 0 477 1 0.004776693018895882 12.15551072986836 2.8444744092756693 53.16149287780562 0 0 0 486 1 0.004847636816270205 12.26073671064088 6.076690794048867 53.21504668400147 0 0 0 475 1 0.004947364640304675 9.040040817235289 2.889766035319422 53.06748298173317 0 0 0 484 1 0.004877498945486558 9.02932427783253 5.993056807434475 53.09321896659049 0 0 0 1247 1 0.004918949482110182 5.714738411850206 9.217017783184543 59.52671757368774 0 0 0 1254 1 0.00500702324569925 2.4215811375025686 12.45861947953123 59.52911558242842 0 0 0 1256 1 0.004970616142111528 5.726680357221351 12.46186171699057 59.450650932392854 0 0 0 1245 1 0.004977292681062194 2.4570111131175985 9.332278075184407 59.52550691010724 0 0 0 508 1 0.004785839689892249 4.2374629452876125 7.517228615307979 57.91607377203384 0 0 0 1217 1 0.004808871308488385 0.9478663457681585 10.798514474904684 57.94510002183875 0 0 0 506 1 0.004696651183694516 1.0252199168621023 7.58030037548421 57.93244668957738 0 0 0 1226 1 0.00462972193250126 0.8799377042393812 14.139942774045375 57.91774183283457 0 0 0 1219 1 0.004882478612053069 4.2434557527228565 10.711321632725962 57.917764183401786 0 0 0 1228 1 0.004720433463465944 4.061020800985134 13.979593640700537 57.980547261035106 0 0 0 1229 1 0.004882279189243305 5.825801257083874 12.473656172561803 56.40455721214131 0 0 0 1227 1 0.005000720473606411 2.5968415023427918 12.476025653387616 56.30209346714889 0 0 0 1220 1 0.004847717775097363 5.840412453810085 9.264744266276596 56.25441691570192 0 0 0 1218 1 0.004863964175405969 2.5424614988755465 9.238580216453396 56.34771375036496 0 0 0 479 1 0.004750949318639506 1.0361913415048483 7.725595400496104 54.73193623161843 0 0 0 1190 1 0.004871026796905143 0.9149570778228266 10.869033446079673 54.79606384453631 0 0 0 481 1 0.004945477913685197 4.276219231415971 7.698753280748314 54.72281523887666 0 0 0 1201 1 0.004762002745189132 4.125826494779468 14.020948298911208 54.73801496324126 0 0 0 1192 1 0.0048826350694614745 4.126927738338788 10.764144192888017 54.70087557307886 0 0 0 1199 1 0.004685392450483716 0.828406794465975 14.10473983030963 54.77639310352047 0 0 0 1193 1 0.004707516637245437 5.802737063636825 9.27593811706376 53.131183239102846 0 0 0 1202 1 0.00472615649830877 5.694942787589363 12.463011272299923 53.120877176784056 0 0 0 1200 1 0.004646464889018501 2.4705633178229705 12.474741195147221 53.206970501211046 0 0 0 1191 1 0.004661391957732498 2.5010030519384427 9.331553204887173 53.108531711973434 0 0 0 1206 1 0.004830895108730847 12.036454886856815 12.47624227582609 53.15918540605704 0 0 0 1258 1 0.005015161919102172 8.965124165786285 12.418217271713566 59.535878565820504 0 0 0 1260 1 0.004816273352060224 12.213823249430572 12.42299825641225 59.51993479226907 0 0 0 1249 1 0.004838017908970933 8.900937745579213 9.25205739423054 59.53413897844251 0 0 0 1251 1 0.004948458992905842 12.10789737341736 9.295725715023163 59.55179093929791 0 0 0 512 1 0.004737009979140614 10.459186210414117 7.6901628075981305 57.93542022847429 0 0 0 1221 1 0.004648560448347782 7.377918431942513 10.850562076727831 58.0161349290769 0 0 0 1223 1 0.00473052312527774 10.537013395227708 10.861819675807608 57.92234208857181 0 0 0 2692 1 0.005092602652482011 13.670012470259012 7.6849029988009026 57.962423314091616 0 0 0 510 1 0.004758429754619976 7.404663813045162 7.596338649436133 57.95697180527559 0 0 0 1232 1 0.004903745337963726 10.53394864895893 13.976544410788012 57.895572025669594 0 0 0 3403 1 0.004829223611665006 13.708730725751174 10.833263062647783 57.93003102343196 0 0 0 3412 1 0.0047388621590362615 13.765495354463706 13.992486368821481 57.840351569026026 0 0 0 1230 1 0.004681996351398595 7.364967405944 14.089269723150718 57.945536538826474 0 0 0 1224 1 0.004637709139599183 12.135012134420913 9.267647980308011 56.33311636979409 0 0 0 1222 1 0.004581260463075264 9.017834934263437 9.279987568672126 56.39634698287347 0 0 0 1231 1 0.004686349674119799 8.916496152406323 12.406332008356479 56.31448126361664 0 0 0 1233 1 0.004681075575598149 12.103869686824883 12.43574751803776 56.28325961314496 0 0 0 485 1 0.0047416155151132 10.499570676913764 7.7008209990863365 54.82187119851029 0 0 0 1205 1 0.004687661565106855 10.47010605835498 14.089316783853173 54.756604673703166 0 0 0 1196 1 0.004625255183181746 10.476951458549278 10.893874473557213 54.74968190419992 0 0 0 483 1 0.004902047321344508 7.5042712503544475 7.643608658068278 54.70542192556575 0 0 0 1194 1 0.00488420912054194 7.335719722222799 10.908519476633746 54.78553521321378 0 0 0 2665 1 0.004670701162368351 13.741632189554547 7.76030650176165 54.74681048575623 0 0 0 3376 1 0.004590703876003809 13.711389763308318 10.808058195421792 54.78234772841899 0 0 0 1203 1 0.0048188696081691105 7.2703482850209 14.156389796116901 54.70492659772522 0 0 0 3385 1 0.004703329369763415 13.693278278456457 14.046440571527008 54.72719561597549 0 0 0 1195 1 0.004764986860767819 9.044733032699092 9.323905350985898 53.16874683863434 0 0 0 1204 1 0.004697776522504105 8.917051791949149 12.562077566177349 53.136287125226296 0 0 0 1197 1 0.0048078498967458125 12.117619552808751 9.256920454857312 53.19590693245288 0 0 0 608 1 0.00019149802110081035 5.820341775951133 2.9038891746098945 69.00910833757537 0 0 0 606 1 0.0011119924897305608 2.612329103514689 2.7935076102207534 69.07516105979111 0 0 0 617 1 0.0008466886243793104 5.722403568746931 6.025617366322532 69.06076512058524 0 0 0 615 1 0.0007471193931839863 2.5077893639187168 6.087575375844985 69.11575751007753 0 0 0 578 1 0.004621361139745745 0.9241323411842598 4.536278342379929 67.6016648209169 0 0 0 580 1 0.006073636602981597 4.13406043283529 4.568549798799932 67.50177207913747 0 0 0 569 1 0.005528616641871726 1.124346634131107 1.3855091920126048 67.53933991373691 0 0 0 571 1 0.006169935434598876 4.273048024457433 1.387429942615231 67.45082030832327 0 0 0 588 1 0.005565777611661044 2.6686164153296774 5.997132071947362 65.88223718005064 0 0 0 579 1 0.005251938543819017 2.590814551287702 2.9493005827540935 65.9704159609949 0 0 0 590 1 0.005368606441729262 5.780031771701698 6.125156346239864 65.89829547269409 0 0 0 581 1 0.005468291414203843 5.807431087829993 2.8458491346188177 65.8862113415125 0 0 0 544 1 0.004550719565545596 4.161067573889915 1.2730585356883457 64.28220176952931 0 0 0 553 1 0.00424865799245221 4.2341828840993045 4.409836254612111 64.37068744374204 0 0 0 551 1 0.004597745005213772 0.9187002843827596 4.449080890780995 64.37325424017301 0 0 0 542 1 0.0043878785691581195 0.9731048580886469 1.362988199835168 64.32728076008858 0 0 0 561 1 0.004593343567161548 2.6050586111608105 6.0957347285857315 62.72172217572201 0 0 0 554 1 0.0045107932883977665 5.814665560521135 2.914927824984573 62.74196467323959 0 0 0 563 1 0.004505644457331483 5.843819632322476 6.123578111904769 62.72649219861918 0 0 0 552 1 0.004466063289800185 2.608682665797801 2.9623914890061647 62.78245682948979 0 0 0 517 1 0.004879114232754032 4.1518436107261785 1.4307955923244724 61.1836237950478 0 0 0 515 1 0.004954611548012447 0.9603136728554637 1.3498251630517806 61.1591944363274 0 0 0 526 1 0.004882913497780111 4.200496111769423 4.5688071774100365 61.268101141620534 0 0 0 524 1 0.004683033087736394 0.9578897333379058 4.519687544147834 61.292233389810875 0 0 0 610 1 -0.0002464443294508574 8.933190467534505 2.8772413145098352 69.0495044039389 0 0 0 619 1 -0.0002198444951207537 8.913393182535525 6.1262132377231495 69.00494203897854 0 0 0 621 1 -7.189654699633202e-05 12.215860143450016 6.204277125919824 69.08081964159123 0 0 0 612 1 0.0007245877863455066 12.102085772345397 2.9354917998417487 69.0410056584546 0 0 0 582 1 0.006614270556842848 7.408129629588069 4.468437089013672 67.45925238964156 0 0 0 584 1 0.006157344162792188 10.585667923802275 4.505921988668787 67.54607956509903 0 0 0 2755 1 0.006000344403897004 13.652453394196275 1.3446051242932355 67.48029036672312 0 0 0 2764 1 0.00501010654664478 13.77794119634924 4.525861668575948 67.45059870898433 0 0 0 573 1 0.006443683466072473 7.498996103347237 1.2411435599182619 67.4087207707578 0 0 0 575 1 0.006567836478838823 10.554982946666334 1.3165252630609716 67.4112048671168 0 0 0 585 1 0.005660870167934873 12.028262905397106 2.970110914739112 65.89251611221454 0 0 0 592 1 0.005949506437881674 8.97480945974707 6.125140216719214 65.91523125245543 0 0 0 594 1 0.006372568642473913 12.139980035966415 6.1102762465780875 65.8122598855132 0 0 0 583 1 0.005583121817673056 8.932968906466204 2.917356759712998 65.76621022777303 0 0 0 557 1 0.004346868174044177 10.559787183586351 4.531256321416839 64.19092707307354 0 0 0 2728 1 0.004400052111710802 13.670493262345891 1.3694058708375216 64.24921156604964 0 0 0 555 1 0.004356202481050942 7.405679483546906 4.525806968154279 64.30039544079567 0 0 0 546 1 0.004364226322420964 7.395146690057852 1.2736165556114054 64.29185772418397 0 0 0 548 1 0.004394423219182854 10.660942424194442 1.2820049887989227 64.13461691759335 0 0 0 2737 1 0.0048104364162145745 13.790845900442546 4.470143031550155 64.182074592307 0 0 0 565 1 0.004287682742592133 8.949210779803396 6.101197559202703 62.67033014881971 0 0 0 558 1 0.004100706624605786 12.125727448031883 2.9019651925901626 62.61936235892713 0 0 0 556 1 0.004284445175922294 9.029540863464872 2.8893955041414583 62.71422484939903 0 0 0 567 1 0.004139604421428222 12.175110160675557 6.107784588594269 62.735868502584076 0 0 0 528 1 0.004878907491446623 7.43145317049666 4.440966918361288 61.14564779384113 0 0 0 2701 1 0.004827842378841438 13.729167322665653 1.3782247534452776 61.16498842358642 0 0 0 2710 1 0.00458231356186253 13.83987493644676 4.524117193285129 61.07982860488699 0 0 0 519 1 0.004820114145493852 7.402834555294719 1.2521101699408135 61.14653509297826 0 0 0 530 1 0.004717665634929471 10.67873156141771 4.505937826918347 61.15492792773691 0 0 0 521 1 0.004918367176220408 10.6005940984508 1.3141124298009752 61.06234508283437 0 0 0 1328 1 0.001223902389298117 5.7540051888867385 9.248003227195706 69.09157880762177 0 0 0 1337 1 0.0019785239157094955 5.671853162823805 12.434851484405904 69.15367243389524 0 0 0 1335 1 0.0024288373266347692 2.4463936750681063 12.441560410599502 69.05624400488249 0 0 0 1326 1 0.00103220672854884 2.496084282921534 9.241544365856196 69.10989777571194 0 0 0 589 1 0.006607106609180966 4.17694851370279 7.690053281785635 67.42335941198229 0 0 0 587 1 0.0053140025192741965 0.985155378930139 7.725280891665161 67.45150339455466 0 0 0 1300 1 0.007542896401303649 4.176692516102604 10.862102142501563 67.49701958304595 0 0 0 1309 1 0.0076895156368097135 4.028412957223481 14.038833962776415 67.4416344361044 0 0 0 1307 1 0.007372245276120109 0.931463162515285 13.958313210484862 67.41250188154515 0 0 0 1298 1 0.006119738501622309 0.9561772278137044 10.858010804970167 67.47122836135101 0 0 0 1299 1 0.005574503685231557 2.568621846070362 9.257237416221974 65.86993270843122 0 0 0 1310 1 0.005472713989473042 5.864725963583831 12.387309466732606 65.9380986630592 0 0 0 1301 1 0.005597092029605266 5.786505583201251 9.351988165658232 65.92047875023542 0 0 0 1308 1 0.0052270659012681134 2.554184956569561 12.393863081719383 65.82213871505908 0 0 0 560 1 0.004663797988624463 1.0510928798430306 7.702168046630489 64.25621300776827 0 0 0 1282 1 0.004067039512666444 4.227517134103036 14.097461251776513 64.35848413174725 0 0 0 1273 1 0.0040707344159401915 4.17446416765257 10.80927095638285 64.19542449443237 0 0 0 562 1 0.004315839227244812 4.257053593886644 7.648218503115906 64.27345687713758 0 0 0 1280 1 0.003950370656108775 1.0230702751123624 14.039418167639603 64.31764263780241 0 0 0 1271 1 0.004251130182113974 0.9986952576402222 10.81302241250901 64.34879573804659 0 0 0 1283 1 0.004424750916662381 5.742129591979719 12.439583688687815 62.69205002044974 0 0 0 1274 1 0.004348782406183501 5.630637463395327 9.335095835786056 62.64848221684362 0 0 0 1281 1 0.0044310825543731995 2.4994094926042747 12.352529455106806 62.600714977126344 0 0 0 1272 1 0.004312603170778157 2.4485767520976234 9.309257952424815 62.70971526400152 0 0 0 1255 1 0.005147666400994335 4.098384351834857 13.955795740238898 61.1735976103231 0 0 0 1246 1 0.004882379294552859 4.138840708457234 10.901190410114854 61.13427063642932 0 0 0 1244 1 0.004824922429154763 0.7996239287467214 10.884289622501207 61.15628072601956 0 0 0 535 1 0.005011703109478247 4.060913401660271 7.779663791843906 61.08040404391891 0 0 0 1253 1 0.005056168616850631 0.8892162468004723 14.013371187498532 61.13892533491914 0 0 0 2719 1 0.004557670461476029 13.72871485704076 7.697627132419323 61.18062236172787 0 0 0 1330 1 -0.0002062153679822723 8.968304052487207 9.208268214685043 69.07296156627147 0 0 0 1341 1 0.0034964943518407364 12.149173308945604 12.476983171083303 69.06574668424219 0 0 0 1332 1 0.0009093735558553459 12.190604030372228 9.394680379264212 69.01477366352124 0 0 0 1339 1 0.0022941776072241734 8.9654958484689 12.4051088141445 69.10272003810451 0 0 0 593 1 0.0043255734903974545 10.525622571459767 7.6773463676131515 67.48512873278739 0 0 0 1304 1 0.0031603190069838197 10.626388067114696 10.988270828399072 67.45087236923139 0 0 0 3484 1 0.0019159015690266012 13.783001429669103 10.989900588977031 67.4302915248539 0 0 0 591 1 0.006147955134257716 7.309003561030959 7.674708476356093 67.49291782529107 0 0 0 2773 1 0.002964435948070719 13.752658441954566 7.671138771616211 67.47848985840272 0 0 0 1313 1 0.0037448546500257994 10.488657887068765 14.139194926817126 67.42385557003558 0 0 0 3493 1 0.002210346435979225 13.715595587892278 14.143845131288579 67.44118014115672 0 0 0 1302 1 0.005142381881116554 7.396615133403393 10.91271240756965 67.48510226894376 0 0 0 1311 1 0.004926061730566377 7.247122349750303 14.008282361769114 67.5278414578852 0 0 0 1312 1 0.005705354459248626 8.886020444409581 12.48904097196026 65.9086883859822 0 0 0 1305 1 0.0066294492698768335 12.147877891247397 9.418617983934839 65.8478282902486 0 0 0 1303 1 0.006377293307659118 9.026237556817282 9.345208116279114 65.91197466292304 0 0 0 1314 1 0.00584397252135305 12.195292711341533 12.610297014992371 65.8519672701579 0 0 0 564 1 0.004528944884925751 7.439689242252631 7.795507806970162 64.25297568003931 0 0 0 566 1 0.004762383026665795 10.527995390673139 7.648507873412939 64.24783925548013 0 0 0 1286 1 0.005005497563693758 10.5184307894592 14.083401517301155 64.3574737127702 0 0 0 1275 1 0.004392491531368812 7.325700562390426 10.89983264068092 64.30603438376069 0 0 0 1277 1 0.005140009784793481 10.608729010669142 10.922846360616843 64.25265508220988 0 0 0 2746 1 0.00523048143024976 13.688218135372061 7.7538483574236485 64.32955109824303 0 0 0 3457 1 0.005363815445884582 13.762854830850001 10.937562458045901 64.29853828836609 0 0 0 1284 1 0.004340981848084435 7.342823150827434 14.005596374276534 64.33781365737339 0 0 0 3466 1 0.005238829540835582 13.776168031421923 14.122427935022504 64.28274015069202 0 0 0 1278 1 0.004239965423870609 12.181156009755465 9.283601699448818 62.664353377291754 0 0 0 1276 1 0.00443902799640203 9.030225475467896 9.297754832226811 62.65053021582333 0 0 0 1285 1 0.004508750351565919 8.949416884058563 12.525638614560062 62.732690872295414 0 0 0 1287 1 0.004369435207078481 12.106897198950502 12.528346841482334 62.67090695926808 0 0 0 537 1 0.004902792135104727 7.306988428046921 7.582904868546433 61.13474845786048 0 0 0 3430 1 0.004434173081483155 13.737647701208864 10.95068943980162 61.18861496879544 0 0 0 1257 1 0.0049574217336783525 7.376884570406467 14.018216370862856 61.15371137607049 0 0 0 1357 1 0.009134506169680506 8.86104906855717 9.336237919526049 72.21472156008886 0 0 0 1250 1 0.004579394490464418 10.5913327683355 10.85500572174157 61.138182882125435 0 0 0 1248 1 0.005015452443677933 7.320696071791588 10.785500180794347 61.15050188042216 0 0 0 1259 1 0.004794449089888303 10.566566321703442 14.078452100914285 61.104359113094795 0 0 0 539 1 0.004650488012268061 10.485025134124905 7.702929981631447 61.05898364805391 0 0 0 665 1 -0.06889820289242919 4.0625985702305565 1.2791272475097377 77.024442151948 0 0 0 669 1 -0.0704906738532649 4.168364248764435 4.527551014660208 77.03889776734243 0 0 0 668 1 -0.03193816768663588 0.9112569975645474 4.266500893097721 77.02472743480276 0 0 0 664 1 -0.04431231803949641 0.9900461640629988 1.1643681601550406 77.10507698835477 0 0 0 655 1 -0.0023561251748880924 2.620344036861468 2.8826852198683244 75.43694062142283 0 0 0 660 1 0.001520957664398425 2.460375436047838 6.043198124119724 75.47222892263578 0 0 0 661 1 0.0015324069398045086 5.688781005386052 6.16167001392987 75.4361440880857 0 0 0 656 1 0.008244072074220753 5.704405893863168 2.84346727933762 75.48239482941494 0 0 0 623 1 0.012916774800309151 0.9357667938894436 1.264737442022057 73.8927479044474 0 0 0 634 1 0.009158265776678335 4.204492776119101 4.504970842039883 73.91855653336935 0 0 0 625 1 0.008151022616847943 4.134796592622532 1.1497408077640139 73.90283936459332 0 0 0 632 1 0.004938969787584478 0.8431943393273894 4.362130047644597 73.86925547476929 0 0 0 633 1 0.002568126966958793 2.628789217428403 2.8344323126124324 72.27944574534722 0 0 0 644 1 0.005108046784493683 5.722411635088817 6.102727420061649 72.24409985576628 0 0 0 635 1 0.009341916735341514 5.718392305045875 2.8082466001854454 72.32380529878088 0 0 0 642 1 0.005466570255861437 2.5667533657105355 5.922996611726019 72.31518620145128 0 0 0 605 1 0.009762030515864396 0.9903584973668825 4.4797506525542214 70.67314215314825 0 0 0 598 1 0.006475782066925078 4.204428427897866 1.2085166458163128 70.59290386867399 0 0 0 607 1 0.008194283016616635 4.0773835073755995 4.402203259654703 70.61987084019884 0 0 0 596 1 0.006542034900415715 1.043078911026197 1.252029632428298 70.72234606652407 0 0 0 670 1 -0.0408207138399498 7.2676569447254 4.471959471337168 77.01738248112039 0 0 0 2848 1 0.06350928316650935 13.757622672138426 1.2377125978103543 77.01702104050304 0 0 0 666 1 -0.08044604638133317 7.3125442247487 1.2693693627414835 77.16742235947035 0 0 0 667 1 -0.07511683852820733 10.506307507062724 1.2583247932620407 76.97063980302292 0 0 0 671 1 -0.08968663287712003 10.56016289673952 4.488034490105065 77.05884816357978 0 0 0 2853 1 0.08901012468132749 13.70769130462639 4.485310773944283 76.83476890439103 0 0 0 662 1 -0.0064638639848293294 8.89294109336898 5.989147621891047 75.52819968984396 0 0 0 658 1 0.005048663016231953 12.058621106682498 2.879495823438073 75.42086383808312 0 0 0 663 1 -0.018491077245030046 12.124697179485054 6.076512983146287 75.49950737774864 0 0 0 657 1 0.010629502121345714 8.972055622814105 2.874691983466231 75.48659030063982 0 0 0 627 1 0.00705087306753978 7.276189639876039 1.2391446162465285 73.92994978261761 0 0 0 636 1 0.005902333984091755 7.319419723340655 4.424581558898821 73.88587293297921 0 0 0 2809 1 -0.0021747399522110463 13.69343532181483 1.3833423672711416 73.82472209255832 0 0 0 2818 1 -0.0064481732194544405 13.67233081038559 4.393124644780769 73.82999589957087 0 0 0 638 1 0.009949471498263657 10.587559634509537 4.559652132868167 73.79867689126644 0 0 0 629 1 0.006284517943908888 10.502562647904984 1.2779664879705235 73.75557818712478 0 0 0 646 1 0.007535358617437421 8.929262399340086 6.158508865578323 72.27969650229369 0 0 0 637 1 0.013325792333894852 8.907187307957523 2.9455125512158182 72.30064361941922 0 0 0 648 1 0.005029372868488591 12.191798591591304 6.105723756863944 72.1873728178765 0 0 0 639 1 0.00802985090321557 12.106102080115692 2.9897596617526996 72.19612748025158 0 0 0 609 1 0.006597028349952606 7.369136131288749 4.432830686730842 70.69608952456782 0 0 0 2782 1 0.007616332622762862 13.749443444629494 1.3575368408757504 70.60822036124819 0 0 0 600 1 0.004750603703844643 7.295834847563497 1.2736334651732573 70.65506879748212 0 0 0 602 1 0.003296598715974614 10.493728035087676 1.3312740580640905 70.6124620240881 0 0 0 611 1 0.006555415832461931 10.505850686847579 4.5249913800293635 70.68305295818055 0 0 0 2791 1 0.009832144056037575 13.845118406203925 4.536067582864646 70.61602407884494 0 0 0 672 1 -0.0903023567432734 1.0425617478802989 7.597381211784925 77.2213668148981 0 0 0 1398 1 -0.030591302107255074 4.19133872811436 14.028994937668644 77.18469956271655 0 0 0 1394 1 -0.042707416786212586 4.073539634205842 10.948079057027941 77.13744408519159 0 0 0 673 1 -0.05039562595417991 4.165158813823158 7.613384946808438 77.04762354865579 0 0 0 1397 1 -0.029711947410639473 0.8992602669234859 13.959952966219092 77.064806489938 0 0 0 1393 1 -0.04365108244007036 0.9387574737641103 10.788770808851217 77.11262471263868 0 0 0 1384 1 0.012382941703062695 2.548161587861065 12.445882239291855 75.52590143705307 0 0 0 1385 1 -0.0017032133507273312 5.720953069537877 12.346299701989231 75.54763670643894 0 0 0 1380 1 -0.013957486375752032 5.688836653114814 9.302842642518712 75.515951174092 0 0 0 1379 1 0.005754601157354593 2.5158743979789935 9.257162726349172 75.53939969103398 0 0 0 1352 1 0.013033066861148676 0.9389676973482807 10.92594292771375 73.88570865710423 0 0 0 1361 1 0.01677360627854727 0.8488880861425813 14.089733646367534 73.84611661340888 0 0 0 641 1 0.011899504036778596 0.8624123924251639 7.671096732081671 73.8857848610024 0 0 0 1363 1 0.009772781160948617 4.052077451715548 13.998165660049187 73.91089294205707 0 0 0 643 1 0.009593806818968138 4.13167308568066 7.6679754331074 73.86356145682966 0 0 0 1354 1 0.015709069371930645 4.166149665467363 10.812966764956903 73.85287105435296 0 0 0 1353 1 0.012892434350996247 2.510682826276779 9.233952140803055 72.34248642818048 0 0 0 1364 1 0.009461312762082438 5.78136166770172 12.44167807920347 72.27547137449783 0 0 0 1355 1 0.008187404207886752 5.851398909666399 9.293670634445194 72.31891679580689 0 0 0 1362 1 0.014189189821548338 2.440309618060788 12.437289174900794 72.238876829781 0 0 0 614 1 0.0061786363791056075 1.0067192011812585 7.6759054196144785 70.72457512316834 0 0 0 616 1 0.005780203856395522 4.1501849744470025 7.739207198720949 70.71712200363102 0 0 0 1327 1 -0.0015144373504960389 4.052032717505847 10.903729005048252 70.7116517118238 0 0 0 1334 1 -0.002274668003245047 0.888372338236726 14.020237020748143 70.68106690147646 0 0 0 1325 1 0.0013628951149137064 0.9672227878489997 10.862074119885207 70.7850763965879 0 0 0 1336 1 -0.0014584523412428559 4.0919941905692 14.088501185514243 70.68989591708531 0 0 0 1365 1 0.01795311513982074 7.341862616949899 14.04721568045763 73.86703976051939 0 0 0 1359 1 0.013792103153057352 12.177530649571457 9.330966805159223 72.34686496037659 0 0 0 1340 1 0.0079243910443392 10.429332118990187 14.065296799633561 70.71219829486603 0 0 0 3511 1 0.005560113673515034 13.752887442556197 10.893946849191286 70.67085689914666 0 0 0 1368 1 0.01634193790566523 12.13324844909936 12.455353506643283 72.29546847778613 0 0 0 1329 1 0.006117634468149929 7.320388904512275 10.853388872652133 70.61950501675277 0 0 0 620 1 0.011601283001738717 10.578111748181447 7.714024072168468 70.66661833070269 0 0 0 618 1 0.00721628324164858 7.330846512240947 7.630176671078866 70.67665678348807 0 0 0 1331 1 0.007909485146783093 10.548326086228563 10.843643990732575 70.62166495532442 0 0 0 3520 1 0.004705202395198907 13.624431928744041 14.029786278490711 70.67207901219375 0 0 0 2800 1 0.010465349131086685 13.825208877363805 7.764435642815597 70.61837959191638 0 0 0 3582 1 0.5258193587603335 13.670840135824317 13.960817518368819 77.21259531867786 0 0 0 2858 1 -0.02070246360950334 13.75254513930789 7.618276082167914 77.10168432159321 0 0 0 1395 1 0.01942813976121985 7.410069763755407 10.794510021234519 77.13974396652446 0 0 0 1396 1 0.006506396748710784 10.456977206403446 10.901099126989058 76.9785237170645 0 0 0 3577 1 0.15726971803472367 13.680326867126194 10.710919823848155 77.13619224544381 0 0 0 1400 1 0.09380320597890673 10.456300024247483 13.94365277687585 77.24934274467628 0 0 0 674 1 -0.027215902371324936 7.3829557711505895 7.650254820700741 77.03941710196851 0 0 0 675 1 -0.059955579037783584 10.39262381073836 7.692957114892775 76.93708746347431 0 0 0 1399 1 -0.04080813154627902 7.349017964217245 14.066682307548557 77.08680962530755 0 0 0 1386 1 -0.04146361819403578 8.893804079335334 12.416647050376886 75.54092912010866 0 0 0 1381 1 -0.03171332866395005 8.8589776399806 9.251013147952959 75.51862458084429 0 0 0 1387 1 -0.053726472211762646 12.089175672316564 12.568841524738144 75.42016547458373 0 0 0 1382 1 -0.04740638184597612 12.066212690330536 9.222931287301234 75.46062003517753 0 0 0 1356 1 0.00952288296899972 7.402859239788787 10.92758926947211 73.89405017930707 0 0 0 1367 1 -0.005637796014906054 10.449426269381473 13.939393885166261 73.79981624288165 0 0 0 647 1 0.01084003207520113 10.493138345387518 7.651021621874226 73.92364196655001 0 0 0 645 1 0.00966370375773218 7.407292737407884 7.725290783575541 73.95771165306348 0 0 0 3547 1 -0.026090635429018585 13.677464151990899 14.089517090476642 73.88483780108324 0 0 0 2827 1 0.0013396528084763052 13.640705607075937 7.711742788284612 73.86847010825785 0 0 0 1358 1 0.012319441066385071 10.487777303094832 10.819178259794104 73.91564748402932 0 0 0 3538 1 0.001993509194544203 13.598495290105207 10.960222047535076 73.88030609365839 0 0 0 1338 1 0.00582457924531056 7.299668706639881 14.03542714233469 70.69965978090576 0 0 0 1366 1 0.008273711395761421 8.947199799570042 12.31515635839735 72.2631445565123 0 0 0 533 1 0.0047049997443771065 0.8965738088502527 7.677368197004753 61.03684199684901 0 0 0 3439 1 0.004583432613872234 13.718626199029298 14.070897446765386 61.05923853419253 0 0 0 723 1 1.613575025531377 4.057819173084876 6.677160775108033 85.28339338397564 0 0 0 4919 2 -0.657269994866267 2.8121218720221552 3.5476416601863523 85.63119952983855 0 0 0 707 1 1.624788800482289 6.246359931755281 0.1514164778503355 84.90917037852202 0 0 0 716 1 1.4797968264662185 6.074663027618755 3.8904543987325115 84.84175905932769 0 0 0 4595 2 -0.8206049691951409 4.70485084246236 5.118143571132641 84.24020932357547 0 0 0 705 1 1.2241768883964323 2.769112779808653 0.26995721567908826 83.8103296970693 0 0 0 714 1 1.4367852903761926 2.2835719991225143 3.2018358800232405 83.99305272554997 0 0 0 5004 2 -0.9304028813949422 1.0067691440244584 1.6367723602568434 83.6788463011626 0 0 0 4497 2 -0.8115202093107021 0.576952862843435 4.313073426713121 83.10278139382922 0 0 0 5128 2 -0.8124694755076175 3.5896818740285092 2.277947532055967 83.24155605579294 0 0 0 4779 2 -0.7182265704931386 6.69026608945663 3.9127006845234185 82.72013016191772 0 0 0 4383 2 -0.7424195689802312 2.9537125604451067 4.645489738254264 82.54069761224092 0 0 0 688 1 1.4714012113857868 4.740996024067391 4.66040134628933 82.09775444039555 0 0 0 686 1 1.2589943476630767 1.232900233436523 5.133155088748725 81.39823100749625 0 0 0 679 1 1.2672809729649634 4.257617199184332 1.368355837491018 81.50133222355318 0 0 0 677 1 1.332216466794342 0.969170973486968 1.3316939003637036 81.47733500496217 0 0 0 4822 2 -0.7594337256144593 4.940547334314919 3.2033773245677506 80.9907604810104 0 0 0 4430 2 -0.8033653675080964 5.147338662042534 5.97958025669429 81.0540865240246 0 0 0 4683 2 -0.8162456846442676 2.716278910378645 6.4925813616252555 80.83721568479002 0 0 0 4423 2 -0.7162910823750928 1.2872748546889867 4.048742528041062 79.9999992771032 0 0 0 4396 2 -0.7885351908559014 2.8141208141379095 1.4675404919823067 80.46437090955432 0 0 0 689 1 0.13529076166516513 5.757174943324506 2.9998947896408477 78.80705041759752 0 0 0 698 1 0.33850974828387265 5.681329776776247 6.124507192162235 78.9205792016376 0 0 0 696 1 0.2256117373214484 2.5936315349857013 5.936555256568891 78.66593007757791 0 0 0 687 1 0.4132744342514464 2.71362267166399 2.872210318485389 78.74255563532765 0 0 0 4568 2 -0.6919813890407932 5.986147905277019 2.198437723056355 84.38341359546853 0 0 0 4451 2 -0.6963340491027769 13.818008950482009 14.18875282156861 82.23479715037311 0 0 0 4649 2 -0.6694760242797099 8.9146163773579 1.458903169490405 85.27276439155774 0 0 0 4828 2 -0.6326001136854454 7.595738682132295 4.746640848560237 84.85014951021364 0 0 0 4525 2 -0.6605520183609983 12.493670563653424 4.837947160405858 84.9402193338404 0 0 0 727 1 1.7286852938331332 9.205338699121086 6.168945320671523 84.21115403065198 0 0 0 4725 2 -0.707389787660819 10.716230767983376 2.4522814029894398 83.19876088395618 0 0 0 4520 2 -0.6116777991574726 13.516923850571184 2.266718187548104 83.99421923031984 0 0 0 718 1 1.6112052681870637 9.203269054257625 0.9743051825439863 83.57629903827291 0 0 0 4476 2 -0.8047113579715638 9.306750639103775 4.862574323068733 83.02838368260363 0 0 0 692 1 1.4727940884545512 10.965748932506445 3.858945811308341 82.1432909149771 0 0 0 2863 1 1.6718611551791784 13.582585676509389 1.97986890619152 82.2463821045284 0 0 0 4770 2 -0.7304438872594159 13.10143738936824 4.146372213680078 82.42275038771025 0 0 0 4901 2 -0.7911389574340659 8.589903708138007 1.862306096234097 82.11835995403243 0 0 0 4627 2 -0.7387689153495758 11.552495767600997 5.881932042238534 81.8560030877872 0 0 0 2872 1 1.6968886149029672 13.774216034266265 5.770547442321757 82.21870812072719 0 0 0 690 1 1.2194201524713812 8.100362139772747 3.8587020483292536 81.65266611237216 0 0 0 4438 2 -0.7891249618895356 10.46457810375727 3.5548534848475626 80.48178176607898 0 0 0 4461 2 -0.7480637477047263 12.307967835346341 2.0767521687379378 81.02819288943255 0 0 0 683 1 0.6527562554994638 10.43163964055093 1.2365290818052455 80.67226109025836 0 0 0 681 1 0.44450585920759494 7.286980593902233 1.277957221545396 80.49046995027885 0 0 0 4697 2 -0.6746435302796504 13.558571117939048 5.9491607355195475 80.46173043733296 0 0 0 4700 2 -0.7929775268770951 7.776500509263825 5.068751469144924 80.38492408860037 0 0 0 693 1 0.5090574680781159 11.865593940625425 3.0026037168394364 78.82657924580548 0 0 0 700 1 0.4749290258485105 8.8925982780168 6.199040839102663 78.88286836053555 0 0 0 691 1 0.05122301689214331 8.88491924934299 2.954236506591234 78.7614499511384 0 0 0 702 1 0.4679609862082728 12.134291191419342 6.086115135562474 78.7535099925314 0 0 0 4534 2 -0.7115301767405875 13.94915757430121 3.0632724284966923 78.53444414950137 0 0 0 4666 2 -0.7396397638428339 7.29599583625252 0.11152425634890915 83.51819724299844 0 1 0 711 1 1.6471707746672493 12.533174793806088 3.179243870362342 85.70084261768321 0 0 0 4709 2 -0.6910770462861484 13.068402009819014 0.1691365905289255 83.22577647152092 0 0 0 729 1 1.5657905389111322 12.64436537774477 6.867012429391173 85.54650409472721 0 0 0 4762 2 -0.8020781945669769 13.393654188261685 6.952804833857044 83.5221533574913 0 0 0 4855 2 -0.704464864578872 10.812342942578908 6.814306859772786 84.32350996704373 0 0 0 684 1 0.1464631810842236 12.083331627694765 -0.06279314101180473 78.59701152508434 0 1 0 4495 2 -0.6767026430891762 5.349411544126235 7.79008400309191 85.15078543933353 0 0 0 4618 2 -0.7486009870626331 2.896682591484395 11.881563616319216 85.37112851683499 0 0 0 4566 2 -0.6557235394066415 1.9856718716874109 7.170271420534858 84.98920324331705 0 0 0 5059 2 -0.645727129594687 5.403491095758932 13.47669652902229 84.60502144861677 0 0 0 4598 2 -0.6526207526283644 4.982556389819351 10.231682264939343 84.24425807933767 0 0 0 4576 2 -0.6759133850790076 1.5721391606424793 10.159934050455846 84.64301195593627 0 0 0 1436 1 1.748531482397723 6.6963196189062035 8.921095289794224 83.85100931544974 0 0 0 1434 1 1.5034439365765584 4.2456606541564925 11.808268888171286 84.19840232104238 0 0 0 1432 1 1.620934685646319 1.25090479095621 8.52711435618026 84.17496374992558 0 0 0 1441 1 1.6230308246927643 1.2911658330629474 12.221033318794094 83.83381317782127 0 0 0 4658 2 -0.6589348214473691 3.4304556516673554 7.758825798713216 83.49992903852421 0 0 0 4548 2 -0.6857577288842637 3.435087413154365 11.600630657469432 82.6236625623046 0 0 0 4825 2 -0.7013588417014854 5.895448088021506 7.878054160014586 81.99633601080059 0 0 0 4429 2 -0.7185125208741588 1.880467959233636 13.545166395394407 82.77603755765826 0 0 0 4453 2 -0.712744860235186 0.5245131625291624 11.335205401156133 82.5093666323241 0 0 0 4846 2 -0.7077270349233531 1.8006643866753547 8.42329356068054 82.477645770189 0 0 0 697 1 1.576772054927552 3.8021765602734265 7.586937264738782 81.75987008932499 0 0 0 4464 2 -0.6899151106804365 5.827415884227288 12.800075054590064 81.36697268861312 0 0 0 4556 2 -0.7254029740836752 4.246077025184874 8.953452345170707 80.64814043492389 0 0 0 1408 1 0.5261603635447096 4.06672271110495 11.106325026213119 80.67829559643269 0 0 0 695 1 0.5202994799209143 0.9643728974400768 7.973071370217297 80.56021654035571 0 0 0 1406 1 0.19761616844240606 1.2349984097834223 10.9401407373049 80.38756551285849 0 0 0 1409 1 0.4822159477654589 5.787782666892962 9.248374092767458 78.91813930700842 0 0 0 1407 1 0.010530404158030231 2.5837908632004716 9.280776863625155 78.74226926344856 0 0 0 1418 1 0.07981260171898666 5.768967355187824 12.427838337010686 78.73791360899281 0 0 0 1416 1 -0.16217870285197292 2.646859201572339 12.570218510243398 78.72339696399831 0 0 0 1415 1 0.6278593204337891 1.3635694055152863 13.98442268972523 80.73191624537363 0 0 0 1417 1 0.40502194986671664 4.212795000918168 13.863588268093393 80.46318020564624 0 0 0 4552 2 -0.6368311074480061 0.143091687935597 13.023342936938453 84.88932685760814 0 0 0 4917 2 -0.6823699415564386 6.958153163127373 9.796511169187722 82.33159064631042 0 0 0 1410 1 1.1951216753734957 7.061232065802021 11.53347229720307 81.1464757449918 0 0 0 4439 2 -0.7254562669789789 9.150881443582202 7.187683660101053 82.03960666753687 0 0 0 699 1 1.4529144946366523 7.2432412951951255 7.06623851824649 81.24080758395426 0 0 0 4482 2 -0.7933179331533287 7.311523084054984 10.777861308146282 79.52875654509832 0 0 0 3592 1 1.6289225047174447 11.418956510580083 11.723241686376763 85.50838717253168 0 0 0 4953 2 -0.826739058974852 10.220225506047758 13.040463374203274 85.52374511838966 0 0 0 4724 2 -0.6204647886030822 12.464321592645002 9.913102924116385 85.07977356293924 0 0 0 4907 2 -0.7837146823323553 12.921171016685655 12.57598840897595 84.30911241447393 0 0 0 4558 2 -0.7844390542714499 7.748322088005069 13.780781077198684 83.84577283341919 0 0 0 4764 2 -0.7279796957094123 7.6256896767876565 7.395808403871968 83.59353807502926 0 0 0 4531 2 -0.6656859780455765 10.660249427681912 10.744704367230277 83.76837626939587 0 0 0 2881 1 1.5355143382409873 13.082312717538647 9.077024478756838 83.66801894596405 0 0 0 3601 1 1.61367185056053 13.906563031016455 12.53076530212479 82.83054544107648 0 0 0 4391 2 -0.7717244020712631 11.808585716925423 9.041070495448622 82.43666334678947 0 0 0 1412 1 1.529126094198063 10.34885947369987 10.9026556922465 82.03775725766496 0 0 0 4593 2 -0.8237513691152769 9.047369031593087 12.053183881318242 81.87145654759316 0 0 0 4609 2 -0.738301445770266 12.246135231643228 11.96498109177798 81.74440088141014 0 0 0 701 1 1.5783479392806061 10.81740435014185 7.49175728006924 81.46553976553348 0 0 0 4719 2 -0.702442505050732 9.78283981732241 9.462523709510585 81.10745883426853 0 0 0 4747 2 -0.801955774149843 7.4169144389452555 7.895607033651841 79.66972454515653 0 0 0 4614 2 -0.7974713017459174 10.563180593270697 7.365290393980019 79.71467395120395 0 0 0 4524 2 -0.8191351425247244 10.777520069712512 10.922210479089712 79.40421880110661 0 0 0 1422 1 1.2016454222752984 11.71402414433427 12.321579389556726 79.88763146233794 0 0 0 4484 2 -0.7075854709121414 13.363043546483784 8.180436452225857 79.59101444955273 0 0 0 1411 1 0.7936262610345974 8.87075029558208 9.321660593189483 79.2082058086853 0 0 0 1413 1 0.5695532975629298 11.747457717245963 9.183472984381147 78.71604811099775 0 0 0 4519 2 -0.8119826644786191 13.56831003152252 12.531349247416015 78.8854607140147 0 0 0 1420 1 0.4263234054084761 8.903912529806055 12.499803971296394 78.92436383880198 0 0 0 1443 1 1.6157772662209937 8.191058222209906 13.370900646390478 85.47082958278338 0 0 0 1419 1 1.6636161731253545 8.714060711164704 14.123660174931311 82.07159112133323 0 0 0 4648 2 -0.6809421156279143 7.7722758642935155 9.68129584379889 84.96404235394981 0 0 0 5063 2 -0.7343203019430631 14.229540984091809 8.360235762865074 85.442793488184 0 0 0 4416 2 -0.7602661477875451 10.969494720054803 14.001473591884789 79.63489772603631 0 0 0 4479 2 -0.6815747391975969 10.310953019922012 13.857591545979865 82.67433661235826 0 0 0 4753 2 -0.561103935757327 4.512190540786272 0.07474588424107198 90.98984726725539 0 1 0 4443 2 -0.6772949542091395 10.516230520008417 -0.013808341256875243 87.36762520265745 0 1 0 4854 2 -0.6312048683161342 1.3030559954054124 3.616612109996915 93.7552245823906 0 0 0 4852 2 -0.7393825855865979 2.7863206287835567 1.1840086540101735 85.68392037001698 0 0 0 5017 2 -0.5865238986054901 5.857437124255942 3.321132038756049 92.98657121457894 0 0 0 5070 2 -0.586803449207416 3.7375805232666623 4.8889216565317595 93.15293529952524 0 0 0 5 1 1.7052046829132617 5.0391267178852654 1.2808935845809382 92.92918467511998 0 0 0 21 1 1.6736821826714317 2.345428504871131 4.074756031964754 92.42606811461889 0 0 0 4921 2 -0.5889807087861402 3.4224063537872693 2.3758496902891246 92.30476097275289 0 0 0 4417 2 -0.6135870230244836 6.522725324876208 0.8574510896008787 92.08894752655134 0 0 0 4973 2 -0.6140335520453054 0.7874437065054305 5.307253340277727 91.51064366699423 0 0 0 5273 2 -0.6037005574618418 1.3736061566845565 2.586476907581247 91.03326924675342 0 0 0 4420 2 -0.6315799973723887 3.219972087311418 4.78620925049618 90.51539533938134 0 0 0 5477 2 -0.48854234864675383 6.314789817448972 2.9301751152801248 89.8395307571017 0 0 0 12 1 1.7829443422993103 1.4333715679280061 1.4509225123339398 89.64780283859433 0 0 0 725 1 1.7765232152909096 3.548872189417572 5.920265298906792 89.16539789765699 0 0 0 5030 2 -0.6511669426210711 3.106532442491455 2.1514925842761894 88.49479628474079 0 0 0 5302 2 -0.6765118160239503 0.4257431016382278 2.875910326419604 88.23652634159946 0 0 0 4868 2 -0.6528019382283597 5.009615200194341 5.197648513679398 88.41183069264503 0 0 0 5376 2 -0.6098521622746188 1.7944228092264964 5.112184456317763 88.08184503004216 0 0 0 4756 2 -0.5979848197262411 3.5559746599391198 6.5219426753837 86.91214673964262 0 0 0 706 1 1.6426405803584865 3.842287866488889 2.0199043333818874 86.86847095105718 0 0 0 5352 2 -0.7676579125602307 5.5576326057026995 3.221510435743057 86.83540721460365 0 0 0 5339 2 -0.647654659748177 5.022102665882046 0.7639461179595625 86.75044608867022 0 0 0 717 1 1.5569206873129497 6.630671370877478 3.7900496133994652 88.35957806888432 0 0 0 4847 2 -0.6140211680743854 1.6885512237254496 0.16972614370029224 87.77712947767174 0 0 0 4894 2 -0.42353020872865244 5.612980871850759 6.970715812430212 93.37386109855065 0 0 0 14 1 1.614150326775522 5.940149769305514 4.841298433712412 93.87264775158694 0 0 0 715 1 1.7241744275259143 0.036807124576842855 4.6550951245806385 88.05560527176252 0 0 0 2890 1 1.6552781277976376 14.078753835697752 1.0584191613472156 90.3354193117053 0 0 0 16 1 1.5861930406768827 10.76052855901787 1.8954461226040804 93.84245687797446 0 0 0 5093 2 -0.6052393641473733 10.573827835125579 4.117865062562976 93.42678496527594 0 0 0 4998 2 -0.5936827878931614 11.851746590035674 0.5008902046393225 93.77942355291043 0 0 0 726 1 1.7171781737327687 9.678335751012792 5.629454096381573 93.34624841825016 0 0 0 2899 1 1.7484200242507888 13.442101918933073 5.960937180834918 92.59383703713374 0 0 0 5196 2 -0.5746862693716376 11.67506433329169 6.377728788768933 92.68922508242039 0 0 0 4842 2 -0.575320301965647 9.27467951115909 0.91703721566231 92.3482949907519 0 0 0 5275 2 -0.5169672166212567 10.961086423695036 2.348747423061819 91.79193519824817 0 0 0 5399 2 -0.4907769432833711 9.80869427612376 4.621423945284868 90.86222969580065 0 0 0 5258 2 -0.5841324113476846 12.446661579871959 4.7174228831577105 90.97859480157922 0 0 0 710 1 1.6911870129808468 11.197034747253014 3.688122688263522 90.21691561957212 0 0 0 5106 2 -0.5989434843133293 12.629335861710565 1.9820531200313323 89.74525615157883 0 0 0 5385 2 -0.224572328114968 8.13104448688216 6.733065519031916 89.55688454233763 0 0 0 4851 2 -0.6208567920007096 10.274192146867428 2.0478973682455544 88.91606467692864 0 0 0 5005 2 -0.5666613490998091 12.775399697760253 4.341272759295337 88.77863195158542 0 0 0 4797 2 -0.5735983071063911 10.669296686674562 5.172027478198602 88.52444759030244 0 0 0 4450 2 -0.406187330292848 7.864477716419948 5.589318604144986 88.68890287853867 0 0 0 4584 2 -0.6288743585289522 7.990924494815953 0.5488575127011578 87.89983828967354 0 0 0 719 1 1.6824555860724721 9.743648689004226 6.621949312303697 88.066971778351 0 0 0 720 1 1.7586780595302036 9.518244766914746 1.425882229031024 87.43911933368328 0 0 0 5107 2 -0.6276732720701036 8.200882481670716 3.1978079537511803 87.71974828940169 0 0 0 4529 2 -0.5894052046712575 13.762361896797874 3.4785688132097112 86.91550762243516 0 0 0 4910 2 -0.6557959104409252 11.171394120205363 2.2210257491593683 86.13549483744829 0 0 0 4970 2 -0.6145854302134415 9.201381399565395 6.041282245069061 86.00768203117849 0 0 0 4435 2 -0.5629686842014916 13.468275857938178 1.1392692917883094 86.12701654339526 0 0 0 5211 2 -0.609945638565992 13.927523756055026 6.108244267292552 86.44522485456041 0 0 0 5431 2 -0.5012983320775178 13.923106902078878 4.015613704375196 93.58882935002411 0 0 0 5381 2 -0.42510424266461105 7.7322994818470825 5.26102121568952 92.65119378628142 0 0 0 5064 2 -0.6142249891195903 2.0741713486685316 0.0025953461087162566 90.38407059477568 0 0 0 4703 2 -0.5827418864092099 4.657192813979041 14.028893109494984 93.18411455010505 0 0 0 4694 2 -0.6095119407951184 5.222147488062289 13.978566779788041 89.47001902533994 0 0 0 4895 2 -0.6335132989502652 4.788199260692107 7.182270385538689 90.55376551565037 0 0 0 1446 1 1.7690993935091295 6.293351825936202 13.32868844561352 93.04397425375865 0 0 0 5351 2 -0.539359323716595 6.649809130628242 9.486438325935499 92.10312181093911 0 0 0 724 1 1.6056801240328884 4.98552702138512 8.376238857999383 91.7794300242998 0 0 0 5433 2 -0.5884299748474601 5.122757545090285 12.501034455773551 91.38128402287167 0 0 0 4882 2 -0.4769977245516967 3.610502648419208 9.446087457093073 92.09145127122636 0 0 0 5164 2 -0.650873373969161 0.5854249971677148 7.817847564946141 90.7873725265838 0 0 0 5421 2 -0.6035301576144183 4.8804873489170175 9.976486127346796 90.12511314733905 0 0 0 4763 2 -0.6153605383619817 0.8156651486847378 10.437060217407357 89.72351886653965 0 0 0 1445 1 1.6802692547251452 5.0599988032674315 11.693677857680202 89.8519752302435 0 0 0 722 1 1.6741247565089945 1.0454917449925083 8.69432163873534 89.34013071932317 0 0 0 4713 2 -0.6093128010376108 6.77111853882299 11.723124015232127 89.46035017953952 0 0 0 4993 2 -0.6839327076549395 2.844408203206763 7.48924975604969 89.15850934652232 0 0 0 4657 2 -0.7255033450898956 3.7588616348465442 11.843514013987614 88.15521054685418 0 0 0 4750 2 -0.6076614368335875 0.7466495890412156 12.202794026033981 88.26071458582136 0 0 0 5068 2 -0.6086603896599683 1.6326492682287583 10.009521019532608 87.60385974887288 0 0 0 1433 1 1.69951932312186 2.226287124156495 11.658162135030091 87.32659539854441 0 0 0 4496 2 -0.5999574419003773 1.7998874003099026 13.57425561191942 86.42363715961166 0 0 0 5349 2 -0.5536668256124937 6.230978254440251 11.655410256201261 93.45015897872608 0 0 0 4579 2 -0.7297226301364228 8.305540828445073 14.212411064663799 80.383182978903 0 0 0 4652 2 -0.5993362292714274 0.14118532205485265 13.569076547118183 91.0456999710765 0 0 0 5208 2 -0.601363641820623 14.086873861390158 7.2702187952190735 91.61066092907325 0 0 0 4997 2 -0.5182951694755814 0.17256182882760396 11.299945039204886 91.7684793065522 0 0 0 4721 2 -0.41220663833699467 10.71256351363857 7.781105288915796 88.94123616833771 0 0 0 734 1 1.6609970892333497 8.04529171215335 9.996172233856612 93.58805381805512 0 0 0 1447 1 1.7253009205213554 12.21240986468619 13.6259657821892 91.38051713664832 0 0 0 4759 2 -0.6047036306706682 10.419110486997338 12.67231446638668 90.47767589672856 0 0 0 5461 2 -0.17486088611387718 9.664100695972014 7.453386960419451 91.84016156841788 0 0 0 5439 2 -0.6190217510697329 7.692216804900991 13.095236295810318 91.36215066170647 0 0 0 5331 2 -0.5698885687772376 11.14478626807947 13.035900330457672 93.33421101862014 0 0 0 5177 2 -0.6082662380969314 8.824644949768455 10.82504549525424 91.70596386423246 0 0 0 5153 2 -0.5335504806923264 8.088953847820099 14.056518288719925 93.71269498838441 0 0 0 4620 2 -0.5987135273661801 8.577594622850594 10.592007867083181 88.71714457971227 0 0 0 4446 2 -0.6113183148553215 8.48990572749895 8.296165637659369 87.05066797507293 0 0 0 1437 1 1.5415676806481755 13.869221648195625 10.552447077386002 93.3855966559373 0 0 0 4827 2 -0.5812497401325714 12.785714559751062 12.081214992404307 89.97075890006545 0 0 0 1438 1 1.6704730565207218 8.436809495646983 10.037653675526995 87.0329036190122 0 0 0 5286 2 -0.5490947778802847 12.980809357560767 11.655415454401686 92.2912952471348 0 0 0 4677 2 -0.5929663624179049 10.108442133605456 10.383452586262376 86.5710384334345 0 0 0 5328 2 -0.3248958923413979 8.800454701926999 7.675068674999075 92.90400508964973 0 0 0 5389 2 -0.6569527280080929 8.68119343360799 13.746386286876376 88.89740650773653 0 0 0 1449 1 1.7526722883737276 13.992820585439851 11.779831242095682 88.7133148777532 0 0 0 5348 2 -0.5610456824208037 12.248288132225502 11.796086965439768 87.02764321626907 0 0 0 1435 1 1.766900903351198 8.73999933477502 12.027523118926437 90.40174279465322 0 0 0 5060 2 -0.5908628476632927 11.45528387850875 7.273857294443184 86.79982407206883 0 0 0 4616 2 -0.6831707717627316 7.598168759217448 11.892510858647809 86.1879396052794 0 0 0 5366 2 -0.5198106392667116 13.779844452802314 14.051474079267503 90.0294907911614 0 0 0 4930 2 -0.8534734302721325 5.319684811240405 -0.013221122835435542 81.1715957993395 0 0 0 5505 2 -0.4104811572298067 13.492898851925746 14.157227807889246 92.49640679448467 0 0 0 5343 2 -0.5876459787439512 14.24260487236639 6.557000998852679 89.47530672191196 0 0 0 4581 2 -0.4865529623316033 1.3674028550154955 1.124493014793195 99.19433019664068 0 0 0 1467 1 1.6761585530335583 1.7036381036204968 0.4033693388261899 97.65511861894389 0 0 0 4768 2 -0.6127451333671717 3.828224493581997 0.9704000353908743 97.40471567878845 0 0 0 5465 2 -0.4202411723438649 1.222150602476506 2.330863593924648 96.53417258519035 0 0 0 4564 2 -0.24387240245635167 1.8952510811816756 3.5414605387054974 96.4735315768034 0 0 0 5066 2 -0.45092982741860327 5.388513857652705 4.5718323422024545 95.53049993772278 0 0 0 5276 2 -0.6041766969087627 5.491223649658759 1.3947171706872115 94.64012673584688 0 0 0 5316 2 -0.5397158132826664 6.908769017798839 1.9425788302068998 96.88020098645259 0 0 0 5158 2 -0.5314327832672961 9.887947804937843 9.291923243150126 94.12351788027632 0 0 0 19 1 1.72112774061476 -0.08262020058955116 3.628766235691313 95.46386455117955 0 0 0 5256 2 -0.4926613897364346 1.9807140692768717 6.860259106917814 94.49333746014192 0 0 0 1481 1 1.5865991147220724 5.375582414299227 0.4274605511072076 96.6951490190858 0 0 0 5342 2 -0.46842789575884947 7.923535647892621 4.993671523865549 94.42981782505053 0 0 0 5161 2 -0.6057729073402952 14.053613271705656 6.06825793096294 94.2593069807794 0 0 0 5245 2 -0.3950588774538932 13.414318367039828 4.353339252167474 99.13821133183177 0 0 0 4448 2 -0.2082903806367655 8.954315999310257 1.8322438210395688 99.62543537215906 0 0 0 5392 2 -0.3936413505445852 8.49192763242477 0.9034665870439823 98.75255968298578 0 0 0 5121 2 -0.2240101424446359 12.085410811051766 1.6593093325158454 98.16527531500728 0 0 0 5212 2 -0.363722209121765 10.766838244667843 1.593296462869654 97.5973619504294 0 0 0 5289 2 -0.45794998280038973 8.44748108345852 4.2430613954691685 98.1075956687506 0 0 0 27 1 1.514444548951307 8.680799760028963 2.64424544607064 97.418854235905 0 0 0 4706 2 -0.504068457062698 13.517092094107802 1.0568886415762797 96.10466954677425 0 0 0 4602 2 -0.4151507860791152 9.74074845560571 2.9183579745285813 95.64735192184905 0 0 0 5246 2 -0.37991843585847357 9.028029237108166 1.5716158328360847 95.2070451816636 0 0 0 5024 2 -0.5332892091162832 9.936721850936042 6.43373866199888 94.88473349481325 0 0 0 4931 2 -0.5345402762622788 12.194371232084737 2.4984072828578463 94.81360681286787 0 0 0 5472 2 -0.3626772896676425 5.396979087799229 8.168619182579366 96.55646195087154 0 0 0 5101 2 -0.4550732560852037 2.403959979803376 13.326259263340367 98.1119395939785 0 0 0 5491 2 -0.45923578872091075 1.3396649271880874 11.009087711345856 97.38735043699994 0 0 0 3645 1 1.5983590507142367 1.4421303611590832 12.637010851580378 96.83514473192564 0 0 0 4538 2 -0.5900378526820583 2.7675716374045827 13.58768549020775 95.30151862483474 0 0 0 4670 2 -0.5518428361180684 0.4173193968852836 11.704760572618698 94.95784819219345 0 0 0 732 1 1.6550404196930761 0.45606488343236534 7.488503900346918 95.05520100243533 0 0 0 4811 2 -0.40978604824235376 6.876707793433829 10.77850766422439 97.31720974557696 0 0 0 5344 2 -0.46109348425742636 0.44171766916973143 7.782312549332327 96.76178097924911 0 0 0 743 1 1.3890297377468528 6.9898909481106735 8.877166042812275 97.32257549984706 0 0 0 4918 2 -0.5371950979035046 7.046522726567338 0.5716540918760784 103.09759723987543 0 1 0 5055 2 -0.2024217509091942 12.375579358510107 11.203602989415138 95.21886932438242 0 0 0 2929 1 1.5583558963075204 10.579906991138172 8.582271271529887 95.95378837757625 0 0 0 5396 2 -0.5443232937377384 7.240014864356182 9.215425742855395 94.96708580170805 0 0 0 745 1 1.5925102643815088 9.912860917503169 13.460691448288298 94.56503621582017 0 0 0 5067 2 -0.34635018968011355 12.159540878096896 9.90030170779285 94.85686154960375 0 0 0 5262 2 -0.5406423269621404 12.33751264480838 7.394087475376989 96.08075530976174 0 0 0 5430 2 -0.47687057561618645 10.822272857200259 9.844640974145547 97.11973258075203 0 0 0 4465 2 -0.47897058546292914 6.918859997727379 8.229514960244098 99.11089549394072 0 0 0 5261 2 -0.6001273200175095 9.020834744857728 8.090928667401736 96.59558760154634 0 0 0 5485 2 -0.4598282476717191 9.679037053214007 12.487571691372539 95.99975388131017 0 0 0 5189 2 -0.5240859058192207 14.080106371167423 8.565086338250927 94.03779834884328 0 0 0 4967 2 -0.19176790886934622 4.989464350714329 8.052405968198332 94.03755285065839 0 0 0 5361 2 -0.5804617917097367 8.45210967131369 11.65390897670392 94.11457145270316 0 0 0 4458 2 -0.6316895282043868 0.46334045922958433 9.421070195516478 94.10282714324049 0 0 0 1488 1 -0.0006214756250943624 2.6441345203019697 18.742898845565154 2.1821365242180133 0 0 0 777 1 -0.0009073483598281838 2.5752795288506434 15.641545111255793 2.1761811939302906 0 0 0 1490 1 -0.0008653300900579868 5.827127000334918 18.70773768420418 2.2090956123924386 0 0 0 779 1 -0.0011875009566323694 5.870482977915296 15.622458434519148 2.17189650775823 0 0 0 749 1 0.017001126538328512 1.0576757128607501 17.234353392475352 0.6703055929143767 0 0 0 1460 1 0.01555006576219159 1.0159493036055098 20.39838023565422 0.7512310493871173 0 0 0 1462 1 0.014538404629124438 4.240724147589385 20.347217186248788 0.8540531621924686 0 0 0 751 1 0.016175760478462906 4.299875823310942 17.234470575353505 0.7157274882288224 0 0 0 781 1 -0.0014029447785678375 9.074861484655367 15.653497546965696 2.199354333616133 0 0 0 783 1 -0.0009093140764038 12.215076985223005 15.665007226878345 2.165475230178349 0 0 0 1492 1 -0.0011752117169599205 8.944164181832168 18.81080480189343 2.253208811756583 0 0 0 1494 1 -0.0006370735922463472 12.152960528089991 18.815840154214097 2.164021249412752 0 0 0 1464 1 0.01604878407899877 7.332277180598787 20.359557960195144 0.762423066612967 0 0 0 1466 1 0.015747947893221245 10.574721989173325 20.399202631378373 0.7442612770030184 0 0 0 3646 1 0.01611026079001767 13.854508504433902 20.38770838007506 0.7114169078075832 0 0 0 753 1 0.01572488840983162 7.543871479468653 17.231916140304513 0.7087427842816754 0 0 0 2935 1 0.01666708077253197 13.849762281874588 17.17509935814536 0.661959373054056 0 0 0 755 1 0.016569074929566482 10.597127174557125 17.210139691716638 0.6415430716917093 0 0 0 1499 1 -0.00019244772707477338 5.825462631654175 22.02153872478534 2.266460932002356 0 0 0 1497 1 0.00019040679431392367 2.634861923073634 21.95689871946213 2.1838250452842756 0 0 0 1506 1 -0.002545293353469886 2.5870058438101555 25.261063632049552 2.076934650734893 0 0 0 1508 1 -0.00024118582079685246 5.81367423608112 25.261299439789695 2.1471676094885224 0 0 0 30 1 0.0007990131315474304 2.6242051804223383 28.44445506264397 2.0365402952272573 0 0 0 1471 1 0.009664457366276701 4.2734851702373575 23.494987142318628 0.6290403755782648 0 0 0 1469 1 0.010365355647987504 0.9450710806665963 23.505180426966866 0.6112622788813791 0 0 0 1480 1 0.011043305992510976 4.382242892705617 26.81916739784925 0.5095129625972487 0 0 0 1478 1 0.004479229858647044 1.0275432877604105 26.838830299200403 0.5460262265895863 0 0 0 1479 1 0.025114641221626523 2.77002240821074 25.07083187935132 -0.6020411585697306 0 0 0 32 1 0.00033116762992330183 5.7971746973695 28.36138931691041 2.1276754093283996 0 0 0 1512 1 -0.0014377808016540167 12.16604577127628 25.102273052213494 2.199482722419439 0 0 0 1501 1 -0.0005949084848954642 8.961785834893195 21.97960662561989 2.2052880565481163 0 0 0 1503 1 -0.0008450566016513312 12.094745964579891 21.957403284309546 2.186556576971831 0 0 0 1510 1 -0.001088901082884446 8.990499475017057 25.09820828260935 2.194544294855587 0 0 0 36 1 -0.0006252631820924184 12.203966675263516 28.425958638327053 2.1138827307443524 0 0 0 34 1 -0.0005133074405951528 9.008502314497225 28.23146775017191 2.170111395530647 0 0 0 3664 1 0.01612930619956117 13.794717730634027 26.67037459580863 0.6808645805850356 0 0 0 1475 1 0.017379140326990415 10.564980904016604 23.547937770708643 0.6150651865397618 0 0 0 3655 1 0.014867634724246695 13.757274555597517 23.58019361885 0.7764633349410002 0 0 0 1473 1 0.015062713537088414 7.406096638953119 23.551887631047876 0.7413415524655681 0 0 0 1484 1 0.015381474940923276 10.686846127915246 26.70506726024431 0.7443896019613593 0 0 0 1482 1 0.016339119786092413 7.550988261202377 26.729484811111607 0.6560188710972854 0 0 0 832 1 0.004600299599347234 4.260043769681854 17.327969720244596 10.169861519749142 0 0 0 1543 1 0.004651408341316455 4.192178019069399 20.55079300248809 10.121553049990371 0 0 0 830 1 0.004383066027153231 1.1482559430549313 17.225447016890254 10.170406235000724 0 0 0 1541 1 0.004510935795601082 1.0157231399605744 20.46646345750985 10.118200555597959 0 0 0 1542 1 0.004610380399234877 2.6077037409470036 18.79847706788628 8.524418168855266 0 0 0 1544 1 0.004529365561333975 5.785014989012263 18.867038425063555 8.618469341465874 0 0 0 831 1 0.004493881092154669 2.712475699800887 15.61245791407799 8.530077022921226 0 0 0 833 1 0.004665126905430375 5.877570106560152 15.592461107998405 8.50757693597899 0 0 0 805 1 0.005377973590684648 4.277146471211321 17.185077916053572 7.002760230534055 0 0 0 1516 1 0.005282798130072869 4.278074879423501 20.43887542280306 6.922551026235911 0 0 0 1514 1 0.005148674280950788 1.050121834970649 20.363419470431165 6.939406460408013 0 0 0 803 1 0.005323406235383512 1.0720665390339679 17.24395165333146 6.902931804580461 0 0 0 1517 1 0.005501925451560759 5.73030913664748 18.78499160960592 5.277152293017583 0 0 0 1515 1 0.005673761245683542 2.665907549226324 18.784739706097675 5.279780887906068 0 0 0 804 1 0.005710923658099899 2.571320071949309 15.607266403543138 5.322635844177574 0 0 0 806 1 0.005665080285360899 5.833063585530905 15.627913957222615 5.2784787867310605 0 0 0 1487 1 0.0039791463641352665 0.879307517818909 20.392646869538083 3.798139651708267 0 0 0 1489 1 0.003748968377658788 4.255852607173522 20.379591247068984 3.722718832458104 0 0 0 778 1 0.003719047573587427 4.220808120526484 17.18869540290515 3.6858362153816238 0 0 0 776 1 0.003908589739077267 0.9693003011924163 17.278339761877994 3.6952156089870716 0 0 0 834 1 0.004658384419297997 7.40091392926812 17.256419075620208 10.087643072555641 0 0 0 836 1 0.004655041243450007 10.673139035879311 17.191855962718904 10.112291581790593 0 0 0 1547 1 0.004399266152538446 10.613000754854854 20.446872925861257 10.105587369826896 0 0 0 3016 1 0.004579030769800586 13.86399540921523 17.241864690692637 10.19058318231351 0 0 0 1545 1 0.004566555670218729 7.393279035510476 20.54063779436398 10.036388828948285 0 0 0 3727 1 0.004524713580608944 13.77488994920397 20.463109458757877 10.161067101875746 0 0 0 1546 1 0.004446446253386893 8.97866795970063 18.87178765821596 8.582737974446136 0 0 0 837 1 0.004531595290480382 12.275655891650956 15.680158443402759 8.521923997784917 0 0 0 1548 1 0.004526271834648149 12.197745426103937 18.831078058688938 8.532239710038922 0 0 0 835 1 0.004618387657083087 9.050155824586003 15.64991340638958 8.538391487353413 0 0 0 1520 1 0.005092023863767137 10.504653098651035 20.46595984798129 6.997926485550121 0 0 0 3700 1 0.005347820169252004 13.852973606665728 20.412597282900734 6.9489507654042475 0 0 0 807 1 0.005494953741795558 7.508551537490965 17.364107457596514 6.947349016205256 0 0 0 2989 1 0.005167961690100887 13.785910624267714 17.231728212502173 6.940755722440973 0 0 0 809 1 0.00524810596396561 10.621884457294877 17.297731979402645 6.9115235863282125 0 0 0 1518 1 0.0051207248147381364 7.305388680312125 20.50027234120576 6.920289290640557 0 0 0 1521 1 0.005659947723471767 12.158578575403624 18.8557914881951 5.406790096867766 0 0 0 808 1 0.005744437348673557 8.946844129423244 15.605388858124217 5.391710890703158 0 0 0 1519 1 0.005387782722483997 8.983473992144555 18.87358093136878 5.348743598720424 0 0 0 810 1 0.005557667908354146 12.218497309374742 15.647179406987119 5.349732599001209 0 0 0 1491 1 0.003997762991888854 7.418771727585429 20.403537668338302 3.7955585745031892 0 0 0 1493 1 0.004024867859100232 10.560676000389897 20.43754382640747 3.841534266503396 0 0 0 3673 1 0.003974836307099621 13.778776585756574 20.357199593619473 3.675204630670313 0 0 0 2962 1 0.004105591036246482 13.800170582772619 17.224854020171108 3.778872844514186 0 0 0 780 1 0.003974871141879438 7.455507905644302 17.186748478475696 3.7551851612982077 0 0 0 782 1 0.004215630699844998 10.564652093982176 17.258053712349344 3.7361469566627976 0 0 0 1552 1 0.00458475649040084 4.23128686540305 23.706697154295558 10.147283484220955 0 0 0 1561 1 0.00458217112291061 4.213727446134497 26.768589207353436 9.978220640141071 0 0 0 1550 1 0.004714931751933897 0.9695616302417263 23.624946861679575 10.134052178763266 0 0 0 1559 1 0.004747963128419172 1.0716169670557214 26.78328358681985 10.108172156829758 0 0 0 1551 1 0.0044839988748327664 2.6469302381235624 22.124256697773138 8.521410381211668 0 0 0 1553 1 0.004302047872618304 5.732357415946007 22.09348091141894 8.550284142138697 0 0 0 1562 1 0.004494588318338877 5.850685917392689 25.191759233671426 8.403382486022029 0 0 0 84 1 0.004342823991042558 2.6171165939111978 28.296800453111995 8.468950336740109 0 0 0 86 1 0.004369977393145199 5.7490154069703925 28.381198258370517 8.537365844372188 0 0 0 1560 1 0.004245179843949858 2.6288364088555944 25.1567280280742 8.512954397841284 0 0 0 1525 1 0.00507721027990438 4.1859444570652355 23.621833595463087 6.914270878679336 0 0 0 1534 1 0.005047135197353333 4.204048669524858 26.78748807395256 6.89414428883123 0 0 0 1532 1 0.005204313192920928 1.027128365867817 26.851476836802632 6.840627699780002 0 0 0 1523 1 0.004943344365949096 1.0344803771942988 23.584114287211293 6.910613179127694 0 0 0 1524 1 0.005666486147153258 2.592531690917318 21.999325940311767 5.296519311552059 0 0 0 1526 1 0.005361070068296364 5.77873531103569 22.019333573039905 5.297109797444822 0 0 0 59 1 0.005319038292166872 5.8031272153071205 28.352954436130577 5.423470612672232 0 0 0 1535 1 0.005541633656500244 5.754812234120675 25.239535670926 5.348917887441449 0 0 0 1533 1 0.005865578638275743 2.5347763890715838 25.20779237127912 5.283992426848191 0 0 0 57 1 0.005708290028492656 2.593841624798441 28.492371081364904 5.288562358651889 0 0 0 1498 1 0.004622868432078365 4.135414480783148 23.563891417888797 3.6628004771739064 0 0 0 1496 1 0.004695158629048917 1.0350960956151802 23.636434186025255 3.664453220804343 0 0 0 1507 1 0.004799727431113822 4.165162523770818 26.788112724343776 3.679733642819385 0 0 0 1505 1 0.005420622824297956 1.0397209002192682 26.81323848815474 3.7117684874663825 0 0 0 1511 1 0.0037665059251218713 10.62208314962562 26.704069882259283 3.7429119676972293 0 0 0 1509 1 0.003887357614814766 7.405459544943337 26.804376184417873 3.7493470163048723 0 0 0 61 1 0.005331098255089152 8.930509069567663 28.335490733544244 5.340949294315358 0 0 0 3691 1 0.004012899526488542 13.699883401138749 26.808430710339056 3.7339495984474294 0 0 0 1554 1 0.004720024075835555 7.526852193898913 23.666575043162467 10.180260933223172 0 0 0 1556 1 0.004486381599048335 10.63703335117991 23.608552814039793 10.176919020950038 0 0 0 1563 1 0.004477871315614168 7.429572126739839 26.84106350756316 10.112161480279276 0 0 0 3736 1 0.00457521202247314 13.788266158995288 23.58745980357786 10.121070173340874 0 0 0 1565 1 0.004441941002514872 10.62293715027895 26.804402253059695 10.117519005982807 0 0 0 3745 1 0.00450897044206367 13.738817522898064 26.791894439559385 10.09466673492349 0 0 0 1566 1 0.004509754452220818 12.125258412015988 25.247127000007684 8.472051557970431 0 0 0 1555 1 0.004413231713305812 9.080674571452604 21.966144301643155 8.547651473824757 0 0 0 1564 1 0.004665356018810848 9.039832548605544 25.242372704336248 8.52238811969399 0 0 0 90 1 0.004583253444981153 12.136190675264016 28.42732796318185 8.479183110757784 0 0 0 88 1 0.004522123301669973 8.931453150144641 28.374376635474277 8.47950859115169 0 0 0 1557 1 0.004508537486670962 12.155331226679209 22.02315823534019 8.483561310174524 0 0 0 1529 1 0.005144273255802932 10.543902409222921 23.631120527202686 6.930803971019784 0 0 0 3709 1 0.005237600765131096 13.769431552464944 23.612301166242936 6.9185879734620706 0 0 0 1538 1 0.0052264783261889 10.558713737846984 26.78291701251181 6.914279745850813 0 0 0 1527 1 0.005285450706704215 7.296694891047531 23.52217899675154 6.874524007216122 0 0 0 1536 1 0.004976240722190552 7.397797547165133 26.805769691611715 6.944321142768755 0 0 0 3718 1 0.005361490803414732 13.75211304661955 26.800141179237624 6.91380647192764 0 0 0 1500 1 0.004117425356314161 7.2211088983482865 23.64420083299111 3.771630018588161 0 0 0 1530 1 0.005708947364512896 12.175553423763768 22.105595317498835 5.406133896973301 0 0 0 1537 1 0.005701777553537889 8.94893131774886 25.163491490515327 5.295097164586096 0 0 0 1539 1 0.005622044415381937 12.185312640006188 25.16666226165828 5.3369702776738555 0 0 0 1528 1 0.005392128273890125 8.983662447158832 21.99441296987637 5.391979431677797 0 0 0 63 1 0.0053147423490165525 12.19717838273717 28.404459447439958 5.307367018510363 0 0 0 3682 1 0.003971251799699727 13.806633081032139 23.546270515853866 3.682701930055687 0 0 0 1502 1 0.004014338897084531 10.586525947833643 23.577164551214814 3.68860815335535 0 0 0 1623 1 0.0047682082566919935 2.6297506191459727 18.944493830531744 18.03978070715887 0 0 0 914 1 0.005031130497324527 5.824703115278052 15.69818674873055 18.10740853958546 0 0 0 912 1 0.004849494378411987 2.6687133285851576 15.70348150208204 18.087072843410755 0 0 0 1625 1 0.004807481871432123 5.828691349704694 18.940811076419845 18.10677467035187 0 0 0 888 1 0.004643543363515105 1.0103690071358034 17.238119634089383 16.42090331584805 0 0 0 1609 1 0.0048908497524496105 1.0953887179381419 20.46907648344562 16.483864331165577 0 0 0 1610 1 0.004811105729306877 4.2754011868525374 20.512392858186182 16.429218415409068 0 0 0 889 1 0.004764745105817989 4.204318339626413 17.3343956907497 16.610814637839585 0 0 0 1595 1 0.004776482227232126 2.6645342626706636 18.80702035380069 14.85972729861159 0 0 0 877 1 0.004852071801873411 5.763799503109973 15.691790113393353 14.910122796405133 0 0 0 1596 1 0.004730105371324303 5.822558277567351 18.832660478822195 14.896246666194852 0 0 0 876 1 0.004716929296598936 2.6006375176334737 15.656309659791457 14.945400142888715 0 0 0 1570 1 0.004808581936320121 4.2728920296959965 20.496774604692035 13.27635746432933 0 0 0 859 1 0.004847653255530758 4.338596275683491 17.296147891059963 13.283758949669442 0 0 0 1568 1 0.004710115710187594 1.043834450297003 20.43500307681298 13.281902246713168 0 0 0 857 1 0.0046746934833662036 1.128059566831169 17.196668089078845 13.38084395910409 0 0 0 1571 1 0.004884209891195975 5.855168849996618 18.956830287795444 11.765050775718091 0 0 0 1569 1 0.00487606149633979 2.5923558110907177 18.925968438848518 11.744749014089903 0 0 0 860 1 0.0049981286233458 5.90826323696142 15.592114313024773 11.712876674014213 0 0 0 858 1 0.005008610433759027 2.743231896308349 15.749924506463612 11.646397251770718 0 0 0 911 1 0.004623484858259025 1.1166097940850317 17.30801636517868 19.63510229318453 0 0 0 1624 1 0.004709812516035049 4.224757973150869 20.500618517970516 19.662066913731586 0 0 0 1622 1 0.0047296974439567825 1.0136269992029225 20.42489388065053 19.74259051449604 0 0 0 916 1 0.004882554966188633 9.005780432114673 15.640090984272883 18.07494259128333 0 0 0 1627 1 0.0047539303521956094 8.978438131373434 18.87952929389874 18.14787398147363 0 0 0 918 1 0.0047865180556465724 12.222090676985964 15.705338677227823 18.05779809720957 0 0 0 1629 1 0.0048012162911330175 12.25905673914236 18.84754990383758 18.18102943145632 0 0 0 890 1 0.004864868949439152 7.4030002757883615 17.329162561109428 16.505737378188602 0 0 0 891 1 0.0048083718359557635 10.56403954530417 17.354627447084013 16.514465262131264 0 0 0 1611 1 0.004783617597032002 7.435470303942983 20.43945877723791 16.533796316027257 0 0 0 3074 1 0.00472393608247333 13.842099136398444 17.28373132335672 16.644666881598607 0 0 0 1612 1 0.004850371559489659 10.583861703538078 20.545839369428837 16.569152782153747 0 0 0 3793 1 0.004522317064257295 13.760224595954396 20.572045680512677 16.727741931006577 0 0 0 1598 1 0.004675008005528773 12.207749188187291 18.913416332342432 15.066044299067007 0 0 0 879 1 0.004583622465512789 12.177440715876841 15.746442821181601 15.00652533772159 0 0 0 878 1 0.0047870293215475975 8.994529437593332 15.69099663825076 14.932068454937667 0 0 0 1597 1 0.004661105120888806 9.01004700892411 18.896124656690887 14.880964967835208 0 0 0 1572 1 0.004777059296075097 7.469682152129444 20.410451258513504 13.30195680427216 0 0 0 863 1 0.004783741046929805 10.733184230650199 17.320098325454698 13.363066147727977 0 0 0 861 1 0.00481435872547319 7.480516823100985 17.28416143137124 13.233796589307127 0 0 0 3754 1 0.004815411348766861 13.704407863794556 20.370741016722086 13.470761149321138 0 0 0 1574 1 0.004808612935587304 10.566135413536237 20.43549316217922 13.314234809080741 0 0 0 3043 1 0.00486100608064708 13.721434715786495 17.25943656601402 13.41942280872101 0 0 0 864 1 0.00482825671336049 12.243157287926913 15.698728267194682 11.7740970643022 0 0 0 1573 1 0.005033358376224272 8.990091011978166 18.83867166824285 11.705577733281327 0 0 0 1575 1 0.004977282669740754 12.226683201581645 18.91799920911422 11.727357161638421 0 0 0 862 1 0.005076858231449599 9.141880689512597 15.626965889731807 11.814072783628488 0 0 0 915 1 0.0048609843188008525 7.521343455561425 17.262956177771844 19.745856513821863 0 0 0 917 1 0.004770709252600425 10.618044151685872 17.243812611887787 19.738289166485036 0 0 0 3097 1 0.004718373653694085 13.848432307635036 17.248552128941515 19.70876284357372 0 0 0 1628 1 0.004772721749108883 10.684791283961243 20.38850140877222 19.769143047774026 0 0 0 1643 1 0.004797738814855512 5.9160839233835985 25.279985743801564 18.197686775030235 0 0 0 165 1 0.004800951393527294 2.6625936381641484 28.376070884295714 18.08537516786154 0 0 0 1641 1 0.004714157925999451 2.6660615775827483 25.207148349330797 18.0844588857865 0 0 0 167 1 0.005006089835169515 5.840858139660331 28.413814604082727 18.200630524878672 0 0 0 1634 1 0.0048468653697834735 5.8596482090798725 22.14218881204072 18.16776153032333 0 0 0 1632 1 0.004825458829945464 2.6958706759251867 22.058901836729515 18.121859139843718 0 0 0 1614 1 0.004743340669218844 4.313593882066108 23.6882107376252 16.552643513452317 0 0 0 1613 1 0.004760665095161681 1.0895980733229784 23.62808190009894 16.550160445733848 0 0 0 1617 1 0.0046547040082274595 1.0423972631382818 26.836119194814927 16.543010081690518 0 0 0 1618 1 0.004792207263353701 4.250371581781623 26.82536629632094 16.44793985815882 0 0 0 1600 1 0.004713057295644517 2.639017979553364 22.029722164616718 14.930351810204638 0 0 0 137 1 0.004759271504481849 2.6817331832949054 28.30828340038644 14.845438323968958 0 0 0 1605 1 0.00471165964288448 2.7147344168338923 25.202475332545795 14.93289061533312 0 0 0 138 1 0.004767593489799375 5.8945393740117416 28.436891789029094 14.996851077436789 0 0 0 1606 1 0.004637814014898855 5.876424190892282 25.25108848987908 14.944935575539631 0 0 0 1601 1 0.004741293772787661 5.883925497377577 22.140238961494514 14.958519812070444 0 0 0 1588 1 0.004814743193315377 4.330010779438424 26.787745514998658 13.20359695185365 0 0 0 1586 1 0.004786078247324478 1.1122630518215284 26.831131842974397 13.315557244186326 0 0 0 1579 1 0.004817569440159982 4.219362494958792 23.642008841021717 13.341342185723494 0 0 0 1577 1 0.004749850708691361 1.0954287560909666 23.593154351708712 13.299234583968499 0 0 0 113 1 0.0049479947148942174 5.810237340350141 28.428715413132515 11.712357048117404 0 0 0 111 1 0.004997622556660473 2.6466762985910335 28.41327355451066 11.679236653340952 0 0 0 1580 1 0.005046610383214094 5.886480882460888 22.049525312466912 11.701386526358048 0 0 0 1587 1 0.005011107631585422 2.66741903988419 25.219845449658465 11.72540682404366 0 0 0 1578 1 0.004840428643165168 2.6525403418540567 22.057386739038357 11.767017123324516 0 0 0 1589 1 0.004889672834952421 5.898113278572049 25.239651699648437 11.659173441836417 0 0 0 1642 1 0.004757841943997507 4.164743071586114 26.754672477441442 19.66870324274357 0 0 0 1640 1 0.004819257049532266 1.0206823755156644 26.80602482880996 19.654073509008427 0 0 0 1646 1 0.004836468154140527 10.69932728783516 26.785039182564585 19.65565323686432 0 0 0 1636 1 0.004881882851968675 9.067202097487915 22.09579078183873 18.05386283823394 0 0 0 169 1 0.00482788748932461 8.957341409257173 28.492492801876214 18.15051927367097 0 0 0 1638 1 0.004714417863464318 12.223596325033112 22.067494647517094 18.214545911953063 0 0 0 1645 1 0.004819713221509543 9.056558097954577 25.244930955875894 18.081579424869748 0 0 0 171 1 0.004779603329592682 12.218625744665696 28.40460775400667 18.148687902043296 0 0 0 1647 1 0.004691541886991217 12.20573694026377 25.203233988148863 18.051159478657496 0 0 0 1619 1 0.0047898712950157005 7.438796441061346 26.81075468546568 16.42198768841785 0 0 0 1616 1 0.004584152960244815 10.624804147560623 23.717891397616953 16.494606373709324 0 0 0 3798 1 0.004544758127596265 13.819490849116729 23.611077403434365 16.50404058154818 0 0 0 1615 1 0.0046053547397604915 7.485934933112226 23.588839640650654 16.53058829400284 0 0 0 3803 1 0.004763370789354229 13.715445383016027 26.805536753812465 16.45624051729569 0 0 0 1620 1 0.00470689375478908 10.580842063530692 26.882849978284163 16.50351745792597 0 0 0 1608 1 0.004745700937817704 12.14308986112222 25.209938460792515 14.920380773138701 0 0 0 1603 1 0.004769347988257585 12.239236207089268 22.041079804576935 14.99651965693103 0 0 0 1602 1 0.0046792742478131075 8.989975276631577 22.053541385104833 14.880649664192632 0 0 0 139 1 0.004689956322078581 9.00699293627109 28.43373751699217 14.896636463688134 0 0 0 1607 1 0.004630478872898417 9.105065094597123 25.230196591656448 14.982245669220138 0 0 0 140 1 0.00482154852676946 12.153234903382293 28.415992306063973 14.857447530932733 0 0 0 3772 1 0.004848656279754513 13.779426635366695 26.882463699902512 13.344585005566165 0 0 0 1590 1 0.004728446157661737 7.391702902512389 26.820180183737627 13.266720672259392 0 0 0 3763 1 0.004928622635475775 13.778782931008703 23.607788171450487 13.247277576477579 0 0 0 1592 1 0.0048774533337562365 10.53882747001023 26.854878099771632 13.243534327506275 0 0 0 1583 1 0.00490413689343264 10.555720703366875 23.615327692250013 13.255349449874958 0 0 0 1581 1 0.004857351282167233 7.3879458297502065 23.69956243215562 13.382481115836603 0 0 0 1593 1 0.004938528756114608 12.208669254214948 25.27065141858233 11.721146011379922 0 0 0 1584 1 0.004892309247991064 12.20341597974792 22.03594690488791 11.713863078163804 0 0 0 115 1 0.0048774645623007856 8.97596638320464 28.408757732327427 11.64613505232819 0 0 0 1591 1 0.004757825634454132 8.98054485897793 25.2988998014085 11.730987766441146 0 0 0 1582 1 0.004862252746429157 9.113886500376106 22.047520428036467 11.707889210026094 0 0 0 117 1 0.004967978650571206 12.180368176587146 28.4629095792291 11.632946335037696 0 0 0 1644 1 0.004887208945499887 7.43406415084491 26.800372616828056 19.75117078109766 0 0 0 3817 1 0.004676793157068874 13.771211869765434 23.716811571728517 19.630232231810947 0 0 0 1637 1 0.0047946381686575015 10.609427333688503 23.647733597871436 19.758801436473348 0 0 0 1635 1 0.004764742364435335 7.4602518024658 23.637999903895995 19.73326591514621 0 0 0 3826 1 0.00474086022704405 13.817346483805734 26.827318067949477 19.732684778052626 0 0 0 913 1 0.004797785201884862 4.295889288160672 17.325641886844583 19.73819611141901 0 0 0 995 1 0.004659177725059254 5.778862701735747 15.728258754240802 27.692471629212605 0 0 0 1704 1 0.004784052122514223 2.6640489964103113 18.79117574630759 27.639663214261958 0 0 0 993 1 0.0047034540723299816 2.6401671655185437 15.663836163837706 27.702024757948966 0 0 0 1706 1 0.004675375358002514 5.841224682869889 18.846145840951543 27.723559264863333 0 0 0 969 1 0.004754601689353858 1.008552333907559 17.16415747119018 26.059768778278446 0 0 0 1690 1 0.004787707417297012 1.0564173329203572 20.422387329018676 26.129547062687458 0 0 0 970 1 0.004797156154748343 4.215554674171349 17.254421718470976 25.983078963739146 0 0 0 1691 1 0.004808946882372239 4.255446607053679 20.44910548759408 26.080953939286584 0 0 0 958 1 0.0046834986496060976 5.864422348919279 15.678784175618727 24.578402050900564 0 0 0 957 1 0.0047763412210385416 2.6455477594665178 15.637566927770838 24.46545213259562 0 0 0 1676 1 0.004978877678540406 2.652192024051426 18.867911821781778 24.45680109450894 0 0 0 1677 1 0.004769222070757747 5.913593083642306 18.827966985173962 24.496466898304426 0 0 0 938 1 0.004867584796142323 1.03964693057836 17.164298331454276 22.83418000294864 0 0 0 1649 1 0.004998921705430806 1.0688453158520683 20.377603802697468 22.91670779594108 0 0 0 1651 1 0.004798401180625411 4.2425716467116175 20.408568452983975 22.856635210605855 0 0 0 940 1 0.0047985377575986525 4.331952415598795 17.27458527570119 22.823696658592294 0 0 0 939 1 0.004841908328449348 2.6001408311732983 15.694637293622845 21.236510462893214 0 0 0 1652 1 0.004604839199301257 5.852705044320336 18.918434010351344 21.316762089409416 0 0 0 1650 1 0.0047111863041083574 2.6340472134575568 18.841936309376038 21.20556396063218 0 0 0 941 1 0.0047111538585697475 5.815801292663473 15.705633886375544 21.33249288571339 0 0 0 3808 1 0.004665231186303992 13.928250905452309 20.43668776655171 19.797291216473777 0 0 0 1626 1 0.0047950258396368805 7.477177783357531 20.38792096002507 19.74917049184957 0 0 0 999 1 0.004804301894012354 12.290971698639643 15.61779908295767 27.674713399101627 0 0 0 1708 1 0.004868844694564577 9.080502306382778 18.81871489323285 27.696416193731757 0 0 0 997 1 0.00478390012537761 9.058142812660279 15.668460378251881 27.728326925151254 0 0 0 1710 1 0.004844814896064623 12.227906746371128 18.758852038579988 27.668357517212613 0 0 0 971 1 0.004778202647156322 7.440583154460648 17.21473302112068 26.048432700541426 0 0 0 3874 1 0.004841278877848798 13.829022183137768 20.349850416915515 26.14205691172902 0 0 0 3155 1 0.004790282667208941 13.874845173411643 17.251936003885312 26.083335175159142 0 0 0 1692 1 0.0047881026696971595 7.443723916499659 20.424115046366264 26.122873678887668 0 0 0 1693 1 0.004897446551699698 10.666174573045994 20.47022184443181 26.134682635185918 0 0 0 972 1 0.004877295615160459 10.645448076965419 17.209606045516754 25.970730664810098 0 0 0 960 1 0.004847855337094038 12.252478837694625 15.667952414177284 24.507225589176734 0 0 0 1679 1 0.0048197997855070705 12.189521889088 18.870100091029997 24.43661038577843 0 0 0 1678 1 0.004923003380943473 9.030835848872687 18.929946625424392 24.51454280146922 0 0 0 959 1 0.0049284847006115014 8.980461078642334 15.619211231152907 24.461902910415287 0 0 0 1655 1 0.00478401558661219 10.659087944121456 20.349919428402135 22.86751798850352 0 0 0 944 1 0.004813713207679577 10.656405028543913 17.162433987207727 22.888727158493975 0 0 0 942 1 0.004743566525372873 7.363282946697149 17.236242339813902 22.859274079631287 0 0 0 1653 1 0.0047297795137260495 7.438972444336398 20.488388066406582 22.90269338190108 0 0 0 3835 1 0.004800977040339384 13.818574034653551 20.490937780742637 22.927725670477614 0 0 0 3124 1 0.004659453761871282 13.835968282695614 17.262619608522154 22.882864625357804 0 0 0 943 1 0.004773158131418216 9.119486701008697 15.5996040330423 21.316066531592288 0 0 0 1654 1 0.0046474929580195504 9.044885289365418 18.770960353053724 21.270946708847408 0 0 0 945 1 0.00464276849101984 12.30452520604252 15.628481218561049 21.330251602783292 0 0 0 1656 1 0.004713017677164937 12.24629621932517 18.840588806356294 21.277205572601208 0 0 0 1633 1 0.004583069066071307 4.252041258708229 23.716000219980447 19.762268396553317 0 0 0 1631 1 0.004782934051300893 1.083013726234356 23.64645063846528 19.720396701344875 0 0 0 1715 1 0.004706152026120774 5.87454043644595 21.963216495631496 27.618854369325728 0 0 0 1713 1 0.004741031248423443 2.685696889248867 21.978419217194038 27.671366864764813 0 0 0 248 1 0.004816547254302179 5.891821575489607 28.37581643227646 27.685492893164202 0 0 0 246 1 0.004889165833467584 2.7634460601212423 28.3891546286925 27.799166501122514 0 0 0 1722 1 0.004737562918378664 2.774818787039472 25.220961841306313 27.67882160082451 0 0 0 1724 1 0.004793487815221818 5.861592233164673 25.179989373096994 27.801007451990333 0 0 0 1694 1 0.004890052633502949 1.0331942530718754 23.58821177729562 26.004416559172707 0 0 0 1695 1 0.0047691181657255576 4.20558151556091 23.63133584015905 26.13400035306162 0 0 0 1698 1 0.004749104354471886 1.1356725890860142 26.846713312045086 26.005905079656568 0 0 0 1699 1 0.004861949593517104 4.316690895272709 26.816312975455954 26.064932880217622 0 0 0 219 1 0.004791875680175091 5.924324776478206 28.32558415280867 24.47410094492654 0 0 0 1686 1 0.004707563021253455 2.633939723250012 25.272004899519786 24.560420901540613 0 0 0 1681 1 0.004734453058274477 2.645364173643978 22.052507744209397 24.4986962308929 0 0 0 1682 1 0.004826854980826181 5.867010681603331 22.030297160693678 24.470696711365303 0 0 0 1687 1 0.004894049662490038 5.873312113305922 25.151759199933032 24.560814669587597 0 0 0 218 1 0.004826363121924136 2.706784124721831 28.508130590681652 24.478896288832704 0 0 0 1667 1 0.004739386610603226 0.9862575701737132 26.82339768211745 22.982660460166247 0 0 0 1658 1 0.004835619817845747 1.2141368709507112 23.600797536944842 22.88341494635207 0 0 0 1660 1 0.0047854140998015385 4.258922062995153 23.615943992627557 22.908363279601296 0 0 0 1669 1 0.004922335364924943 4.31151994484604 26.82103199659135 22.930484394039343 0 0 0 1661 1 0.004701286826600636 5.838757093466343 21.995068860884526 21.255844460510577 0 0 0 1668 1 0.004727268028210968 2.658290719897199 25.19593120951684 21.33146024153695 0 0 0 194 1 0.004850450455413947 5.915182948579072 28.39067870882219 21.418374292809197 0 0 0 192 1 0.004916426732451179 2.681261051979175 28.35266744387905 21.282493783034273 0 0 0 1659 1 0.0047231087654736985 2.6976700098584208 22.01404598107172 21.30234033517491 0 0 0 1670 1 0.004675077514732666 5.824928638499773 25.175671136485736 21.280986776179727 0 0 0 196 1 0.004840426760187233 9.112363111012035 28.464827793539722 21.312825237614817 0 0 0 1674 1 0.0047952105205210545 12.221068644189424 25.26638798775595 21.38889330023774 0 0 0 1728 1 0.004719252357483971 12.25171125154697 25.30433937826911 27.56843807778918 0 0 0 1719 1 0.004708979962374243 12.250066435586552 22.038160052121434 27.70571479730319 0 0 0 1726 1 0.004776456592326665 9.024975852294897 25.213355497090824 27.680992679480497 0 0 0 252 1 0.00465710537675274 12.171479011644788 28.406229982538118 27.693524099452915 0 0 0 250 1 0.0045419729119025535 9.050046223257585 28.425402170527903 27.73773687076782 0 0 0 1717 1 0.0048132126652344915 9.108801420852403 21.999696179980077 27.716831581249533 0 0 0 1701 1 0.004681348702801949 10.623085835156372 26.846202708616634 26.09244340847109 0 0 0 3884 1 0.004579363764405811 13.820715342419073 26.84551700234787 26.08636072715764 0 0 0 1697 1 0.004674224320865469 10.64883825542596 23.61125209829878 26.110599022821745 0 0 0 1696 1 0.004814080574372407 7.479506812799936 23.58899433337033 26.105310543719472 0 0 0 3879 1 0.004779005913948801 13.826913491486655 23.682435428999927 26.088028550168943 0 0 0 1700 1 0.0047843199669142245 7.5312621515579075 26.857438346023297 26.171424967409447 0 0 0 1684 1 0.005007912127084183 12.242047764515418 22.153112773962174 24.443185723986787 0 0 0 1683 1 0.004750589218037407 9.088595953545205 22.053609465556217 24.45786802699494 0 0 0 1688 1 0.0046659460302920786 9.056710707113629 25.133266233673186 24.511756766894184 0 0 0 221 1 0.004769690612402615 12.259928458539312 28.376346154505352 24.51717896957096 0 0 0 1689 1 0.004689518048363513 12.114469228077773 25.253072540620707 24.442554201352014 0 0 0 220 1 0.00475742494869877 9.066204535958558 28.40401247344047 24.515648380723267 0 0 0 1671 1 0.004879760131673376 7.5267501128977585 26.688235247376102 22.915107013386187 0 0 0 1664 1 0.004592621921829231 10.581363679419027 23.62589387427208 22.89696523834666 0 0 0 1662 1 0.004695215868876822 7.419581740900713 23.58858816258054 22.874318867702247 0 0 0 3853 1 0.0047011488908842314 13.832909849413392 26.872235941988595 22.91741637605194 0 0 0 1673 1 0.004663280718738465 10.633344473489892 26.82618217839469 22.965965430819764 0 0 0 3844 1 0.004687441479967044 13.909831029556102 23.72454642544946 22.888206017279177 0 0 0 198 1 0.00470995526024043 12.194786080666082 28.388229684439974 21.29598715517755 0 0 0 1665 1 0.004823938058952424 12.287196814430041 22.101102595904113 21.236154772915114 0 0 0 1663 1 0.004806616286862565 9.1076008605607 21.943883362608705 21.342612771631508 0 0 0 1672 1 0.004763015608975607 9.041077667028903 25.168040098451705 21.326613692672346 0 0 0 1046 1 0.004828890811509286 1.07384406393355 17.193671113998008 35.63908295077938 0 0 0 1048 1 0.004713500849355713 4.18104634132988 17.22408462869717 35.587226868326 0 0 0 1757 1 0.004746314010158435 0.9881941484570649 20.5497151669622 35.64436659872892 0 0 0 1759 1 0.00467970163003833 4.282012641592978 20.46897629223905 35.64791913099052 0 0 0 1049 1 0.0048336006800054915 5.758478715572458 15.660097503152384 34.037528754523144 0 0 0 1047 1 0.00484288505491294 2.686561490881114 15.627132487610847 34.12622214133091 0 0 0 1758 1 0.004834927714484835 2.6255269730440443 18.946984045340997 34.14752356007223 0 0 0 1760 1 0.004809976444100479 5.779506803026644 18.88056365664446 34.03763869260276 0 0 0 1021 1 0.004864627265103833 4.2674032224599285 17.264596172880015 32.412140620638006 0 0 0 1730 1 0.004788316277359237 0.9824584910078428 20.42576629762307 32.5382794261118 0 0 0 1732 1 0.00484715652339361 4.214004422699906 20.451470795786587 32.459758699467656 0 0 0 1019 1 0.004916919157587529 1.1259816258406268 17.235900972332722 32.44943515130956 0 0 0 1733 1 0.004702462266768967 5.925870293943169 18.910999850533685 30.9105811996888 0 0 0 1731 1 0.004873317161140717 2.6157148543828286 18.869799439825673 30.89798606068568 0 0 0 1022 1 0.004762449227695153 5.882294752119391 15.686619766204227 30.814851392734937 0 0 0 1020 1 0.0048253000497471485 2.64958572319525 15.69501050136344 30.859351562258716 0 0 0 994 1 0.004758056733544319 4.286210412666618 17.278259214775495 29.225194903381336 0 0 0 1703 1 0.004655958682487275 1.0823983037693923 20.375102320314586 29.29661662344605 0 0 0 992 1 0.004716419599932872 1.1037695876936509 17.209053764016893 29.21137943718889 0 0 0 1705 1 0.004795073136096171 4.291661735280725 20.394646242161564 29.257969981008518 0 0 0 1052 1 0.004595700035019603 10.594592621677917 17.254404361886525 35.65661310738494 0 0 0 1763 1 0.004834674363124642 10.594714741796537 20.38275806890563 35.65792386578567 0 0 0 3232 1 0.0046882056200057975 13.888096437148942 17.256450733001213 35.723147383407586 0 0 0 1761 1 0.004723489061658719 7.452966496990636 20.45575768276958 35.77203029827871 0 0 0 3943 1 0.004695571133712639 13.922367563482737 20.43770147243869 35.67582833939527 0 0 0 1050 1 0.004888926760867435 7.4265622635973445 17.259545429312343 35.593788628304246 0 0 0 1762 1 0.004707141825201253 9.015382037518954 18.8253991215255 34.04522525211739 0 0 0 1053 1 0.004698861865398434 12.161298893490073 15.777013844311538 34.12710450322918 0 0 0 1051 1 0.004738764722733312 9.029470221915957 15.67361631099709 34.055582795668634 0 0 0 1764 1 0.004850417015224326 12.254630739923668 18.849011477098788 34.20961139190545 0 0 0 3916 1 0.004731264812338721 13.876041731060624 20.447192856152153 32.389569381658795 0 0 0 1023 1 0.0047822103710911355 7.4432763190283 17.240842375942304 32.398106327012236 0 0 0 1025 1 0.004715052589101598 10.628367512102948 17.247341174179613 32.449376930606036 0 0 0 1736 1 0.004770133676155938 10.62633296948692 20.367933348425968 32.50943568916061 0 0 0 1734 1 0.004595354517544821 7.43322715025071 20.425798887755303 32.60861923067851 0 0 0 3205 1 0.004869843167782941 13.79294955572715 17.27214901069309 32.483532982335504 0 0 0 1735 1 0.00463347091351648 8.969887182306596 18.913917566611264 30.917273737446553 0 0 0 1737 1 0.0048284784637825425 12.230312554236786 18.847159703389643 30.930939055482682 0 0 0 1026 1 0.0047422976630959995 12.226120195261807 15.682440938163976 30.882234503666123 0 0 0 1024 1 0.004750492170205314 9.086490315771092 15.71267086599708 30.810219108846738 0 0 0 996 1 0.004636288649409412 7.428089190791557 17.275368901768196 29.218262792356278 0 0 0 1707 1 0.0046743076315976986 7.428487702724453 20.3968498576086 29.306052324659866 0 0 0 3889 1 0.004809809339359773 13.77882059271296 20.4697030149318 29.21205522817797 0 0 0 1709 1 0.004801361993068534 10.613814136235995 20.47898479909724 29.4015109374305 0 0 0 998 1 0.00479628643574077 10.60830813362003 17.339293232094796 29.288348149688694 0 0 0 3178 1 0.00483353471667056 13.816219830859078 17.209922933191958 29.22027095414567 0 0 0 1766 1 0.004772589440249319 1.0947334510644515 23.684201444727023 35.65014552145766 0 0 0 1775 1 0.004566657449340749 1.0016190840884416 26.860795359757404 35.63081714497137 0 0 0 1768 1 0.004685545529602384 4.224085624557257 23.72444029301814 35.645467518315975 0 0 0 1777 1 0.0046469025324664456 4.2011939421959665 26.916947777541317 35.62392712069419 0 0 0 1776 1 0.0047681621315955654 2.619688849399842 25.264575153937432 34.04090874680115 0 0 0 1767 1 0.0048648742492156515 2.6135082718392195 22.096648169342824 34.004903859035046 0 0 0 302 1 0.0046233704379186336 5.912616094648881 28.445392660285616 34.05280264653609 0 0 0 1769 1 0.004799883817524161 5.864378928171803 22.035276800930028 34.072217158757326 0 0 0 300 1 0.004781893733271028 2.7255490325735683 28.440168969389468 34.052273527330904 0 0 0 1778 1 0.0047995148712484045 5.732830868088958 25.23298634327983 34.09865117123437 0 0 0 1739 1 0.004758014443548756 1.1045611767920978 23.661158840965868 32.34210032482699 0 0 0 1750 1 0.0048262708844334905 4.296431051909799 26.920379953015395 32.45203279470027 0 0 0 1748 1 0.004801771754116977 1.046413152832254 26.84208866415367 32.465941073621124 0 0 0 1741 1 0.004878731794983869 4.209405154636031 23.640005730665905 32.41436472358853 0 0 0 1740 1 0.00474134049923375 2.6630121375752775 22.026338035084 30.843811508160364 0 0 0 1749 1 0.004656267317071781 2.6607802752378373 25.23505573064535 30.802730316442418 0 0 0 1742 1 0.004816263515979918 5.910372135041916 22.04664974436007 30.830294140765872 0 0 0 273 1 0.004796262128134445 2.6655498945093727 28.430360080050768 30.86851642105081 0 0 0 275 1 0.00481301718004468 5.8773390069755544 28.48006270924583 30.89697583588748 0 0 0 1751 1 0.004817539323506273 5.840586790269225 25.23954400145291 30.87928430687442 0 0 0 1712 1 0.004721955366907055 1.1201540124077278 23.619986121574478 29.267379476719327 0 0 0 1714 1 0.004656871414018941 4.228657574436784 23.587049417286025 29.268386938305177 0 0 0 1721 1 0.004787066631620308 1.0716028779919107 26.839774908352886 29.23604298293115 0 0 0 1723 1 0.004656917533164799 4.217949301479565 26.77375834437466 29.34034224937238 0 0 0 1781 1 0.004923038451433109 10.654647611502039 26.755190136464368 35.63324185905143 0 0 0 3952 1 0.0047831153495919345 13.797575539315655 23.654731045522052 35.60376985609612 0 0 0 1772 1 0.004783722442582322 10.559342979755593 23.624617441481323 35.578750807638485 0 0 0 1770 1 0.004627870914840269 7.349678928131817 23.62547504033533 35.62074620914241 0 0 0 1779 1 0.004713948335713047 7.337461772652982 26.78056297886326 35.59830044437185 0 0 0 3961 1 0.004915299747577271 13.818168173818853 26.870593566203574 35.50665961512879 0 0 0 1782 1 0.004791963448546491 12.231953203076262 25.196559491771865 33.957480805738435 0 0 0 1771 1 0.0046452761503899785 8.977048468797623 22.01959529747749 34.106104222365005 0 0 0 1780 1 0.004776413512215572 8.94553833708166 25.171702606331557 34.031996978450586 0 0 0 1773 1 0.004892328341027992 12.303530451027125 22.035265938548996 33.99797054117611 0 0 0 304 1 0.004905348571774508 8.993284711948954 28.36503461352865 34.01421921048884 0 0 0 306 1 0.004862621433957959 12.214668103299237 28.45983378689928 33.87885831986324 0 0 0 1754 1 0.004858599982554345 10.630772231844531 26.720099786896355 32.46786303191028 0 0 0 1745 1 0.004719998619159548 10.577515622240202 23.576844489642536 32.51522607118382 0 0 0 1752 1 0.004790278488626053 7.438408387555657 26.855563937609666 32.43872309391836 0 0 0 1743 1 0.004750319544012409 7.436527166804795 23.615528463236533 32.41019925130844 0 0 0 3925 1 0.0046249487276639675 13.823064788232672 23.59963650104054 32.33387281284241 0 0 0 3934 1 0.004587987989211598 13.880353730486613 26.83950134179562 32.43977937560857 0 0 0 1755 1 0.004745135140254738 12.244723378730333 25.19981062878801 30.8956010464681 0 0 0 1753 1 0.004821820488633539 9.029305866213132 25.13722707281853 30.76768926643885 0 0 0 277 1 0.00477247128512116 9.005533048248703 28.319908576595655 30.78700940023488 0 0 0 1746 1 0.004623193840946364 12.194319235869033 21.99643484653158 30.952082601448787 0 0 0 1744 1 0.004757098365876386 8.993410249227807 22.031593014366337 30.968589224318603 0 0 0 279 1 0.004760524917578817 12.269571076863778 28.39042563894365 30.893780364762897 0 0 0 1727 1 0.004754282711153558 10.665038615380583 26.78341037511062 29.32123491511893 0 0 0 3907 1 0.004680679123649022 13.82116631795142 26.80566467073748 29.222377455665416 0 0 0 1716 1 0.004680324409762401 7.392785631044319 23.569432124046852 29.21956739981828 0 0 0 1718 1 0.004863882942556481 10.70986575337837 23.59272909758504 29.23163712122305 0 0 0 3898 1 0.004737898365228902 13.752678329932547 23.650992002775805 29.28966846680157 0 0 0 1725 1 0.004609114626215171 7.480911925880089 26.77413589333469 29.293064789764653 0 0 0 1128 1 0.004871337048077696 2.6801475526404053 15.681306703357343 43.60490566522831 0 0 0 1130 1 0.004836083430441326 5.929223149484868 15.69731840775807 43.549981498459324 0 0 0 1839 1 0.004722783920595197 2.6884092922620706 18.968572215635195 43.56410370187608 0 0 0 1841 1 0.004859281857390412 5.762214527264253 18.879899327113176 43.6188921111002 0 0 0 1105 1 0.00490399478648243 4.186898688717837 17.31217518763104 41.91716437797464 0 0 0 1104 1 0.004916200259073319 1.0166194143460001 17.271100209229434 41.984179474863886 0 0 0 1825 1 0.004590011130966527 1.0672592441239135 20.508076911999296 42.065058755886454 0 0 0 1826 1 0.004583202785406032 4.2224346421292305 20.522662208880984 41.97220048520158 0 0 0 1092 1 0.004714321165766006 2.6138446556089594 15.584048237688771 40.47658071653614 0 0 0 1811 1 0.004769408308687698 2.6581120095726805 18.902121122775355 40.451009953777735 0 0 0 1812 1 0.0047893166204007395 5.816939039444933 18.88863463091215 40.41372554706487 0 0 0 1093 1 0.004791543663653761 5.8680132851044915 15.670316305942269 40.35409314692869 0 0 0 1075 1 0.004776702840822548 4.212572764194942 17.23158930519653 38.76361773566632 0 0 0 1073 1 0.00484282228945092 1.1255575490171752 17.158608345338713 38.871797276522756 0 0 0 1786 1 0.0046532415498228025 4.2389843519506005 20.388709597365356 38.78601010217959 0 0 0 1784 1 0.004723851661842993 1.0693087925876144 20.49037048620209 38.783243408901484 0 0 0 1785 1 0.004797130284727303 2.565689787787121 18.893765976225247 37.22356941553484 0 0 0 1074 1 0.00471434902723627 2.6508561690846464 15.63649039537665 37.29104579160032 0 0 0 1076 1 0.004779588117388997 5.803447538635538 15.701383963169825 37.19909638322867 0 0 0 1787 1 0.004811501849159579 5.778682135082721 18.841841172457187 37.247074327166274 0 0 0 1843 1 0.0047891590763717296 8.943729830403601 18.780575379100853 43.5550899330066 0 0 0 1132 1 0.0046800359663271025 9.12504169507231 15.663963265074706 43.61130664414663 0 0 0 1845 1 0.004738958219086679 12.220159756601184 18.863336095140152 43.64722597325234 0 0 0 1134 1 0.004699682861101581 12.150080464608097 15.652959691642714 43.64734277622391 0 0 0 1827 1 0.004741517431847746 7.385590700402006 20.41170536016956 42.101221086679146 0 0 0 1828 1 0.004776311794887094 10.56721958315455 20.38965276020009 42.02159791927575 0 0 0 4009 1 0.00501330188031095 13.714500484787408 20.543031024907425 42.053222390566646 0 0 0 1106 1 0.0048445129232648244 7.445150261060922 17.25168621185547 41.91641844911401 0 0 0 3290 1 0.004700412589672914 13.769651375584115 17.271740773773267 42.07184503113146 0 0 0 1107 1 0.004629643063471238 10.652352917991871 17.270550328542136 42.03705968105017 0 0 0 1813 1 0.004767118268276759 9.139074602898242 18.850464630873027 40.38379991186995 0 0 0 1094 1 0.004800723511474618 9.092091253662586 15.637861352271726 40.425786540555244 0 0 0 1095 1 0.00464011852919681 12.215431171728822 15.70047130907786 40.476916835642264 0 0 0 1814 1 0.00463523803510804 12.231511786405767 18.77780676091049 40.44820884919403 0 0 0 1079 1 0.004619946664451325 10.679798726773237 17.240599968474868 38.76638670017565 0 0 0 3970 1 0.004811463053658252 13.815351537904105 20.46832539326713 38.91701399535107 0 0 0 1077 1 0.004795036126405994 7.474203031054683 17.23784640121774 38.8193680778573 0 0 0 1790 1 0.004708730091430342 10.648309819628608 20.408025904411378 38.88211246781464 0 0 0 3259 1 0.004626920883065036 13.74465370519093 17.257252889058627 38.85714178446112 0 0 0 1788 1 0.004920112177754879 7.3922330965274945 20.419898327316314 38.88507479775082 0 0 0 1791 1 0.004770507155050362 12.307722259488584 18.917154128495245 37.28693082260994 0 0 0 1078 1 0.004730366083645176 9.054067462391268 15.66538112964755 37.27760470241035 0 0 0 1080 1 0.004674478377256725 12.158696534889009 15.708440261556705 37.23781278556226 0 0 0 1789 1 0.004763482522752799 8.981440420559064 18.802001438715052 37.23935100476889 0 0 0 1857 1 0.004721634178675006 2.5698212501523447 25.219698062291073 43.5903530462318 0 0 0 1850 1 0.004659023425102174 5.850571676402449 22.04327502349365 43.58946320192646 0 0 0 381 1 0.0046476448198204505 2.616136439198549 28.39481355815373 43.632907655839354 0 0 0 1848 1 0.004761781589557101 2.576873747344842 22.06170678645675 43.57191217484549 0 0 0 1859 1 0.004747264441370904 5.821283873252335 25.261188103954506 43.686189048926124 0 0 0 383 1 0.00464032774736165 5.686369485734527 28.43774259253615 43.58861494076498 0 0 0 1833 1 0.004746586739892884 1.024988463325449 26.802213614946638 41.963399932376866 0 0 0 1829 1 0.004700365428422308 1.0430077512338325 23.71348317152539 41.95351589166083 0 0 0 1830 1 0.004801248142052315 4.232791276480344 23.573520147139508 41.947053683258815 0 0 0 1834 1 0.004786379678426883 4.219656354788085 26.754365688405738 42.00906933693381 0 0 0 354 1 0.004814733914187814 5.804986528047591 28.385945951994813 40.41315710212708 0 0 0 1822 1 0.004674092348151589 5.844909748563719 25.237881928364065 40.44796496817889 0 0 0 353 1 0.004938271712943124 2.6618364715343903 28.338756125784176 40.37877753177898 0 0 0 1817 1 0.004616591836181601 5.924032186459341 22.035357842094513 40.40049197989591 0 0 0 1816 1 0.004593877359972043 2.6750539589277706 21.976819045795324 40.431515863623886 0 0 0 1821 1 0.00478184562136107 2.689965443122737 25.170064352693228 40.401909059959074 0 0 0 1802 1 0.004791805192889534 1.0530252307382884 26.78905612513158 38.77365365246705 0 0 0 1793 1 0.004883432487286661 1.0127094929676899 23.59084323558078 38.7837323223272 0 0 0 1795 1 0.00484363251043079 4.20856978372653 23.56129094044806 38.885187499351396 0 0 0 1804 1 0.0048068486378450345 4.252359547803828 26.82707082631389 38.729902992103895 0 0 0 327 1 0.004714166289545759 2.692280175101188 28.471664864075066 37.16011109250085 0 0 0 1796 1 0.004708961861877662 5.78927143081914 22.126863903858307 37.15888645440053 0 0 0 329 1 0.00465098218275792 5.873391975489386 28.427308469461064 37.269066491225 0 0 0 1794 1 0.004761772136159959 2.741228688407452 21.974029566851886 37.22891945471998 0 0 0 1803 1 0.0047426621585889474 2.5819791552906945 25.31768635978794 37.155428020454764 0 0 0 1805 1 0.004705316363001552 5.788269054966273 25.19854899535724 37.25348173124044 0 0 0 1863 1 0.0047774571984617615 12.10392941170416 25.13774386972167 43.584248289607274 0 0 0 1852 1 0.004620730780677859 8.952592100916538 22.020821017228513 43.593155787849 0 0 0 385 1 0.0048442888274474565 9.01058058001472 28.421071313185788 43.61344867196374 0 0 0 1854 1 0.004867044121385989 12.081369643358052 22.058033233993296 43.688024445585626 0 0 0 1861 1 0.004642748522349147 8.986717922740379 25.235958309447277 43.543155449389346 0 0 0 387 1 0.004818937874430338 12.22460287209075 28.30397447930176 43.60058549342897 0 0 0 1832 1 0.004734881622643726 10.580352395585175 23.64213909283149 41.996740127344204 0 0 0 1836 1 0.004752450870658852 10.602262479171015 26.7562922142317 41.9584348001317 0 0 0 1835 1 0.0047738986607152745 7.390939438216522 26.72892670390564 41.96577728780712 0 0 0 4014 1 0.004776734453017019 13.853979735776365 23.686444436199945 42.00179027055912 0 0 0 4019 1 0.004766359626431389 13.79611399017887 26.779206531674088 41.95937140194476 0 0 0 1831 1 0.004736312200535886 7.421139111011395 23.559520404528584 41.99615020754107 0 0 0 1819 1 0.0047549453239294805 12.164848551632888 22.007348862518302 40.39457611500076 0 0 0 1818 1 0.004782068849438534 9.100831867723153 22.034816233109062 40.37199512697073 0 0 0 355 1 0.004790613261156689 8.950003749418004 28.29096074883724 40.41170217880429 0 0 0 1823 1 0.004701611699361081 9.001227461651876 25.199671855684386 40.372251167858074 0 0 0 356 1 0.004807549737249882 12.155045899050554 28.416017051827335 40.429375826722975 0 0 0 1824 1 0.004890841895087572 12.24238572954695 25.162114186630234 40.42117882165694 0 0 0 3979 1 0.004783190120101807 13.783811810812812 23.602337116450723 38.77928102493132 0 0 0 1797 1 0.004825366988022014 7.375232704450169 23.61960209080031 38.88748884353239 0 0 0 1808 1 0.00473744986934764 10.569886830998238 26.75809694050854 38.77828497883871 0 0 0 3988 1 0.004851173923605045 13.797208625974914 26.92200250197612 38.7397892462083 0 0 0 1806 1 0.00463498931923915 7.368174926836756 26.763957543364235 38.76680328060475 0 0 0 1799 1 0.004759832199576573 10.6273613757242 23.578947300664993 38.74274471458595 0 0 0 331 1 0.004754563985868637 8.97581209266604 28.326793461755827 37.21517590535735 0 0 0 1807 1 0.004810544955775226 9.00945215238823 25.22522438252751 37.168244779232246 0 0 0 1800 1 0.0048239805091879525 12.238460521330879 22.027094984835678 37.159244772878004 0 0 0 1798 1 0.0048476944780852654 9.061760082884753 22.016293273970785 37.1868221633347 0 0 0 1809 1 0.004776164801089153 12.241982737272984 25.187836015541368 37.257169167013274 0 0 0 333 1 0.004743799360046052 12.137141895400246 28.38295423928892 37.229174842023454 0 0 0 1186 1 0.004741090322294628 4.221447505000196 17.252562576179894 51.665759935089014 0 0 0 1906 1 0.004758153765763674 0.9734594404810141 20.501276858169348 51.56299721149498 0 0 0 1907 1 0.004766772222047843 4.182859240569726 20.452656813204435 51.50055215555999 0 0 0 1185 1 0.0048204376939673475 1.053209454492656 17.232450065918627 51.53850814127341 0 0 0 1174 1 0.00491209087274953 5.709064564835619 15.6656860110562 49.95000150577382 0 0 0 1173 1 0.00489806108652918 2.657465392621849 15.611715166360938 49.97540859235876 0 0 0 1892 1 0.004923677495463246 2.6329743083882615 18.80408546389178 49.862352243394305 0 0 0 1893 1 0.004783905566249301 5.710645417307309 18.866135535795546 50.005565347245614 0 0 0 1156 1 0.004679792540530357 4.238812710018321 17.13593246863797 48.367935114312196 0 0 0 1865 1 0.004810396327667511 1.0050810673965187 20.52020741638712 48.366138736283276 0 0 0 1867 1 0.0046985060543745655 4.12276775039209 20.383783008805302 48.3351125645973 0 0 0 1154 1 0.004716050819581805 1.0180864192809158 17.306810817889087 48.31407334708709 0 0 0 1155 1 0.004723471726312996 2.5712940612430266 15.690605537133393 46.77919084526868 0 0 0 1868 1 0.004702267866969652 5.779612757977982 18.89578821870334 46.85973189973891 0 0 0 1866 1 0.004627958008445005 2.5975034997471886 18.833089918223145 46.71060748336556 0 0 0 1157 1 0.004862592524359723 5.766937428450734 15.701162139983738 46.68031476052456 0 0 0 1127 1 0.004630937479965054 1.0488213352052589 17.278044146536928 45.22255658524482 0 0 0 1838 1 0.0046140295665207005 1.0597628417040086 20.401381719859916 45.211570023016925 0 0 0 1840 1 0.004690469890989922 4.242475451140238 20.519651912316036 45.22099626022036 0 0 0 1129 1 0.004807587625867934 4.166327946423202 17.306399586637983 45.1812606526731 0 0 0 4090 1 0.004784703543107449 13.688755093672171 20.521626324920952 51.56092678582713 0 0 0 3371 1 0.004712662599965629 13.700427744727927 17.27442098396489 51.565714502374455 0 0 0 1188 1 0.004746415418875095 10.464974278231075 17.33725113146779 51.52531480710417 0 0 0 1187 1 0.004833430672564094 7.378303210083025 17.333947641573037 51.61620713881617 0 0 0 1908 1 0.004755000648267678 7.405623128981242 20.48540698581027 51.603013873457 0 0 0 1909 1 0.0047721178880766255 10.589103353638691 20.5028709432734 51.56144890239473 0 0 0 1895 1 0.004828155746984891 12.156560667218411 18.85273963225131 50.006136052051545 0 0 0 1894 1 0.0046952361036851215 8.84127007811159 18.944367034999416 50.017103373697005 0 0 0 1176 1 0.004911670340554442 12.051718028174276 15.62244782240803 50.01522104233086 0 0 0 1175 1 0.004874240260363507 8.858705501297107 15.764210588536125 49.95162129670348 0 0 0 1871 1 0.004817168568494087 10.564915081352801 20.399764207771174 48.37609909877328 0 0 0 1869 1 0.004762166753319846 7.33503687610493 20.42523655745977 48.37999858788582 0 0 0 4051 1 0.0048395434355492945 13.718431892473152 20.42808093975419 48.30111769528801 0 0 0 3340 1 0.004725789188419769 13.71193303205861 17.256030678076986 48.37068124834945 0 0 0 1160 1 0.004660682725812812 10.483907638046254 17.24677892580601 48.37743293663328 0 0 0 1158 1 0.004716954000510103 7.355010167270809 17.281589039919304 48.331226583429704 0 0 0 1872 1 0.0046724543370654705 12.112340583304025 18.78463510932807 46.79376646860713 0 0 0 1159 1 0.004669756868757129 9.04604931801352 15.690693565368049 46.70749366569531 0 0 0 1870 1 0.004682849153272011 8.98011648364967 18.808017903726203 46.817561415222706 0 0 0 1161 1 0.004712257791515599 12.09742451271044 15.712308094752572 46.87574575032011 0 0 0 4024 1 0.004796490688496991 13.72767278735409 20.458024682474615 45.21850548560593 0 0 0 1133 1 0.0045729578398826225 10.551667563785614 17.262981418976356 45.19813509328453 0 0 0 1844 1 0.004717530539003973 10.485987357464136 20.463488738145497 45.194108122705366 0 0 0 1842 1 0.004659226585196548 7.4067697396304295 20.478464439078365 45.20240803312107 0 0 0 3313 1 0.0047554460361181414 13.700854410307246 17.286876729975486 45.168341582866915 0 0 0 1131 1 0.004806688102491578 7.379334062281157 17.274153220482393 45.19986945347752 0 0 0 1914 1 0.004703938286016592 0.9023907094488749 26.76314288226336 51.65342072058007 0 0 0 1910 1 0.00485099994294892 0.9636877405097903 23.66112941591653 51.582872059826116 0 0 0 1915 1 0.0046635647787428725 4.146750828136789 26.751972200069797 51.56453818104473 0 0 0 1911 1 0.004787861107994779 4.135752399010235 23.631650087676633 51.57442709870774 0 0 0 1898 1 0.004790868766437705 5.742806833146539 22.096503558336167 49.99822413373511 0 0 0 435 1 0.004649719139538442 5.740285809145532 28.350989407112916 49.96351295870482 0 0 0 1897 1 0.004782655137264552 2.636933718279135 22.099875033141753 49.95216158229246 0 0 0 1902 1 0.004708523529480988 2.6193211572396904 25.276044109901118 49.99273379194335 0 0 0 434 1 0.00471207219564153 2.530820194435679 28.36448706802899 49.9530185385858 0 0 0 1903 1 0.00467613303334668 5.817454725937407 25.194464362477852 50.0216760154907 0 0 0 1885 1 0.004746758348687048 4.202559038673176 26.78225709605114 48.38769802182448 0 0 0 1874 1 0.004794084031932277 1.0579262396849924 23.70640863383922 48.396353428126524 0 0 0 1883 1 0.004588635528526624 0.9691669937907547 26.827952779092463 48.413503052289364 0 0 0 1876 1 0.004851916217433135 4.26346043106608 23.641920940059762 48.38582603525096 0 0 0 1877 1 0.004784363471490138 5.775296754610786 21.968062513268723 46.7575092438195 0 0 0 410 1 0.00473853051982482 5.773332664057164 28.368251763376772 46.793376130651254 0 0 0 1884 1 0.004801127271320479 2.628244530852522 25.317100910889017 46.81308171551013 0 0 0 408 1 0.004883857592699603 2.615026424080145 28.389380761864825 46.77609746501797 0 0 0 1875 1 0.0048351239752980665 2.5793853321042146 22.065381201390768 46.78577123277504 0 0 0 1886 1 0.004761541958899523 5.897824586210751 25.20850424914123 46.786642910381055 0 0 0 1856 1 0.004589132424874808 1.0882893897286312 26.805959281846164 45.14746515136146 0 0 0 1849 1 0.004935128015094877 4.1733481624925295 23.683541240772065 45.163302236397904 0 0 0 1858 1 0.004674719117345634 4.322549952657788 26.809833986761504 45.1507707062134 0 0 0 1847 1 0.004778517320413404 1.005304841198235 23.680096567680835 45.21945599933372 0 0 0 4095 1 0.00474326919636274 13.781971675259225 23.756803066367162 51.58251283629455 0 0 0 1917 1 0.004711221739794675 10.59872984908166 26.79468541623517 51.458111485069765 0 0 0 4100 1 0.004710743365572801 13.770198162874385 26.813846069447862 51.55997915045179 0 0 0 1916 1 0.00469573010850341 7.367343476038921 26.73668324667382 51.57511111328005 0 0 0 1912 1 0.004744888198694038 7.416881465213463 23.647252917052505 51.53679121492639 0 0 0 1913 1 0.004830259858948083 10.508290323104113 23.62629836001924 51.60991300102782 0 0 0 1900 1 0.004935844582884574 12.081574181517114 22.042746862053487 49.995428847115946 0 0 0 1904 1 0.00472480456589517 9.057211657615756 25.2681746448524 49.93015239919205 0 0 0 437 1 0.004679918039876614 12.185398143199038 28.362511632698336 49.96697924659717 0 0 0 1899 1 0.004702656462603297 8.887764826972886 22.060340607717137 49.974640954127146 0 0 0 1905 1 0.0047767385486002945 12.249667104380096 25.209912721420114 50.050201288025804 0 0 0 436 1 0.004805817696341147 8.916336314030206 28.369581206285602 50.01394165509287 0 0 0 4060 1 0.004996321755861136 13.778635086365087 23.615949160657912 48.32725685338672 0 0 0 1889 1 0.0047700356804897485 10.696513466375018 26.860551925349064 48.33580910213603 0 0 0 1880 1 0.004863568442557538 10.530468785646564 23.613203424709738 48.35689522899138 0 0 0 1878 1 0.004784466932230676 7.435897211822325 23.647766661811126 48.385564719723575 0 0 0 4069 1 0.004812803791665293 13.817845213017053 26.80154732503106 48.37000943434903 0 0 0 1887 1 0.00467394569383992 7.354492220401534 26.794142242351825 48.415352517778594 0 0 0 1890 1 0.0048145602150697075 12.099911010550015 25.22932167491836 46.76374640897738 0 0 0 414 1 0.00467991489265185 12.183067599383335 28.4336391775893 46.826255823349136 0 0 0 1881 1 0.004724618477345316 12.125198763646246 22.019724261603635 46.72759401324623 0 0 0 1879 1 0.004659588744626157 9.031688679637803 21.979517995964393 46.794394284797285 0 0 0 1888 1 0.004660375421049311 8.993698959590533 25.26570055551983 46.80552857900877 0 0 0 412 1 0.004841441200180213 8.89949301776208 28.411715180845345 46.83897399026955 0 0 0 4033 1 0.004934724377525193 13.790181371629544 23.666087010559952 45.21099794351074 0 0 0 1853 1 0.004623290963886181 10.470431358726183 23.662211945332377 45.203046718529166 0 0 0 1851 1 0.0047597872202354355 7.386418058537533 23.560367191521404 45.197803714467064 0 0 0 4042 1 0.00488942246550291 13.694921846979627 26.84733281835395 45.1986974985429 0 0 0 1862 1 0.004736174627844208 10.518920414470221 26.802038576228092 45.1798838054433 0 0 0 1860 1 0.004703495695606493 7.467039655141096 26.745398768353365 45.15047407188115 0 0 0 1263 1 0.004879035188886844 2.5009319509567405 15.601707554934782 59.46348440089148 0 0 0 1976 1 0.00482327648382516 5.761750441651214 18.832723261129257 59.604608114994335 0 0 0 1265 1 0.005036446172758188 5.736650741986271 15.59315234544971 59.57976910041523 0 0 0 1974 1 0.004903381520644075 2.529721403703688 18.691481596303152 59.52669192146969 0 0 0 1946 1 0.004610230921835061 0.9838811410636606 20.35978105040899 57.97034631510457 0 0 0 1948 1 0.004757305131867206 4.067074466988674 20.447147178005874 57.923456942764695 0 0 0 1235 1 0.004662196415838191 0.8778841628173658 17.204306919366257 57.92281477267259 0 0 0 1237 1 0.004747907483018293 4.152428586075087 17.26144249249775 57.943443610797395 0 0 0 1238 1 0.004818685322357125 5.676951806199217 15.648473426204694 56.38375873867983 0 0 0 1949 1 0.004859416594495774 5.780407916149662 18.84565837412945 56.380308305450306 0 0 0 1236 1 0.004723495742968006 2.505705274757282 15.61962105315732 56.26876058816282 0 0 0 1947 1 0.004889079283311134 2.5805646481107853 18.852803085600822 56.31831460725304 0 0 0 1919 1 0.004792004390877267 0.9569882397782674 20.461020435408376 54.680979272347 0 0 0 1921 1 0.004870572571261259 4.1801669349093995 20.546897977248868 54.733605611568414 0 0 0 1210 1 0.004789011604717123 4.104488344582078 17.223562643867982 54.7814596061462 0 0 0 1208 1 0.004781879859685036 0.8990974546759427 17.28335284277358 54.719726318423135 0 0 0 1211 1 0.004666625082335814 5.666253530625688 15.721067418175702 53.212010340747156 0 0 0 1922 1 0.00484066615335277 5.752065290415944 18.906822598048276 53.20519648352839 0 0 0 1920 1 0.004881267771044893 2.5346280502130822 18.841001624628518 53.08901154534509 0 0 0 1209 1 0.004678339459370405 2.516178789708155 15.640081614450917 53.21199812015552 0 0 0 1269 1 0.00492958489351931 12.141747360366818 15.564771498024365 59.37479801798196 0 0 0 1267 1 0.004927916857547579 8.857188449157627 15.669370490100718 59.50305934184497 0 0 0 1980 1 0.00500768167117608 12.137119707272134 18.78512571702098 59.52953926556534 0 0 0 1978 1 0.004853014073802175 8.951332530002272 18.844019448964563 59.591402394647055 0 0 0 4132 1 0.004681727772826735 13.739157976056962 20.45614501497595 57.985422852657145 0 0 0 1952 1 0.004924723024238058 10.535787153810292 20.48234270796534 57.95143771986892 0 0 0 1239 1 0.004676044702873262 7.319920735765178 17.288334115205775 57.97636093190475 0 0 0 1241 1 0.005031142402053863 10.457410601718301 17.209127629776606 57.92098438075745 0 0 0 3421 1 0.0047633386006456675 13.681796028373927 17.185684387329164 57.86610903275423 0 0 0 1950 1 0.0048101791745444634 7.33327710582258 20.413464086653136 57.9549920483873 0 0 0 1242 1 0.004723717044372133 12.153509102085305 15.619411595152442 56.32747094744184 0 0 0 1240 1 0.004770056621045805 8.858250833193045 15.623960871038548 56.29585636338826 0 0 0 1951 1 0.004736487449261988 8.900461737292842 18.840415123316287 56.37148971304384 0 0 0 1953 1 0.004924461819041048 12.170855274176093 18.86415582450364 56.30450755880949 0 0 0 3394 1 0.004709896795239326 13.66019052879456 17.24901338577945 54.664484511030736 0 0 0 1925 1 0.004806740650054021 10.590634831241875 20.4859579809558 54.85704160037305 0 0 0 1214 1 0.004788292443180495 10.51247912223508 17.250289858013893 54.73090922766005 0 0 0 1212 1 0.0047325793382741455 7.297550867664752 17.2467986570186 54.72368821294282 0 0 0 4105 1 0.004709993841536942 13.758582977082863 20.430347818159085 54.65903691415576 0 0 0 1923 1 0.004776062442767397 7.431255526440736 20.376892726299133 54.780682578888204 0 0 0 1213 1 0.004697357147022688 8.976964787084462 15.710032354967066 53.17068964875122 0 0 0 1215 1 0.004748576031312127 12.125710753869097 15.650744639032261 53.17320371285021 0 0 0 1924 1 0.004667218068230939 9.036859919621259 18.892133011501436 53.19539956782826 0 0 0 1926 1 0.004705808346156824 12.080251777970165 18.85104104602593 53.10634246414839 0 0 0 1994 1 0.004763235342510516 5.743385627790586 25.17583326252367 59.52055501815105 0 0 0 518 1 0.004858858012234372 5.887772041453693 28.411923670326992 59.567532463768046 0 0 0 516 1 0.00483752249169422 2.6189633322247023 28.459538957045197 59.53407775058366 0 0 0 1992 1 0.0047518296952924165 2.5423678283895104 25.191510239997967 59.55621109997657 0 0 0 1985 1 0.004892321878369171 5.717570716533784 21.995988967851343 59.49527794061364 0 0 0 1983 1 0.004658290354764508 2.5368002277968666 22.005619564931795 59.59144610082851 0 0 0 1957 1 0.004650130337135943 4.104547708132831 23.62060508865658 57.96304839681737 0 0 0 1966 1 0.004788257119741313 4.201102094530562 26.85234116965518 57.97909231399637 0 0 0 1955 1 0.00453413511674601 0.9629260821945921 23.638851924859754 57.993414252829844 0 0 0 1964 1 0.0047643209665354964 1.044138338290138 26.830313458640113 58.01313210008564 0 0 0 491 1 0.004854664967172859 5.784679985176477 28.42379628390104 56.343182818999196 0 0 0 1956 1 0.004801680669092524 2.5473883172654714 22.00155219743062 56.43747402479276 0 0 0 489 1 0.00466967679414473 2.6602270139601036 28.485184711743994 56.35440233210311 0 0 0 1965 1 0.004688880343035617 2.603554069732666 25.178749924195767 56.44425474967476 0 0 0 1967 1 0.004684239984846595 5.736878527200576 25.200008129592263 56.29748248845136 0 0 0 1958 1 0.004939823366203279 5.700173513462895 22.10676332946556 56.36057127351424 0 0 0 1939 1 0.004692953539300061 4.150365316152158 26.775922392502128 54.774797736421114 0 0 0 1928 1 0.0047862961807020425 0.8993258561490933 23.643765008978306 54.83757675406236 0 0 0 1937 1 0.004871880154428345 1.1415541153321895 26.806949986576473 54.82420844780957 0 0 0 1930 1 0.004733065773468196 4.093358397098627 23.680812309368797 54.69531034680646 0 0 0 462 1 0.004756229685969471 2.538384879227222 28.42879510194404 53.14493169404565 0 0 0 1931 1 0.004798229536482297 5.775204248573042 22.069255170889804 53.16501227577104 0 0 0 464 1 0.004878645219305798 5.718210923559295 28.270757419299937 53.06543270389753 0 0 0 1940 1 0.004621220076224732 5.787638534648383 25.265818836904504 53.251184308721406 0 0 0 1929 1 0.004808839925735785 2.621904444560491 21.990511486623234 53.16919355399047 0 0 0 1938 1 0.004635569658038279 2.5525303011510627 25.287116027435523 53.238514196676675 0 0 0 1935 1 0.004841189607855944 12.164788812230162 22.126259547345438 53.229478129079276 0 0 0 466 1 0.00484555252105885 9.002424156185858 28.35949738525586 53.182683085178056 0 0 0 1933 1 0.004764525570926161 8.93544570375459 22.05167198249851 53.248723452469385 0 0 0 522 1 0.004874770255329024 12.194061975188172 28.34192759515716 59.582072704396765 0 0 0 1987 1 0.004928297094357919 8.871136829303191 21.961830967549073 59.55134904688924 0 0 0 1998 1 0.004937159142018716 12.075708584837495 25.168523868128474 59.55635849445051 0 0 0 520 1 0.004971417953780132 8.907347213792802 28.3409925052844 59.59276317455571 0 0 0 1996 1 0.00496538512345999 8.941577075322103 25.168773787359637 59.53448738836084 0 0 0 1989 1 0.004708528778326828 12.142832857759787 21.97710045222061 59.58957768065152 0 0 0 1970 1 0.004803437564129549 10.621277430109938 26.82024540535213 58.033103315797284 0 0 0 4150 1 0.004847258429381579 13.775643891083515 26.79599132755597 57.97199149025913 0 0 0 1959 1 0.004786139273125822 7.3850156966586225 23.716522685738948 57.94900878938251 0 0 0 1968 1 0.00470914900009373 7.374131353342089 26.715985518678494 57.920936165291074 0 0 0 1961 1 0.004752375644031725 10.561057100312087 23.501860669350442 57.862996173745 0 0 0 4141 1 0.004777122273810115 13.742146180302761 23.552297824719425 57.987337113137414 0 0 0 495 1 0.0047188044520962615 12.228656478761115 28.426065176236165 56.326202644003956 0 0 0 1969 1 0.004627170753715104 9.013902248202335 25.2003878009486 56.37189924974936 0 0 0 493 1 0.00470831446037118 8.974094561963586 28.367588178861272 56.36321466232547 0 0 0 1960 1 0.0046871674497477814 8.914982372997862 22.051546384227734 56.38789702200188 0 0 0 1962 1 0.00453001081337678 12.259944108178525 22.019201457620834 56.40406849465896 0 0 0 1971 1 0.004801026124235766 12.118385589309094 25.14377046916502 56.41233167542549 0 0 0 1943 1 0.004801967602741744 10.544743252921604 26.785831442118944 54.78856472921187 0 0 0 4123 1 0.004860399085380985 13.771383832219803 26.852769203940355 54.7659930469102 0 0 0 1934 1 0.00461402793937318 10.529537398847165 23.601286712045212 54.81505513040821 0 0 0 1941 1 0.004771951271326255 7.396875238483054 26.723833552226694 54.763603198889776 0 0 0 4114 1 0.004674338730827468 13.775030897972954 23.625829542280986 54.841443815721135 0 0 0 1932 1 0.004711202525261346 7.3012199207502775 23.630215963016283 54.714447817408015 0 0 0 468 1 0.004754070747227975 12.140631557462832 28.377352133922184 53.09616298591236 0 0 0 1942 1 0.004741779264120347 9.004976947049183 25.19847202781447 53.18568893875203 0 0 0 1944 1 0.00486027265756165 12.15966918527246 25.23103911933369 53.25671025717729 0 0 0 2057 1 0.0007166752662835785 5.743808237697429 18.77268295060414 69.11213585525773 0 0 0 1346 1 0.0029376687178182294 5.723574200253836 15.583065169667865 69.11853805781907 0 0 0 2055 1 0.0038190846638877767 2.487190753627017 18.786351751809605 69.03440316212773 0 0 0 1344 1 0.004604525504531196 2.498732572587007 15.600428314540896 69.07429017924146 0 0 0 1318 1 0.007032542843033042 4.050025986909191 17.237138648433227 67.56763491641726 0 0 0 2029 1 0.006042529143563744 4.151204432199414 20.378204563721834 67.56909770726722 0 0 0 1316 1 0.007811575874190719 0.858567426561276 17.2454625835375 67.47524752383583 0 0 0 2027 1 0.007188600800661233 0.9274644565192403 20.378715932529087 67.48526411977726 0 0 0 1319 1 0.005346137849039107 5.815310821657817 15.72080090160724 65.93249762723683 0 0 0 2030 1 0.0055572366766793516 5.677652802900056 18.915124891257967 65.91351505380604 0 0 0 1317 1 0.004855370350720263 2.5571960632488464 15.613472801696274 65.89711824835739 0 0 0 2028 1 0.004916887545384109 2.601451963616755 18.78252491822259 65.94896799832567 0 0 0 2002 1 0.004354941075372393 4.1106752570677685 20.385743672735902 64.27609672999188 0 0 0 1291 1 0.004088189380358641 4.158452410601332 17.2153759305691 64.29452346367816 0 0 0 2000 1 0.004318368104157687 0.949597881136012 20.368760465703495 64.30361070608873 0 0 0 1289 1 0.003877775915919422 0.9898861250029695 17.217499094833805 64.28591727105787 0 0 0 1290 1 0.004571958685383704 2.554912096071561 15.52130679793654 62.67350700829166 0 0 0 1292 1 0.004591475917474512 5.749264162166384 15.592910925302734 62.780499261371546 0 0 0 2001 1 0.004587036714077826 2.5401901737474 18.739420854385777 62.80106444919895 0 0 0 2003 1 0.0045406582248823536 5.683866148290857 18.78268165775953 62.630015368962944 0 0 0 1973 1 0.005121639120779212 1.0069696764839862 20.45616921789222 61.120534931460924 0 0 0 1975 1 0.004871805601685819 4.0987150628056686 20.456458511216095 61.16290591565447 0 0 0 1262 1 0.0051762191811888635 0.870361932286888 17.149871569048596 61.14489582117871 0 0 0 1264 1 0.005073643587827267 4.025305855325847 17.25222007224076 61.09339976639373 0 0 0 2059 1 0.0020905960140869158 8.855637522134344 18.77569348138152 69.1497925814879 0 0 0 1348 1 0.003117462176552236 8.886356219405796 15.67098963894583 69.1475447349009 0 0 0 2061 1 0.005706002062610214 12.086266117025867 18.8577583480195 69.10521399405697 0 0 0 1350 1 0.004774096879939946 12.072590462440575 15.639536643934415 69.16960329634493 0 0 0 2031 1 0.00368485766217015 7.386326872803379 20.37968557899386 67.60316171814436 0 0 0 1322 1 0.003266542491474832 10.484567380269082 17.334292928147228 67.58321930535632 0 0 0 1320 1 0.004422487536517465 7.316747475270564 17.195922528636334 67.57121509160595 0 0 0 2033 1 0.002691088609496361 10.47419462176906 20.437185315724065 67.58432374337882 0 0 0 4213 1 0.001683101392722864 13.650134002886272 20.440030506949263 67.51296686565814 0 0 0 3502 1 0.0023935840990170175 13.598350562237103 17.219401525308008 67.53998730131663 0 0 0 1321 1 0.005443719391593053 8.903250204347879 15.603073626240368 65.90540678974311 0 0 0 2032 1 0.00577855129899719 8.832431280469883 18.7808408594968 65.88602113681455 0 0 0 1323 1 0.005321371880034575 12.128280229838571 15.705436578087992 65.91019496608527 0 0 0 2034 1 0.005281350703802397 12.042780749586099 18.792540474808845 65.9174361304257 0 0 0 1293 1 0.004680908493978113 7.247608019812192 17.188204778825295 64.21370353151816 0 0 0 4186 1 0.005264601385133044 13.81456399731791 20.40602830749071 64.33198526449958 0 0 0 1295 1 0.0050428484172394174 10.46378916975071 17.261516898792408 64.26710197868996 0 0 0 2006 1 0.005477833336426081 10.530547611385023 20.449993598980118 64.34132965718854 0 0 0 3475 1 0.0051643644529730855 13.73791138211025 17.309487779656774 64.3272438288962 0 0 0 2004 1 0.0049455507736632254 7.233398891909514 20.374342381266914 64.35525316375404 0 0 0 1296 1 0.004605727629617178 12.080413193735765 15.698597059663793 62.72110831328694 0 0 0 2005 1 0.004608634607248804 8.882979867698353 18.848086578055515 62.76854426123185 0 0 0 1294 1 0.004584152323999231 8.922629453760184 15.671269288743286 62.69135584372194 0 0 0 2007 1 0.004622906419829665 12.190039630091732 18.78444497217554 62.79000418214909 0 0 0 4159 1 0.004559230009937536 13.668002702439647 20.45226222380602 61.09348149452866 0 0 0 1268 1 0.0047077445527282345 10.478956746707581 17.264713435145264 61.176736697060555 0 0 0 3448 1 0.004680487501775101 13.658741455899573 17.139126549848687 61.144929451391285 0 0 0 1977 1 0.004560847710961862 7.289703125516705 20.518934968974143 61.17612895306104 0 0 0 1266 1 0.004684821669186221 7.24328947578649 17.279540869237824 61.09398447783097 0 0 0 1979 1 0.004606507017419621 10.519422476692355 20.3779308806078 61.193325076933675 0 0 0 597 1 0.002827943053218372 2.5131612522092666 28.350000330696776 69.01867984879523 0 0 0 2066 1 0.0003979035391164544 5.800261028703598 21.968072423615602 69.1574400643939 0 0 0 599 1 0.000691139638468943 5.721727329910153 28.3750393173357 69.07760154622926 0 0 0 2073 1 0.0034351666921944163 2.532999253530953 25.253955009846702 69.03061997105851 0 0 0 2064 1 0.002813155108929948 2.5665145276172296 21.963666548694597 69.0628626529614 0 0 0 2038 1 0.005585405688098148 4.16867885404193 23.623686339128984 67.59675417683252 0 0 0 2036 1 0.006495906705276144 1.0259223209992978 23.621712691749245 67.51648037952162 0 0 0 2047 1 0.0059277001386601694 4.1834740133854424 26.885811778864895 67.50889041365322 0 0 0 2045 1 0.006425666104140575 0.9746978107429874 26.7760479517435 67.48246772451081 0 0 0 2037 1 0.0051966958481834725 2.604514052255543 22.078683222153487 65.97280031193495 0 0 0 2048 1 0.005431521006701355 5.788365728100065 25.183129396816316 65.94988429620082 0 0 0 570 1 0.005098668205994233 2.5294623899121698 28.4142234504682 65.90301418955836 0 0 0 2046 1 0.004882733180530646 2.638305284014534 25.156995329925287 65.81585009284177 0 0 0 572 1 0.005506540228627819 5.843065473600711 28.321905511419246 65.95640656034202 0 0 0 2039 1 0.005598013804043704 5.723876913872146 21.995343112597038 65.93154814380259 0 0 0 2018 1 0.004297727580871977 0.9775348364981481 26.87585077860693 64.3490141643296 0 0 0 2020 1 0.004522454836301369 4.235535986712229 26.8425657331259 64.35808353116819 0 0 0 2011 1 0.00426253796949148 4.16168526733234 23.56589567945507 64.3533088606197 0 0 0 2009 1 0.004148795461238197 0.9449866663230463 23.658121895510153 64.28106011850899 0 0 0 2021 1 0.004551922973380949 5.681816015246683 25.157056270597185 62.76500524162234 0 0 0 543 1 0.004822979394689723 2.609288206928363 28.40525245542375 62.66570283071355 0 0 0 545 1 0.0046096223826263445 5.825846360861137 28.382911113098256 62.737109137724026 0 0 0 2010 1 0.0046477719679103805 2.5604017759295585 22.036836535508545 62.744770142789406 0 0 0 2012 1 0.004375823370107262 5.70115698550558 21.957681393226242 62.74796269448491 0 0 0 2019 1 0.004740758223558374 2.56045016801546 25.171431562742306 62.76342652859303 0 0 0 1991 1 0.0050631386430204355 0.9830635139597345 26.77224194521371 61.18259317514287 0 0 0 1982 1 0.004800705387050304 1.004713085089957 23.575722116684826 61.14994022609338 0 0 0 1993 1 0.0050339007115390265 4.15415610609127 26.780280310523448 61.112593280700274 0 0 0 1984 1 0.004823450088826266 4.2329320118271605 23.562280077785875 61.167915497113334 0 0 0 2075 1 0.001744499616939182 5.706141477373031 25.257379352078402 69.10733972226275 0 0 0 4168 1 0.004805895740188672 13.74852026515255 23.571066697291077 61.09315326137797 0 0 0 2077 1 0.0017796427956992822 8.912125028050244 25.221495364191437 69.11576243877232 0 0 0 2079 1 0.0022111213467238943 12.052615135439323 25.135437278678932 69.04198397428735 0 0 0 601 1 0.000273063177625054 8.935069217980013 28.458414559232573 69.12973927474394 0 0 0 2070 1 0.003923756606787253 12.024383133648856 22.043666813935346 69.11141549573071 0 0 0 603 1 0.002309647238443114 12.213869884351912 28.388813379426022 68.96322001244756 0 0 0 4222 1 0.0020246781434516935 13.651575410405707 23.582598465030824 67.42675946919815 0 0 0 4231 1 0.004668207393834008 13.721156265679607 26.727415190536814 67.42963222226246 0 0 0 2051 1 0.005089585241976518 10.527712019536885 26.803435715700154 67.50198359369637 0 0 0 2042 1 0.003413684027913689 10.435430182108204 23.52167717946229 67.5300178873102 0 0 0 2049 1 0.005460019919503298 7.3670628496108455 26.760065598704927 67.50627658414474 0 0 0 2040 1 0.004480891778442256 7.256998022533222 23.582738828246747 67.48708404227109 0 0 0 2050 1 0.00568874140022285 8.923785571229558 25.18226202267508 65.88312771169394 0 0 0 2043 1 0.005596255237351789 12.166585405456777 21.970111456893832 65.96172109522594 0 0 0 2052 1 0.0057200544469308365 12.127045017734844 25.18530362607107 65.9554998030668 0 0 0 574 1 0.005599933481626827 8.90681970127844 28.356896636200396 65.89988237785121 0 0 0 2041 1 0.005877443219275344 8.933755640922461 21.97008679562402 65.8951227870727 0 0 0 576 1 0.005500135545052813 12.139587273780498 28.43035075820439 65.93201977731582 0 0 0 2015 1 0.005232740017212646 10.492154470881031 23.585875881531155 64.38524875335256 0 0 0 4195 1 0.005286338425888505 13.765992346067444 23.528666200356852 64.34832945024725 0 0 0 2022 1 0.004601770536745379 7.501664040206865 26.738535442425984 64.23687174236271 0 0 0 4204 1 0.004631728151440421 13.753104765062597 26.770890546265864 64.28523035167595 0 0 0 2013 1 0.004766555826389497 7.267262992860832 23.52476515330058 64.29198658421846 0 0 0 2024 1 0.004801109874544551 10.595367886898531 26.81598504924887 64.31990668820266 0 0 0 2016 1 0.004651469854248807 12.150701757762002 22.032923299744667 62.75689308750366 0 0 0 547 1 0.004439263973012867 8.968787579658455 28.435781752959958 62.742919499734995 0 0 0 549 1 0.004372551101224954 12.265700560139077 28.34446400002982 62.67778794667615 0 0 0 2023 1 0.0045325489247050165 8.945969964808741 25.12187552171765 62.6060038268185 0 0 0 2025 1 0.0045957119833055365 12.116505463155946 25.208683310377733 62.73604231855007 0 0 0 2014 1 0.004510669838524767 8.927780286316603 22.015736450614217 62.68731403772063 0 0 0 1988 1 0.004616500621617432 10.539412669808652 23.56415340693596 61.166216530861725 0 0 0 1995 1 0.004749987239513972 7.203248794777653 26.732580315424723 61.120801940042256 0 0 0 1986 1 0.004616331831998902 7.283460170077358 23.608044862798323 61.167756988404385 0 0 0 1997 1 0.004829670461960365 10.549329371084244 26.773912040357843 61.19231734364972 0 0 0 4177 1 0.004811033513068257 13.779594786219596 26.696604737810116 61.131278191353424 0 0 0 2068 1 0.001709143109425229 8.902332152921176 22.063208120247854 69.24283066896245 0 0 0 1402 1 -0.050114126556947504 4.122307393692694 17.2238987063783 77.0659117942241 0 0 0 1401 1 -0.028959959107334555 0.8809229028707654 17.115971320799968 77.11052798138813 0 0 0 2123 1 -0.0682788826206161 4.092775032836466 20.390281292380976 77.05592918555449 0 0 0 2122 1 -0.023322264588972835 0.9089147907380778 20.366336622025607 77.01200100648926 0 0 0 1390 1 0.0065846236570906 5.585715101087373 15.577122953953909 75.48127584469515 0 0 0 2109 1 0.0007296364141710105 5.667674158112603 18.89125395363109 75.45067276558774 0 0 0 1389 1 0.010358459600256643 2.5202486422590584 15.536044978139099 75.49336242250962 0 0 0 2108 1 0.0150791966272449 2.591247615873033 18.764706613803167 75.46607996638916 0 0 0 1372 1 0.014208733271942518 4.029205015197416 17.166317072308555 73.8367872879288 0 0 0 2081 1 0.008080129176336978 0.9130923730170033 20.364927132696405 73.99831560153572 0 0 0 1370 1 0.01202010344574217 0.8302410571217774 17.194624823893403 73.84880233014877 0 0 0 2083 1 0.01047009520309182 4.077063613571257 20.50707792990336 73.86579388498917 0 0 0 2084 1 0.007962456107533567 5.70781730374651 18.928341422331943 72.2024369081938 0 0 0 1373 1 0.007753546576785224 5.6558567969448825 15.687106934745458 72.25963524477183 0 0 0 1371 1 0.007061159526721726 2.4995944318682506 15.578857313052213 72.25479008829444 0 0 0 2082 1 0.008777993858784878 2.5176504976442464 18.733804554369254 72.27614100651202 0 0 0 1345 1 -6.158101656422894e-05 4.131456624365497 17.22597584096187 70.61949067383135 0 0 0 2056 1 0.0048761482158992 4.123880023301275 20.402891441938728 70.71933817233989 0 0 0 1343 1 -0.003672101281318972 0.9229133510634739 17.211470340699993 70.68493357897259 0 0 0 2054 1 -0.00249475807558433 0.9592665220700546 20.324529588730517 70.71334532132266 0 0 0 3587 1 0.705624249926482 13.948712464545643 17.309087519401558 77.43337058849892 0 0 0 1404 1 0.1581561602767988 10.563223892270885 17.214336259541092 77.27112445809445 0 0 0 2125 1 0.21453533416101106 10.604793804648637 20.449781117461704 77.32193897416668 0 0 0 1403 1 -0.022601150233651543 7.257009460653369 17.313436651919933 76.97279579815618 0 0 0 2124 1 -0.09957700149054477 7.255104752719809 20.468479360552895 77.18896295898186 0 0 0 1392 1 0.09448101471903524 11.998982309900022 15.593165001386826 75.51917947183483 0 0 0 2110 1 -0.0447412434181947 8.91943705343917 18.88060720230383 75.62507530620613 0 0 0 1391 1 -0.04250136385342908 8.830405588804018 15.642247252169174 75.56364084154913 0 0 0 2111 1 0.006715847464110691 12.017980134057817 18.857850987608973 75.52221773681468 0 0 0 4267 1 -0.007362032821705267 13.725891815622639 20.402931138192823 73.99637338595332 0 0 0 2085 1 0.01557283790344508 7.352666235500558 20.438280269040064 73.94947016374782 0 0 0 1374 1 0.006799262228155793 7.318045525743915 17.291513936146643 73.94181645104867 0 0 0 1376 1 -0.015395589590534683 10.488361404056475 17.286512093540676 73.91625758888411 0 0 0 3556 1 -0.020479592530788907 13.51110283348863 17.268408698760524 73.95620720136135 0 0 0 2087 1 -0.0026547588524888123 10.511051624915913 20.464129514979927 73.89561272407686 0 0 0 1375 1 0.005954466028080198 8.882184975427682 15.653468257973431 72.3947244869937 0 0 0 2086 1 0.0046908370607786735 8.877069162041787 18.781069508456902 72.42597402493823 0 0 0 2088 1 0.011213859914555865 12.10681485563579 18.881581384305726 72.29740243939182 0 0 0 1377 1 0.005366094049611681 12.016696660318141 15.632603126662664 72.33319329508709 0 0 0 2058 1 0.012322371478692884 7.369907725176153 20.3706076074186 70.71771334049916 0 0 0 4240 1 0.003830170228885389 13.614045072768668 20.466243272175063 70.66623211277695 0 0 0 1347 1 0.009155613361196774 7.313657002165236 17.295751467881395 70.77456499375991 0 0 0 3529 1 0.0028412803188194655 13.749531144788339 17.29525121060993 70.68041799002712 0 0 0 2060 1 0.009135582718899887 10.534894586753465 20.407635856848366 70.74506645238723 0 0 0 1349 1 0.011175143902156537 10.539096327337578 17.264876739716268 70.70464903212836 0 0 0 4306 1 0.3245592745251929 13.579214773095854 20.46031428478355 77.35568421790072 0 0 0 2126 1 -0.015639828449127646 0.8432891721124643 23.552756024616208 77.09648406526567 0 0 0 2130 1 -0.02474561096146573 0.9319359452604079 26.72414727430622 76.9903421942845 0 0 0 2127 1 -0.05763307643055272 4.07171706446555 23.55385710564538 77.01947949887668 0 0 0 2131 1 0.027212268903887567 4.0163682151507665 26.789522811202584 77.01704962837428 0 0 0 650 1 -0.009790863724410178 2.5258691414308867 28.344601410459223 75.4241334585559 0 0 0 2118 1 -0.0034454724964903434 2.5426889356507005 25.170713614409404 75.41623200851971 0 0 0 651 1 -0.004174830342850336 5.6561482401879815 28.316316703298533 75.48602190164641 0 0 0 2114 1 0.00644914839819416 5.69702379331187 21.942218464927283 75.41819245203938 0 0 0 2113 1 0.005849753278574661 2.5089652418496113 22.124816853460263 75.41680317097804 0 0 0 2119 1 -0.005882935496145689 5.664401194512895 25.14952264251427 75.50835235099787 0 0 0 2099 1 0.00959427768940848 0.9729748662524906 26.810220300355457 73.84333623284604 0 0 0 2092 1 0.011410475634322584 4.157880839308086 23.599996220255623 73.89045074547408 0 0 0 2101 1 0.00970566219387417 4.1270294113746395 26.756555091988915 73.81332025984744 0 0 0 2090 1 0.012767798567374403 0.9407052617361192 23.61597820422499 73.87273157037117 0 0 0 624 1 0.005458874196378258 2.5014635284080766 28.357592533623883 72.19579234321941 0 0 0 2102 1 0.0003940723151320529 5.742428203209516 25.268470295477464 72.2545666811776 0 0 0 2100 1 0.007236856621655083 2.56160920103035 25.1185007945674 72.17311365519423 0 0 0 2093 1 0.0012940854997812359 5.717828848111951 22.034702193777 72.28163920435139 0 0 0 2091 1 0.008176327969207864 2.5720969055555214 21.935762820141797 72.2740351984402 0 0 0 2063 1 -0.0004514443976436529 1.0225858940827732 23.598184061936912 70.65261110761867 0 0 0 2065 1 0.0068615544652837965 4.198400798700828 23.57305712980841 70.66293147449987 0 0 0 2074 1 0.005397292886696176 4.106564506683675 26.750147928477425 70.6197907357395 0 0 0 2072 1 0.0018415330744589713 0.9707095590430805 26.724614988526465 70.71534551730412 0 0 0 626 1 0.008219609561173975 5.720045626345065 28.37056397549155 72.26535546368602 0 0 0 4249 1 0.013104050870028212 13.739060766409247 23.66519592188633 70.64099166940362 0 0 0 4258 1 0.008805782391615894 13.721318377907473 26.861317714280542 70.68364279457 0 0 0 628 1 0.011744360962896175 8.895683220258874 28.41981102970159 72.23309280964897 0 0 0 653 1 -0.006820372379059197 12.162477620940546 28.5190884662549 75.40047824784747 0 0 0 2078 1 0.006807138935887233 10.54733423809395 26.83249706809267 70.70483777916479 0 0 0 2067 1 0.012963128650105966 7.2863436234258865 23.592553723379563 70.72446155283103 0 0 0 2129 1 0.13626888872815252 10.417612963495719 23.68323287441716 77.16938425116003 0 0 0 2133 1 0.039723511192075275 10.589528895960624 26.746016208597414 77.00807088460036 0 0 0 4316 1 -0.042712284799744704 13.695208095676344 26.775680730728084 76.99435169019968 0 0 0 4311 1 0.0504922036402264 13.510720348707961 23.693103207390397 77.15376272806972 0 0 0 2128 1 -0.06749822269862289 7.207674001730421 23.42898924274449 77.02251977870733 0 0 0 2132 1 -0.06559452710240277 7.2796576746184 26.734307675373373 77.0396383489396 0 0 0 2115 1 -0.02748069695154124 8.909305904427116 22.04661250200749 75.57373795133923 0 0 0 652 1 0.0095345095726443 8.91819007301976 28.377826794153943 75.4722850784749 0 0 0 2120 1 -0.029672695977328134 8.880672705438748 25.1621689742563 75.48861394885947 0 0 0 2076 1 0.005705042144680737 7.289543745443641 26.76208980526401 70.68932084248166 0 0 0 2116 1 -0.026609350967617098 12.107583492754461 22.086479631743376 75.45654377630002 0 0 0 2121 1 -0.039407443075464364 12.089870825789193 25.2083177431086 75.44855387655744 0 0 0 4276 1 0.006948281250225364 13.665968323739248 23.68530867387027 73.82917346563836 0 0 0 2096 1 0.0023419553177546504 10.500572673367852 23.656747647175568 73.8303469421264 0 0 0 4285 1 0.011499183246331023 13.644491302118231 26.86428156631486 73.84206854030529 0 0 0 2105 1 0.004488546849186266 10.490327571402716 26.800765138569286 73.78754895108501 0 0 0 2103 1 0.016617681185963303 7.307438016001268 26.77824007154276 73.90294341892267 0 0 0 2094 1 0.005081015606348159 7.402020561996467 23.584123262388946 73.82010325267004 0 0 0 2069 1 0.010242506266770153 10.545527396587815 23.683862005434474 70.78649500374209 0 0 0 2095 1 0.00378802334244578 8.933800823301729 22.043256786642342 72.31320039815691 0 0 0 2104 1 0.006477926747486028 8.919006279433136 25.247467325100693 72.24170250292107 0 0 0 2106 1 0.004706103314655619 12.171393395547925 25.315300530169637 72.26309178850715 0 0 0 630 1 0.007289750750478569 12.110505484892766 28.4925713327272 72.21773368498569 0 0 0 2097 1 0.007846912937192939 12.103895640779648 22.139556181165954 72.31590607448521 0 0 0 4518 2 -0.7515346943873942 5.762919252378709 16.757388184113847 84.85315586081515 0 0 0 4403 2 -0.8083049323211091 0.44695274514700156 19.383356753377598 84.75056106622354 0 0 0 4840 2 -0.7418763313393892 1.2719727496791613 15.144083141350324 84.5870217865213 0 0 0 2172 1 1.5614296208246348 1.9529440688211988 20.678793270114138 84.06987719180653 0 0 0 1452 1 1.5368477265656761 5.883958290218355 15.3078826889344 83.8595716999931 0 0 0 4494 2 -0.6663676227539818 3.3169326488102104 17.506406461891682 83.90216743912642 0 0 0 2163 1 1.652785273144235 4.795403919226169 18.486988927586648 83.9291669018609 0 0 0 4560 2 -0.6926350878259019 3.9994020334870513 15.330294066356629 82.99105885999398 0 0 0 1450 1 1.5159524211170698 2.2345597359036784 15.745386282026649 83.2135460527874 0 0 0 4433 2 -0.7712198647311664 4.9497475105630535 19.747662349061695 82.67285075165802 0 0 0 4393 2 -0.726508451314712 0.8889033301008243 17.335427406345886 82.6913268825441 0 0 0 4501 2 -0.7309254610274627 6.919240418445806 15.3780082295857 82.49288306381513 0 0 0 4624 2 -0.6908463093999567 2.0878356892950807 20.30848602222041 82.3522959231509 0 0 0 4765 2 -0.7997341424977329 5.690047940218202 17.332959821908236 82.24208096868877 0 0 0 2139 1 1.3879616192335686 6.736526761455139 20.59943409613477 81.86184345876585 0 0 0 4382 2 -0.7870883651495297 2.7556354273801964 15.695613832310851 81.13506683473992 0 0 0 2137 1 1.0537616223114004 3.776825648605781 20.364724479262126 80.89523606228137 0 0 0 1426 1 0.91849836002985 4.1097994448275434 16.863924472901616 80.98443243763528 0 0 0 2135 1 0.4385177678066099 0.8696975661169492 20.266858822037484 80.5791141122212 0 0 0 1424 1 0.4162998075853842 1.0100370281043165 17.21687799961411 80.44282010973164 0 0 0 4740 2 -0.7469532718084375 3.237837581634609 18.68433306088494 80.71370632888949 0 0 0 4480 2 -0.7819003740583919 6.036381437421602 20.477537406437023 80.27580970587671 0 0 0 2138 1 0.2918618885935946 5.66706353225694 18.736337188099363 78.83320888213065 0 0 0 1425 1 -0.015690227638150676 2.4848129342877616 15.682809056890756 78.66763918372682 0 0 0 1427 1 0.11957752013544165 5.691817413311042 15.735307539639424 78.79304861846201 0 0 0 2136 1 0.03269066021607904 2.515737164058795 18.739881443775015 78.56641614102408 0 0 0 4755 2 -0.7591390447253397 5.190266589074575 19.270448303086848 85.5307331029523 0 0 0 4490 2 -0.7057264140313262 3.320082043090022 19.903724183771367 84.77148404390557 0 0 0 4426 2 -0.8069334432192506 7.1208796052869605 17.210029308098765 79.77027631651143 0 0 0 1428 1 1.4799082050407515 7.337170941774013 17.35672897562665 81.5053983102915 0 0 0 4859 2 -0.6722454047658886 7.951927995717927 18.741862490854306 85.33663584746482 0 0 0 2167 1 1.6691503821459521 9.682470480341198 19.168647702653278 85.38418676974987 0 0 0 4663 2 -0.6336803808898499 10.136160190823894 15.423062613838294 84.15931580811693 0 0 0 5333 2 -0.6247041917866982 13.07516217200245 20.617059408098417 84.21690998597703 0 0 0 1421 1 1.485377235215766 11.5634934981316 14.454875388788501 84.39386807768972 0 0 0 4638 2 -0.7266429707670796 9.571697182293702 20.57862971652824 83.76123418302546 0 0 0 4617 2 -0.7576531879062285 9.980094884529525 18.459201639009425 83.36690091475938 0 0 0 5045 2 -0.7772158357501832 12.40367186952225 15.977230921966202 83.21121873106333 0 0 0 4606 2 -0.753426959115455 12.456351536264258 15.823468622877295 77.78451684871312 0 0 0 4321 1 1.5726343159007128 13.277348522231298 20.833486323308218 82.46307170206069 0 0 0 1430 1 1.5745444727033617 10.522751540697032 16.989259371437505 82.58041841134305 0 0 0 4695 2 -0.805279632864098 7.986461694887938 19.000557468562075 81.94242550054025 0 0 0 5136 2 -0.7828115333341675 11.52678105133546 19.981804540143294 81.87225252904986 0 0 0 2141 1 1.6923115053372537 9.82302036739882 20.203363259610054 82.01180291535886 0 0 0 4547 2 -0.8080534795580624 9.1107467854337 16.213626029531643 81.8995015296863 0 0 0 4604 2 -0.8013875062823577 11.342818275998336 17.089424793546804 81.03040319963506 0 0 0 4578 2 -0.7338441057108245 8.555123801634453 20.917070672592825 80.55108722413276 0 0 0 4623 2 -0.6707096472695773 10.250529443324838 19.132938225522476 80.09826751716164 0 0 0 4775 2 -0.7399119056215134 12.791006001596891 20.549310693219205 79.96114390254202 0 0 0 2142 1 1.4314886342484723 12.27107450807991 18.825528281564168 79.98764115000978 0 0 0 1431 1 1.2107339006312796 11.946438892502234 15.737733888362948 79.52190165350535 0 0 0 2140 1 0.44281275689316063 8.675643555204513 18.708725401062896 78.92358828448842 0 0 0 1429 1 0.3770259178813833 8.757490664016983 15.662242961189897 78.79785292120381 0 0 0 4455 2 -0.7984150859545424 12.440113096050059 18.454565949725275 78.27047857830233 0 0 0 4557 2 -0.7847721716649783 13.638041448114294 17.826680570064457 81.27808323132187 0 0 0 3610 1 1.688063556452314 13.874489549994719 16.356771539445127 82.3610130258345 0 0 0 5513 3 -0.7177075463635251 13.602596735400132 15.587369865625313 80.33341148120404 0 0 0 5061 2 -0.5743260962467992 4.316945066006935 28.124186651176217 93.38444749402215 0 0 0 4408 2 -0.8501825751762687 0.1394582709736078 27.579302701879715 84.51251756951959 0 0 0 2181 1 1.7423291884821246 1.8856557987643034 23.491864192855246 85.26062695274574 0 0 0 4474 2 -0.7047412723811871 2.7804650972713554 27.205162554247412 85.18067459772905 0 0 0 2183 1 1.6245260987786674 4.2745116867272435 25.98888770714736 84.51018747836902 0 0 0 4432 2 -0.7568413540279104 4.703572349179308 28.198726979057703 84.3602270666524 0 0 0 4394 2 -0.7457005599746663 0.4323282112167869 22.09181734934022 84.34553698250406 0 0 0 4580 2 -0.6900825913684246 0.5683822645787373 24.688141063909416 84.09349915210672 0 0 0 4820 2 -0.764377070968703 3.2256814919382455 24.5821205842797 84.1367636831946 0 0 0 4387 2 -0.7346013239036713 2.4159454324700085 22.583862246652277 83.27054339616816 0 0 0 4707 2 -0.7842398675427593 4.8047164168549905 26.44130921539713 82.844440658355 0 0 0 4795 2 -0.7102753490317814 5.312373301847868 23.58588511200451 82.07069747895282 0 0 0 2146 1 1.583206312249715 3.2413293132566317 23.5726318440537 82.0528490973839 0 0 0 2157 1 1.5258140259265098 6.545593368266901 27.257332618512205 81.87317548156713 0 0 0 2155 1 1.1510182031197365 3.541249457575652 26.858771800822264 81.23322382230414 0 0 0 4704 2 -0.8419290074017847 2.548548201668893 25.11517879769079 81.41781736601506 0 0 0 2153 1 0.7141696374276598 0.7163523569836855 26.40793245777139 80.95138290549355 0 0 0 4610 2 -0.8233822187376882 3.1812413905910835 22.37736456865827 80.8397389747068 0 0 0 4434 2 -0.8003187822024808 6.451507252384724 25.844434299547686 80.86595924820043 0 0 0 2144 1 0.3714987057534341 0.8241958386628851 23.40409957888759 80.52906209537488 0 0 0 4431 2 -0.7353357396065858 4.2498712863615244 26.627441622860164 79.59952366746917 0 0 0 2156 1 0.42050872358106406 5.691949447293484 25.177743890975513 78.82110559556607 0 0 0 678 1 0.3233119679860381 2.565110354938203 28.380087653489586 78.95648081287804 0 0 0 2154 1 0.11320512217347724 2.3933195147234247 25.157203647335017 78.81242559868949 0 0 0 2145 1 0.049431952516711126 2.462483691549809 21.947538083479394 78.72967936443418 0 0 0 2147 1 0.35854390472610786 5.405670043726157 22.081975820426667 78.80321783646757 0 0 0 680 1 0.25096003523276117 5.69523454006484 28.317118988710543 78.84433777253422 0 0 0 2148 1 1.476457382945934 7.001459634990204 23.912468088751986 81.56477240527414 0 0 0 4517 2 -0.7294981446776667 0.7191509303816105 28.518787865488957 80.56639700234999 0 0 0 4395 2 -0.8098733723795511 2.4819316184968616 28.286548789070892 82.24763150765428 0 0 0 5254 2 -0.6726170719269347 5.513789643763151 25.403763265124816 85.62973462289493 0 0 0 4729 2 -0.7703717504724527 7.0315993040807125 23.157056109174096 79.95201417533696 0 0 0 4462 2 -0.7523113902094851 13.719107912634346 23.25896216026064 79.40099357461918 0 0 0 4512 2 -0.7103195342825381 7.388942292001229 21.91897048179712 82.84972710476856 0 0 0 4636 2 -0.5697928685300627 7.519096362908251 22.46465351297984 85.50871093153049 0 0 0 4671 2 -0.623935380878715 10.322220549338805 22.904890983945585 85.19879771377173 0 0 0 4693 2 -0.6571279345946064 12.963862292044693 26.975234191531133 85.35473834279593 0 0 0 4481 2 -0.6274849046655624 10.259385570565852 26.479217364305352 84.72233941151208 0 0 0 2176 1 1.5447952954378141 8.841449311835152 22.522154315454934 84.34617946527587 0 0 0 2185 1 1.5840641814936516 8.783213272289931 25.59918700543411 84.28716467714366 0 0 0 709 1 1.6524913535393915 12.065121398801582 27.566951246706292 83.92303667970756 0 0 0 5168 2 -0.5914593428125039 13.176599123099923 24.513403683455806 83.8831487889999 0 0 0 4986 2 -0.679975357785003 7.366318819002023 26.59275974264518 83.68700121220272 0 0 0 4549 2 -0.8266471926689297 8.272932911623785 23.926981818155344 82.85669661671818 0 0 0 4594 2 -0.7762541410793832 12.716992668599714 26.412633924279138 82.77997561540441 0 0 0 4330 1 1.6404566419352267 13.598994667587393 24.61559024836875 82.18663271253526 0 0 0 4572 2 -0.7560105369486126 10.373723888682038 22.18286329648448 82.0958435117081 0 0 0 4781 2 -0.764878385945959 9.620485831041043 25.67746512059045 82.31174339577417 0 0 0 4760 2 -0.7680389373733569 13.11241464825996 22.532823463699653 82.00434772028548 0 0 0 2150 1 1.3061571347270022 10.227285308683228 23.81314165725134 81.54129098949485 0 0 0 2159 1 1.2843799791640829 9.884994308140682 27.124850700922433 81.14245417224848 0 0 0 4339 1 1.1894601890796486 13.519433098304567 27.655963084822957 81.0510515610251 0 0 0 4605 2 -0.8005890681185676 8.07236387345119 28.02737675199885 81.18429053141656 0 0 0 4672 2 -0.7369378402283638 11.573388585568425 28.190551673045654 80.9836099230421 0 0 0 4440 2 -0.7940556571837115 12.132307715410219 24.584186014042288 81.07546282701243 0 0 0 4583 2 -0.7569333378612597 9.504302253003301 23.765573787448254 79.9231695373965 0 0 0 4628 2 -0.7766997637457502 13.710087264161297 26.408354474620978 79.7859662925105 0 0 0 2151 1 1.2456183060409098 12.170938353787248 22.51380645576418 79.92124418323317 0 0 0 4533 2 -0.7825998136421369 10.315727585765671 26.617320175938186 79.48091238786033 0 0 0 2160 1 0.6427598034832506 11.944046526950808 25.4300573138085 79.01318223573331 0 0 0 2149 1 0.8883107732173618 8.625040706822558 21.97909769306834 79.11170540730865 0 0 0 2158 1 0.3867063254047311 8.578587756934397 25.25175024808063 78.74307869753535 0 0 0 682 1 0.062020235837988505 8.980070138599276 28.45171926576021 78.593405920608 0 0 0 4398 2 -0.7528824227687818 10.911805822185762 22.1855972290901 78.75200537303148 0 0 0 4473 2 -0.6945903276647706 8.258657788435583 24.510972728734888 85.56144919783667 0 0 0 5012 2 -0.5732471857905607 13.849310639103493 22.947947806523466 85.43938896980252 0 0 0 4551 2 -0.7726321644083711 10.226913480730554 28.242246122353876 83.21101561077903 0 0 0 5146 2 -0.6393483803683003 1.0737909080481325 17.90552378392447 88.90641691670066 1 0 0 4421 2 -0.6252576719155107 0.1509095632067077 15.992964717339714 91.2850027851926 0 0 0 4619 2 -0.6554726692397717 1.4537209779458142 14.665327411388684 93.31375029046971 0 0 0 5119 2 -0.5226597599409876 4.323427779156637 16.492475632795706 93.26085955945771 0 0 0 5008 2 -0.5809575167743374 6.49919962297837 15.484811872262357 92.16191848367916 0 0 0 5084 2 -0.6350185026370331 4.589646892552615 18.66891006858472 92.9131590210517 0 0 0 1453 1 1.7272477157914716 6.079228209306486 17.17571890525258 92.2663048677187 0 0 0 1461 1 1.6867127446707684 3.022361954910289 19.31730179968016 92.36738496848884 0 0 0 4585 2 -0.6258566861813283 0.5665768028279674 20.899789333539143 91.62395418319448 0 0 0 5082 2 -0.6430667026898436 1.897241367913082 18.076455673693076 91.66499748368368 0 0 0 4664 2 -0.6399246798011703 6.30971383132146 18.594841204207942 90.63085102036771 0 0 0 4995 2 -0.607751061687778 4.793370580261895 16.415212344925294 90.63816677798056 0 0 0 5480 2 -0.6405728302522534 3.8344821425401094 19.596091358327648 90.84975957007892 0 0 0 1451 1 1.6799259377236437 1.2920041749436402 16.64792441634681 90.13006976716193 0 0 0 2164 1 1.7316722368604265 5.73947858943884 20.058941751947177 89.9016804345973 0 0 0 1444 1 1.7263002027028933 4.755906149132507 15.590454862412516 89.11350083207356 0 0 0 4876 2 -0.6541224696216846 2.68896108182976 15.593402158506896 89.8136267690513 0 0 0 4831 2 -0.5826767138784155 0.9797563931530905 15.538666092049473 88.20552471386495 0 0 0 4717 2 -0.6128464173918389 2.5101874617680897 19.664009361603032 87.23119489173244 0 0 0 4940 2 -0.6062655740998506 4.33354706035879 20.847244167873676 88.3744711771677 0 0 0 4615 2 -0.6876684984590468 6.013621909940254 19.39185387846034 87.86874549372875 0 0 0 4469 2 -0.6162606345321477 0.48676810664266196 20.862162380141772 87.61656770463343 0 0 0 4698 2 -0.6561385763118357 5.351274729944091 16.83976619215157 87.51203915793803 0 0 0 4757 2 -0.6741927987573243 3.656484455097562 15.287783926007146 87.30204807844689 0 0 0 1442 1 1.54075504694828 1.986223810388862 15.33357947815814 86.74862920021079 0 0 0 2162 1 1.7100580644711298 0.9653940376085502 18.82719736828762 86.82743132468094 0 0 0 2165 1 1.6803501609286862 6.455782876733409 18.002778470695986 86.83339976930415 0 0 0 2174 1 1.6888176494491394 4.288599575960785 20.794320915743015 86.60924994514109 0 0 0 4503 2 -0.7112257711123621 1.2526725717149803 17.25546362847816 86.10638983848193 0 0 0 4472 2 -0.5969082285345252 6.8749791028421186 15.858849184967632 88.98648378757183 0 0 0 4974 2 -0.6084872507884518 7.069100643665852 17.95649490867962 93.54134664350386 0 0 0 4777 2 -0.6075911497337166 2.527204100923034 21.358412261962105 92.61935591228664 0 0 0 4407 2 -0.622822113284545 12.381261658434836 15.397279443970483 85.58664487161255 0 0 0 4737 2 -0.6479491192525347 9.995271540027105 20.72218428800925 86.23999380067325 0 0 0 4837 2 -0.6456031518920269 11.090872349910098 18.200831534682894 85.79418905082153 0 0 0 4988 2 -0.5820828273143138 8.603096957785292 20.01672277301514 93.66931636897196 0 0 0 5198 2 -0.617372173174118 13.830298398797522 17.280269798300395 86.03288459546208 0 0 0 5102 2 -0.52245647879845 10.26545097458604 15.495702873529158 93.13937759603331 0 0 0 2177 1 1.713953675638573 9.940236394934205 20.847551925988263 92.79412782044012 0 0 0 4845 2 -0.48891296186625616 10.396288511786926 18.945318197529623 91.85782852718488 0 0 0 2168 1 1.6012491855473503 10.12433054275324 16.828057663353476 91.92714698834789 0 0 0 5387 2 -0.48235617185034596 8.233159396036301 17.262896956277604 91.5532837017459 0 0 0 5166 2 -0.579764885975852 11.283046844064863 15.099750242925152 91.0921417435518 0 0 0 5122 2 -0.5688929120021478 12.242670843925124 17.452340983940772 91.39328957590963 0 0 0 2169 1 1.6554543887377868 13.406512101865435 18.34868578262807 90.34846044471016 0 0 0 4521 2 -0.583212385819205 9.586101497392862 16.03664646580942 89.9429523232223 0 0 0 5072 2 -0.5514642914493112 12.8867661285035 20.04290682186829 90.34070486528725 0 0 0 4635 2 -0.529114331397076 7.177459218346329 20.963571948901542 89.64336094293155 0 0 0 1454 1 1.7737013022185408 8.591285672839414 15.422389179420907 88.58425962686803 0 0 0 4749 2 -0.6320918006452477 12.411941025461212 17.9942109940746 88.47838122971018 0 0 0 4708 2 -0.6438520383812137 10.232583045898194 16.351599025213975 87.44572659263734 0 0 0 4656 2 -0.604261124359975 12.74182040025173 15.426441941090586 88.20322699499374 0 0 0 1456 1 1.7179808500998384 11.950204434200232 16.7566391783553 87.27181917483719 0 0 0 4774 2 -0.5785653417973854 7.97290428085477 17.41467956125199 87.56682724657546 0 0 0 4457 2 -0.6795783876835431 7.956895487705268 14.72779524859601 86.53577712742194 0 0 0 5332 2 -0.5769318750637099 12.701189394418614 21.183499662217212 86.8053670331896 0 0 0 5473 2 -0.19063073539929598 10.382618389461442 22.926610890207833 93.59845408494779 0 0 0 4821 2 -0.50308204457677 13.947287553566783 20.146914394880547 93.73583295719891 0 0 0 4838 2 -0.7251918285554746 13.36536783511472 28.42947026012088 88.3202857619783 0 0 0 4748 2 -0.6505566078233381 11.012950749675866 26.8581664930448 89.73524165972154 0 0 0 4625 2 -0.7336695467009419 2.8159941892362883 22.035873269590986 85.7089463486873 0 0 0 4378 2 -0.6253258003005874 1.0420539370310786 27.067177171190256 93.4467962823258 0 0 0 5079 2 -0.5599911102442521 1.0966734501162212 23.31381833994356 93.82280450578567 0 0 0 5437 2 -0.5943270620487381 6.357866955521926 23.62800359417355 93.0594622265486 0 0 0 5307 2 -0.5709742149284995 2.893333605595428 27.03738909725073 92.26201276852484 0 0 0 5284 2 -0.5829200261356741 3.7754363315002735 23.491856181764735 92.56611729443803 0 0 0 1477 1 1.7309159070347402 1.577033897529153 22.858738581643763 92.16439429808169 0 0 0 2173 1 1.6905293630245875 5.270265475205286 23.667769049960615 91.65224228183017 0 0 0 4869 2 -0.5797939035973 5.0240777117196345 25.70237861974621 91.07455235242345 0 0 0 4915 2 -0.5342350956494744 5.573358859463434 21.6730346531591 91.17649539377562 0 0 0 2182 1 1.698047302039363 3.7593048098453936 27.244980963876113 90.73334464141519 0 0 0 4681 2 -0.5886306679979689 1.7984654876048225 23.78153522539061 90.6790945111029 0 0 0 4798 2 -0.6099865730975859 4.01537276656608 23.242731368055413 89.96895224900152 0 0 0 5023 2 -0.6379920080548597 3.117180158890619 25.770162517652565 89.2065220631872 0 0 0 4766 2 -0.6140837257981939 5.076951967804878 27.528022477954615 88.95295351989972 0 0 0 2171 1 1.7375641103063215 3.022908765993571 24.048369600936642 88.72726418550994 0 0 0 4814 2 -0.5892077820185121 1.539311367808719 23.12865471356217 88.57580442031845 0 0 0 5229 2 -0.6086545600455531 5.202825441613891 23.982818871034425 87.94483097832084 0 0 0 4488 2 -0.6324135136158777 0.2242897896264419 26.794278802868956 87.18383477524891 0 0 0 2175 1 1.748759318344754 6.576824749920387 23.911412098668876 86.88532185521508 0 0 0 4789 2 -0.6751279697338383 2.4017536674178355 24.397894145650138 86.67119761368618 0 0 0 5099 2 -0.6150835782405871 5.227649948831672 22.19997674648962 86.21825922950255 0 0 0 704 1 1.4892014780917489 1.2760708900429665 27.963332296536144 86.33069844788628 0 0 0 4483 2 -0.6249699850751687 0.07426657607408761 23.365712783327112 86.45339121119922 0 0 0 2184 1 1.707756735109395 6.753958659969774 27.526038020116648 88.40990106602445 0 0 0 4778 2 -0.6215929316590427 7.015810222987336 28.00431676424711 86.27807105472539 0 0 0 5135 2 -0.5975778338510155 7.1700710217370265 25.87903032592132 87.76252679823833 0 0 0 5499 2 -0.5732397494913855 14.144949158436152 21.97882713157674 91.91248711159433 0 0 0 5329 2 -0.6107074249912027 11.378997158738901 21.476747474525904 91.33134517409471 0 0 0 2186 1 1.7574316623843829 11.21199733470786 25.66283772458783 91.53021310830054 0 0 0 4870 2 -0.608095232736438 7.110210387375349 23.904631893110952 90.4279365999025 0 0 0 4832 2 -0.5665436801709615 12.027255926031142 23.804976426041097 86.68883444390381 0 0 0 4651 2 -0.6138805312268026 13.42696214061077 26.274024294692534 89.56557885591684 0 0 0 5172 2 -0.6224715263736949 8.883230363195707 21.875811122487843 91.1803010125823 0 0 0 708 1 1.662676493895004 8.253719417044238 28.22875230778762 91.89137484695048 0 0 0 2166 1 1.7132918766076535 8.66397858622999 23.114693431174693 89.95061205230286 0 0 0 4723 2 -0.6159347161594398 9.829687831481317 24.44862332752064 90.13928575777574 0 0 0 4504 2 -0.5927438446224523 9.740321521603851 27.335705627927148 91.5619430518971 0 0 0 4366 1 1.7019855068147431 11.933999285792716 27.43887582027291 88.38331491430125 0 0 0 5492 2 -0.5774441994162608 12.562305065929287 22.550051033169343 88.98179665920907 0 0 0 4357 1 1.7608367846209223 12.830488386255526 22.33145515909527 90.68454661951883 0 0 0 5031 2 -0.6313138339370512 13.66996824045273 28.479927229626472 91.45381199768315 0 0 0 2178 1 1.7743697282696975 11.263143460165416 22.26941630988136 87.109647606414 0 0 0 5094 2 -0.6024589333821966 7.7150409269048374 23.126812717847265 87.96727551601252 0 0 0 5222 2 -0.6491066982460799 8.113082018440407 27.379104360329592 93.45835252748931 0 0 0 7 1 1.7084693004246025 13.738446277670763 27.86104149387557 93.5893448443161 0 0 0 5103 2 -0.5969300720743015 12.647734798385079 26.48888182691905 92.32292196667792 0 0 0 4850 2 -0.6068998342874132 10.187258238123098 22.378292279197197 88.54304272323274 0 0 0 2187 1 1.7754576503908335 13.692604579061815 25.06632415513564 86.00010376388855 0 0 0 4744 2 -0.5782786757769204 10.266622704325638 25.486420095443577 93.03987852967148 0 0 0 4896 2 -0.6005105540818151 12.296570256482147 26.031707164488044 87.38511334823926 0 0 0 5484 2 -0.6500188042090488 12.208556717429044 24.243798268573222 91.4679201361761 0 0 0 5071 2 -0.65656689175007 7.431448477234283 27.43230904538113 90.03616311309186 0 0 0 5178 2 -0.35931846870698236 8.996992948854944 22.635133924217843 93.79185504064371 0 0 0 5435 2 -0.2548875955644849 0.5360034147884182 17.855065160199988 101.69863399007664 0 0 0 4881 2 -0.40817594723560396 4.268587358426301 20.361847486118183 100.22036433453839 0 0 0 5494 2 -0.42114827271899624 4.701736382895925 17.800897324410048 99.20849916723769 0 0 0 4922 2 -0.4457316677780822 6.5765501827470825 20.295732157054108 98.53248150737004 0 0 0 748 1 1.5667793650555417 0.14705219380975368 17.573069351592146 99.4869500226335 0 0 0 1472 1 1.5089067218643357 4.800464629749995 19.58911900923381 98.56261233778338 0 0 0 5157 2 -0.5893924805662584 1.0684360299745128 18.34175515917841 98.14837516669961 0 0 0 5181 2 -0.5512324234390675 5.769861192181998 19.471025442340235 96.34178528631749 0 0 0 1455 1 1.6337137163938487 6.701228095033188 15.620655804642627 96.24291803592995 0 0 0 5260 2 -0.5675088309843465 3.1733759921419216 19.2266518199459 97.02592777582814 0 0 0 5359 2 -0.6009330386834831 6.417858094916522 17.26406197404416 95.82078027444335 0 0 0 5402 2 -0.5514118423317238 4.360878953399437 15.332639963460197 95.83670310533054 0 0 0 4445 2 -0.5740353192894156 0.9807811500505784 20.659164631667203 96.19932079269992 0 0 0 1463 1 1.6035777965007214 1.8349981741568049 18.55252298574913 96.04654785623329 0 0 0 4739 2 -0.6060098784388273 2.0924632722541574 16.551095285556766 95.50853188698504 0 0 0 752 1 1.6422899031621072 3.2246033558090064 15.097242039663032 94.49285622327363 0 0 0 4751 2 -0.25576189009634936 1.8010861054854714 17.89026218225119 101.1013898108303 0 0 0 756 1 1.7039435039722157 7.154634895051856 19.40681367189631 95.19902782580945 0 0 0 2198 1 1.4937429177799513 7.072961291961798 27.63590779476052 102.46306893870025 0 0 0 5113 2 -0.6308782774613105 2.1604865452205715 19.213392018667864 94.43072255589654 0 0 0 5438 2 -0.21700440055513506 5.855529808561495 14.343747598090511 97.9874645273745 0 0 0 5490 2 -0.6221295357883276 6.806365012748889 21.15810687384112 94.86664171867136 0 0 0 5370 2 -0.2818694326704428 6.652082229401686 15.398074101117267 98.44509750452306 0 0 0 5502 2 -0.4472648543417723 14.164030124441634 19.48113517863942 96.42595498585722 0 0 0 4586 2 -0.5355209235328922 10.067559327083423 17.629920510780398 94.05696099228223 0 0 0 5163 2 -0.4945598849049012 11.050682814451768 17.67291480057008 97.34529374901251 0 0 0 5251 2 -0.6333871368249564 8.47349204843758 15.963897122608207 96.25176350511498 0 0 0 3637 1 1.6453323229663612 12.762621470320655 19.9902469727941 95.49633264415434 0 0 0 5444 2 -0.6400672817821043 8.621609853449794 18.687616496028625 95.87062351438993 0 0 0 3639 1 1.6058819972127931 10.193252308681329 17.21787817116903 95.83018179328829 0 0 0 5486 2 -0.569833687071292 11.993786080748809 18.410036017091244 95.29477406452601 0 0 0 5488 2 -0.523688033800488 10.584022904573864 15.232324861587081 95.354736778371 0 0 0 5291 2 -0.255299230684688 10.019681922976487 21.425171698060907 96.88462854837202 0 0 0 5393 2 -0.41811774304201343 11.442073815778743 21.106515481770252 96.76933782961561 0 0 0 5207 2 -0.5574910726738623 3.7578169718051435 21.541610768062714 97.64488669502528 0 0 0 5193 2 -0.4795733861332544 4.155472132922886 26.028737969401558 100.51062288890407 0 0 0 5334 2 -0.5339152065916694 5.992726618709637 25.293497822350123 98.10283093453471 0 0 0 747 1 1.500940556419747 4.263348404777971 26.335333407734 98.788850184689 0 0 0 5190 2 -0.6037976353998997 5.168337642081382 27.84007176888759 98.43030276234157 0 0 0 5303 2 -0.5755254893323706 2.4944249705202166 27.395383182866855 98.4473206924628 0 0 0 4498 2 -0.6443655433590827 3.5842586515536086 24.45911372135717 97.81716514797147 0 0 0 5417 2 -0.559838654038041 5.7927248240252425 22.81403496303554 97.95801161376926 0 0 0 1470 1 1.710290411089476 3.7324923805548975 23.03362633551682 96.7617072661369 0 0 0 4511 2 -0.5979119510550378 2.2808427681014507 22.68973446225136 95.7873247862749 0 0 0 4955 2 -0.547782311371614 3.2344238558129788 25.443561021765703 95.02425704675036 0 0 0 5018 2 -0.603174609915449 4.707070288575212 27.813597456949807 95.64386708720636 0 0 0 4375 2 -0.6243259931208135 5.422229369818838 23.311577999710725 95.51562176100916 0 0 0 3 1 1.652502837919193 2.9793673281393738 27.079179800179517 94.50537723012876 0 0 0 1459 1 1.7522643282956205 0.1887368489584151 22.025316127710195 95.47989273390998 0 0 0 5507 2 -0.4744866945606168 6.4794122927093625 23.409945774689188 100.47136011009253 0 0 0 4908 2 -0.6508167411447274 2.218109554339791 28.079794782320683 95.70192173252151 0 0 0 4968 2 -0.4547135991609177 7.279592339625968 27.733073228541777 100.35569676410749 0 0 0 1465 1 1.5991163178284746 7.069113395552693 23.642202747846884 98.82278013202561 0 0 0 1474 1 1.7480966060443768 7.175189146960111 23.28071082177383 95.09129672240073 0 0 0 5319 2 -0.48986248988267644 11.703118187508124 21.00748235899401 99.86758865248217 0 0 0 2940 1 1.5239365313694933 11.105926305898373 22.183744294492048 98.72293055625651 0 0 0 5459 2 -0.23763897247942722 9.662709089925485 22.614164883829158 100.50851924098139 0 0 0 5511 2 -0.44132587620320773 12.36858057111511 23.37504424993767 98.84536432393502 0 0 0 5365 2 -0.17698726170271198 12.926602822089768 22.388109382910727 95.30040093712942 0 0 0 5506 2 -0.43244652674327966 9.103676577770923 22.879587828673568 99.25942428948193 0 0 0 1483 1 1.691179925377005 9.375229214361557 26.377925259059626 94.86811986495952 0 0 0 5131 2 -0.37880236172997234 8.584366248036753 27.23567673904312 100.81135124331418 0 0 0 5481 2 -0.5889760048789646 8.169503236853664 25.567349430354124 98.90719794209099 0 0 0 1476 1 1.6440192265070372 8.45692179925489 27.309608475358278 98.63193836414254 0 0 0 4716 2 -0.4229716722009513 12.641037139143346 27.339775264194305 97.96495914757045 0 0 0 4861 2 -0.5304196646640302 10.12288623348727 27.55385109043881 98.02115147946407 0 0 0 5271 2 -0.5714484671486975 7.733773416471307 24.944623139434484 94.70731115319371 0 0 0 5132 2 -0.5819916566625938 7.8823389691565495 23.240707484054408 96.74541009765238 0 0 0 5414 2 -0.5515142381071718 8.660465373106895 26.82076058228064 96.35453728208249 0 0 0 5407 2 -0.41463956049464246 10.259721799969677 24.953404912461878 95.35728959337966 0 0 0 5377 2 -0.584794382101337 10.694711955310892 27.8762387818141 95.63900676693521 0 0 0 5475 2 -0.5774607682354278 13.006268031452795 27.468153713919737 95.1773265645466 0 0 0 5269 2 -0.2754772824333234 7.856199892605532 26.137177795553367 104.19946481455945 0 -1 0 9 1 1.6114301295512243 11.977728196503161 28.52235827528821 96.81724002079835 0 0 0 5452 2 -0.3427977156505382 14.164238232562873 21.85266818789586 95.54461976634701 0 0 0 5065 2 -0.47657612908200897 5.405051447563702 27.08997196155795 102.72048017585735 0 0 0 4888 2 -0.28334967447647297 8.860075566939534 26.629686807583862 103.42490930142925 0 -1 0 5317 2 -0.5022226104423482 7.092924123708416 27.985227994003086 97.15597921763055 0 0 0 5413 2 -0.5603995045027406 11.180911929990925 20.751897726380037 94.06531019351014 0 0 0 5367 2 -0.5872277948876946 6.5596032948240195 14.243981092682509 95.03871203108268 0 0 0 4642 2 -0.6219111568412334 0.16564444417993027 28.50360971537968 97.17339301284824 0 -1 0 2234 1 -0.0009078514173417097 15.351928748132295 6.041953437537866 2.1910390321808313 0 0 0 2225 1 -0.0010777914933956419 15.389903171448957 2.9840927858017006 2.173247716305697 0 0 0 2236 1 -0.0012754410514635751 18.522783236995796 6.0174715015659235 2.2117818988146216 0 0 0 2227 1 -0.0009149132695978738 18.564138437421825 2.8033134473537946 2.169065174035498 0 0 0 2199 1 0.015501397160596925 17.01225839671086 4.47095086093332 0.7506095782688816 0 0 0 2201 1 0.016263131663656276 20.188792181427587 4.460809252713246 0.670829113343874 0 0 0 2190 1 0.01584033566196373 16.934297064346403 1.2740149210423293 0.6887048412231358 0 0 0 2192 1 0.016500560603383056 20.173973501952176 1.2959593636415554 0.6376355094521619 0 0 0 46 1 -0.0007237539354689342 28.113684932684336 6.067291466591629 2.141897407208716 0 0 0 2229 1 -0.0012404712540261416 21.706341545639102 2.782123239864371 2.235229526335662 0 0 0 2238 1 -0.0010316987801386886 21.78928031605092 6.022693360302418 2.189584914963446 0 0 0 2231 1 -0.0006272076528550062 24.880239696568577 2.9005576667905273 2.1993432320598254 0 0 0 37 1 -7.35807446761726e-05 28.16366144020723 2.9232797800699806 2.163900794141176 0 0 0 2240 1 -9.86432904463335e-05 24.88057515881498 6.039921819117329 2.1703236211169745 0 0 0 2205 1 0.01584582763988726 26.56081519676528 4.489952314796471 0.6125475276786071 0 0 0 2196 1 0.009706969005264129 26.395462425697843 1.5513648480593631 0.617383729783405 0 0 0 2203 1 0.015908338218352303 23.312663667105355 4.338792429652642 0.7075105525959038 0 0 0 2194 1 0.01485701738121481 23.232045336683207 1.309371865436652 0.6749789321113826 0 0 0 2945 1 -0.0012345089187315418 15.426609127039471 9.183417113648776 2.1552153137100336 0 0 0 2947 1 -0.0008325090121858345 18.594408434482744 9.250012939152327 2.348133640242894 0 0 0 2956 1 -0.0007374555394581898 18.56598181510283 12.416893170929754 2.1316282700537013 0 0 0 2954 1 -0.0014048106065570392 15.394963197290757 12.417897035076878 2.2577563315856755 0 0 0 2919 1 0.015601041762386594 16.958501579009223 10.791724351031068 0.7377611769048465 0 0 0 2921 1 0.015132046618365612 20.150478557887354 10.782152079191686 0.838325936956919 0 0 0 2210 1 0.015434789888332905 20.099375587354977 7.595806545805486 0.7777812174646171 0 0 0 2208 1 0.016366421740512165 17.00679505970023 7.661912962249954 0.6979656107045762 0 0 0 2930 1 0.017071672567474876 20.201299047489485 14.003240254484927 0.6659201931411698 0 0 0 2928 1 0.01670707037677207 16.922072685202675 13.941418413657587 0.6522353607361745 0 0 0 2960 1 -0.0009964321998605441 24.929379900707477 12.380370351341858 2.2449042756266455 0 0 0 757 1 -0.0010717501873762905 28.198147540119706 9.233150468791445 2.121126590034466 0 0 0 766 1 -0.0012030284505666466 28.049181620417002 12.414384718972935 2.0921833131996577 0 0 0 2949 1 -0.0008437149171144007 21.78036677712418 9.204503907643515 2.2219985562359175 0 0 0 2951 1 -0.0007870688783916592 24.99119931152904 9.220772667741285 2.1510414603322277 0 0 0 2958 1 -0.0010794937381296992 21.786823641434413 12.375369546458716 2.23982638197959 0 0 0 2214 1 0.01642357671021963 26.55979696269046 7.697968381502315 0.6550151837502276 0 0 0 2925 1 0.015945048152341025 26.55496015616505 10.866405451885186 0.6585801046093115 0 0 0 2934 1 0.01598759643246911 26.398875676613788 14.04867436532443 0.6742910680261976 0 0 0 2212 1 0.016416904745015358 23.242741474023788 7.675909778277591 0.735756428698621 0 0 0 2923 1 0.016425569811455 23.323052920685594 10.868278092853192 0.7112209171500691 0 0 0 2932 1 0.01547615692215406 23.321354149872242 14.038070196908523 0.7277617880051477 0 0 0 2282 1 0.004547053358859406 20.12900194165773 4.444542505298135 10.09539398386119 0 0 0 2280 1 0.004531784198541874 16.991554595382215 4.414978373543719 10.210862534425278 0 0 0 2271 1 0.004418109039841139 16.91783446901425 1.2982104932884069 10.173153743268847 0 0 0 2273 1 0.004686368609104853 20.051966347978343 1.203415848532228 10.18175950375719 0 0 0 2288 1 0.004427574701019697 15.307887751563161 6.024607833161871 8.55469367870442 0 0 0 2279 1 0.004572761872267354 15.34419125818262 2.85680952349468 8.49741179448244 0 0 0 2290 1 0.004504574908984675 18.565763613917614 6.035655337624034 8.479552889213325 0 0 0 2281 1 0.004427842345418766 18.496742046189112 2.878409212586246 8.547009770038981 0 0 0 2253 1 0.005303903532852448 16.83678385986871 4.433038129062599 6.938748535493728 0 0 0 2246 1 0.005395723418410388 20.06391356887948 1.4343478093351447 6.951101523378299 0 0 0 2255 1 0.005133086648212441 20.174224449451003 4.477225516640645 6.945989816385114 0 0 0 2244 1 0.005401320043459825 16.93902844258715 1.263240773658661 6.883308900356042 0 0 0 2261 1 0.005458007295771049 15.354334114571287 6.0612181480136105 5.3269377790646 0 0 0 2254 1 0.0057461402160529345 18.551802257753792 2.877684524349669 5.354391505156597 0 0 0 2252 1 0.005477344620555545 15.294833565948329 2.912754410615629 5.30229995949242 0 0 0 2263 1 0.005581966023638757 18.587491998331164 6.031400948978356 5.397411623709179 0 0 0 2219 1 0.004084816375078655 20.14000157376017 1.2272999094418453 3.6999534403775134 0 0 0 2228 1 0.003901456502144126 20.151449158817385 4.460458926400639 3.7089393954788754 0 0 0 2217 1 0.0039275668795600155 16.94926063493342 1.2553237176103378 3.6298352702308714 0 0 0 2226 1 0.004121337516987822 16.951427349927318 4.5127793614813365 3.8238022770770725 0 0 0 2286 1 0.004447810837395486 26.575229775132623 4.520682924386368 10.164973757105637 0 0 0 2284 1 0.004542789181747584 23.344477764159546 4.569627850090532 10.181165950825756 0 0 0 2275 1 0.004742513913318961 23.300579079894646 1.251600947442124 10.114385896094959 0 0 0 2277 1 0.004691085481631569 26.507320317605725 1.3096306659535648 10.082600857132345 0 0 0 100 1 0.004461031370309874 28.17808088573521 6.106159631128892 8.604732079068452 0 0 0 2294 1 0.0046562349484268965 24.99423009324876 6.047470287133219 8.574117795019207 0 0 0 2285 1 0.004554015798628982 24.93662879899607 2.9401557454108556 8.550946337049107 0 0 0 2292 1 0.004667355633109823 21.75176972932427 6.0644895670943555 8.454106509760404 0 0 0 91 1 0.004334948687594929 28.08592928349482 2.870322567473772 8.513646798117245 0 0 0 2283 1 0.0046881622343265174 21.792326471691183 2.8837652530615148 8.563289651212598 0 0 0 2259 1 0.005273930145543825 26.61690089002005 4.522136647235242 7.034733946095005 0 0 0 2248 1 0.005289083845333961 23.320869513370702 1.2504031853875128 6.917084772409143 0 0 0 2257 1 0.005329272700789223 23.397221465491825 4.521910058847033 6.895885292326913 0 0 0 2250 1 0.005237081072854784 26.542665101962307 1.368731471420253 6.818793739325426 0 0 0 73 1 0.005587174528999154 28.107030634672665 6.133567033558875 5.384282520809953 0 0 0 2267 1 0.005675901278828036 24.97139599257402 6.072188404188676 5.266652663796238 0 0 0 2265 1 0.005445335695713139 21.714419670437515 6.073070209030606 5.341131975346031 0 0 0 2258 1 0.005718093335842032 24.88109070214767 2.862156196879227 5.2828827117407995 0 0 0 2256 1 0.005474382475055788 21.74916182753052 2.905313963215714 5.344846075248651 0 0 0 64 1 0.0054719532834471285 28.09391185784742 2.9588846666644106 5.2442941934422915 0 0 0 2230 1 0.003972657305460028 23.247121235401142 4.515726193872796 3.7763138771592075 0 0 0 2221 1 0.004243593876327558 23.31155358250618 1.320426952947725 3.786833039747446 0 0 0 2232 1 0.004063132733096166 26.44838762566581 4.510082447306159 3.6714303108157638 0 0 0 2223 1 0.004650901248803331 26.51391118022463 1.284101887849353 3.650582017565723 0 0 0 2289 1 0.004504303967519628 17.017226886890818 7.54507728602422 10.086715028545209 0 0 0 2291 1 0.004594770300847149 20.191785112948242 7.557235706380428 10.151641167890121 0 0 0 3000 1 0.004569135710090523 16.983719981384734 10.906408404792296 10.128679461735963 0 0 0 3009 1 0.004448528765136657 16.97242502710119 14.011745906672683 10.305542853545266 0 0 0 3002 1 0.004482316613805427 20.212756835790376 10.812562871461138 10.186779663620266 0 0 0 3011 1 0.004509457855825669 20.16881738005091 13.886072873108727 10.176032677564846 0 0 0 3001 1 0.004562923272215136 18.64411013614934 9.236475653076491 8.58498825434037 0 0 0 2999 1 0.004626544383675588 15.397902933962074 9.172269588500441 8.514887701428918 0 0 0 3010 1 0.004535750232823628 18.589214419772752 12.38121572707867 8.545705554077207 0 0 0 3008 1 0.004492366033328005 15.442759901062438 12.498518825048686 8.576292880362482 0 0 0 2984 1 0.005308621906635539 20.192188007102896 13.979736662116377 6.943410716403737 0 0 0 2975 1 0.005027957697677365 20.216086709918976 10.708277591963478 6.979194274538675 0 0 0 2262 1 0.005300159685736468 16.922371841394664 7.582255268273354 6.94201885005957 0 0 0 2264 1 0.005142456863806218 20.123158520548433 7.648554292619823 6.940072414193625 0 0 0 2973 1 0.005336591279643999 16.960324529991954 10.782348883293905 6.956973982302339 0 0 0 2983 1 0.005699456133789015 18.62621572500306 12.378859857688926 5.397482114350487 0 0 0 2974 1 0.005513764554927109 18.566227146206426 9.28969368519469 5.370032516451488 0 0 0 2972 1 0.005530329765217279 15.37771816152355 9.243202593207352 5.330053397932854 0 0 0 2981 1 0.005604139077182329 15.420138973018277 12.442820725719885 5.409252409963819 0 0 0 2948 1 0.0038846784990137807 20.15148317749934 10.829928757271446 3.878396876448753 0 0 0 2237 1 0.003981368547951067 20.13044483815188 7.618214203242864 3.7903489833712354 0 0 0 2235 1 0.00395318013807194 16.96719608061236 7.615823105937838 3.7186038110062167 0 0 0 2957 1 0.0038396596030981396 20.207544574468194 14.111145121469308 3.667928566952561 0 0 0 2946 1 0.0039692100827278115 16.92073891836404 10.810161510546614 3.773944652507022 0 0 0 2955 1 0.004190167517348374 16.975624501495847 13.999220315307431 3.7761943737436012 0 0 0 2982 1 0.005105700404147777 16.980351220001733 13.982954398773499 6.987904461273398 0 0 0 2986 1 0.0051469518441755995 23.369081997927456 14.034807223198973 6.97443216987304 0 0 0 3015 1 0.004692984497468435 26.651268676676008 14.056055331212754 10.192597766126894 0 0 0 2952 1 0.004132468038199928 26.54012740841227 10.806454171116512 3.727599172660187 0 0 0 2293 1 0.004559798338325436 23.414698881422733 7.657175785940121 10.148500595163306 0 0 0 2961 1 0.00420123230450797 26.51046216569866 14.004328758643105 3.774036224218016 0 0 0 2295 1 0.004436152905104228 26.569592981339767 7.666232573401693 10.19278459131217 0 0 0 3013 1 0.004553942598776572 23.359292567528833 13.96729176251555 10.072969800853643 0 0 0 3006 1 0.004612237385316589 26.617490670859006 10.925484566659396 10.144534089420853 0 0 0 3004 1 0.004511487134836822 23.295670579298857 10.883346222435183 10.143433489523634 0 0 0 3003 1 0.004418420037753126 21.793055940417744 9.283888888923995 8.551372434494935 0 0 0 3012 1 0.004396714794056048 21.705083949093304 12.405948226613964 8.537332581339816 0 0 0 3014 1 0.004485649828295539 24.984760644522147 12.40234870299498 8.547177992797916 0 0 0 3005 1 0.004555990431570997 24.905650730691896 9.31025490698327 8.53725641835744 0 0 0 811 1 0.0044836963603485 28.177142261488736 9.237826781973716 8.575537176267973 0 0 0 820 1 0.004414766045814193 28.147727987413845 12.417181378376048 8.429139412023131 0 0 0 2268 1 0.005368585434973523 26.532312011044105 7.818025435886927 6.999524334074837 0 0 0 2266 1 0.005443538908625832 23.363071820312495 7.827637999581217 6.918999428536936 0 0 0 2979 1 0.0052307377961770315 26.59990613995903 10.852060979126335 6.8536303690616 0 0 0 2977 1 0.005224877789526546 23.386647898091447 10.940179120745217 6.918125259990615 0 0 0 2988 1 0.005187242023344779 26.580121697563076 14.021799093601178 6.978512447296652 0 0 0 2959 1 0.0038066536263871523 23.367576478763535 13.962089332009432 3.712084787931037 0 0 0 2985 1 0.005522646572181973 21.739030299595044 12.46544174108977 5.287297015927892 0 0 0 2978 1 0.0055928641761121365 24.896110198684138 9.242470544774658 5.307808151363993 0 0 0 784 1 0.0054317641724751994 28.161366193868822 9.227871867773318 5.367889374023623 0 0 0 2987 1 0.005525428812583132 24.971595692658653 12.462257585194994 5.37274228750807 0 0 0 2976 1 0.005458602668952055 21.686302150330096 9.29575163474037 5.328703349221052 0 0 0 793 1 0.005579591331264866 28.1578089508568 12.424637931968455 5.298040238932492 0 0 0 2950 1 0.003988237151836346 23.331150171442225 10.857568311422302 3.7340905904972166 0 0 0 2241 1 0.003941857821468749 26.635770744554378 7.690477531511606 3.7780264265799453 0 0 0 2239 1 0.003821354628037524 23.35811673789744 7.585008722122254 3.7281315957260737 0 0 0 2354 1 0.004739199803518409 20.190878907522364 1.2857462358527647 19.67645619132392 0 0 0 2371 1 0.004790904350264637 18.61942476687007 6.080181296933891 18.042557027178212 0 0 0 2360 1 0.0046827989877697845 15.42982779463932 2.9393380937964886 18.11672972899155 0 0 0 2369 1 0.0046820019568335584 15.435223645437562 6.148150903122206 18.12549197603821 0 0 0 2362 1 0.004660433147222923 18.65504686099391 2.8605275576144593 18.136303483891837 0 0 0 2342 1 0.004758540907405101 20.229263262903867 4.418808705674596 16.4878224276514 0 0 0 2337 1 0.004592850994599813 20.175602783352936 1.2933641574749029 16.47095677381385 0 0 0 2336 1 0.004826940032136462 16.9974616577956 1.3521816962465283 16.48895215818985 0 0 0 2341 1 0.004787888401022167 16.993319607998075 4.502332615245765 16.515605511033776 0 0 0 2331 1 0.004481424830085111 15.433133605150323 6.161824269045082 14.935219270933143 0 0 0 2332 1 0.004758291464763892 18.562432937845916 6.152444007295419 14.887634179190334 0 0 0 2327 1 0.004672064888839103 15.356448893222272 3.02384532464779 14.940684361522699 0 0 0 2328 1 0.004772023657938822 18.58322147676323 2.8864412966390733 14.856429688191819 0 0 0 2309 1 0.005002334439307915 20.21328371580202 4.459014063514602 13.329339655364606 0 0 0 2298 1 0.004913413877449053 17.03731205316841 1.227512784515378 13.320902407826448 0 0 0 2300 1 0.004948653893176296 20.266205456663716 1.2193039702418333 13.340250639827946 0 0 0 2307 1 0.004742129604111694 17.03324817692478 4.439580136687128 13.381246864055187 0 0 0 2315 1 0.004837136623432653 15.38245162611831 6.066562102939082 11.807652867586519 0 0 0 2317 1 0.004914315183201604 18.520554871016852 5.981446446841192 11.738926513709039 0 0 0 2308 1 0.004926637001278206 18.634500490762555 2.808801816537626 11.699652845237194 0 0 0 2306 1 0.004966421387007144 15.421196621746805 2.857542818797619 11.734635028402312 0 0 0 2361 1 0.004724512067261627 17.010622557866675 4.481229211413058 19.681711391144308 0 0 0 2363 1 0.0047654366841463555 20.104832973724587 4.490846240894118 19.628163249398707 0 0 0 2352 1 0.004722709172034411 17.007715932626233 1.2476931621618623 19.657043309192083 0 0 0 2365 1 0.004754340406471769 23.354853602161487 4.441843973320017 19.72452705471387 0 0 0 172 1 0.004739424868552784 28.152872486454086 2.9189874150708324 18.043355429002528 0 0 0 2373 1 0.004731174549809503 21.776053668220367 6.060775389139274 18.024879727732877 0 0 0 2366 1 0.0047632670719238695 25.004194279085258 2.9365886742730223 18.05964893084935 0 0 0 2364 1 0.004722588749240433 21.73609438860098 2.856402614448346 18.130843784227963 0 0 0 181 1 0.004876619716258199 28.25419953328581 6.01133341477011 18.065723531418403 0 0 0 2375 1 0.004980111847848327 24.97920649596269 6.0954442950315055 18.093002954117576 0 0 0 2344 1 0.00461334781166961 26.605353223550917 4.4773230098976295 16.46856732820629 0 0 0 2343 1 0.004682111076672109 23.40431361075835 4.459627661374966 16.562154568914693 0 0 0 2338 1 0.004707504535611598 23.413067216786203 1.2904864452762326 16.51634230040052 0 0 0 2339 1 0.004678375255574298 26.616189304018622 1.2632063743613013 16.461798772044187 0 0 0 141 1 0.004713962430022336 28.152048775377796 2.9099861129739875 14.897203185640652 0 0 0 2334 1 0.004571388649877894 25.07944182311024 6.07511250584127 14.943505587223994 0 0 0 146 1 0.004696454974453035 28.18121734491086 6.090920741797588 14.938459436650552 0 0 0 2329 1 0.004715097916987326 21.82967876445077 2.8222988993946365 14.971133486197122 0 0 0 2330 1 0.004596324951154335 24.954098866578633 2.8965625026217956 14.952837587723677 0 0 0 2333 1 0.004678366342038599 21.795839103724624 6.033225417489738 14.980643040143638 0 0 0 2302 1 0.004748096038442199 23.398715774756205 1.2621754445394464 13.303311142163503 0 0 0 2313 1 0.004768536227232284 26.52307165305296 4.442021715587095 13.31658828174126 0 0 0 2304 1 0.004764828357388085 26.501095798484453 1.2722957548821163 13.337974709296 0 0 0 2311 1 0.004889113502794463 23.425302797910987 4.491526789465627 13.375634022269862 0 0 0 127 1 0.004863247792356733 28.17133350311019 5.984547805267694 11.67313439019622 0 0 0 2321 1 0.004808945638300094 24.956995417885896 6.131967871769517 11.73776384187468 0 0 0 2319 1 0.004967230144609659 21.805715957960615 6.042348836542778 11.721826436579601 0 0 0 118 1 0.0049638271528756675 28.18234437454067 2.8468958339404518 11.701368365523328 0 0 0 2310 1 0.005110719889143047 21.831424439843136 2.8965083375404297 11.716683463329332 0 0 0 2312 1 0.00502975937303847 25.0378144980744 2.896369026668357 11.695614957616543 0 0 0 2367 1 0.0050056078259604845 26.68747706606648 4.389767513493475 19.699953030368064 0 0 0 2358 1 0.004816358380832197 26.65233324761547 1.2202330054156945 19.658653962360322 0 0 0 2356 1 0.004759763237265246 23.415244688456333 1.37071842379261 19.612575844495538 0 0 0 3090 1 0.004682926652667131 16.990799376723473 14.05546894517159 19.69987578858103 0 0 0 3083 1 0.004662328009997333 20.195901477311295 10.868770487849186 19.715531868233338 0 0 0 3080 1 0.004949073997703285 15.380363005690436 9.273936429554565 18.044838344151938 0 0 0 3082 1 0.005020609203077909 18.64579332234508 9.297517050819943 18.110520106947966 0 0 0 3089 1 0.004778974954599212 15.41420148497565 12.525515803509121 18.121902023581356 0 0 0 3091 1 0.004657298507440337 18.644346244334194 12.503747651154432 18.119519452731804 0 0 0 2347 1 0.004788078347404141 20.25017397019393 7.661710216618058 16.44080582682662 0 0 0 3071 1 0.004694239075727693 20.079815323289868 14.022909158954333 16.508343283340853 0 0 0 3066 1 0.004844030939019313 20.139953400898452 10.944534685179146 16.49721255312187 0 0 0 2346 1 0.004618092927809514 16.985174529303297 7.6777106828404165 16.515481992983133 0 0 0 3070 1 0.004723422905411284 16.938762783135893 14.019812778322782 16.50973454036367 0 0 0 3065 1 0.004744498332674391 16.99297236279307 10.918300004603642 16.435865595383458 0 0 0 3057 1 0.004577839186465881 18.6467783696088 12.4166319017847 14.865854169552128 0 0 0 3053 1 0.004771029555184925 18.49176665855148 9.239746891996532 14.966276250992424 0 0 0 3052 1 0.00454155216678011 15.453468604901104 9.28397723981582 14.946427770935813 0 0 0 3056 1 0.004761693891573332 15.479172856780952 12.454300932894123 14.911088635039219 0 0 0 2318 1 0.004922417024239728 20.14195742521812 7.684960653374942 13.303871289222625 0 0 0 3038 1 0.004720172736902794 20.15390322375873 14.010163426609227 13.29193944249943 0 0 0 3029 1 0.004906252986229955 20.221910373264798 10.895861680361229 13.362015990341394 0 0 0 3027 1 0.0048375967950061455 16.963784426591797 10.83465283045563 13.24315660967183 0 0 0 3036 1 0.004771614310997117 17.039539460620052 14.06543113989702 13.320691652651991 0 0 0 2316 1 0.004628293044735658 16.954976916011766 7.644211370316648 13.277093037810237 0 0 0 3026 1 0.004851690897001645 15.459026127840868 9.256539508087904 11.657197576551598 0 0 0 3037 1 0.004771703935888615 18.585596694903614 12.47397195643033 11.766773104805306 0 0 0 3028 1 0.005097644175339358 18.54202455273827 9.189246397387338 11.70649743018967 0 0 0 3035 1 0.00487988072482105 15.377453040378578 12.486855895087349 11.76562096444018 0 0 0 3081 1 0.004869212003684393 16.975460745130547 10.874087913652257 19.723562726251572 0 0 0 2372 1 0.004678226311219044 20.284955372929534 7.622996823138905 19.672922600107054 0 0 0 2370 1 0.004847604318716276 17.092040276426935 7.618340389610662 19.712171490984897 0 0 0 3092 1 0.004670835689389773 20.117757102224033 14.069365191414093 19.63514363450916 0 0 0 2376 1 0.004941483942065684 26.651355848139094 7.689560307735157 19.67326984562871 0 0 0 3084 1 0.0048896815924081155 21.78623352202565 9.245326578911579 18.055611692047364 0 0 0 3095 1 0.005025529278071044 24.94983449571042 12.457145607622776 18.083231762014723 0 0 0 3093 1 0.004859499946983609 21.809359808744475 12.498579145829817 18.053036322939526 0 0 0 901 1 0.004873786011075781 28.10816453155407 12.46355392567492 17.974696866872083 0 0 0 892 1 0.0048958584664709395 28.12656268904811 9.31147937666788 18.153136687557062 0 0 0 3086 1 0.004876392448280496 24.93677733889268 9.221862260270235 18.065022497737655 0 0 0 3072 1 0.004651895546360675 23.36340473311241 14.038182784802176 16.462473613279208 0 0 0 3067 1 0.004793403675495415 23.397509430714447 10.815163917717276 16.494861245089798 0 0 0 3073 1 0.0046668685772657224 26.615923537419203 14.060036890357354 16.488032609414013 0 0 0 2349 1 0.004688100481172124 26.573389459188867 7.6153643904528865 16.45756650543278 0 0 0 3068 1 0.004675512163356148 26.624970444183404 10.767776851680406 16.50252926653536 0 0 0 2348 1 0.004582811240691218 23.42660647705994 7.631569553186298 16.445259717340026 0 0 0 870 1 0.004620082010364873 28.110512324342483 12.451230800011473 14.855695277068456 0 0 0 3058 1 0.004787659455084669 21.865759141911436 12.486573162223726 14.897936288229783 0 0 0 3054 1 0.004772004088439525 21.782808071248194 9.26552508076644 14.81898739134752 0 0 0 3059 1 0.00478767537992889 25.027930946453917 12.419445834430588 14.921780744168528 0 0 0 865 1 0.004679972969350698 28.156320036513538 9.274726855269392 14.841829239603996 0 0 0 3055 1 0.004607497088083201 24.960992989337743 9.236022167257714 14.974945343924313 0 0 0 2320 1 0.004790454720118761 23.37591432035874 7.602765196294214 13.399607970712692 0 0 0 3040 1 0.004869289130418234 23.360883184211215 14.085246542430845 13.253173207592193 0 0 0 3042 1 0.004810918394541298 26.57177865988673 14.08972495422799 13.393074548024902 0 0 0 3031 1 0.00482383930030993 23.425464040097335 10.771065995939331 13.26188769850429 0 0 0 2322 1 0.004783939558232402 26.66221181224673 7.616060725899955 13.25476358157199 0 0 0 3033 1 0.004729208438837047 26.51132906591707 10.811859373585252 13.339018537654345 0 0 0 3039 1 0.0048166684463875845 21.74440784749783 12.402458408486602 11.740365130573721 0 0 0 3030 1 0.004962415438548168 21.799110598420757 9.164840937169101 11.7106439202429 0 0 0 3032 1 0.004962163526116729 24.99347634105903 9.261613223015917 11.769064647379198 0 0 0 838 1 0.004812244555829312 28.15167602474347 9.194091693773405 11.68441319152652 0 0 0 847 1 0.004944444557094993 28.160042494588122 12.446387230276223 11.762455345189167 0 0 0 3041 1 0.0050597032465684675 25.0079901371336 12.422791933393796 11.716405473043663 0 0 0 3096 1 0.004846096057968801 26.565082532126038 14.086540284291809 19.713643782604326 0 0 0 3087 1 0.004837923187964411 26.54829493746619 10.91641884832712 19.75012266547836 0 0 0 2374 1 0.004720326202968408 23.339672335970263 7.679423151396376 19.678477860211558 0 0 0 3085 1 0.004879440014142972 23.30915005938703 10.866226411174535 19.71109695523622 0 0 0 2441 1 0.004685053942692271 15.385168105501025 2.995215616438471 27.646294540623476 0 0 0 2450 1 0.004781999925764514 15.418853964388976 6.1888478314285145 27.568652050487593 0 0 0 2452 1 0.004811633747595266 18.688115855404387 6.144374894119995 27.69149349246171 0 0 0 2443 1 0.004603605803347488 18.727865362789633 2.9242185759394026 27.690517322632378 0 0 0 2423 1 0.0047212780274140925 20.147620154165946 4.50983602678508 26.01498698904388 0 0 0 2417 1 0.004925580091352405 16.99980805529801 1.34082526309559 26.11959607561362 0 0 0 2418 1 0.004812734338278052 20.21608407460298 1.3259639236299077 26.1628670102293 0 0 0 2422 1 0.004836090608030285 16.953029090026586 4.532536828058603 26.14141312261282 0 0 0 2412 1 0.004781021235217394 15.386975640540136 6.086284840703537 24.504574097407957 0 0 0 2409 1 0.004916131248915011 18.64970079607693 2.92540597338717 24.470477379767736 0 0 0 2408 1 0.004862165249886001 15.359461029657028 2.910311354944366 24.464381313157595 0 0 0 2413 1 0.0048886091021974245 18.531962167262574 6.107121091699385 24.477951004086222 0 0 0 2388 1 0.00481183960098823 16.96812304472116 4.466331742068288 22.86322051534945 0 0 0 2390 1 0.004879493871998682 20.141145570406394 4.586281948660625 22.82994708032252 0 0 0 2381 1 0.00483476040431023 20.3180658173904 1.414082969424728 22.900718760349392 0 0 0 2379 1 0.004922828980172591 17.01842494898272 1.257044450594286 22.917997239367722 0 0 0 2398 1 0.0046748574461821756 18.599657885863945 6.108768812294685 21.2407028188065 0 0 0 2396 1 0.004806504095972783 15.357957446817458 6.105189636001201 21.287930599288675 0 0 0 2389 1 0.004832483234691673 18.484314296474167 2.885403257279816 21.292285596199644 0 0 0 2387 1 0.004688951158105201 15.374392050587806 2.955212082458234 21.2590666037314 0 0 0 253 1 0.0047736069344254655 28.119135524966712 2.899424383149914 27.689620095571644 0 0 0 262 1 0.004884392858980355 28.1415392341929 6.074243643268367 27.691700559542234 0 0 0 2454 1 0.004736856020410204 21.80525858957324 6.095774971115983 27.618016885303092 0 0 0 2445 1 0.004774553058058736 21.788767055278615 2.9246132786613273 27.726454436147787 0 0 0 2447 1 0.004855345561872098 24.887538742179302 2.9682214891324463 27.663712576166994 0 0 0 2456 1 0.004866376350788218 24.944124786074273 6.069370913697047 27.53298527840852 0 0 0 2419 1 0.004810093980908391 23.415603307995394 1.331437776100782 26.022588917279545 0 0 0 2424 1 0.004687420261294451 23.379999775377886 4.551852080071154 25.998228410076976 0 0 0 2420 1 0.004858296873556479 26.564634411297238 1.3703952589844386 26.145751481951383 0 0 0 2425 1 0.004781772401485316 26.561399173391756 4.351727009304007 26.09367589012582 0 0 0 227 1 0.00475195016646349 28.26980379940716 6.080605175508109 24.495625003353176 0 0 0 2411 1 0.0047421593670781345 25.021116588437813 3.0156952341048315 24.461560186858247 0 0 0 2410 1 0.004770762956834044 21.79916609591057 2.911993603295107 24.492561008860182 0 0 0 222 1 0.004793877152425291 28.19859695083408 2.9042121753347807 24.359884206233332 0 0 0 2414 1 0.004788234521835659 21.71815385780221 6.1104747543215625 24.50705129701395 0 0 0 2415 1 0.004777100393146777 25.030848442552962 6.202130835966367 24.375357246741313 0 0 0 2394 1 0.004885469466544673 26.518056274721975 4.582305617972134 22.873202223860787 0 0 0 2385 1 0.00490374527778472 26.58084340131728 1.323674718184341 22.90482087099188 0 0 0 2383 1 0.00478310883897665 23.44820845152328 1.3676679995463217 22.913711239548213 0 0 0 2392 1 0.004811460933198444 23.327074407384735 4.583375363914715 22.849596571279868 0 0 0 2391 1 0.004810592154942225 21.808429917064267 2.9060651614702033 21.300202781541195 0 0 0 2400 1 0.004713923576455574 21.78933921626352 6.08594533750839 21.223945910622838 0 0 0 2393 1 0.004845160640548633 24.944279982722854 2.8282124442288903 21.235348821849822 0 0 0 208 1 0.004901159669358503 28.158307170116952 6.078388885795632 21.36004498384462 0 0 0 199 1 0.004700994254393749 28.234821129931976 2.8539487295806243 21.269165372799097 0 0 0 2402 1 0.004901360779902865 24.900494573199197 6.09229569365977 21.246883529923302 0 0 0 3172 1 0.004916290302270485 18.71203398115783 12.520960202825338 27.635684825822747 0 0 0 3163 1 0.00483866109338842 18.615963147965168 9.335422523805978 27.650766093418166 0 0 0 3161 1 0.004679015280575143 15.38584778473145 9.329190868083218 27.69430474873795 0 0 0 3170 1 0.004789382490035108 15.434986419752303 12.452485965306519 27.62137322553939 0 0 0 2427 1 0.0047965788382523245 16.956400570688256 7.7287817641017496 26.05837902915777 0 0 0 3147 1 0.004648086384178346 20.22688217622925 10.908645219128747 26.050252585890735 0 0 0 2428 1 0.004786517039249153 20.238462896837184 7.752871512531427 26.079909116914735 0 0 0 3151 1 0.0048070010093224196 16.969993147174787 14.054941219123224 26.074317842548236 0 0 0 3146 1 0.00476097443019231 17.000877256142807 10.84576091563988 26.020193605986545 0 0 0 3152 1 0.00465121330339802 20.25217657494353 14.137736238284372 26.067169161335958 0 0 0 3134 1 0.004802223715646087 18.66016528979242 9.328253486935914 24.431796110089056 0 0 0 3138 1 0.004818515560825088 18.561354001873735 12.49073259046814 24.501983222005656 0 0 0 3137 1 0.004624546413898924 15.43991184752964 12.484578299793306 24.520659145387025 0 0 0 3133 1 0.004602729023263176 15.428779857937663 9.289237773063316 24.471078946977638 0 0 0 2399 1 0.004773582395188207 20.19755071623866 7.758960460019215 22.860305368892213 0 0 0 2397 1 0.004898731339826962 17.058117522029168 7.698250260893488 22.88272005437606 0 0 0 3110 1 0.0047294552930025845 20.147649162611273 10.864145399858105 22.851110593154104 0 0 0 3119 1 0.0048804788534713255 20.171744524464312 14.056936935497818 22.91325666411694 0 0 0 3108 1 0.004746826703180723 16.919325225678108 10.926493100582759 22.83941890856017 0 0 0 3117 1 0.004916848623601316 17.08876104429167 14.03027530834696 22.87364282620057 0 0 0 3109 1 0.004721399704950771 18.65771917487937 9.245938583702394 21.190261265835293 0 0 0 3118 1 0.0046629048329666235 18.594429583347843 12.396098234672571 21.232633946427352 0 0 0 3107 1 0.004720149661177047 15.412420266850386 9.275229898193203 21.336100219501002 0 0 0 3116 1 0.0046584812093103944 15.41108483948193 12.463283059564839 21.22992775109777 0 0 0 3094 1 0.004844309434573023 23.30614730220771 14.14753366950795 19.683725043164305 0 0 0 3153 1 0.00472643136151058 23.332480877089314 14.059349336275565 26.098032581097197 0 0 0 3174 1 0.004736031978693342 21.679642464006236 12.52895672042086 27.73200203114595 0 0 0 973 1 0.004698012322785834 28.159243854858758 9.30230971661782 27.652930788593824 0 0 0 982 1 0.004850033787732617 28.182178910372105 12.57402163519739 27.656034158018 0 0 0 3167 1 0.004779244030758013 24.93289023101659 9.334050716171452 27.644300176997977 0 0 0 3165 1 0.004740261831773085 21.74960318000617 9.32574130900813 27.63713451050968 0 0 0 3176 1 0.004899308655423243 24.955387499504425 12.46288879804332 27.733819252700222 0 0 0 3154 1 0.004914728788292721 26.519828313344583 14.073949447270142 26.044920643025474 0 0 0 2429 1 0.004843642368597623 23.408166968898698 7.641418961768699 25.920171385491734 0 0 0 3113 1 0.004766912755363265 25.023951721036678 9.308074574607286 21.273425211800514 0 0 0 2430 1 0.004888932041814101 26.61526413390808 7.769764739690985 26.03011509125847 0 0 0 3148 1 0.00488105638689061 23.361726207488562 10.916238397183472 26.120804701850666 0 0 0 3149 1 0.004878677795652327 26.59689083166293 10.810777545415844 26.04167360465275 0 0 0 3135 1 0.004730772860494449 21.752444730309406 9.321144419955932 24.41490565978308 0 0 0 951 1 0.0048998880119424035 28.22416639374871 12.447354675035385 24.45683171538726 0 0 0 946 1 0.004616715228284739 28.204239642943943 9.231719410400384 24.469885648475806 0 0 0 3136 1 0.004723256113957863 24.967941775937415 9.387171543860907 24.41137664033354 0 0 0 3140 1 0.004861310300797686 24.92393952596411 12.505215050982597 24.48253847022468 0 0 0 3139 1 0.004766658100877076 21.793897209954267 12.445943849536743 24.486441734567737 0 0 0 3123 1 0.004795679122285101 26.613315341899792 14.038972551480112 22.846917547618208 0 0 0 2403 1 0.004652611411373346 26.542718503660982 7.772418340134902 22.9093362207878 0 0 0 3121 1 0.004774616492438382 23.380532779394002 14.032920921997572 22.8842203908384 0 0 0 3112 1 0.004756171633710187 23.320182082599636 10.95628017463568 22.81128769072253 0 0 0 3114 1 0.004808702736128337 26.608324093286402 10.845245039866155 22.87996263490779 0 0 0 2401 1 0.0047441040018358655 23.37967054409296 7.783248741324544 22.811751129801273 0 0 0 928 1 0.004738404740263512 28.170224964066534 12.439535776578829 21.24826537238809 0 0 0 3122 1 0.0047845495414153075 24.985362795093017 12.56288988868089 21.29586198816943 0 0 0 3111 1 0.004563912327764529 21.841866101771647 9.299151074702962 21.258011619341566 0 0 0 3120 1 0.004763535579056325 21.708501331974023 12.516479928748144 21.227508661589766 0 0 0 919 1 0.004742395646661842 28.173384883768215 9.201620314217257 21.235269731514283 0 0 0 2489 1 0.00485621280904466 20.123854370049585 1.2837385177269887 35.55212481117581 0 0 0 2496 1 0.004883926016531731 17.019133676593658 4.432379422859434 35.6667787383995 0 0 0 2487 1 0.004666641548618535 17.00015530950804 1.3400034143654938 35.59379559562899 0 0 0 2498 1 0.004735500547037799 20.202600983448118 4.528313117248862 35.737475762779894 0 0 0 2495 1 0.004662629226693273 15.416516781751366 2.9050237001974115 33.998488655985824 0 0 0 2497 1 0.004697765065755619 18.637492895905112 2.8863530823145234 34.01827015201944 0 0 0 2506 1 0.004834527771778379 18.646485554447906 6.063000306888293 34.06466169301417 0 0 0 2504 1 0.004880802237687824 15.490923179035054 6.160741610350432 34.105148415546175 0 0 0 2460 1 0.004692601967418197 17.01820519831141 1.3760409880038662 32.430762219047885 0 0 0 2462 1 0.004702351708394559 20.20960511631355 1.328231873901906 32.394603890804284 0 0 0 2469 1 0.004876374119780367 16.959773401620406 4.44611887762925 32.452811503526945 0 0 0 2471 1 0.004812252040578098 20.173962375178476 4.541204065661504 32.48491129852693 0 0 0 2479 1 0.004863569982447425 18.594532597561336 6.112013641778784 30.755893259435982 0 0 0 2468 1 0.004735126985545235 15.441838651595935 2.9651950640071885 30.81145071618304 0 0 0 2477 1 0.0050760786668228985 15.432582361535795 6.1410842702365755 30.794353550336595 0 0 0 2470 1 0.004754104747982461 18.60413785586573 2.9441221114912772 30.865801605102376 0 0 0 2442 1 0.004749415607642887 17.094366364260587 4.458838894826175 29.145557168881847 0 0 0 2435 1 0.004662036781063769 20.253104173846257 1.3498311893217612 29.310268030275793 0 0 0 2433 1 0.0048771051446336085 16.996427383275808 1.3267362283243862 29.206977440069792 0 0 0 2444 1 0.004609866579625208 20.17449671055129 4.4853260518472124 29.20266689422151 0 0 0 2493 1 0.004701102996099122 26.608870148340856 1.2601480199574546 35.662503637431804 0 0 0 2502 1 0.004824592362002915 26.559912505401265 4.472536182959645 35.66526794507681 0 0 0 2491 1 0.00472870122609966 23.42146999335554 1.259554420803378 35.63423199815013 0 0 0 2500 1 0.0047220985320585804 23.367016098804314 4.448777240734098 35.64555910292796 0 0 0 2510 1 0.004801830231762351 24.977774941677513 6.042604330749834 33.92377399089086 0 0 0 2508 1 0.004757413915051507 21.74714810387379 6.036788776104964 34.05790492539213 0 0 0 307 1 0.004767328849951463 28.180619620853893 2.915658752966862 34.0374164697075 0 0 0 316 1 0.004734060489320145 28.09328703386511 6.10937998340694 34.08083314548657 0 0 0 2501 1 0.0048350219167345755 24.96972998266554 2.93808546996932 34.125879352651964 0 0 0 2499 1 0.0047969523884466795 21.78815689006149 2.9151114664725886 34.0885967797486 0 0 0 2466 1 0.004833028516851551 26.620132603125978 1.3283905775373714 32.47933086195437 0 0 0 2475 1 0.004711301782979269 26.589439453801646 4.549963742576231 32.4195299850812 0 0 0 2464 1 0.004881261592848135 23.3499695313302 1.3423417129868926 32.431312186075395 0 0 0 2473 1 0.004707546259811969 23.373237286880293 4.4853387238175735 32.45592124254681 0 0 0 280 1 0.004899247440833938 28.254201354364287 2.8704835957991675 30.92635823522474 0 0 0 289 1 0.004937102786215827 28.13051112591822 6.149848164895347 30.861091833884704 0 0 0 2483 1 0.00477976607668577 24.964360676217737 6.121145173552401 30.920083056936726 0 0 0 2472 1 0.004729812088635691 21.793322319839927 2.934144711664925 30.88044878173332 0 0 0 2474 1 0.005021394997017264 24.97566845879684 2.9335945102367686 30.892868818089646 0 0 0 2481 1 0.00494506978835544 21.725973276819243 6.1341127071325054 30.846158561828176 0 0 0 2437 1 0.004811208472765642 23.35511406807473 1.28939740839873 29.311592594467232 0 0 0 2439 1 0.0049215894682289405 26.623681578634358 1.1693600888704376 29.327282335974168 0 0 0 2446 1 0.004817479303521263 23.356491379890297 4.599349166970123 29.232223314944616 0 0 0 2448 1 0.005016081073927455 26.54258920043593 4.495598566701178 29.26060139732354 0 0 0 3227 1 0.0047681933994612735 20.127259049813333 14.130253409809754 35.64517770185859 0 0 0 2507 1 0.004789376855010671 20.27909079569903 7.664645976430033 35.688129403935825 0 0 0 3225 1 0.004819466328395729 16.912909373493527 14.130705117687473 35.70710701119424 0 0 0 3216 1 0.004993805529335824 17.006840014442922 10.877333615123437 35.70940505816719 0 0 0 3218 1 0.004843925062579605 20.23785760282388 10.897372715938069 35.733714736372555 0 0 0 2505 1 0.004736834816703736 17.021373949590775 7.6863106477197105 35.64878201872231 0 0 0 3226 1 0.004838789024358721 18.565157671939414 12.519822106372487 34.126222274278135 0 0 0 3224 1 0.004836114098100069 15.33502187346666 12.51203702247578 34.001099842002894 0 0 0 3217 1 0.004861306818197667 18.57733551082271 9.289320662873077 34.12567649438334 0 0 0 3215 1 0.004752656531513889 15.37168735308437 9.247412450998507 34.08721615325108 0 0 0 3189 1 0.004820073584975484 16.97432059453019 10.95548229429346 32.496419745998594 0 0 0 3198 1 0.004658104127789069 16.966238187559924 14.101867174247225 32.47326737495306 0 0 0 3191 1 0.004842615211748766 20.134658202085355 10.97338644344477 32.50995084230994 0 0 0 3200 1 0.004778733141087753 20.192173581425394 14.162246771348284 32.52896558603899 0 0 0 2478 1 0.004858509277478171 17.12799548428455 7.718436001510629 32.47398629406492 0 0 0 2480 1 0.004760270736237129 20.18909774160905 7.752937048963651 32.494723516145704 0 0 0 3199 1 0.004742505769839636 18.643581488575155 12.509213125887323 30.87928507753888 0 0 0 3190 1 0.004694565838663865 18.53945659819787 9.300416242006504 30.825629141442274 0 0 0 3188 1 0.004694363230787474 15.470949202138128 9.308098563941272 30.86411926269219 0 0 0 3197 1 0.0046742168382632315 15.534497228742358 12.48117485076164 30.89661618811378 0 0 0 3164 1 0.00467026354444393 20.185481117121537 10.796263796364418 29.30854327803271 0 0 0 3171 1 0.00478292729151319 17.096989375792784 14.037823315483106 29.28825254155775 0 0 0 3173 1 0.004657451738336604 20.263600215900386 14.033778733998687 29.330473567800897 0 0 0 2453 1 0.004598471703017151 20.190734757132343 7.802251263310934 29.29360575074304 0 0 0 3162 1 0.004790952406323224 16.948023818489226 10.911661452022356 29.261501312809596 0 0 0 2451 1 0.004710020466402327 17.03007671414566 7.700966691368134 29.253869568869543 0 0 0 3222 1 0.004799850043951488 26.582799153875552 10.875310928061294 35.59416350417841 0 0 0 3229 1 0.004633796283506365 23.38686344983482 14.019382343864809 35.64681737307858 0 0 0 3231 1 0.004765084080025451 26.506915432234244 14.020925344380776 35.68678098132374 0 0 0 2511 1 0.004819842383267542 26.535081629223043 7.619900199313635 35.61893427623396 0 0 0 3220 1 0.004782153977542015 23.392535494206296 10.887009301067742 35.70572490531239 0 0 0 2509 1 0.004894146041900192 23.29133871547098 7.665860608257502 35.61368918950548 0 0 0 3228 1 0.0048944696388020185 21.774070804790995 12.509880612282046 34.1222264089223 0 0 0 3230 1 0.004725688145549545 24.969204998727708 12.456710224043254 34.11864451518147 0 0 0 1027 1 0.004923375091503715 28.22964980926685 9.283262482096266 34.15043756330298 0 0 0 3219 1 0.004769275882057651 21.69811040710449 9.283857195292043 34.08649188688787 0 0 0 1036 1 0.004770313289814773 28.145076592607904 12.454933193719263 34.06882671053205 0 0 0 3221 1 0.004779828412355146 24.89989032995759 9.284412476074914 34.066292534003196 0 0 0 3202 1 0.004685477948987587 23.42875178896892 14.146820781729533 32.41518709275638 0 0 0 3204 1 0.004692239562162238 26.555761990322072 14.012917679778433 32.44523461214865 0 0 0 3195 1 0.00487763104599289 26.49227079512706 10.85307876805461 32.38932920176691 0 0 0 3193 1 0.004937206884786641 23.317443491377553 10.84072362342043 32.50843078713786 0 0 0 2484 1 0.004706077959016406 26.584982574645093 7.774223989001551 32.493269224810625 0 0 0 2482 1 0.004845567120155426 23.42544246930412 7.722405386262823 32.3809651601075 0 0 0 1009 1 0.004636051936693843 28.149255398909308 12.517740758547545 30.896737418526005 0 0 0 3192 1 0.0047169859344867275 21.66429835298909 9.303312637305684 30.930527117806758 0 0 0 3201 1 0.004789662184156844 21.746526446036572 12.55140439260334 30.919045881469184 0 0 0 3203 1 0.0046273250018570335 24.924603531229263 12.529251918822656 30.93834907416376 0 0 0 1000 1 0.004749926160421185 28.101432544473635 9.282888876715273 30.863227338461336 0 0 0 3194 1 0.004639371281430582 24.972202989785817 9.275302879775358 30.84835983142337 0 0 0 3177 1 0.004754455516403536 26.561545248347258 14.019262898844588 29.322020620682853 0 0 0 3168 1 0.004811785015076082 26.50232243760515 10.891622909720796 29.265324637008042 0 0 0 3175 1 0.004818752420462317 23.404187934528366 14.070270828970079 29.33437873257991 0 0 0 3166 1 0.004941179620199597 23.33571269334112 10.865904533072072 29.317265679925157 0 0 0 2457 1 0.004876321898634628 26.48696539788785 7.757296131161668 29.23288779556197 0 0 0 2455 1 0.004960118745090144 23.320176939086664 7.696466358575575 29.158503649201826 0 0 0 2585 1 0.004783084457449155 15.410261269914914 6.090110595696049 43.622001096261315 0 0 0 2576 1 0.004787577234953808 15.409214891144593 2.894376403221038 43.619735696717676 0 0 0 2587 1 0.004853644184807139 18.616412601790316 6.083832100785656 43.624683736180394 0 0 0 2578 1 0.004831524452335036 18.552219378416844 2.978227290316783 43.61352157890402 0 0 0 2552 1 0.004788648666945413 17.042532586599872 1.245956344262319 41.98709780851431 0 0 0 2553 1 0.004701875813536049 20.215159493241877 1.3271013259519304 42.050170426957436 0 0 0 2557 1 0.004931205048970638 16.951846403407934 4.498564675083365 42.03355320135332 0 0 0 2558 1 0.004788091690688169 20.19268742012531 4.456493559628698 41.94079263028116 0 0 0 2547 1 0.004831499886993423 15.329706844370046 6.12038479123981 40.36267397659809 0 0 0 2548 1 0.004952185929862355 18.696608518553408 6.097415255027298 40.444036522282616 0 0 0 2543 1 0.004854817043207909 15.319370003479523 2.9139762634140705 40.42549537396277 0 0 0 2544 1 0.004818947501329966 18.596532604779604 2.8897888563729404 40.358327844251484 0 0 0 2516 1 0.004862325424143093 20.271218358961068 1.2538712342659473 38.84966537588251 0 0 0 2523 1 0.004874925535954108 17.02342649573404 4.403952349143261 38.84159212395881 0 0 0 2525 1 0.004716404280350129 20.212404828947456 4.521916236394965 38.78497725387712 0 0 0 2514 1 0.004751675627254294 17.036024178305304 1.3083539835774802 38.791888801127385 0 0 0 2524 1 0.00472199302772781 18.597741056692964 2.8028547575578484 37.24565166425255 0 0 0 2531 1 0.004727186027207054 15.505820471465682 6.09431195548243 37.27832018497803 0 0 0 2533 1 0.004796567702453767 18.644326928122855 6.077114960661662 37.24686319465327 0 0 0 2522 1 0.004674946754496253 15.399717289486361 2.8429698346207615 37.22140763129456 0 0 0 397 1 0.0049079681779719345 28.117121099169914 6.112529057982902 43.62744759205151 0 0 0 2582 1 0.004780733902413266 25.000986713914216 2.9650494514479884 43.525286390656404 0 0 0 2589 1 0.0048491196016310426 21.710050892242272 6.130023455377757 43.62019160097565 0 0 0 388 1 0.0048239758882945155 28.150396962700192 2.934684247540066 43.58178203689827 0 0 0 2591 1 0.004696472742217557 24.90032949082072 6.223944449001093 43.66802790943287 0 0 0 2580 1 0.004821817874464113 21.69188539673313 2.857888323713314 43.66770312765508 0 0 0 2560 1 0.004909114286021655 26.573209683696557 4.540106509313086 42.043662182688124 0 0 0 2554 1 0.004876322182325419 23.466161676469333 1.297187701992524 41.981004379626526 0 0 0 2555 1 0.0048177818095186675 26.542639207600825 1.2280732209605343 42.00138865226094 0 0 0 2559 1 0.004850518702845502 23.39802042934203 4.519475332475153 42.08839455289182 0 0 0 2545 1 0.00477501018636413 21.793723333915082 2.865408166614377 40.41320398341967 0 0 0 357 1 0.004912885631516168 28.096897886595528 2.8860524338667735 40.41727369894461 0 0 0 2546 1 0.0048161851090382304 24.947619845180164 2.876499469572145 40.38965326163939 0 0 0 2549 1 0.004850112037245719 21.79293202130868 6.020789939660198 40.43809937189586 0 0 0 362 1 0.004769155665112023 28.1679984275657 6.051047954990594 40.41764955475302 0 0 0 2550 1 0.0048720623316422865 24.90937955383291 6.1230058799068905 40.454650705974004 0 0 0 2518 1 0.004701431292443329 23.302490103945246 1.3052974896446938 38.798228204996164 0 0 0 2527 1 0.004784671271902042 23.49893175415853 4.420057796926366 38.83097772771616 0 0 0 2520 1 0.0047722708608353755 26.532028708763505 1.257086488501966 38.7602264689263 0 0 0 2529 1 0.004850119304667786 26.660026343746324 4.454985345182416 38.76303126908403 0 0 0 334 1 0.004588517976421796 28.225594609079703 2.9322435634982833 37.272209759663724 0 0 0 2526 1 0.004777917755910462 21.85432409249948 2.9372560000098376 37.25855725331137 0 0 0 2537 1 0.004847353792173209 25.01947856725634 6.169661613079289 37.27009114290065 0 0 0 2535 1 0.004672043838271614 21.92844295359673 6.042344842967399 37.26667072483559 0 0 0 343 1 0.004741845638171722 28.22417048501978 6.076828714172596 37.21793068648081 0 0 0 2528 1 0.00470515515056175 25.000777834004033 2.7725437072622583 37.17006686883219 0 0 0 3305 1 0.004748175182310934 15.387178267137918 12.483060535161723 43.60761233907867 0 0 0 3298 1 0.004831266055714481 18.51232988956427 9.287249003912347 43.53576685153725 0 0 0 3296 1 0.004773910893708044 15.359868075146117 9.264369752632218 43.66795376119969 0 0 0 3307 1 0.004746790780366911 18.53244126814547 12.53016644433357 43.64832567777746 0 0 0 2563 1 0.004689975184095238 20.147402658521315 7.804234820520376 42.03002108407861 0 0 0 2562 1 0.004868429212663537 17.03028154761261 7.634069420709835 42.02269645775034 0 0 0 3287 1 0.004786452161227542 20.076704210405122 14.11693765711428 42.10062466913441 0 0 0 3286 1 0.0046557354259099855 16.97044285701052 14.140204034992943 42.06850840470364 0 0 0 3281 1 0.00474990761874922 16.864631278540617 10.850730082397476 42.086613332206035 0 0 0 3282 1 0.0047584428840457774 20.157918972367487 10.957838024225808 42.11709925445761 0 0 0 3268 1 0.004775995878976596 15.456160304350886 9.239653763438989 40.40882031634009 0 0 0 3272 1 0.00463243999394693 15.356699587374013 12.484481039113074 40.50366041873324 0 0 0 3273 1 0.004868978293606689 18.511416225229514 12.495070736954698 40.51334842305321 0 0 0 3269 1 0.0048677555648831815 18.637555117708185 9.304922927278856 40.41531025097371 0 0 0 2534 1 0.00469970379288054 20.32128268268323 7.664425393653596 38.80742617357957 0 0 0 2532 1 0.00495465654233241 17.03169328754461 7.708294535655292 38.74068660829391 0 0 0 3254 1 0.0048157966153383296 20.13383403527075 14.020182915405693 38.86841680925961 0 0 0 3252 1 0.004784926141369368 16.953696989297153 14.095638588054518 38.9197246455252 0 0 0 3243 1 0.0048279016818146 17.003913115032933 10.861375438159872 38.874506845976065 0 0 0 3245 1 0.0046716873521039735 20.28149745895195 10.86929184963963 38.91745596806694 0 0 0 3253 1 0.004863217466322655 18.550995353888062 12.439548477373284 37.306407696318445 0 0 0 3242 1 0.004713164091750361 15.262903097778885 9.286069789675038 37.12759813415117 0 0 0 3244 1 0.0048376139982866245 18.700088854547108 9.3019342844779 37.31313278603335 0 0 0 3251 1 0.004856142252421767 15.415779110179344 12.49052531406565 37.374019262153034 0 0 0 3311 1 0.004867395149189357 24.99499562301975 12.497551841074435 43.73520460047179 0 0 0 1117 1 0.004712290002748535 28.13099522454037 12.549536989270871 43.699026906924345 0 0 0 1108 1 0.004736302026113394 28.133773901448382 9.405185592757777 43.561877599173016 0 0 0 3309 1 0.004659574536040927 21.80470895895054 12.501944739071298 43.620104476979314 0 0 0 3302 1 0.004755799463924789 24.878771808935532 9.39949799917828 43.66924397277615 0 0 0 3300 1 0.004727403608847032 21.779194237830335 9.333801297828968 43.56157771993578 0 0 0 3288 1 0.004901086016473443 23.37956526298767 13.996232588203329 42.080449694604134 0 0 0 3284 1 0.004836141306233534 26.596674363003984 10.998928201662345 41.88406310107777 0 0 0 3283 1 0.0047078046444535195 23.34537215544543 10.849473239573767 42.069672018363256 0 0 0 3289 1 0.004850831737692084 26.721206164897158 14.122240620031253 41.995131931642476 0 0 0 2564 1 0.004721518566660317 23.344524576618262 7.718432319871374 42.060794201743484 0 0 0 2565 1 0.004975468731079491 26.504358292755732 7.821233694363043 42.02374423876106 0 0 0 3275 1 0.004881651346433324 24.948510048447595 12.456349160655742 40.39014052625389 0 0 0 3274 1 0.004852174198579286 21.734883195577407 12.46017188049072 40.48191684401081 0 0 0 1081 1 0.0047219939770478305 28.184152596347577 9.282728399131267 40.347483522356804 0 0 0 1086 1 0.0046067735293406215 28.10390274110331 12.45521239142698 40.33567685563176 0 0 0 3271 1 0.004691629430367021 25.01947090356103 9.339288311760871 40.43509687555655 0 0 0 3270 1 0.004669394106375022 21.8081714849172 9.22534476471267 40.401141875892115 0 0 0 3256 1 0.004730777751529013 23.32376841189111 14.117545265571959 38.85419917109697 0 0 0 3249 1 0.004745212688216642 26.593366709015072 10.850569601009452 38.77722183729915 0 0 0 3258 1 0.004609502704507409 26.541863470275537 14.11150035665897 38.83760679626737 0 0 0 2538 1 0.004810075326499342 26.59573457308799 7.5965388354408185 38.859941134521165 0 0 0 3247 1 0.004746589351094005 23.42937421578565 10.843834191622223 38.90801905522166 0 0 0 2536 1 0.004649803679355611 23.460259689010968 7.688649549246373 38.87686668441973 0 0 0 3248 1 0.004871923641786291 24.941802168533833 9.25830962566956 37.17392430411046 0 0 0 3257 1 0.004738086675718007 24.93154912433434 12.510975060746594 37.2506952370043 0 0 0 3255 1 0.004804942447754177 21.737915272154574 12.588415369139504 37.31490690134864 0 0 0 1054 1 0.004974489872130717 28.191873262226732 9.275319465169915 37.2444133123822 0 0 0 3246 1 0.0046521871486843724 21.83234314848627 9.334576518495782 37.362029530137455 0 0 0 1063 1 0.0046935938146857245 28.144698438949707 12.485464123922993 37.269881502995204 0 0 0 2638 1 0.0048478978757428536 16.967644655667545 4.509778117437439 51.583551827007106 0 0 0 2633 1 0.004813709770317887 16.980553220646943 1.3387785425755045 51.58371084427483 0 0 0 2634 1 0.004679205216067949 20.186216983559063 1.3102764082989775 51.52635162360022 0 0 0 2639 1 0.004698525090378054 20.180429026386705 4.455209436379529 51.588260647474755 0 0 0 2628 1 0.004796102803279188 15.310800311578433 6.15883133772073 49.94218293216583 0 0 0 2629 1 0.004757362598542996 18.52647486053369 6.100776357661733 50.01649126975773 0 0 0 2624 1 0.0047559976109078205 15.267446920908396 2.930610525104303 49.92439784078476 0 0 0 2625 1 0.004777603862100736 18.559816936863633 2.9076917052461932 49.935543544859385 0 0 0 2595 1 0.004698904274816226 16.888628983707633 1.3426304599948407 48.29348240720528 0 0 0 2597 1 0.0048937131157633824 20.178062461016616 1.3781304865497257 48.32149620794059 0 0 0 2606 1 0.004534805085063499 20.17484417027482 4.469492341724245 48.421195194230826 0 0 0 2604 1 0.004752419608670419 16.955738451351316 4.512521312284192 48.41980596260713 0 0 0 2612 1 0.0047536704215495554 15.304498810981476 6.111081686730503 46.81602416602318 0 0 0 2605 1 0.004655725271772855 18.534166876548564 2.962317498668395 46.866568369000646 0 0 0 2603 1 0.004620991805052495 15.391745207553003 2.9381858473016904 46.81281763628213 0 0 0 2614 1 0.004815019869049515 18.565475507032478 6.028286486622685 46.86294784625481 0 0 0 2568 1 0.004719633750378342 16.963006416774487 1.2754574580004534 45.25667394643192 0 0 0 2579 1 0.0046914601360760096 20.14939682422466 4.525412064798345 45.227246928751846 0 0 0 2577 1 0.004726692623034127 16.935094329033323 4.502199835524751 45.24423269247 0 0 0 2570 1 0.004765860162469694 20.108942436057614 1.3705021773984938 45.13594970335499 0 0 0 2636 1 0.004724620518996284 26.676793120713054 1.3766005119219724 51.558892755258725 0 0 0 2640 1 0.004842234084758213 23.398902084965535 4.521322209171574 51.64799633501636 0 0 0 2641 1 0.004797865876288792 26.551215204894188 4.508647388562087 51.58607671127088 0 0 0 2635 1 0.004822255277015134 23.330156268921666 1.3082323170120518 51.51712360714767 0 0 0 438 1 0.004572329247252706 28.09747111781857 2.87364557583613 50.01947372520822 0 0 0 2631 1 0.004587960672364366 24.880138570752116 6.095058127621325 49.93354321905373 0 0 0 2627 1 0.004884081246889747 25.03768877323743 2.897856210336078 49.97738079953869 0 0 0 443 1 0.004842342122085376 27.984549500465636 6.120467506498245 49.97101184795809 0 0 0 2626 1 0.004743666214538776 21.745270162538382 2.9832074740353995 50.01531551634496 0 0 0 2630 1 0.004670764865483606 21.741639903547018 6.016525181646691 49.929729796446075 0 0 0 2610 1 0.004603404053564034 26.561959325870436 4.411742954036662 48.344948504231546 0 0 0 2601 1 0.00476367879430078 26.494099567969087 1.214498787892815 48.35552216021877 0 0 0 2608 1 0.004748013101298217 23.402645766420097 4.506705325461415 48.35304221914284 0 0 0 2599 1 0.004752111111829932 23.394533089603765 1.362044759174309 48.33014468973259 0 0 0 415 1 0.004753123199346947 28.096078812337932 2.847956518607312 46.755780477428665 0 0 0 2616 1 0.004727695148393598 21.676737272749037 6.15701265598039 46.88726128260288 0 0 0 2618 1 0.004546903888710634 24.942040006663273 6.04160586239252 46.78959532255764 0 0 0 2609 1 0.00454340261433956 24.932768218214175 2.93265034587577 46.79613765648794 0 0 0 424 1 0.004777358158996353 28.160257619588926 6.074428987315221 46.77313701166944 0 0 0 2607 1 0.0048356682825071474 21.712941390889196 3.0081113614376895 46.73680110514865 0 0 0 2572 1 0.004878068593529454 23.384204370221163 1.3661909019019078 45.19269377912912 0 0 0 2574 1 0.004843725222687912 26.54199285491281 1.3328118813560883 45.176191482737174 0 0 0 2583 1 0.004714261542765068 26.529036479323292 4.521772823408239 45.28906156777116 0 0 0 2581 1 0.004825024046097179 23.417878692073423 4.52126067966114 45.130266195480765 0 0 0 2643 1 0.004707748612205203 16.96134005680848 7.603321026245429 51.56242590305195 0 0 0 2644 1 0.004745123982199161 20.18610905369636 7.612393726335362 51.514274639121005 0 0 0 3362 1 0.004749129673876485 16.8811889577105 10.880808049777446 51.47842607027893 0 0 0 3367 1 0.0047471707709186295 16.827896899217418 14.082673017088615 51.51321589701087 0 0 0 3363 1 0.004814601424882834 20.145305247733052 10.825542770733174 51.548587552732215 0 0 0 3368 1 0.0047485351543613465 20.043169746365344 14.017049984857794 51.59243740396904 0 0 0 3350 1 0.004812288473125637 18.580600715628332 9.24513319794563 49.93523894325378 0 0 0 3349 1 0.004782425787148704 15.401170406833213 9.248163496317146 49.954193145935555 0 0 0 3353 1 0.004624863397720844 15.223193238429351 12.512319344797872 50.02549148414234 0 0 0 3354 1 0.004745763325334983 18.449015083130423 12.472303862521484 50.06255032816569 0 0 0 2613 1 0.004644076216931714 16.953795423246525 7.7418529249155705 48.35148982453238 0 0 0 2615 1 0.004646400082552224 20.117410535035937 7.712261968307412 48.38477851585785 0 0 0 3324 1 0.004806144332194869 16.876926058199224 10.919179376882354 48.36582031000075 0 0 0 3326 1 0.004661297697706896 20.14099616650918 10.925839156476666 48.40748668675764 0 0 0 3335 1 0.004883676134123594 20.138833030639198 14.08091714479741 48.509524249106526 0 0 0 3333 1 0.004877604140828627 16.878534348430637 14.097929998892566 48.47704390831692 0 0 0 3334 1 0.00487187032024688 18.547854279291105 12.481026987632125 46.806345556986294 0 0 0 3325 1 0.004748857012713617 18.498545433409063 9.355764953455514 46.86282200958506 0 0 0 3323 1 0.004705491003007083 15.379317866971641 9.291202415065626 46.7651331398594 0 0 0 3332 1 0.004859308805901262 15.33479047261189 12.58059392205116 46.785941448481154 0 0 0 2588 1 0.004969217210898559 20.176187603975034 7.704941676783505 45.20230995320907 0 0 0 3308 1 0.004751139447191119 20.224048683216584 14.127161385824508 45.269312838240864 0 0 0 2586 1 0.00488550106382362 16.970046808111473 7.714515349846992 45.28992717073102 0 0 0 3299 1 0.0048887966082496945 20.14763582305809 10.960982150213923 45.172838432197935 0 0 0 3306 1 0.004733277535796885 16.938085651396854 14.098095125134922 45.25857014168732 0 0 0 3297 1 0.0047514785320184605 16.993167558941604 10.931770619622764 45.23952672507991 0 0 0 3364 1 0.004773018191701483 23.321426297947806 10.88767821437621 51.512004386073436 0 0 0 2646 1 0.004778151650832216 26.398127632163213 7.602953243447091 51.59459728840458 0 0 0 2645 1 0.004712623398607271 23.30047773448953 7.6852575071752005 51.59226883320153 0 0 0 3370 1 0.004794137942007254 26.47018738493979 14.04571475932395 51.60859537547888 0 0 0 3365 1 0.004770808176911504 26.523677111804453 10.761100340783102 51.60371103057365 0 0 0 3369 1 0.004833343415329648 23.350432910899585 14.129607558085905 51.53988592769904 0 0 0 3351 1 0.004734698255021735 21.781739744677985 9.257175988319055 50.01129614735349 0 0 0 3352 1 0.004821992838938827 24.95498367056471 9.282973227563872 49.98144520441907 0 0 0 3355 1 0.004694392244727395 21.66299195396475 12.455067763102797 49.937783536421286 0 0 0 1167 1 0.004784205787101396 28.00981654704768 12.443448031697615 50.002963281320646 0 0 0 3356 1 0.004775871135355993 24.8901874968445 12.519057706897192 49.96312359306488 0 0 0 1162 1 0.004720893461110548 28.00550006342306 9.195409933997347 49.97090134114895 0 0 0 3339 1 0.0047773003040453895 26.51826874542784 14.00922245871619 48.424816070660675 0 0 0 2619 1 0.0046076483849005045 26.440631052251085 7.535420470394607 48.33737210082162 0 0 0 3330 1 0.004642587331127549 26.52184946172856 10.843297238238286 48.40637345780198 0 0 0 2617 1 0.004745998982519732 23.347641991233928 7.602842642514893 48.45241402965187 0 0 0 3328 1 0.004874064708749005 23.31285947368859 10.934879313015278 48.356751402721315 0 0 0 3337 1 0.004803725318424762 23.287052728403847 14.087599099508427 48.3690220594437 0 0 0 1144 1 0.004825032193240852 28.10657842671895 12.434617041617374 46.76948691325379 0 0 0 1135 1 0.004732931249904305 28.107803470438455 9.205707731856734 46.94788731274065 0 0 0 3336 1 0.004716989737483374 21.699936368325776 12.492135279449597 46.79416029954849 0 0 0 3338 1 0.004712139989038543 25.066119791525885 12.398681527059065 46.76357059621792 0 0 0 3327 1 0.004927906307862058 21.65301337187531 9.318019334897839 46.90223222875598 0 0 0 3329 1 0.004886994043221604 24.909002744773733 9.298546110911493 46.76000457583143 0 0 0 3312 1 0.004565780409579263 26.505262060857547 14.086886394426184 45.184168409626224 0 0 0 3301 1 0.0047058893295049385 23.340521326488275 10.89247628228977 45.216328311613154 0 0 0 3303 1 0.004634427079949906 26.5957610014118 10.767397955706988 45.225638157767904 0 0 0 2592 1 0.004820531783506282 26.546437879456978 7.687687734590425 45.18802145253899 0 0 0 2590 1 0.004854420281357019 23.303984528124175 7.650125235790679 45.26598449135285 0 0 0 3310 1 0.004716586605410364 23.3725016260807 14.080183304777076 45.26492823864499 0 0 0 2711 1 0.004917639727333466 15.370412474248223 2.914137574205348 59.476539245029194 0 0 0 2720 1 0.004830477311724207 15.316183181267066 6.040651517513602 59.57615857068162 0 0 0 2713 1 0.0049579516826995865 18.54350932659816 2.900256725044883 59.4591528290188 0 0 0 2722 1 0.004813002782389837 18.580825642629325 6.063192296537966 59.594460831427526 0 0 0 2685 1 0.004769418872182242 16.867394207106017 4.552121830306901 57.911521880527665 0 0 0 2676 1 0.004799983807172848 16.902513734057646 1.3245811654499904 57.91330052410447 0 0 0 2678 1 0.004787889373995907 20.051931372208145 1.3211814748427806 57.954653414625405 0 0 0 2687 1 0.004801301349387523 20.04450855281721 4.568413247558016 57.8676331128007 0 0 0 2686 1 0.004815611208265593 18.50946015759268 2.942724617804641 56.21704650559547 0 0 0 2684 1 0.004849089081574401 15.30780312485389 2.9656675518002515 56.35119716728967 0 0 0 2693 1 0.004719926655890662 15.203725515271639 6.141356753215349 56.33445056573109 0 0 0 2695 1 0.004799836219252264 18.407932911666112 6.039138865212615 56.32521299115861 0 0 0 2651 1 0.004713516586574767 20.158408166756676 1.238626257099418 54.70541371722538 0 0 0 2649 1 0.004840917864595718 17.01737367985028 1.367475274842553 54.68732235534442 0 0 0 2660 1 0.004822681184172535 20.160407841949535 4.486358715229817 54.71094206354347 0 0 0 2658 1 0.004617317599490937 16.841711947721898 4.505677913685735 54.74271839464579 0 0 0 2657 1 0.0047949530268610804 15.348152116682698 2.8634559474267323 53.16100590831011 0 0 0 2666 1 0.004751301404922139 15.45066205693368 6.097795386543848 53.22203432360244 0 0 0 2659 1 0.00473723674370986 18.61469099096815 2.9473601085215098 53.09766683379412 0 0 0 2668 1 0.004712660329932568 18.532169889251247 6.127677256833197 53.163062587871465 0 0 0 523 1 0.004999900735169706 28.067210839908068 2.862097366105823 59.59401557913133 0 0 0 2715 1 0.004753655876405291 21.71159692200801 2.901234421646172 59.504734846406805 0 0 0 2717 1 0.004829315382845575 24.9531173794217 2.8618991759332313 59.5796367392569 0 0 0 532 1 0.004810330540710159 28.07811845378349 6.0232230013885095 59.6287786358695 0 0 0 2726 1 0.004698238378889115 24.96336412247754 6.094140961529938 59.59930904404911 0 0 0 2724 1 0.004614197307194987 21.69960817952286 6.020351638839378 59.46018752970044 0 0 0 2680 1 0.004859151171802712 23.315705980770314 1.307436440901898 57.958324202788816 0 0 0 2689 1 0.004852526502203873 23.315159106972203 4.560463360187618 57.97750062853398 0 0 0 2682 1 0.004715947181844184 26.502443635764266 1.2492969160628717 58.04749395964803 0 0 0 2691 1 0.004868079037585295 26.42516497126139 4.529138479161263 57.95710544672847 0 0 0 505 1 0.004805397087269023 28.14187915872651 6.139787489320217 56.318989118341904 0 0 0 2697 1 0.004738896281796981 21.72704443915492 6.012054855205308 56.32444469977806 0 0 0 2699 1 0.004671472050927017 24.96282409458023 6.188321699643364 56.3320301651046 0 0 0 2690 1 0.004806896164650807 24.912483835976886 2.9714960099443615 56.3882355906518 0 0 0 2688 1 0.004811113402462106 21.74976423480956 2.8816015301494424 56.31963491002366 0 0 0 496 1 0.004916650912303004 28.15384007190904 2.9823911776757805 56.42652637827245 0 0 0 2653 1 0.00480276829822978 23.271879614966704 1.3388615078336825 54.78128002664763 0 0 0 2655 1 0.0048082938646520825 26.511850241039756 1.3635721381790693 54.782930302932776 0 0 0 2664 1 0.004814777055921057 26.487767006067035 4.468598224620924 54.81026471863611 0 0 0 2662 1 0.004704168558135097 23.28056803038699 4.463689688873158 54.79503895381045 0 0 0 478 1 0.00499086820855736 28.153375249223995 6.10320163832118 53.213625631570686 0 0 0 2670 1 0.0047848264513323385 21.767285897259388 6.112549319798556 53.128101855740766 0 0 0 469 1 0.004733235389637243 28.220949876412924 2.9287217578479003 53.178713296226235 0 0 0 2672 1 0.004862231318866709 24.91139538992827 6.070632959849482 53.22178794672527 0 0 0 2661 1 0.004678270725571232 21.816847640123616 2.831568182429323 53.13464535580688 0 0 0 2663 1 0.004844133614026544 24.961847977902217 2.841727613654987 53.199958494320704 0 0 0 3431 1 0.004978702253534131 15.36042537997883 9.309778724096489 59.54672112456782 0 0 0 3440 1 0.004796654438540706 15.289511411502778 12.45137103975742 59.528780110134434 0 0 0 3433 1 0.004668456133456532 18.55906492492703 9.260618370524929 59.49470480703311 0 0 0 3442 1 0.004774588591639126 18.537348524600215 12.585915498671017 59.525505983843836 0 0 0 3405 1 0.004982157717857269 16.939677184212734 10.889465184531309 57.91431167793884 0 0 0 3414 1 0.004965512265552597 16.80734101992224 14.08166965314931 57.87919007633761 0 0 0 2694 1 0.00498700224263483 17.003565037158285 7.736333676270142 57.92412838356075 0 0 0 2696 1 0.004793681192453422 20.145518566541906 7.698453494160191 57.929283936633546 0 0 0 3407 1 0.004969260612507572 20.095496195768877 10.907955127756184 57.86654967236707 0 0 0 3416 1 0.004937645226511682 20.090302042767334 14.05297002209587 57.93421706794454 0 0 0 3404 1 0.004663883231927802 15.373036790703999 9.268586941853764 56.34741023999117 0 0 0 3406 1 0.0047311301741529335 18.5311180931628 9.27729820867293 56.28219807727794 0 0 0 3415 1 0.0049388357039927295 18.474171849817225 12.514288669446595 56.2772529030888 0 0 0 3413 1 0.004769518814973709 15.252366453322272 12.38148613443749 56.25621552019898 0 0 0 3378 1 0.0046908505205296176 16.899624041109803 10.839603110451753 54.58522303532172 0 0 0 2667 1 0.004630555237721221 16.862636381709795 7.749615291320619 54.74602926608785 0 0 0 2669 1 0.004887625724000743 20.04855921608262 7.638816269733552 54.74354339541108 0 0 0 3387 1 0.004831372932109628 16.849440717461366 14.033913049656714 54.659498046848086 0 0 0 3389 1 0.004707000977976191 20.18076190603912 14.083042981710301 54.75030538667429 0 0 0 3380 1 0.004909763241657632 20.081382343942494 10.87261839109103 54.68197303557696 0 0 0 3379 1 0.004829934678902718 18.475908743048166 9.251648995501816 53.11136284597935 0 0 0 3377 1 0.004637595984538091 15.284356215310122 9.368012721203105 53.1459066873039 0 0 0 3388 1 0.004757446749850947 18.517200220576512 12.485494169641399 53.14339680037586 0 0 0 3386 1 0.004656057399188965 15.242423792036664 12.40142442048437 53.1070051489814 0 0 0 3434 1 0.004695019661091844 20.086073469523008 10.827011511152755 60.96180999979567 0 0 0 3392 1 0.004846398635501861 24.851678690519076 12.477990451941183 53.12780950267145 0 0 0 3390 1 0.00485234354049454 21.69497739355356 12.481403940634102 53.117900146144834 0 0 0 3437 1 0.004550752894676 24.897080312853817 9.322676665791825 59.63245491920234 0 0 0 1252 1 0.004907144149969338 27.941829962848082 12.452128657327126 59.54392288471671 0 0 0 1243 1 0.004667988144398519 27.98627344570925 9.259869079040433 59.54133906727447 0 0 0 3444 1 0.004807774651951705 21.7245748671754 12.48853852579926 59.59229811806725 0 0 0 3435 1 0.004541442766916495 21.702102034350453 9.19031892184897 59.5090507519872 0 0 0 3446 1 0.004765441863721269 24.85963420941198 12.372414509267767 59.66323175336542 0 0 0 2700 1 0.004684581534606998 26.48604453228921 7.63658429101943 57.96618751207806 0 0 0 3411 1 0.004686882847702519 26.413981659746486 10.878876008851309 57.950414843580425 0 0 0 3420 1 0.004749470068804039 26.459376254143873 14.102823473468185 57.91964376095939 0 0 0 3418 1 0.00483825898402989 23.335033967852574 14.02174305738736 57.90846986039896 0 0 0 2698 1 0.004696417584964339 23.260492661898468 7.712345168346774 58.044861911927754 0 0 0 3409 1 0.004778126358303679 23.246981145984453 10.866840132394548 58.06659250706379 0 0 0 1225 1 0.004812809916394302 28.045657496214154 12.50222818538147 56.41990624204861 0 0 0 1216 1 0.004775693898462099 28.028959794894245 9.19016281641395 56.46062316842803 0 0 0 3410 1 0.004735687032115245 24.847089062300956 9.263185133638672 56.48039910931021 0 0 0 3408 1 0.0047633715654362176 21.696035604089175 9.223673886930394 56.419177073665416 0 0 0 3419 1 0.004769549694773749 24.84681463870847 12.499287005900026 56.405009907228646 0 0 0 3417 1 0.004813540565201517 21.7388099647173 12.507850289727632 56.33567724184776 0 0 0 2673 1 0.0046198704893540485 26.408880190056276 7.695230035393638 54.83628757738287 0 0 0 2671 1 0.004792166467648403 23.253739792882513 7.72700338337175 54.90340967112861 0 0 0 3384 1 0.004923971867527145 26.428775465501193 10.877651431791527 54.81671997053252 0 0 0 3391 1 0.004733511966239249 23.281819292975218 14.13633060707515 54.754884810322245 0 0 0 3393 1 0.004783916392095314 26.460337100363198 14.106400266918524 54.77519690167872 0 0 0 3382 1 0.004911871706845617 23.282950795336866 10.908282672321882 54.75702184633012 0 0 0 1189 1 0.004908176871678755 27.99680653041196 9.182534096964584 53.2679602763112 0 0 0 1198 1 0.004810122410283583 28.055886237077807 12.388445582384268 53.198064908539635 0 0 0 3383 1 0.0048103004807318606 24.83656660555924 9.331112178522067 53.19594272415808 0 0 0 3381 1 0.004847084197327945 21.735429324312726 9.244855093197954 53.16061639545199 0 0 0 3432 1 0.0046410221276691685 16.98933660440681 10.927304210282761 60.995616700855166 0 0 0 2801 1 0.0006920901518663574 15.334692166157518 6.1470352163129744 69.00169078677885 0 0 0 2792 1 -0.0003903477817647442 15.276905644243952 2.922396525234796 68.95396946891985 0 0 0 2794 1 0.001642567342208601 18.515803103813774 2.9405144254896136 69.06522402621684 0 0 0 2766 1 0.00297734758786271 16.91144225317274 4.434736442410408 67.47865955167266 0 0 0 2757 1 0.005412544965060171 16.869991222183334 1.3198496771287427 67.47489747812855 0 0 0 2768 1 0.0015788626276626184 20.14452836598407 4.610567159583875 67.45511118351223 0 0 0 2759 1 0.005452955676122823 20.11058387425938 1.387352974383417 67.4645563558972 0 0 0 2774 1 0.006065854143079634 15.252315814757914 6.094500645380054 65.79046136478301 0 0 0 2765 1 0.005738656780471562 15.221030745888845 2.8523070044646013 65.85335842665343 0 0 0 2767 1 0.005719850022242406 18.52485533304458 3.0075433288198843 65.85709216808004 0 0 0 2776 1 0.005301515136639642 18.447779660652582 6.089815010425495 65.85679376309305 0 0 0 2730 1 0.004489293324873965 16.912306104635256 1.2452571665123822 64.28087203864206 0 0 0 2739 1 0.005365196498222598 16.965633773373202 4.481926271385637 64.32211590523403 0 0 0 2732 1 0.004538806525980731 20.133760832508877 1.376727238498662 64.28451770010025 0 0 0 2741 1 0.005177098009302113 20.17710426986882 4.406083216396158 64.38194836192403 0 0 0 2738 1 0.004531610218533936 15.417434184736887 2.8493771659964455 62.674359863063415 0 0 0 2747 1 0.0044662306710090294 15.314116629154066 6.141420618730616 62.649828897168995 0 0 0 2749 1 0.00484509894451492 18.58972101232233 6.089926798591172 62.63453296078523 0 0 0 2740 1 0.00479251697389039 18.470938703165146 2.899362729814133 62.697105927873714 0 0 0 2714 1 0.004652599852239082 20.20458798948499 4.333408084896125 61.055851661998446 0 0 0 2703 1 0.004822059381395372 16.998437160929274 1.1864563251351634 61.13474149819131 0 0 0 2705 1 0.004900985041831963 20.12624825667555 1.2015074777342687 61.1154866432348 0 0 0 2712 1 0.0045902139297687924 16.917609720214823 4.572553681476372 61.049531540372236 0 0 0 2803 1 0.005535097907241424 18.493846372418776 6.07299515063441 69.0147830630997 0 0 0 2798 1 0.002848483453217034 24.897646906907976 2.8836257042983453 69.1323400999226 0 0 0 604 1 0.0007363666574950432 28.09164910418999 2.8858214639011663 69.1031748778497 0 0 0 613 1 0.0024326388951822955 27.98922024073192 6.145350276848491 69.03083562520946 0 0 0 2807 1 0.006449695446678255 24.81448639775159 6.131222407982337 69.14558055934728 0 0 0 2805 1 0.01012266205910813 21.69655471820776 6.009144796195488 69.12408361832465 0 0 0 2796 1 0.0037440935503008713 21.65012291446954 2.9847038086625637 69.09475676495127 0 0 0 2772 1 0.003549034492113542 26.500739161326237 4.4398775866378895 67.51150585970332 0 0 0 2763 1 0.005314725591948894 26.54805561939602 1.3529389567736774 67.57327077101031 0 0 0 2761 1 0.005110168405466822 23.259616415634426 1.2767450573904155 67.61166714482815 0 0 0 2770 1 0.0020271551015652537 23.3125001949405 4.486263865512132 67.62679945217926 0 0 0 586 1 0.005678909795051371 28.133335648448746 6.126616511268605 65.98438924402971 0 0 0 2769 1 0.005425422775399768 21.765467524882418 2.9677765737282122 65.90045253466863 0 0 0 577 1 0.0056508386689441276 28.15133294273145 2.9533720092493203 65.93849502099974 0 0 0 2771 1 0.005736719878688934 24.93891069472178 2.8126617874038855 65.95450251466056 0 0 0 2780 1 0.004831467079192684 24.8493113551219 6.090206078550572 66.08727534455974 0 0 0 2778 1 0.004359679272420971 21.71485720267654 6.117418375066961 65.9211669152608 0 0 0 2736 1 0.004558345166336016 26.45316044847077 1.28158054067893 64.3704887201475 0 0 0 2745 1 0.005295654934487923 26.40300348419143 4.49467331230251 64.31704530449815 0 0 0 2734 1 0.004389060317407907 23.213806822161008 1.2851380483435162 64.34087292782404 0 0 0 2743 1 0.00518104441219356 23.271791298112614 4.473469158614269 64.24173584611468 0 0 0 2744 1 0.004638298171299009 24.86437276445983 2.9136221447393384 62.767805945170046 0 0 0 550 1 0.004483722851554569 28.126070419629585 2.889452607581501 62.78617525906895 0 0 0 559 1 0.004590336346003147 28.08365796771927 6.036732518631738 62.803648059686495 0 0 0 2753 1 0.004801170127348575 24.841933634654033 6.112490399645099 62.78636669026611 0 0 0 2742 1 0.004498093160253619 21.766960913643107 2.876768050674184 62.692505703190555 0 0 0 2751 1 0.00483609631172607 21.64108418315329 6.072770544433699 62.72079333610691 0 0 0 2716 1 0.004667348321677886 23.26966323023991 4.504154788430912 61.07000825355891 0 0 0 2709 1 0.004754607583579776 26.446936340793428 1.26575644934538 61.14449794016491 0 0 0 2707 1 0.004878686632576408 23.273297268752874 1.3200829771650324 61.17851495660232 0 0 0 2718 1 0.00462154369457988 26.47082341112207 4.5458064061653545 61.244227656959396 0 0 0 3521 1 0.008078318149816369 15.28537498772463 12.48448257554064 69.06637934674181 0 0 0 3514 1 0.008390863576113662 18.44867260262503 9.245073058439758 69.08219720298688 0 0 0 3512 1 0.00356585987431615 15.310547699087333 9.329905730261261 68.98010283398764 0 0 0 3523 1 0.007094895087881355 18.52229771305699 12.483056627611269 69.07992678004706 0 0 0 2777 1 0.0030990636837162425 20.116476493704102 7.774992267580719 67.53772557975712 0 0 0 3488 1 0.00330412335315574 20.10565357984793 10.831301804300814 67.51177259521536 0 0 0 2775 1 0.002253350315859541 16.9307583014424 7.608381000545683 67.46156068540382 0 0 0 3486 1 0.0017987025187197608 16.992028483978338 10.907782447141706 67.49416703182798 0 0 0 3495 1 0.0010754702968906894 16.94856473483505 14.096863099156254 67.4635338381803 0 0 0 3497 1 0.00131093696901146 19.999802694360138 14.02561658542629 67.55885004264226 0 0 0 3487 1 0.005086895714366782 18.483750208353946 9.259382324985038 65.84887228759447 0 0 0 3485 1 0.006003494487549449 15.358116877882567 9.307774969806667 65.9203798592718 0 0 0 3496 1 0.005107788682426857 18.51646892167726 12.50999976313344 65.90189865036767 0 0 0 3494 1 0.005296605780992308 15.322446909738746 12.521937453812235 65.8172085736928 0 0 0 3459 1 0.005420544562920125 16.932978451167624 11.011006243518626 64.17336972864936 0 0 0 2750 1 0.005115120456760637 20.141069588817192 7.597803306035657 64.33877709880362 0 0 0 2748 1 0.0055060048894928736 16.92479753369767 7.762342897857123 64.2664976068786 0 0 0 3461 1 0.0052453966704350055 20.069015652899314 10.875423787430314 64.35752296993549 0 0 0 3470 1 0.005554430447409282 19.981891601123756 13.99094443417911 64.34902239562147 0 0 0 3468 1 0.005398936452912617 16.974882410452693 14.169010464835313 64.25907641273623 0 0 0 3458 1 0.004533923990518978 15.355477059261924 9.395455626482295 62.69309696579922 0 0 0 3469 1 0.0045789945809577605 18.512503941850383 12.50949592945531 62.65439374081697 0 0 0 3460 1 0.004684542116833421 18.605159385962704 9.223419591109302 62.64934135527853 0 0 0 3467 1 0.004525784446926234 15.336381682721473 12.561259215890523 62.64533272989111 0 0 0 3443 1 0.004357727370122558 20.176276895637287 14.068029616491078 61.19516166859424 0 0 0 3441 1 0.00459334800500873 16.98839001942875 14.172129285283289 61.0059040915533 0 0 0 2723 1 0.004539270457713325 20.15874426600212 7.671731750726979 61.16646814799796 0 0 0 2721 1 0.004596365452019691 16.912053148513515 7.728518219109057 61.05586096070868 0 0 0 1351 1 0.010987416029982128 27.964923486788127 9.330213673091633 72.31426187131373 0 0 0 2727 1 0.004598116029928651 26.440378500626338 7.686223060064949 61.117821686349146 0 0 0 3516 1 0.011748716324950375 21.566494101042036 9.262746821106063 69.17545470976941 0 0 0 3518 1 0.00799894478893298 24.83881987159937 9.225387570361217 69.0609753559291 0 0 0 3525 1 0.005181295962733328 21.67960691711274 12.436995880970384 69.08056289947584 0 0 0 1324 1 0.001739289852887042 28.133157381189505 9.151924492463339 69.1922297253656 0 0 0 3527 1 0.00460262446685737 24.815721705479653 12.47198735571136 69.05811212285032 0 0 0 3490 1 0.0033927066584923445 23.253822336675114 10.795069629180457 67.53856459175032 0 0 0 3499 1 0.0025484206917755336 23.225488749675545 13.98901340404674 67.45791164266092 0 0 0 2781 1 0.003038133908372702 26.469307985650108 7.651279667451994 67.56109354808568 0 0 0 3501 1 0.00502163546058438 26.431735043850246 13.97273975247855 67.48429359319162 0 0 0 3492 1 0.003774488840127467 26.498852018979004 10.837039744884427 67.5570054502512 0 0 0 2779 1 0.0024850363986049107 23.178799321824084 7.6988189546495915 67.57230266337295 0 0 0 1297 1 0.00533899833023118 28.071531900326274 9.252892830303667 65.86181754010774 0 0 0 3489 1 0.003973039500858389 21.644814653510434 9.237218090049362 65.8659090126803 0 0 0 1306 1 0.005110881654873471 28.09003863342731 12.389934947652309 65.9385061530354 0 0 0 3498 1 0.005106937615274648 21.643625594267675 12.46582602182409 65.97658196051337 0 0 0 3491 1 0.004296237900036191 24.87616121846132 9.134868355208646 65.90994743913299 0 0 0 3500 1 0.005197654648269517 24.883404172050728 12.430606718409525 65.86860980425753 0 0 0 2752 1 0.005041197433797202 23.284019964600578 7.608659402091807 64.35081653025217 0 0 0 3465 1 0.00487200641111207 26.45539540021488 10.82672419360758 64.32372340063823 0 0 0 2754 1 0.005090369146022348 26.478104515485114 7.687890608190658 64.38910573895859 0 0 0 3463 1 0.005175285593516479 23.252245221079 10.810747140426631 64.36446331202976 0 0 0 3474 1 0.00464645518749676 26.43538469734623 14.05106205108176 64.34577257273176 0 0 0 3472 1 0.005461720501921336 23.189965897084093 14.04335775406231 64.2690695143909 0 0 0 3464 1 0.004875207736092022 24.926577482449865 9.227966153508135 62.84151770171103 0 0 0 3462 1 0.004809597867444023 21.67600017240952 9.341736591995344 62.71122159896514 0 0 0 3471 1 0.004709495971299764 21.70935809327597 12.37598977026004 62.714919261178615 0 0 0 1270 1 0.004576970242429772 28.101669754821195 9.168201810180772 62.74549289837806 0 0 0 3473 1 0.0048480828935897665 24.87263777034233 12.4992423017943 62.698580748642776 0 0 0 1279 1 0.004676694874429878 27.943411169662575 12.468642248587027 62.84879402665263 0 0 0 3438 1 0.00460161388592136 26.481438575354797 10.80675394621293 61.13579914362036 0 0 0 2725 1 0.004857647176745035 23.264509019101936 7.7004906728589715 61.16391499742585 0 0 0 3447 1 0.004790230052147152 26.43244803487271 14.138529635217624 61.15282315508667 0 0 0 3445 1 0.004454952168683669 23.22912847409674 14.158364679036392 61.17376881300938 0 0 0 3436 1 0.00458836783346467 23.304909590378234 10.852995508338683 61.14497309401669 0 0 0 2854 1 -0.07027181056327136 16.908491412060002 4.519739856825097 77.09666891157039 0 0 0 2855 1 0.08581678674051181 20.04070188591198 4.383815969930899 77.23707573122971 0 0 0 2850 1 -0.01582503193830538 20.09206103409166 1.2201894774173825 77.11554016092519 0 0 0 2849 1 -0.07880055980654234 17.03015407921521 1.367958028248958 77.03831836503738 0 0 0 2845 1 -0.04614178263740165 18.484251168847724 6.0078408990866405 75.40225013297149 0 0 0 2844 1 -0.03703684794754841 15.373913472556563 6.121830828252161 75.39776830506483 0 0 0 2840 1 0.004720076111963312 15.238710463729793 2.8757419035841516 75.4499917904421 0 0 0 2841 1 -0.01644950620948793 18.503033489936424 2.93917272016578 75.48698283622056 0 0 0 2813 1 0.012560491425378337 20.053248861960142 1.294688453810583 73.89949649020566 0 0 0 2820 1 0.0056628457041286145 16.825123492614924 4.537188553517828 73.84979156417424 0 0 0 2822 1 0.008847534260590657 20.019703770250988 4.472580356857683 73.90262468787186 0 0 0 2811 1 0.00947817682127984 16.904046040199585 1.3644946328421712 73.96507087981631 0 0 0 2821 1 0.0026154636616832604 18.447554636572896 2.9075745237954624 72.33623124283 0 0 0 2828 1 0.014574219631223217 15.201131172365656 6.111200998464524 72.28897488694835 0 0 0 2819 1 0.009396905716945035 15.378419205005038 2.876346012507808 72.21711409369517 0 0 0 2830 1 0.011100470144373945 18.390919781599006 6.071454401070445 72.19967063965552 0 0 0 2786 1 0.00800898975067305 20.035994186371745 1.2905641475397192 70.6641139019684 0 0 0 2795 1 0.010414032793602777 19.981529744449023 4.587984641379624 70.68217990902686 0 0 0 2784 1 0.009905004989051676 16.937763944854016 1.2824378558755583 70.69445748440053 0 0 0 2793 1 0.01044973231149585 16.901604446548223 4.471676044897974 70.67553809866132 0 0 0 2856 1 0.07783302849723955 23.18875031099199 4.326634320422429 77.04906745500136 0 0 0 2857 1 0.019870900473692936 26.313548589961837 4.368014474903036 77.07209659787318 0 0 0 2852 1 -0.049328364047741005 26.45636275652646 1.1788091074206322 77.09547316793453 0 0 0 2851 1 -0.0734316130083422 23.233684335977266 1.1986493547623174 77.12460219356215 0 0 0 2842 1 -0.034637641254570424 21.582194696972408 2.914782194816559 75.46532821962606 0 0 0 2843 1 -0.021275592238806408 24.810588297386186 2.7733460420589884 75.56737053208342 0 0 0 2846 1 -0.04323096039582438 21.635217476497075 6.049189013866312 75.36180082044862 0 0 0 659 1 -0.026954409515025396 28.05072120881697 6.023003428369018 75.5620811867381 0 0 0 2847 1 -0.05703421952031875 24.87826150331151 6.055123768201921 75.43190002563108 0 0 0 654 1 -0.012809345209829159 27.934870704718666 2.7836271246059434 75.59461254445829 0 0 0 2824 1 0.007340673119043873 23.27358941104496 4.477908852705681 73.87910817702749 0 0 0 2815 1 0.014556549647842474 23.184084974523156 1.2932402255301079 73.97414633396143 0 0 0 2817 1 0.010893728467605238 26.403649789803996 1.2162094674910702 73.91720739772636 0 0 0 2826 1 0.007838064910323008 26.46287834179948 4.4493843958105845 73.90712577097999 0 0 0 2825 1 0.006821190035751481 24.90044650346364 2.923456678349971 72.31071881064888 0 0 0 2834 1 0.006782908143173829 24.878012561253822 6.085456274233251 72.315827310915 0 0 0 2823 1 0.0035991029731768133 21.70090119962183 2.9244434164438915 72.23807961858415 0 0 0 631 1 0.009230451335041166 28.00028252462846 2.7824785637223974 72.29315947837473 0 0 0 2832 1 0.0035797762758560427 21.680475252213515 6.073125742670811 72.3015646728028 0 0 0 640 1 0.007562269993042041 28.02851796311966 6.072611278450111 72.28644311947953 0 0 0 2790 1 0.004970623467666184 26.47727273655945 1.4199468019634651 70.72517415340728 0 0 0 2797 1 0.008662958560595926 23.33776507578863 4.517933328548389 70.78496387973637 0 0 0 2788 1 0.005320761378782433 23.274363111701522 1.3071521801907695 70.74077633563067 0 0 0 2799 1 0.0072776534566744225 26.50257477481988 4.458232391584388 70.70016714161845 0 0 0 2860 1 0.5710223547866321 19.941974535862265 7.429827117133409 77.2858201012854 0 0 0 3579 1 0.6172934866061038 19.916319924761417 10.87241580717984 77.175929998368 0 0 0 3583 1 0.2781382564598398 16.795063413713834 14.004297564986711 77.23250791635341 0 0 0 2859 1 0.1566577364319934 16.839186346230804 7.687948774465409 77.14328734805329 0 0 0 3578 1 0.24324630657205518 16.75537847329683 10.789383143084137 77.38370176372266 0 0 0 3569 1 -0.08296076205162266 15.235195613461862 12.434691626149622 75.42319619366523 0 0 0 3565 1 -0.01854333366726892 15.23781215638953 9.287486013343704 75.35259572439618 0 0 0 3566 1 0.020607413145854455 18.439605681788343 9.267949263113673 75.49319763720212 0 0 0 3570 1 0.026227265404904578 18.39694819319996 12.452190681900593 75.40077690185682 0 0 0 3542 1 -0.022751580141605568 20.004591224077586 10.865123089405078 73.90238449724924 0 0 0 2829 1 -0.013149768115781913 16.869632462792595 7.737331862600474 73.85400555493285 0 0 0 2831 1 -0.0055218501613940076 19.98985262416769 7.643936035960382 73.78712527801811 0 0 0 3551 1 -0.009462342935516918 19.97812919229916 14.073033080453595 73.89122284838672 0 0 0 3549 1 -0.00953856659454369 16.857679191042422 14.05551939200607 73.86774260012207 0 0 0 3540 1 -0.013319429354310994 16.806701657325824 10.846827366952436 73.79376205717412 0 0 0 3539 1 0.011939432342858816 15.33822061893161 9.239647017626911 72.28926405352702 0 0 0 3541 1 0.0067496527884363805 18.485648173567746 9.265889989632816 72.15564626887866 0 0 0 3548 1 0.013730388061294894 15.262745110310862 12.507592672197479 72.19032890569403 0 0 0 3550 1 0.008825077578555045 18.45331694076109 12.53478530234943 72.25145361355018 0 0 0 3515 1 0.0004959074212300615 20.05112195105944 10.909921605462033 70.62387220761885 0 0 0 2802 1 0.007807685868783694 16.877044096106594 7.672766928606855 70.62240674614195 0 0 0 2804 1 -0.002339572354007627 20.10292905021867 7.652080104854426 70.6879608492516 0 0 0 3522 1 0.00328999509877587 16.798042820156763 14.04949315377297 70.68253947267128 0 0 0 3513 1 0.007487077660665425 16.85255147186247 10.858425145770946 70.63831956133879 0 0 0 3524 1 0.008046498799434317 20.049716665077828 13.963659713225402 70.70935271550387 0 0 0 3584 1 0.2580945182730247 20.024244651547214 14.049243814798217 77.24023148330053 0 0 0 3554 1 0.003952887374320589 24.838990194951418 12.438285078412607 72.22879704316054 0 0 0 3552 1 0.010504768172250616 21.637936665578348 12.444543764229419 72.39066671436302 0 0 0 3543 1 0.007108037525137256 21.561338828618357 9.256986025587533 72.23782163519735 0 0 0 1333 1 0.003612092503034098 27.98867907212642 12.372407797574626 69.18965950585597 0 0 0 1360 1 0.00707186955164851 27.999271635947537 12.407732775067744 72.27641061426539 0 0 0 3517 1 0.004843291296586071 23.28467077598375 10.85315127590744 70.70691914215664 0 0 0 3526 1 0.011567334648835428 23.207503413127256 14.104609873163513 70.66594197154117 0 0 0 2808 1 0.008339906361895584 26.481145427715756 7.6867999118269275 70.72064398129703 0 0 0 2806 1 0.004959271988783745 23.191653469076982 7.688713177109589 70.66776669811495 0 0 0 3580 1 0.40244924417590366 23.038820826762635 10.812722522624938 77.25455302028239 0 0 0 3519 1 0.008805279077479251 26.2970970950842 10.78447226896821 70.6788103877949 0 0 0 3585 1 0.014006187871230712 23.212661094076033 13.998317869243595 77.14029422341632 0 0 0 3528 1 0.0062730972690875665 26.337990890970417 13.995920095353442 70.76871085266065 0 0 0 2861 1 0.5605817455990403 23.185058500427534 7.5118179190353045 77.22554001925059 0 0 0 3586 1 -0.00787842921037401 26.354054188320426 14.008417590734911 77.13894971405705 0 0 0 2862 1 0.19663417952841472 26.589423534453488 7.633937477102112 77.10161209632204 0 0 0 3581 1 0.026015547807788544 26.455121768341673 10.78743058067812 77.05864716296503 0 0 0 1383 1 -0.00959496333142065 27.983532861955457 12.486157268986517 75.45964564747013 0 0 0 3571 1 0.004465318661194878 21.56995184351336 12.431305537872769 75.34060413341305 0 0 0 1378 1 -0.025832344404309694 28.197883125718914 9.210822937544739 75.55885167541355 0 0 0 3567 1 -0.04271275117522403 21.51539147676717 9.220182285355708 75.50132477296958 0 0 0 3572 1 -0.05438014859177076 24.750528219254488 12.423490931276785 75.58185204289535 0 0 0 3568 1 0.04891358680632579 24.762591434061566 9.252330667624012 75.51495952378669 0 0 0 3555 1 0.010957140272524413 26.316822103137692 14.04766257870336 73.92684946784814 0 0 0 3553 1 0.006342796121757754 23.1640863925993 14.05792462441347 73.9027361949365 0 0 0 2835 1 -0.00465318298667217 26.524886193010534 7.6286592296157325 73.98742503774507 0 0 0 3546 1 -0.0006994636065193599 26.316547702958037 10.891379232065795 73.88677008423089 0 0 0 3544 1 -0.012341458047692572 23.27044737179288 10.817664685782104 73.85216252952736 0 0 0 2833 1 -0.02007315273436133 23.281770320638785 7.753158384936804 73.79644534531393 0 0 0 3545 1 0.00016054142223823932 24.864148341896154 9.257426435095157 72.24870520860799 0 0 0 4460 2 -0.643363434096809 18.895443927897254 1.4108164039988222 85.46316534055212 0 0 0 2902 1 1.6755051528029987 17.55201594258862 2.3669651581255615 84.81149421630471 0 0 0 5112 2 -0.6408087072476578 16.821166383945297 5.881661866544933 84.48473232733006 0 0 0 4537 2 -0.769090484066506 20.614097115690363 2.046662706573355 82.93931628557762 0 0 0 4385 2 -0.7581586475763653 16.968539735628585 1.7125439437063898 82.89529294678645 0 0 0 5143 2 -0.83670776679473 20.33408360680219 5.65154394351687 83.37910302194665 0 0 0 4969 2 -0.7557513043212903 18.448919522377462 3.500239813360003 83.00553789614007 0 0 0 4599 2 -0.7615959202894216 15.675593137128454 5.015972483334008 82.5672161748957 0 0 0 2876 1 1.510108807712319 19.865047770037844 4.050186532733779 82.15289888817307 0 0 0 2874 1 1.3897563450720438 16.659959583676628 3.785870517233772 81.81515112671629 0 0 0 2865 1 1.5028682949531715 16.820871561299107 0.5891644060424558 81.54662129032074 0 0 0 2867 1 1.3391417864727033 20.38969190058323 0.795903510679852 81.31882726848826 0 0 0 4791 2 -0.7599489281916956 15.065204800982235 2.576693396987286 81.40721361052985 0 0 0 4655 2 -0.7946391219472783 14.819718247842838 0.17686135294983085 81.33456005385294 0 0 0 4542 2 -0.7857316583119321 18.90723283406231 4.169021693068659 80.69353238421714 0 0 0 4613 2 -0.8116854936800547 16.585186791129647 4.405203059637493 80.12360006636003 0 0 0 4785 2 -0.806639311806353 17.201497274520406 1.3751981281632668 80.00236072671163 0 0 0 4862 2 -0.7993843438923511 20.088377970859757 1.4957106838745386 79.75876819928592 0 0 0 2884 1 1.216406690812252 18.00177933146141 5.9765790410286375 79.81855962593716 0 0 0 2873 1 0.7735123942962354 15.595127613244715 2.6607347515949398 79.14146953091497 0 0 0 2875 1 0.6266929507642398 18.49091159149045 2.809264662594899 79.11071104676144 0 0 0 4758 2 -0.8171334661312321 19.567851310255424 6.0785853475445935 78.9333907475795 0 0 0 2882 1 0.40681893642225037 15.128255503007033 5.677183806761371 78.82538984382109 0 0 0 4893 2 -0.7845604681457798 21.06787783525637 3.8245390603814986 85.39729790867062 0 0 0 4939 2 -0.639493540278616 17.936673991321058 3.918774796237693 85.4818257535376 0 0 0 2913 1 1.7091259090713968 20.97893715410894 5.987085437487307 84.98389962126171 0 0 0 4612 2 -0.8295505788465127 18.284439062850456 6.971175597543918 81.75492407082707 0 0 0 4574 2 -0.6454013257596151 16.149509978688627 1.7311930714175725 85.70261645974624 0 0 0 4561 2 -0.6566577892321146 21.10133659654423 0.45444099507723745 84.9715464570748 0 0 0 5053 2 -0.7225367196654314 21.11589724536082 4.192452110152291 80.42543805072441 0 0 0 4452 2 -0.7072531593285629 18.807918737443245 -0.024721010359199526 81.619499752923 0 0 0 5239 2 -0.6664801832770243 23.007047149935342 5.6715182725797595 84.67302805878016 0 0 0 2915 1 1.713862210475867 24.757643348927665 5.968825948602903 84.89460291083135 0 0 0 2904 1 1.7672624267357224 21.58093391086901 2.4283871626257487 84.40114630152537 0 0 0 721 1 1.4698831619342663 27.828531598924545 4.367246726717471 84.34545753334538 0 0 0 4571 2 -0.8243308440484279 27.256466726880863 2.736160247119111 84.05408978629568 0 0 0 4989 2 -0.7152952110043939 26.12461855345786 0.3686718520300024 84.24259535417902 0 0 0 4745 2 -0.7508378152301112 25.512088977365476 4.364037501489012 84.79522697765339 0 0 0 2906 1 1.6385075330170955 25.199778022862414 2.4751600649540375 83.96371493752333 0 0 0 4662 2 -0.7453427242680722 23.166479487654204 2.4677601003949516 83.66553286146511 0 0 0 4562 2 -0.7904837684618127 26.707636892825004 6.071217254829851 83.71439601967673 0 0 0 4937 2 -0.7105759446828487 21.889347291899746 3.94317404453137 82.72492590660774 0 0 0 4928 2 -0.7069126392832964 24.095195966221223 6.093346708352499 82.88634211663948 0 0 0 4541 2 -0.7153985450776167 25.216595740979116 1.6064987196973282 82.38338153589127 0 0 0 4399 2 -0.7529220589471686 25.446240437178812 3.8189112020973504 82.17707535050648 0 0 0 4388 2 -0.6937355243214606 27.67250934658964 0.44516129703170065 82.43352282464014 0 0 0 2878 1 1.5714162088498542 23.405553758059874 4.113313010705768 81.81126040247685 0 0 0 2880 1 1.142000757687423 27.030368119262064 4.066156856057924 81.34261251844896 0 0 0 4467 2 -0.8745980048167126 28.113735842356117 6.171358126863599 81.25653660843025 0 0 0 4680 2 -0.7933660071031273 23.617197925531624 5.636212080091424 80.82101838147084 0 0 0 2869 1 0.941117891275573 23.736656227573977 0.7989994812195702 81.07721888540988 0 0 0 4475 2 -0.7661023966951737 23.065904135896808 2.7908905073556327 80.60816919324138 0 0 0 2871 1 0.5402429561830648 26.55917593409711 1.104745821496624 80.73295460995531 0 0 0 4570 2 -0.7766715294087234 26.440679834900482 4.3913547160327155 79.70737226797208 0 0 0 2886 1 1.2569781182106414 21.43544093300907 5.842685785123446 79.88070800433132 0 0 0 2888 1 0.9507378806147698 24.794131088274078 5.518443772683593 79.12028611693934 0 0 0 2877 1 0.5477414244399696 21.738048633187844 2.6354047459648506 78.93971571847172 0 0 0 694 1 0.37792947985401454 28.136056881012745 5.940370816716781 78.95186267862334 0 0 0 4647 2 -0.7790375026640193 22.58678653540188 5.902740799622178 78.53092762877789 0 0 0 2879 1 0.07530868255735208 24.965112714076586 2.640729015820665 78.82590213523005 0 0 0 685 1 0.3052000798145376 28.169665938574248 2.823593956919613 78.83373947351919 0 0 0 4415 2 -0.6019631311151354 24.56046780206731 1.4352167841491823 85.30167315514217 0 0 0 712 1 1.5738150989947615 28.19106940060312 0.8301766107690983 84.03177852017406 0 0 0 4489 2 -0.7300218482707639 25.838444169575837 6.9726641027225895 78.93638905298825 0 0 0 5287 2 -0.6233635613106756 24.896029814365576 13.109864732614806 87.57194577996437 0 0 0 4701 2 -0.5671156315452623 16.181368566566388 -0.09438017290702272 90.77378253444537 0 0 0 4386 2 -0.8486347054606741 20.06559391676961 13.79464156232989 79.74908862202582 0 0 0 2883 1 1.4532718448029986 16.584656859903934 7.095777407689846 82.77002085788679 0 0 0 4800 2 -0.6390519279736563 19.892072094046572 10.059340512862084 85.82729046341869 0 0 0 4442 2 -0.6992250745464099 18.646492207202524 12.306562753270786 84.9234414226526 0 0 0 3605 1 1.690984712896514 20.7906104570385 13.383305779979752 84.52518886844882 0 0 0 5130 2 -0.7052786995464296 16.30078519032121 8.56028456420554 83.59998791769073 0 0 0 4667 2 -0.7749129238446384 15.981698047853909 12.514127690011241 83.38336142265798 0 0 0 3603 1 1.5973163462766844 17.624256543455548 13.08901087059512 83.274772082014 0 0 0 4447 2 -0.7427751684398142 20.036433637405192 9.20134862144821 82.93679713943544 0 0 0 5199 2 -0.7296232616721071 19.727200285500942 12.367824458075319 83.04491391928558 0 0 0 5206 2 -0.7196122213067176 17.849114175468124 10.802415417529337 82.89571849825887 0 0 0 3594 1 1.5638337129649005 16.196741296964518 10.390838072421083 82.45079888356886 0 0 0 2885 1 1.4539398974005993 20.081570159284762 7.511610494006925 82.2964952892638 0 0 0 3596 1 1.581349293019221 19.771689438515256 10.933592864896024 81.92717105556272 0 0 0 5010 2 -0.7816473795662936 15.3649560461289 7.278107443054385 81.5153608513862 0 0 0 4546 2 -0.7045823517317726 18.06808033535669 13.544074802907932 81.62814624107665 0 0 0 4833 2 -0.7693988970301473 14.944871176384783 11.657333410824291 81.226272860325 0 0 0 4639 2 -0.7683889408265552 16.555409856621075 9.727377638350966 80.85560998051801 0 0 0 4535 2 -0.8731527505169748 21.000891158848955 10.98652991418039 80.61269370663827 0 0 0 5015 2 -0.7635401153068366 18.285810667707448 11.185608899459528 80.3440134824915 0 0 0 4523 2 -0.8119940306336929 19.629526510694248 8.841922436435613 80.67421590412066 0 0 0 3593 1 1.2948228311758305 15.098373172881718 8.321339432522686 79.7328026941797 0 0 0 3602 1 1.2337230004884943 15.08976688539091 11.931856790120811 79.51110629076399 0 0 0 3595 1 1.3565679306015919 18.196198540398065 9.189896104748318 79.65394186191205 0 0 0 3604 1 1.2197397146692872 18.130290070141893 12.839300079190558 79.58521040213053 0 0 0 5160 2 -0.8324448033472848 16.075933063439358 13.743358509057508 79.53511364553042 0 0 0 4669 2 -0.8589875883806343 16.97839507033839 7.348191411491845 79.41498582863056 0 0 0 4839 2 -0.7843649124286496 15.22766987086462 9.872742645574418 78.80504917298268 0 0 0 4611 2 -0.794055083680197 18.887617833993996 9.19811134613601 78.02499719456941 0 0 0 4761 2 -0.7798272745689729 18.62266150500903 12.425896135796558 77.93630368895812 0 0 0 4690 2 -0.7417837941225851 21.46038606432482 7.933037932501542 84.4955491524214 0 0 0 3622 1 1.7239762453656309 21.30785050433505 9.699485782523091 84.82176610008662 0 0 0 741 1 1.6511280790084957 28.198977686290966 10.846252957306529 93.70927347772066 0 0 0 5139 2 -0.5880150893962512 14.262424570351648 0.9068181933336905 93.64646822980838 0 0 0 5002 2 -0.6916003752661117 21.436655014426748 12.029443736427325 85.3800092584889 0 0 0 4943 2 -0.7851716912948193 21.571323642096257 12.185598101713307 78.1151009252294 0 0 0 5037 2 -0.5910513652154351 26.456804877917445 11.324869877927396 85.14185985256464 0 0 0 5088 2 -0.6012986099989327 24.26573059081792 12.699606353803459 85.07683417413519 0 0 0 3626 1 1.6090227284960579 26.468679380301058 9.14474139229755 84.90921743478567 0 0 0 4414 2 -0.6860711557733095 25.105985753165857 8.099153498034621 84.70423773404394 0 0 0 4401 2 -0.8351705773113052 27.921758437874242 8.362661481144949 84.0634070486044 0 0 0 3635 1 1.6155846861300291 25.596735786045066 12.395593324339087 84.00508965529609 0 0 0 4966 2 -0.7570219082196123 26.516282103885015 10.538042106285445 83.238199765684 0 0 0 5221 2 -0.7222051678543107 21.718093824623807 10.777017153898132 83.03961930706564 0 0 0 5109 2 -0.6607285985803647 23.468881702229893 8.981799601630879 82.88728091464304 0 0 0 4659 2 -0.6538322254662035 24.606822031567177 11.582191736648634 82.3325847500016 0 0 0 2889 1 1.478561547746631 27.141508705938904 7.177750749819251 82.33887371111149 0 0 0 2887 1 1.525266297666435 23.649410061800275 7.482770222011738 81.93799267022396 0 0 0 3598 1 1.4742888471366375 23.0729454805174 10.852767319741483 81.82132671389904 0 0 0 3600 1 1.4522845549842456 27.283504764809862 10.605222853621052 81.6522249863823 0 0 0 4515 2 -0.7452942623962232 22.426018947924423 12.8341875653846 81.75074900777778 0 0 0 4397 2 -0.7630891446085483 25.687951518216327 7.587341107147803 81.39877100595288 0 0 0 4428 2 -0.789570562597464 27.773587947373642 8.909051705559994 81.25336002986172 0 0 0 4687 2 -0.9031371874206641 21.569454040106034 7.2293647444476035 81.5046669840548 0 0 0 4727 2 -0.7251163346357052 27.412477569903153 12.407499681378361 81.08652179219723 0 0 0 4726 2 -0.8723169908194537 23.34643769642267 8.910555405103004 80.28674700440945 0 0 0 4646 2 -0.8161534462803607 26.046801254385507 10.52564441750014 79.89843611883614 0 0 0 4485 2 -0.7111777509172948 23.557923511187944 11.990549582535836 80.1045895199636 0 0 0 3597 1 1.2641764639652497 21.619025512856503 9.103226280493883 79.98760447994117 0 0 0 3599 1 1.2866865575513826 25.237748218875247 8.95884200254215 79.53961430404992 0 0 0 3606 1 1.332888479992851 21.52718180603458 12.810692678058635 79.72161990175773 0 0 0 3608 1 0.8662658787264561 25.03414256844958 12.247180171434918 79.15289285721448 0 0 0 1414 1 0.18984932845282834 28.040418221660943 12.461314934681159 78.93739485339108 0 0 0 1405 1 0.09399150648423205 28.009405837078113 9.2416446600073 78.82588092483853 0 0 0 4720 2 -0.7288221918245938 21.466038332786887 8.518139962852722 78.30617042122674 0 0 0 4746 2 -0.7520703381236532 24.409059408658024 9.173536520271218 77.971173433684 0 0 0 5009 2 -0.7860996110061182 26.851863404759328 14.040816906324531 83.66200937001591 0 0 0 5192 2 -0.7088128247860718 24.754503427500385 13.81071311798406 82.63067732090965 0 0 0 4502 2 -0.7494671848506821 25.788554364949412 14.017422815934085 79.81186970459576 0 0 0 4926 2 -0.6724813362878956 19.50206747331613 6.397260555594071 85.72832966359607 0 0 0 2900 1 1.739620747967208 14.38244657112366 5.0890353581141134 88.48894903714279 0 0 0 5380 2 -0.5190878836757793 20.268689111181608 0.2489042485037036 93.92580490332112 0 0 0 4660 2 -0.4600285265611821 15.991375690791035 3.0032198070192546 93.55022733189348 0 0 0 2189 1 1.6836993028363763 19.48766684223782 4.991035052155029 93.3336981992309 0 0 0 2193 1 1.7212071113111131 20.32719256629606 1.3027265210297696 92.51665788184737 0 0 0 5468 2 -0.6357853524148512 19.578918616747337 2.795285572446009 92.85518767993632 0 0 0 4916 2 -0.6057641624792515 18.25622531443653 4.702861755062048 92.00861155574343 0 0 0 5382 2 -0.6024984436423492 15.409788703489097 5.233816510565433 91.74683937335493 0 0 0 4951 2 -0.5143106948099133 20.75293880330802 6.3299928262046965 91.66242991357822 0 0 0 2892 1 1.6806511737909364 16.370388235432408 3.780664222585282 91.52621686827071 0 0 0 4856 2 -0.43967855506377634 17.480672620339796 2.821640394178141 90.54847402878002 0 0 0 4654 2 -0.6213630394589953 14.805694720240723 2.3425150895482947 91.31325330116198 0 0 0 4390 2 -0.6137840054046182 19.03420689071938 0.23409567516687507 91.13312296146132 0 0 0 4608 2 -0.6097458895347748 15.480403217642293 4.294969298391944 89.5699149171136 0 0 0 4492 2 -0.6334505743049109 26.745878250961105 7.26788441361478 90.1913983547608 0 0 0 4805 2 -0.769670477897028 28.481144027810338 2.554615217390468 81.09829060295583 -1 0 0 4668 2 -0.6125953791481844 15.284100488617563 0.9266300185486216 88.58782870076173 0 0 0 4849 2 -0.591967730873839 19.63233961852585 2.1410276600968796 87.63674625041702 0 0 0 5047 2 -0.5952777008621325 18.99357193854713 4.961440309471679 87.39621446127376 0 0 0 2903 1 1.628782981921766 20.347779833582862 3.7675638205466484 87.39619674272986 0 0 0 4630 2 -0.614124864302974 16.142224294547223 5.162353130020939 87.13911098744413 0 0 0 2891 1 1.6898689754507275 14.872421820927116 0.3803639336657127 86.94662976218 0 0 0 2911 1 1.76651699816906 17.415795460732994 5.95039405856776 86.23403089281855 0 0 0 2894 1 1.6823978802467914 19.163764769307072 -0.02061948167634582 87.16015106611079 0 0 0 5267 2 -0.5520274225786415 21.298364100046317 5.05088569094439 93.52960368083181 0 0 0 5498 2 -0.6177368836875456 21.890699251796814 12.931114570944127 90.62462498394413 0 0 0 4972 2 -0.5913801114483277 14.380354191045615 9.640768568741032 89.53509481194745 0 0 0 4982 2 -0.6736826206126916 21.62412371091407 3.9897577270748052 88.61811266228118 0 0 0 5234 2 -0.556001219473618 26.687734994149984 11.583458503840099 89.93294698820502 0 0 0 5098 2 -0.7498167282644852 28.426076641167203 0.8229590801688178 86.22702557320679 -1 0 0 4459 2 -0.5953442853305159 21.305295983034558 2.591723558438301 90.98200916256131 0 0 0 4686 2 -0.7309373561765412 28.403975344614143 1.018721662034934 89.36793830241272 -1 0 0 5347 2 -0.6015926281746459 25.177412230163608 1.6389034682661214 93.54399703553197 0 0 0 4732 2 -0.6245365610197763 27.520163790594477 3.362147166049148 93.60235301295138 0 0 0 4733 2 -0.5869435255743187 24.59579164956347 4.2234954481723905 93.36163440156874 0 0 0 2907 1 1.745491936667729 25.91892984476144 3.090527130861348 92.86416663031547 0 0 0 5204 2 -0.5079976514358677 23.1150818317296 6.513632013990431 92.49689516834617 0 0 0 4544 2 -0.5904435810973407 26.62879710166404 5.062479720709516 91.854200924987 0 0 0 2916 1 1.7027115323440427 27.923170219920095 6.252399261220057 91.72729710937563 0 0 0 4402 2 -0.6245166109156985 26.483525463529574 1.85868532521258 91.1854241284402 0 0 0 4436 2 -0.5668662589943616 24.14288634938877 2.7211711042188274 91.4106809009271 0 0 0 2180 1 1.579952918547733 26.530804356468735 0.21790412651004482 90.44280118931789 0 0 0 2896 1 1.6618990690349627 22.834131965334866 3.1127547648533875 90.27121871946237 0 0 0 4384 2 -0.6604599956286259 23.09531166568559 1.7647545677391594 89.1539045103582 0 0 0 4554 2 -0.6585446001978547 23.56205875958907 4.92766248316501 89.36444591529529 0 0 0 5186 2 -0.6505894539520958 25.216548637991803 1.3530140697510333 87.7285506708132 0 0 0 4454 2 -0.6071989975685118 26.977408655967942 6.0171511468536885 87.7970237861375 0 0 0 2905 1 1.7489262774180263 22.96466407213562 6.102182024713938 88.18796224715753 0 0 0 4823 2 -0.5703983807071261 26.941364910418116 3.1348952861302215 87.34884402997477 0 0 0 713 1 1.529402737279545 27.37209444398543 1.4193910366875693 87.594260160657 0 0 0 2898 1 1.693502334759551 23.5440709808205 1.0698414772554767 87.18758668722431 0 0 0 4468 2 -0.690918401418239 22.41404795697617 2.120742909380172 86.3429192335588 0 0 0 4904 2 -0.6678044162543678 24.440113515329013 6.181679329086351 86.6379634694734 0 0 0 5052 2 -0.6419851524907783 27.894076925473144 7.032968130922358 93.28532264211722 0 0 0 4787 2 -0.599852314857999 28.249834460615276 5.371791131398911 89.52462485413734 -1 0 0 4981 2 -0.718494273381842 21.76490778125471 5.687035458781588 86.91732526212999 0 0 0 4923 2 -0.63216000752578 22.17311867729218 1.674942345545808 93.45380722853473 0 0 0 3623 1 1.6453320775980522 25.155610814529783 10.237342448159335 91.0383667906792 0 0 0 5295 2 -0.6270267877483361 14.681823340104334 10.611264832853395 87.00511823255005 0 0 0 5483 2 -0.6204058237152192 17.42401859726448 13.46807553470847 86.56065497929555 0 0 0 3628 1 1.6679762092025605 17.80881158579397 8.296220762444987 93.29097113671023 0 0 0 5350 2 -0.5857618117930207 16.529419962816963 7.826162313286865 92.10757240078122 0 0 0 5363 2 -0.5842833892518146 18.620812245728857 9.286793833894984 92.07336224940542 0 0 0 5220 2 -0.5356612884639618 15.07737135852424 9.646980715509562 91.88490500292244 0 0 0 5230 2 -0.610716488948256 17.524314037339664 11.314850101866005 90.80229998970354 0 0 0 1448 1 1.6480641493689123 16.98175968192689 12.945367001177594 90.97345840037384 0 0 0 2901 1 1.7478370452615137 15.334812157778996 8.365061964962548 90.3055270040285 0 0 0 4804 2 -0.6635544446327355 18.985998816733417 13.533648584090221 90.38640874762446 0 0 0 4834 2 -0.6018750078226289 20.06475340972437 8.411208965159847 90.30717796192376 0 0 0 5462 2 -0.6060088440707432 20.08183612318955 11.121760613691016 90.19674195774415 0 0 0 4793 2 -0.5851053474638501 17.04628822892149 8.610370759967767 89.7619126957071 0 0 0 3621 1 1.704153106975465 19.002467053789655 9.750565399816601 89.92441682784255 0 0 0 3631 1 1.7595539141444483 20.508833237923568 13.194295409680638 89.57196628531779 0 0 0 5013 2 -0.5998413283528088 15.526872027193868 11.989440087695632 89.62149757950985 0 0 0 5228 2 -0.5829928145877442 18.720243300934 9.92314652844117 88.13862947299044 0 0 0 5408 2 -0.5869478124568673 15.525454345501267 8.145447907945483 88.0429677153584 0 0 0 4710 2 -0.6244463719826046 19.095213859253434 12.44332662369362 87.85934818521037 0 0 0 5159 2 -0.643027576440663 16.906810579980423 10.60228583192448 86.42263393020588 0 0 0 3620 1 1.7521212064465768 18.44528913733737 11.4730091452399 86.56021830024136 0 0 0 5162 2 -0.6036353508365261 17.133312121222243 7.706913769109409 86.45242581840638 0 0 0 2909 1 1.7374979167670521 15.416132315897924 9.099508963001366 86.56868074439664 0 0 0 4803 2 -0.47023186453207627 16.374362931804914 13.236797289537604 92.52496869102306 0 0 0 5268 2 -0.45512168625236255 21.190986382029454 12.367069422476977 93.23638161474022 0 0 0 5493 2 -0.22589863740699262 21.350216746041568 9.629050241724478 92.6937590679887 0 0 0 4603 2 -0.6134103523602822 27.797681455708783 13.001765249772493 93.26136889250462 0 0 0 4742 2 -0.6368997787440048 28.513062460992344 8.165158339336134 88.23592056456815 -1 0 0 5040 2 -0.6095944382837737 22.21262667484886 7.2184125497579705 89.26674023521593 0 0 0 5282 2 -0.5631043350715416 24.621367228830547 7.531296513586767 88.54953407501846 0 0 0 3625 1 1.7806403124666954 26.39287597976506 7.543829809460309 88.47957095473687 0 0 0 4674 2 -0.36254938060795244 21.44422451119699 8.498909690952281 93.49363869543912 0 0 0 5170 2 -0.5162571106339701 24.41792321446249 11.774192962615183 90.78414945262101 0 0 0 5191 2 -0.6142824061975751 21.750692345005692 12.163767064890388 88.00528906357448 0 0 0 3627 1 1.696800194352131 28.328552637758495 12.270508375025642 90.02755165511827 -1 0 0 4810 2 -0.584777105192596 27.352686308242447 13.933542033919526 88.91558376931673 0 0 0 3629 1 1.6315474666331173 22.78286255119454 12.551197759094922 92.57769519148614 0 0 0 5210 2 -0.5395627826898312 25.818198249940227 9.469811980805007 89.62164803543095 0 0 0 5406 2 -0.5873531697825164 26.672364474972035 10.1034565596074 92.43441124665539 0 0 0 5214 2 -0.4362270767930689 24.101444896720242 10.695706464438627 87.5799326860275 0 0 0 5272 2 -0.5940420438988523 23.777881839546197 11.125516375050887 92.68666487104636 0 0 0 4539 2 -0.5992840404370092 26.660784994303263 8.807383125934724 86.61432649737772 0 0 0 5296 2 -0.6187124992924782 22.685712535567664 10.186238880546522 85.76007641867838 0 0 0 3624 1 1.7264272563254022 23.12467285551395 11.986169984543213 86.89884188729829 0 0 0 2914 1 1.5479234018555854 21.874202887784975 7.710240205357999 91.40373174252498 0 0 0 4792 2 -0.517958316897055 23.632275093189975 8.738609868852093 90.88195554417018 0 0 0 5369 2 -0.6758702459552041 22.657453295633623 13.876379142528295 86.06662734113486 0 0 0 4418 2 -0.6745903274111621 28.530561751271946 4.682067372012304 85.94088735033192 -1 0 0 5371 2 -0.7727290323222966 14.345530008535103 10.252532413961703 83.11869022436369 0 0 0 4577 2 -0.5862285554871984 14.3442234099243 13.304011577454949 87.88791987256857 0 0 0 4555 2 -0.623150690530949 21.57805434999429 -0.07226126998739346 91.37890303029205 0 1 0 5443 2 -0.6493542969333401 19.064134904904712 6.664010814448069 93.78410917562272 0 0 0 5173 2 -0.42689167280199053 15.708369998378181 5.859725639364559 100.08067766889901 0 0 0 4731 2 -0.4222440422249266 16.166340736064 3.2482288350194843 99.87238008739098 0 0 0 2908 1 1.4963993039702876 15.28735832729194 4.535532073244662 98.77734132023691 0 0 0 5227 2 -0.5992129628605347 17.41650106081988 4.344856757674909 97.90021311482056 0 0 0 5322 2 -0.5467352663678964 20.269654358335956 4.122233566162242 97.20442633192954 0 0 0 5308 2 -0.5949301678997817 18.83479491525584 1.8085830775739729 97.54466793434601 0 0 0 5453 2 -0.5269970035381816 14.43267767730056 6.468870908637965 97.41705459258993 0 0 0 2910 1 1.622547906302215 18.445819987108774 3.4148587607289462 96.90629673575941 0 0 0 4790 2 -0.36152766720197443 16.449787580817418 2.64442340530549 95.9410141044341 0 0 0 5390 2 -0.23392567876754292 16.081426273905336 1.308991790602056 95.96868856409755 0 0 0 18 1 1.5670925406526373 14.405882027310481 2.6447392466141038 94.9657914361737 0 0 0 5449 2 -0.5763136591214312 18.603973060631926 4.2915705211737745 95.08768146057692 0 0 0 4471 2 -0.6153881646187404 21.012509784913803 1.5752573576774238 96.69813066366048 0 0 0 4684 2 -0.45965389432711 14.449437137089017 3.839032594254565 96.65741060906485 0 0 0 5469 2 -0.21736228463608875 16.75263472533894 6.815791531688568 96.12236896162766 0 0 0 3665 1 1.6782123695519011 20.250281994043775 0.12665665423633235 97.39449365827747 0 0 0 5457 2 -0.4612862449659286 22.100486397658 0.30694025528634533 102.27299817772469 0 0 0 5355 2 -0.2932887547603872 25.457833814785126 1.8666578441160853 100.88987447920559 0 0 0 5429 2 -0.40814354646314827 24.363768255724892 1.5368749930377013 100.01915881829488 0 0 0 5111 2 -0.6115968957272361 21.925008169662927 2.105017150086176 98.7200340340685 0 0 0 5225 2 -0.47319573164581624 27.375538368400793 3.5868686113477017 98.95471838138945 0 0 0 5209 2 -0.6182991598047995 25.146749265251483 5.033538465472161 99.22811203256998 0 0 0 2211 1 1.6030047765661894 24.143437340471365 6.439206381186634 98.87243475977372 0 0 0 3630 1 1.6606061331722488 25.804787782800013 2.914851424353215 98.92369134924208 0 0 0 4990 2 -0.6052391008302277 22.792001908112297 4.679194212670572 98.37219858389636 0 0 0 5373 2 -0.5449378862549082 26.41246109820759 1.216309498730529 97.92460481883755 0 0 0 5415 2 -0.5978038472916425 24.367421579514644 2.8161015180995506 97.96979359732825 0 0 0 2912 1 1.7208965507146354 22.298721849002128 3.266476641248529 97.43123929346731 0 0 0 5034 2 -0.520609117956566 27.43228809125585 3.5089624931404266 96.68786672010029 0 0 0 5054 2 -0.3877535199293505 24.023722536503694 5.992099061255245 96.5650394679635 0 0 0 10 1 1.7378244246232792 26.9078855300611 0.2524674553082855 96.18205362105647 0 0 0 5180 2 -0.2729068146419696 24.872704426116368 5.0198199758079705 95.9164692599979 0 0 0 4553 2 -0.6113072583873148 23.154249445037635 1.983821913063603 95.9069700167543 0 0 0 4824 2 -0.6043151718059999 25.297878960011953 0.5600438233182334 95.64169647686339 0 0 0 5337 2 -0.494233400166131 22.294101529057894 4.109576831631944 95.39360937726885 0 0 0 4743 2 -0.5956866542879811 27.906232300826957 1.4763973850707275 95.37323990488234 0 0 0 2200 1 1.7773476620216306 23.375721422172827 0.8914502436986556 94.55608328181033 0 0 0 2202 1 1.543837066401253 23.25206721362852 5.658507477374655 94.48683659676261 0 0 0 5215 2 -0.5545902853089245 21.822355119643127 6.746190407488761 95.4651798440948 0 0 0 2209 1 1.5867548277407575 22.520523587854203 0.4117556632898945 100.23287258836692 0 0 0 5033 2 -0.47412313279980195 22.974656273237244 7.263374858558579 99.86899614850729 0 0 0 4954 2 -0.28049327458560824 25.265256871745578 8.049591955599086 103.58453686994493 0 0 0 5147 2 -0.41341628788806606 21.865105606078462 1.6922142252510242 101.85236827817974 0 1 0 5150 2 -0.48186847039821823 23.57411219540175 9.827914294317786 102.45901308318156 0 0 0 5441 2 -0.3633158553473553 16.33355612895381 7.090865458947844 94.84084338589908 0 0 0 5419 2 -0.3550076130399357 17.634323754275012 12.257844813909514 95.9023678736715 0 0 0 1439 1 1.4808341439760773 16.409827703071254 10.876369461137553 96.36810789343163 0 0 0 5183 2 -0.39686976185848033 17.470578222076135 9.853512498707941 97.57562617008452 0 0 0 5471 2 -0.6002472663048131 15.030276840252844 8.976679526930704 96.56685482969705 0 0 0 5496 2 -0.4441095455705868 20.05725058734743 8.360778261954875 97.27187721668813 0 0 0 1440 1 1.6467062150371121 14.422424910051712 7.466316296686846 95.9215656688777 0 0 0 2922 1 1.5847581542384304 20.93576854500093 8.570773909228953 95.78030472472165 0 0 0 5487 2 -0.40566406540690136 15.053778219145133 12.004401710654427 97.06281784251944 0 0 0 5288 2 -0.5344214115069851 15.023797836248308 11.266084525967038 94.55169403875514 0 0 0 4905 2 -0.5210903949825052 19.504005833435453 8.931180321690153 94.80261026933258 0 0 0 5500 2 -0.5319271005679799 17.090756536442964 9.527628144907242 94.42076186748844 0 0 0 2924 1 1.4910518316624484 25.110457016128038 9.465523249373435 101.74940805814403 0 0 0 5232 2 -0.25561509483207234 22.975872477413176 11.347930476302713 99.84824288894191 0 0 0 5450 2 -0.37355039957931596 24.21209240630546 10.579347074721479 99.90401861387427 0 0 0 5478 2 -0.47171621393743585 25.107376130348776 7.69600923203422 100.41070101282918 0 0 0 5311 2 -0.5743794275047381 23.486064746570666 13.89449415828604 99.37755890051471 0 0 0 2920 1 1.5582448065891488 24.296905527931628 12.145119379262844 98.22947647359251 0 0 0 4640 2 -0.5345357171164274 25.965236001113738 12.619392270470234 98.55775391696584 0 0 0 4965 2 -0.5621168664320294 24.832263685748135 7.970323019753324 97.68891629439415 0 0 0 5508 2 -0.47721787558921974 23.37809670715708 13.234602686867225 97.13700735661509 0 0 0 5446 2 -0.47057595731406254 24.95793036061784 10.852307676208325 96.72143640245297 0 0 0 730 1 1.4850128542336456 25.3207494672085 8.829850296280496 95.86813248660543 0 0 0 4634 2 -0.5437819646840717 26.930636537462128 8.105949742007553 95.56644094356666 0 0 0 5244 2 -0.38290975485828044 23.02014908433657 9.309818532349661 95.89020974192509 0 0 0 5510 2 -0.2638349532511692 22.252447940022762 10.296064866531617 96.47786662408814 0 0 0 4597 2 -0.4682236342571553 26.37208563425879 10.481634666473443 94.99233016422095 0 0 0 5104 2 -0.49592013304479377 23.247087174765753 13.52259281323795 94.43089766365581 0 0 0 5442 2 -0.5014401849944281 24.5778995185846 7.368956960511078 94.55004774215259 0 0 0 5383 2 -0.486427560654573 26.499522721233028 10.535185785599541 101.72576804532194 0 0 0 4818 2 -0.26594705550852393 26.54930772753869 8.09176100150536 103.18155423221361 0 0 0 4853 2 -0.38474954063036954 28.101990023862022 13.27946405949909 96.48076447055564 -1 0 0 5318 2 -0.5278702718655743 19.32813421779436 1.0255777502088685 103.98156379854693 0 1 0 2927 1 1.473398604673501 21.094575263317232 1.1964375212127931 103.91952518651634 0 1 0 5197 2 -0.5023582120133061 21.414790874338628 2.7394914046640397 104.71277090562198 0 0 0 5397 2 -0.4500432445529031 28.51090649453312 13.697976233083187 97.83253973186414 0 0 0 4950 2 -0.6255718384687738 20.958787338434497 0.02105324662886558 99.43096476305605 0 0 0 4935 2 -0.603099959966295 28.499291889461027 5.368822254425342 95.09982382016763 -1 0 0 5176 2 -0.28274140675790804 22.596507481962888 0.5259106875957273 105.58279542784793 0 0 0 5358 2 -0.5343154411210896 25.26465299573119 14.21948012059777 96.48909203039169 0 0 0 3674 1 -0.0011063812305091734 15.461879267505227 18.795325806090563 2.1407025366234373 0 0 0 2963 1 -0.0010494394543450578 15.366874598439 15.549436912864895 2.21843323664991 0 0 0 2965 1 -0.0007990472163754579 18.568111469365633 15.577354300390116 2.1797789078841157 0 0 0 3676 1 -0.000902490493339644 18.583275809009226 18.77125409673048 2.149501490065633 0 0 0 3648 1 0.016445303593901388 16.974147099644554 20.40467762462414 0.6766276189677959 0 0 0 3650 1 0.01566416209270652 20.16925217864733 20.35411636908773 0.7769443168940212 0 0 0 2937 1 0.015744965333966125 17.004231332856495 17.170887537137304 0.7453015362859718 0 0 0 2939 1 0.01526528543883697 20.144364409729686 17.198926787384945 0.812283728281539 0 0 0 2967 1 -0.0012872736631041122 21.77193943568668 15.595629005573098 2.253332249033424 0 0 0 1486 1 -0.0010832062403242238 28.044249346433602 18.78754150230742 2.153277638600121 0 0 0 2969 1 -0.0010706819499986314 24.89649688062727 15.617566831767615 2.242847815203493 0 0 0 775 1 -0.0008828441993339719 28.082510333179492 15.58217043366629 2.1167908879981305 0 0 0 3680 1 -0.0013800109743109888 24.893262465887744 18.821088838662227 2.138741824245791 0 0 0 3678 1 -0.0008130471040064789 21.73719200786458 18.81031246651878 2.265070983181049 0 0 0 3654 1 0.016656781318503233 26.47388731081063 20.301703365539716 0.6840648709014235 0 0 0 2943 1 0.016275172390482255 26.4804526244007 17.189840999913137 0.6872147055312529 0 0 0 3652 1 0.015500565181363425 23.36412379353492 20.34671102819955 0.7991371027589296 0 0 0 2941 1 0.015788056250776575 23.246088468361407 17.181436228953185 0.7709293139636968 0 0 0 3683 1 -0.0013693595095373295 15.406950558705935 22.05755547215571 2.1334229781140035 0 0 0 3692 1 -0.0010454123437472046 15.380283663191326 25.213064068787 2.202804817574137 0 0 0 3685 1 -0.0011189797387018575 18.57305367836302 22.014518030042726 2.1649518085308364 0 0 0 3694 1 -0.0012342635755212845 18.512690356385153 25.14103381160076 2.1593641188772144 0 0 0 2218 1 -0.0008150257512448476 18.53350154505908 28.35054330678973 2.1505023802715786 0 0 0 2216 1 -0.0008604282021017675 15.391691508745513 28.352759391757544 2.1322014425172093 0 0 0 3657 1 0.016378552733348005 16.903548016836346 23.54737292823917 0.6325837363103084 0 0 0 3659 1 0.016683685417624036 20.097722406540157 23.51332196876271 0.6160917656268118 0 0 0 3666 1 0.016105813280988333 16.988233726075357 26.675586524203524 0.6643419532540276 0 0 0 3668 1 0.015808208300843327 20.12322647561951 26.747382415124626 0.6602707020511986 0 0 0 3687 1 -0.0007767110476834711 21.705146908667757 21.957176792203356 2.2905553766744453 0 0 0 3689 1 -0.0003345633359764889 24.871920725826623 22.020636964194413 2.2395385907976806 0 0 0 3698 1 0.00026562580171099546 24.91048097739401 25.119711449796746 2.1478417000561296 0 0 0 1504 1 0.0009398785334981162 28.060842101962603 25.173215324605106 2.187298757027643 0 0 0 2222 1 0.0006311758712714221 24.903666182043136 28.40873676735702 2.030477998163995 0 0 0 1495 1 4.018529942321449e-05 28.078070442995923 22.005855017275636 2.2922785063280946 0 0 0 2220 1 -0.0007953445373565951 21.710143062486377 28.35521850554573 2.1749626654938146 0 0 0 3696 1 -0.0013204384441005226 21.716552767063433 25.14301588979584 2.073876709921168 0 0 0 28 1 -0.001873660028235912 28.029109031092986 28.478808781788732 2.095928187860701 0 0 0 3661 1 0.015899876050771235 23.222466401418853 23.604493403312045 0.7289509397522315 0 0 0 3663 1 0.016199551812749853 26.506444143170533 23.485488824244094 0.6586837351658904 0 0 0 3670 1 0.01718262510862996 23.27490650445554 26.770845103794034 0.5447267856072084 0 0 0 3672 1 0.00880817333916432 26.473965131041297 26.63547009439834 0.7401317840328316 0 0 0 1 1 0.027308072886748178 27.974141448975534 28.453242082412896 -0.7202195568201886 0 0 0 3018 1 0.004687540539525659 17.002063968750086 17.21993699713711 10.124421557411722 0 0 0 3731 1 0.004570463422091532 20.12215273466187 20.3801385779237 10.105083537000025 0 0 0 3020 1 0.004425525183916144 20.17059060775876 17.173076145549768 10.027049365329017 0 0 0 3729 1 0.004599797593356233 16.963087688681856 20.393794077493236 10.082738806706598 0 0 0 3730 1 0.004441085118626589 18.6169053405557 18.761491868991424 8.50518317809999 0 0 0 3019 1 0.00453050040454747 18.582491874350552 15.566646826594356 8.548721178206378 0 0 0 3017 1 0.004561006695476644 15.490779523931343 15.558716931876935 8.52039239861735 0 0 0 3728 1 0.004487644034127733 15.365969235763032 18.815541510150783 8.568303871935916 0 0 0 2991 1 0.005261770081547459 16.970432851558538 17.18299512993116 6.877060822013977 0 0 0 3702 1 0.005361494421838149 16.942818749486243 20.363774623147734 6.902626640237432 0 0 0 3704 1 0.005404516968326263 20.194716745149496 20.360945307452614 6.926559998752419 0 0 0 2993 1 0.005263782696157446 20.158159657262654 17.14637115216246 6.960705755056146 0 0 0 2990 1 0.0055279627186354645 15.356199877029184 15.597973560774172 5.382104666374108 0 0 0 3701 1 0.0054809464550943255 15.302804383529377 18.78145723939 5.366653048526924 0 0 0 2992 1 0.005594129077671631 18.50518163506765 15.579221618699213 5.402410202225586 0 0 0 3703 1 0.005484266767884683 18.56551226286232 18.756450431750256 5.315687958397921 0 0 0 3675 1 0.004018132590432138 16.931580658315404 20.39449316083443 3.775998804345616 0 0 0 2964 1 0.0039628749797925335 16.965243597110213 17.18725148810156 3.746001417111693 0 0 0 3677 1 0.004208687876063934 20.12403770993316 20.306496895435117 3.8286334484528712 0 0 0 2966 1 0.00398728864820456 20.231509905153946 17.217517160226464 3.821042093168935 0 0 0 3733 1 0.004699453765017769 23.432209615538003 20.463996982650357 10.183024133112708 0 0 0 3735 1 0.004572455087166747 26.593210979516968 20.41535617370991 10.105242436633057 0 0 0 3022 1 0.004608721033071809 23.380638103578093 17.260797876439618 10.079916201101877 0 0 0 3024 1 0.004667308844150826 26.62407885263025 17.24859006958706 10.095813815094173 0 0 0 3021 1 0.004501638771599948 21.76801244813633 15.60948214630588 8.538941192046632 0 0 0 3734 1 0.004633643385149298 25.027800309300908 18.87444841145102 8.526300215013993 0 0 0 1540 1 0.004491812307980601 28.245632921166912 18.91063564897566 8.548569860794364 0 0 0 3023 1 0.004515489602633191 24.919487508254868 15.608175948471704 8.577508274451507 0 0 0 829 1 0.004525580016688954 28.258333074126167 15.610172020721887 8.55858056843993 0 0 0 3732 1 0.004608400697198034 21.75550379497158 18.874008348121126 8.582876144505697 0 0 0 2997 1 0.005410091558820065 26.59503235669962 17.183536463329332 6.921445996310105 0 0 0 3708 1 0.004994332640313778 26.640712567718964 20.403143704460046 6.96646277119729 0 0 0 2995 1 0.005208473628952772 23.384452789408293 17.155434998553783 6.978621789043167 0 0 0 3706 1 0.005366591782752877 23.436168138487922 20.4096755538956 6.856760160506054 0 0 0 2996 1 0.005571708850776727 24.93469236150589 15.562860369646973 5.4003147521254835 0 0 0 3705 1 0.005544319774867634 21.863685758467163 18.691676250726847 5.39688197272645 0 0 0 2994 1 0.00550291185126855 21.781620151788868 15.542134706576407 5.324138832299721 0 0 0 1513 1 0.005254149756136684 28.059974509089827 18.81952052091858 5.362920943895009 0 0 0 3707 1 0.005397200131068638 24.94332640243814 18.74077588792698 5.376883095647159 0 0 0 802 1 0.005611011750328219 28.099812348491447 15.623783989166219 5.384205842934347 0 0 0 2968 1 0.00397836968831067 23.36076812611431 17.179246858136548 3.778121580701025 0 0 0 2970 1 0.003931890288912842 26.55851641889769 17.18372285337751 3.6948399835798065 0 0 0 3681 1 0.0038870300931992466 26.511373549413623 20.319200495380695 3.8888724407701556 0 0 0 3679 1 0.003917016248052567 23.382814726303685 20.350813041404717 3.840593092514655 0 0 0 3749 1 0.0046839161018913875 20.180662800006797 26.71026026906233 10.174354066230032 0 0 0 3747 1 0.004471427087054296 16.968913481616852 26.794745040362823 10.14480132688203 0 0 0 3740 1 0.0044975386727354166 20.197053690325944 23.51183805044158 10.08158001784672 0 0 0 3738 1 0.004538843831436405 17.024919661811012 23.59620771230461 10.191425264985043 0 0 0 3737 1 0.004571195863764487 15.426721672067307 22.014535543782934 8.520368921362696 0 0 0 2272 1 0.004506765020346958 18.538655898235938 28.391392290040432 8.534781488713985 0 0 0 3739 1 0.004536180439128866 18.56839367308264 21.946177264191903 8.550756682304574 0 0 0 3746 1 0.004547816022380144 15.358334624505037 25.18255261954441 8.576220633811422 0 0 0 3748 1 0.004580916426275644 18.508808005588936 25.093128430163855 8.53582154366949 0 0 0 2270 1 0.004598571810903821 15.433643103582666 28.376152729018045 8.49877715889866 0 0 0 3720 1 0.005162574867372019 17.02361472743772 26.764399884970967 6.955816834168146 0 0 0 3722 1 0.005399075323902878 20.131412646185726 26.786995673503895 6.889609601489614 0 0 0 3713 1 0.0052894215644897925 20.13747052258497 23.510593920328123 6.828528470660816 0 0 0 3711 1 0.005259162137058709 16.9637880808021 23.59337924681599 6.897124151701668 0 0 0 3710 1 0.005520616077592773 15.345563296292392 22.038059589973415 5.251148788741796 0 0 0 3721 1 0.005588164996566411 18.56162631385289 25.18914032831587 5.339110480318771 0 0 0 3719 1 0.005691339436187456 15.416046725961015 25.172642437885575 5.359776801469554 0 0 0 3712 1 0.0055451854218689905 18.51547612456181 21.924994495932054 5.309966108067757 0 0 0 2243 1 0.00554358249878106 15.421608677323013 28.294285613774633 5.301710491425397 0 0 0 2245 1 0.005701721843740138 18.544597196318644 28.314385443527776 5.237331007513407 0 0 0 3684 1 0.004089804213977069 16.94465781585989 23.558483733730622 3.72412858155009 0 0 0 3686 1 0.00405478505722808 20.194249169819948 23.558223351510478 3.7428725139919905 0 0 0 3693 1 0.004025314810089662 16.985550035500882 26.76772046323516 3.7410215283427264 0 0 0 3695 1 0.0037017328558340053 20.064100663424824 26.65333034774351 3.5832360390633866 0 0 0 55 1 0.005811386320033593 28.033021854687792 28.45927359044038 5.327644307653038 0 0 0 2249 1 0.0056164789416709646 24.841743105372398 28.33282631598726 5.277008159166681 0 0 0 3723 1 0.00553767418575885 21.761609017172038 25.126583139935036 5.307892282878703 0 0 0 3688 1 0.0038166899701984423 23.403567550712935 23.59810237336133 3.761374768814259 0 0 0 82 1 0.004469701164929323 28.12051880894644 28.34143853426505 8.384883908733528 0 0 0 3697 1 0.004034836691701269 23.292775983390047 26.675514965548135 3.610399217132552 0 0 0 3699 1 0.0049650686885235 26.543921455804256 26.738093275516263 3.7932055606190582 0 0 0 3742 1 0.004637740895439538 23.432669571257925 23.647965817749174 10.127349652616882 0 0 0 3751 1 0.004648332571302203 23.237774718399468 26.848836927065097 10.127438529295064 0 0 0 3744 1 0.004766775690221053 26.540922647672897 23.59737109006585 10.235836179339184 0 0 0 3753 1 0.004588070622027119 26.535231173765084 26.735228582966887 10.1104073939272 0 0 0 3741 1 0.004622329721148212 21.76009570981753 22.044495027338627 8.466311614705441 0 0 0 2276 1 0.004590795668611779 24.937641434020275 28.45074722601431 8.45487436815329 0 0 0 2274 1 0.00460900022175462 21.602246457592546 28.335142657902328 8.474476256328913 0 0 0 3750 1 0.004631739448317058 21.664987955366538 25.08230826844766 8.459891868860584 0 0 0 3743 1 0.004678137610032083 24.965723045754096 22.012585464256688 8.551689272088804 0 0 0 3752 1 0.004587189395275828 24.932410790844543 25.313238264849243 8.686723275876862 0 0 0 1558 1 0.00440785476157984 28.108714049589707 25.237720936962138 8.473354144747267 0 0 0 1549 1 0.004454172740233775 28.17289494004088 22.11374427929919 8.449460712613208 0 0 0 3690 1 0.004274238831035088 26.538834406655145 23.535048343631363 3.739056556049415 0 0 0 3717 1 0.00499797819052571 26.47989225982525 23.579853251053763 6.8988421900756345 0 0 0 3715 1 0.005185796727505338 23.3940576470358 23.603607128525283 6.9248172016078495 0 0 0 3724 1 0.00530589831681723 23.315419066639596 26.80988991399452 6.95615967623217 0 0 0 3726 1 0.005028688213202567 26.51293432365781 26.762752988018153 6.826098628552221 0 0 0 3714 1 0.005522177434668861 21.82217507717928 22.047880457246087 5.337736009217433 0 0 0 1522 1 0.00534275608516795 28.146917541919315 21.985616787270935 5.403581488145585 0 0 0 3716 1 0.005102446844187513 25.003021166472127 21.94330309553798 5.387836213656663 0 0 0 1531 1 0.005657593382772023 28.155593190810606 25.17049506772762 5.365884334174369 0 0 0 3725 1 0.005471194172234024 24.983968091210766 25.157779955029287 5.334377463416714 0 0 0 2247 1 0.005815875492249751 21.68763576518506 28.312070537774723 5.247523584381002 0 0 0 3810 1 0.00491923743494076 16.981044810872667 20.48884081689786 19.662168377663377 0 0 0 3099 1 0.004846418872644129 17.070174708523844 17.15720216763226 19.666112522360574 0 0 0 3811 1 0.004998651352292835 18.559491172623503 18.908482499475074 17.982833587026963 0 0 0 3100 1 0.004564603171871627 18.59486566549223 15.578519987562489 18.04688296101436 0 0 0 3098 1 0.004760625683566907 15.444971063967378 15.641389466090976 18.13130487551418 0 0 0 3809 1 0.004723157769631024 15.425538773176292 18.84648945912696 18.170618413232187 0 0 0 3795 1 0.0048694611754908235 20.18879370699094 20.505600375291774 16.433179930163753 0 0 0 3076 1 0.004757816649261141 20.198902711607246 17.140496195454208 16.51193585029405 0 0 0 3075 1 0.004763169486686409 16.996111922911208 17.243778797616326 16.4996364313355 0 0 0 3794 1 0.004749224590512616 16.9243510397574 20.53965139155411 16.46179445104236 0 0 0 3061 1 0.004721416074039244 18.57332486495706 15.679464230655057 14.915746503059625 0 0 0 3781 1 0.00484476391640465 15.384804990861667 18.885023444621403 15.061248102159608 0 0 0 3782 1 0.0047493052183087345 18.56151402171375 18.784115057255153 14.86400360653672 0 0 0 3060 1 0.004839739604070975 15.371655556846902 15.642101850463972 14.897276968269388 0 0 0 3758 1 0.0048410472036028804 20.210316434060857 20.432518547832885 13.40583116550303 0 0 0 3047 1 0.004792855485874159 20.264066633462075 17.26210567661989 13.389840476893305 0 0 0 3756 1 0.004887224302561928 17.036722083843266 20.438237038978794 13.414314937342015 0 0 0 3045 1 0.005034491255414731 16.94405490002787 17.22025268138198 13.27472136508004 0 0 0 3757 1 0.005120841610933447 18.71224381692892 18.812646175073475 11.679512688550153 0 0 0 3046 1 0.005046611287575883 18.59248594153744 15.714538763999105 11.732194636228568 0 0 0 3044 1 0.004841298662965796 15.26798312395873 15.57595219987365 11.738073765214217 0 0 0 3755 1 0.005190394735097324 15.358591816882706 18.899153570213564 11.753361982716855 0 0 0 3101 1 0.004756738369189587 20.174600690957284 17.231360299572373 19.594547745133365 0 0 0 3812 1 0.0048677860678533955 20.191512111055236 20.41653836191401 19.65152116661332 0 0 0 3813 1 0.004695278602245681 21.73585144492017 18.77975261025073 18.169322567636222 0 0 0 1621 1 0.004915665078190816 28.178345412287587 18.85681153691425 18.096841932717677 0 0 0 910 1 0.0047818226357684394 28.239923680748635 15.708855159044488 18.11800392021396 0 0 0 3815 1 0.004807195732623925 25.01009771171887 18.867803357290324 18.132155456235832 0 0 0 3104 1 0.004817333483788176 24.94007863126539 15.603812785225607 18.00197102581446 0 0 0 3102 1 0.004736608351637075 21.8442757538275 15.703427324453397 18.102693113959937 0 0 0 3797 1 0.0049332360653131825 26.628802607875695 20.518488905579666 16.456615653828056 0 0 0 3796 1 0.0048421467370908765 23.37760244180843 20.425512865855666 16.63407339338591 0 0 0 3078 1 0.004811220335781423 26.568872110630238 17.17933831138103 16.436724199505207 0 0 0 3077 1 0.004693743229543464 23.393569865437097 17.283123089253962 16.517417865239235 0 0 0 3062 1 0.004762383785632282 21.779143316775137 15.603893263268391 14.891103619854988 0 0 0 3783 1 0.004730581975270235 21.830851435504783 18.829041981473235 15.005963165745678 0 0 0 875 1 0.004448328605479446 28.149139210722737 15.597695817094339 14.857693908691513 0 0 0 3063 1 0.004672556933973658 24.91799147485511 15.604540237367091 14.9397436995472 0 0 0 1594 1 0.004707531175527623 28.122613065572406 18.76527458597498 14.89816350348371 0 0 0 3784 1 0.004731943011083293 24.99308528508295 18.87532117042538 14.924670062103795 0 0 0 3051 1 0.004899234827438571 26.557214345499602 17.272510915485146 13.340478977647026 0 0 0 3762 1 0.004777097405050758 26.609689479079776 20.407068657193204 13.29830776559285 0 0 0 3760 1 0.004861005238278595 23.41656661842482 20.42070864923786 13.30832073925564 0 0 0 3049 1 0.004893740313934391 23.392819942386257 17.330734323077092 13.318496240733618 0 0 0 3759 1 0.005091060905773742 21.754055383963323 18.80067899266773 11.743320418501266 0 0 0 3048 1 0.005137407701151373 21.765898752276705 15.577875603319326 11.72290607356907 0 0 0 856 1 0.004992682518402769 28.254407218845675 15.713269007373391 11.71214289853101 0 0 0 1567 1 0.004888878561079238 28.254667121695768 18.812641335346576 11.7024879268197 0 0 0 3761 1 0.004903124014803761 25.011431769071038 18.83536652377011 11.669689419053194 0 0 0 3050 1 0.005188882221534021 24.948958672361165 15.638626332958305 11.708105160403404 0 0 0 3814 1 0.004632177497668378 23.39692206709426 20.38731852588896 19.75202378252999 0 0 0 3103 1 0.004843229087271167 23.463715461453045 17.352397749352434 19.635449352199476 0 0 0 3816 1 0.004699274302667124 26.528121590027382 20.432096943796527 19.71742657383472 0 0 0 3105 1 0.004800779949800963 26.605494094987943 17.183775124972403 19.643118874415354 0 0 0 3819 1 0.004806157321954028 16.999469076408726 23.69632820469814 19.725523865802813 0 0 0 3827 1 0.004847053605262424 15.334538100885954 25.211517419849514 18.116049125080938 0 0 0 3829 1 0.0047762286542092965 18.522046434716817 25.269928455070716 18.12077974769413 0 0 0 3820 1 0.0048821305659381194 18.619772487481608 22.15356572905448 18.08203117529219 0 0 0 3818 1 0.004725941132318801 15.424328680835353 22.038906161335795 18.123475920665097 0 0 0 2351 1 0.004786930691437031 15.324235559116394 28.480542428556564 18.15720526836846 0 0 0 3804 1 0.004894055769413812 16.954430625520605 26.915431922856467 16.505242615390355 0 0 0 3800 1 0.004805091204430043 20.200470255586502 23.640103123731073 16.629419144556213 0 0 0 3799 1 0.0048403823966916455 16.99315889211512 23.776655186941124 16.415581910026923 0 0 0 3805 1 0.004793053949857844 20.180647152715046 26.76733204034493 16.515799902365888 0 0 0 3786 1 0.004541440324941477 18.556404295441265 22.04314828266307 14.906649110701727 0 0 0 3790 1 0.004605261144748284 18.589495224568076 25.2249350787897 14.908807138127212 0 0 0 3789 1 0.004743285020712779 15.286663269214294 25.30305966014433 14.965251248728988 0 0 0 3785 1 0.004656264196565877 15.259292864160136 22.02869855699621 14.997430277793674 0 0 0 2324 1 0.00455467139956427 18.657643400209643 28.386436493732386 14.969005119252106 0 0 0 2323 1 0.0047377931444613375 15.373875129284462 28.43795963067757 14.879979077020165 0 0 0 3776 1 0.004825312050416681 20.150050081773276 26.724004731631712 13.392089007038978 0 0 0 3765 1 0.004828180759351803 16.947118027840705 23.647712966988014 13.37311599024265 0 0 0 3774 1 0.004809004854879093 16.992772881972925 26.862346600505997 13.3308420078302 0 0 0 3767 1 0.004719644216369386 20.107148697586577 23.56254966371449 13.358405120501994 0 0 0 3773 1 0.005073287656317175 15.288093784160814 25.197897168213878 11.70153532561392 0 0 0 3766 1 0.004991198125499653 18.490560360311388 22.04065404932872 11.81592041669509 0 0 0 3764 1 0.005089969855907749 15.4059352699386 21.951649937956336 11.781423213760192 0 0 0 2299 1 0.0048894232940065434 18.47566987708399 28.2393092990341 11.69592516143793 0 0 0 3775 1 0.0049744708512965245 18.544249478253473 25.1372488410679 11.77736125402346 0 0 0 2297 1 0.004908973132192818 15.366707500616803 28.379340007105593 11.691168660678825 0 0 0 2353 1 0.004699900567286235 18.607597851066288 28.529857498974565 17.996002668392318 0 0 0 3830 1 0.004741705283956264 20.152540775903745 26.817245684016235 19.710157048228687 0 0 0 3828 1 0.004895098330674958 16.93844023838209 26.894028174829373 19.68741726604447 0 0 0 2355 1 0.005003207868394173 21.787637441023307 28.31626881977029 18.081179707270294 0 0 0 1639 1 0.00471973281157795 28.14641936123469 25.212623365350883 18.089110395470783 0 0 0 3831 1 0.004812650655266761 21.80083593509086 25.190327734071584 18.19320866381168 0 0 0 3822 1 0.004754909132135941 21.806012274491078 21.9897176200914 18.18984530297946 0 0 0 3833 1 0.004778600805057815 24.993005487827983 25.190070418488464 18.11112644455482 0 0 0 1630 1 0.004841010681028933 28.192443301466714 22.075092977632526 18.146233832702826 0 0 0 3824 1 0.0047821094333089405 24.948179776637883 22.011939666086413 18.187751217246948 0 0 0 2357 1 0.0049016036904186554 24.968642338163615 28.464669376335635 18.020302922058175 0 0 0 163 1 0.004712733687982954 28.22737171272272 28.465732619792508 18.068258671405665 0 0 0 3806 1 0.004917927967327162 23.475478116058856 26.624063384589828 16.47072042189307 0 0 0 3802 1 0.004785625377970604 26.62949615130499 23.604098718766963 16.523774082649737 0 0 0 3801 1 0.0047814412461023754 23.428740890082814 23.545439806743346 16.62838731330939 0 0 0 3807 1 0.004924356669121542 26.636878054094524 26.80111079986001 16.47588114674897 0 0 0 1604 1 0.004748345721390148 28.27026337034558 25.195561418338496 14.864698339426374 0 0 0 3787 1 0.004719629478211989 21.750304442988394 22.02128503457489 14.910481584262513 0 0 0 3791 1 0.0046725929965888546 21.799097142568204 25.13328441177577 14.951454034596308 0 0 0 1599 1 0.004706739297321167 28.128877342735358 22.06536040271364 14.865438570379508 0 0 0 3792 1 0.004773346323483101 25.050572063066657 25.17372307025754 14.909168983399331 0 0 0 2326 1 0.004777114567222261 24.95069796102978 28.4758865258135 14.856523924289007 0 0 0 3788 1 0.004835860736879444 24.950921511261708 22.033113001637098 14.88533028222151 0 0 0 2325 1 0.004727552848567787 21.792398144910372 28.349511662378468 14.916272946917704 0 0 0 136 1 0.004693694139459283 28.2226331022112 28.381600976619865 14.910512213664477 0 0 0 3771 1 0.004655980725272485 26.606025582833027 23.713589538280157 13.32565286764174 0 0 0 3780 1 0.004748860262538878 26.58233836799811 26.86735970156633 13.239860934665428 0 0 0 3778 1 0.004788983968151878 23.249325741792234 26.749814614809935 13.29854354875191 0 0 0 3769 1 0.004717484228612576 23.274658089330703 23.659023142087488 13.421109889503454 0 0 0 3768 1 0.005155161667985795 21.785357729193883 22.080643760127348 11.717030012743052 0 0 0 3779 1 0.004880870263358402 24.959160822957863 25.206546803701237 11.822387375228473 0 0 0 1585 1 0.0049238004173049275 28.09175590476861 25.304335317314635 11.718763953946235 0 0 0 3770 1 0.004982221463119243 25.02502285032285 22.019676496361082 11.837266315624012 0 0 0 2303 1 0.004991716149722431 24.96524958932825 28.332527344113075 11.696990698094694 0 0 0 1576 1 0.004866384293030539 28.231222949725623 22.014371667805527 11.730446897434605 0 0 0 2301 1 0.0048855355107869855 21.79695584679225 28.363225542023525 11.755099158859869 0 0 0 109 1 0.005098685509099097 28.125795074238393 28.436499269820533 11.646908528284628 0 0 0 3777 1 0.004909753999505493 21.77223646723269 25.12792347947597 11.688925669904483 0 0 0 3834 1 0.00495613924128257 26.524968269433682 26.73336490836882 19.697288544056097 0 0 0 3832 1 0.004865354344441238 23.442580468861664 26.836515443214836 19.697562269230257 0 0 0 3179 1 0.00474899222896817 15.421370907330422 15.650335477983395 27.697653703248346 0 0 0 3181 1 0.004808338052892781 18.67902933597031 15.680482945919492 27.660430704135184 0 0 0 3892 1 0.004681264379153975 18.620442160657664 18.83160653801908 27.550959785330267 0 0 0 3890 1 0.004733429804664433 15.46718513049039 18.906626633773776 27.688077331638304 0 0 0 3156 1 0.004852925046183301 17.02195646505623 17.204231486080083 26.104420055004436 0 0 0 3876 1 0.004718528800191055 20.281674395819117 20.418164472990004 26.036696351964174 0 0 0 3157 1 0.004690120650889862 20.19995715084285 17.323833120815888 26.018472555391664 0 0 0 3875 1 0.004741196517121923 17.022150161339514 20.427959363875523 26.07798499888786 0 0 0 3141 1 0.004833220546347276 15.446651970437847 15.715296881672465 24.513685156468974 0 0 0 3862 1 0.004849676759163882 15.40790810609077 18.9191225006244 24.369733955847884 0 0 0 3142 1 0.004819289185725566 18.685825817763902 15.733257933852594 24.447493377821925 0 0 0 3863 1 0.004780994957040829 18.612757366816233 18.939041239814227 24.475898353540618 0 0 0 3839 1 0.004729162611608214 20.244106353476248 20.45085574896131 22.84449753153823 0 0 0 3126 1 0.004817343532833649 17.083782889354964 17.210499675731402 22.866942560078208 0 0 0 3128 1 0.004777339731736175 20.207473849039946 17.343500867512223 22.79767176946302 0 0 0 3837 1 0.004793551435531056 17.028495480292857 20.48196220092422 22.899727977079365 0 0 0 3125 1 0.004790354714529791 15.363466464319103 15.66899716109675 21.362391809877494 0 0 0 3836 1 0.00480174683024431 15.458626580374569 18.790090275378862 21.345926681352612 0 0 0 3127 1 0.004713884407936474 18.600197038832874 15.661165742871118 21.253867747655743 0 0 0 3838 1 0.004880270773548983 18.582770538730674 18.927003832678622 21.19489285351642 0 0 0 1702 1 0.004697470872676562 28.181761634089113 18.823273388803084 27.665369086655254 0 0 0 991 1 0.0047986142717481636 28.066913707414873 15.67096599086675 27.709526109748193 0 0 0 3896 1 0.0048335174317822825 24.993732879615937 18.84677227404746 27.734941130693304 0 0 0 3183 1 0.004828142529221624 21.79245209744196 15.694681089528098 27.60364262999881 0 0 0 3894 1 0.004900996094610661 21.786205878032934 18.95123337946249 27.737309473291017 0 0 0 3185 1 0.004937813291303713 24.931360813054305 15.710162457319173 27.711606905715232 0 0 0 3159 1 0.004646484123279362 26.576495666963936 17.213566279146384 26.02121072555451 0 0 0 3877 1 0.0048342055347806185 23.44039860074748 20.452377389560965 26.122537515743517 0 0 0 3158 1 0.004740572040736659 23.403763447854235 17.22815422427714 26.066360226018002 0 0 0 3878 1 0.004756823350024286 26.618330187055452 20.439747835804045 26.063958617293185 0 0 0 3864 1 0.004723246253866551 21.820342367290067 18.86231715217089 24.443485037598645 0 0 0 956 1 0.004758858143326486 28.220480027772457 15.59520131849187 24.49826228698439 0 0 0 3144 1 0.004808589729098091 24.983521566883095 15.641436355537948 24.478148796485844 0 0 0 3865 1 0.0047444923673555 25.017016251441454 18.760249247469584 24.584892618077212 0 0 0 3143 1 0.004750671046248331 21.818645799921853 15.69636423418829 24.507340712120524 0 0 0 1675 1 0.004930782113358904 28.089299873938234 18.76057701645774 24.530021269202724 0 0 0 3843 1 0.00474683125993609 26.502198938837964 20.43902087517452 22.831403841883386 0 0 0 3132 1 0.00481765543009758 26.605991169477406 17.235180082110013 22.702706222972388 0 0 0 3130 1 0.004874409309280368 23.41374163225111 17.2091137220515 22.860352721546715 0 0 0 3841 1 0.00476557556089954 23.463725223469964 20.39294190001693 23.02718645957049 0 0 0 3131 1 0.004745710919157783 24.96016228230501 15.646647051589287 21.27856675366117 0 0 0 937 1 0.004619648848369929 28.116529290038073 15.69597232614396 21.27106789610206 0 0 0 1648 1 0.0046826958279634675 28.16430063502162 18.83770129569794 21.22990576015925 0 0 0 3840 1 0.0047169271682691565 21.758356931413704 18.874592226977484 21.32347797222901 0 0 0 3842 1 0.004659848340375059 24.94710999671695 18.952195683784282 21.356641821132552 0 0 0 3129 1 0.004924684119063818 21.706283681000254 15.675544191932373 21.28816862309965 0 0 0 3821 1 0.004718911623212892 20.080124620503835 23.674513521442655 19.73552627022299 0 0 0 3908 1 0.004836787043850252 15.386641810821288 25.229575819511957 27.658793294844543 0 0 0 3910 1 0.0049472618461339525 18.694694416214013 25.23163348189586 27.744359636013343 0 0 0 3899 1 0.004783965172451261 15.375568705328003 22.035625677864935 27.58102408333222 0 0 0 2432 1 0.004632150504319185 15.385861770835907 28.437233463818977 27.59763454622513 0 0 0 2434 1 0.0048247246990508145 18.63227902952529 28.390453932752834 27.67740271816157 0 0 0 3901 1 0.00482884214413154 18.60253600411259 22.04023657401384 27.657309285270763 0 0 0 3886 1 0.004787850707140596 20.28750982756004 26.854171533325516 26.057623804720528 0 0 0 3885 1 0.00474833619998247 17.117131371524426 26.870629977241506 26.05270348542367 0 0 0 3881 1 0.0046984868674347525 20.229133895509047 23.666925443734005 26.01347106555437 0 0 0 3880 1 0.004871631478788484 17.080664211050106 23.707314554288768 26.038124791279966 0 0 0 3866 1 0.0047970883744977485 15.403709641563024 22.081216334909307 24.49377672284529 0 0 0 3871 1 0.004656644349741031 18.661824032864814 25.245972081273557 24.46220165097741 0 0 0 3867 1 0.00478541262065473 18.598077458468882 22.058871259721382 24.47546292717234 0 0 0 2404 1 0.004655647994882602 15.413625365936129 28.312366222769022 24.610257689877088 0 0 0 3870 1 0.0047437520697944865 15.419584210077305 25.241877289764957 24.514967305871266 0 0 0 2405 1 0.004727545176836668 18.629250064158345 28.47375532606457 24.501105557778743 0 0 0 3848 1 0.004714280104841706 20.214225740362377 23.755257548808967 22.8942228452465 0 0 0 3857 1 0.004696802657134401 20.241208970449886 26.923527514502254 22.979526710417698 0 0 0 3855 1 0.004806753413129085 17.002673779172397 26.91827239260533 22.95571538911331 0 0 0 3846 1 0.004654041647106194 17.05845778536512 23.6367164924659 22.937700783414044 0 0 0 3845 1 0.0048005357493177345 15.34349766226761 22.141925124091923 21.305247605044663 0 0 0 2378 1 0.004716539584720281 15.397113703781526 28.446757988546693 21.292514644176748 0 0 0 3854 1 0.004783686614263916 15.431332126079244 25.27395463368007 21.359124581853564 0 0 0 3856 1 0.004777435480595775 18.595368093274935 25.351517003482346 21.304657269216705 0 0 0 3847 1 0.004856529485707105 18.544767781289234 22.15556624537586 21.352452509482553 0 0 0 2380 1 0.004815873232895234 18.676262814694883 28.472893389128807 21.291570012205938 0 0 0 3825 1 0.00479817773017943 26.572870782449215 23.601664048758227 19.769821307185083 0 0 0 3823 1 0.004735606781576146 23.30622020635514 23.606489990076234 19.769897265889604 0 0 0 1666 1 0.004864027980102062 28.23531491423759 25.22616527623929 21.27454245084521 0 0 0 2384 1 0.004840446449574688 24.97311854916816 28.42990932234329 21.27846206356311 0 0 0 3860 1 0.004868774611597343 24.978149885025875 25.17280702322802 21.373352745997988 0 0 0 2382 1 0.0048683065933433755 21.787987701295197 28.378910653597494 21.270703749657233 0 0 0 244 1 0.00474346714558214 28.213753139201696 28.443015388947657 27.71295268560903 0 0 0 3903 1 0.004843594464792609 21.715343358978178 22.181233168685868 27.716484566328973 0 0 0 1720 1 0.004862002547858917 28.249799091335948 25.245850424319435 27.65713847680052 0 0 0 2436 1 0.0046568053950399625 21.882529092252966 28.42299776555739 27.728429168355987 0 0 0 3914 1 0.004772147145342758 24.94540529912751 25.233012796573032 27.692991092985555 0 0 0 1711 1 0.0047080233528914404 28.262455349011944 21.966519767879184 27.705042384724603 0 0 0 2438 1 0.0047469199182997145 24.99631023180419 28.388990070370742 27.762500874899935 0 0 0 3905 1 0.0048036263980814845 24.957576452397134 22.040038536930666 27.734061814334733 0 0 0 3912 1 0.004741154023072253 21.80997440614567 25.19366808304393 27.6987871850737 0 0 0 3882 1 0.004730445995127685 23.381317481355914 23.57848784543335 26.045447657687944 0 0 0 3888 1 0.004826968130105993 26.64817460709867 26.824884047114033 26.146109988371176 0 0 0 3887 1 0.004701644809907483 23.42595319800782 26.908989675152718 26.236670834367832 0 0 0 3883 1 0.0048664909274455225 26.56269165417695 23.636894476264853 26.165853681611214 0 0 0 3868 1 0.00477809702887029 21.790095879761004 22.03427905115391 24.51238874841513 0 0 0 217 1 0.004728363574153082 28.187289494732973 28.398309078119837 24.55648568221239 0 0 0 1685 1 0.004704896746139844 28.191957504488247 25.313368821964797 24.466594980172154 0 0 0 1680 1 0.004839298566638334 28.108737941894013 22.03376299478843 24.450613531274062 0 0 0 3872 1 0.0047665710499838615 21.79491955357766 25.267562798984727 24.517164818918626 0 0 0 3873 1 0.0050159776793989395 24.94346972316866 25.221035466987917 24.494360660307997 0 0 0 3869 1 0.004684174363512423 25.05524069261969 22.03239714213439 24.609317665209108 0 0 0 2407 1 0.00479161225519229 25.02849903043548 28.404069611065534 24.576791017233695 0 0 0 2406 1 0.0046476427991558236 21.854154188848824 28.445768569162183 24.531889665350374 0 0 0 3859 1 0.004857648723093157 23.407618622257452 26.95163009184187 22.975113289245904 0 0 0 3850 1 0.004832805818519848 23.332584309268874 23.59911102961124 22.87466560000749 0 0 0 3852 1 0.004842736111994346 26.626954314486014 23.632588396884227 22.999061491830915 0 0 0 3861 1 0.004854097926255803 26.566583003927843 26.845448635331447 22.876542073142446 0 0 0 1657 1 0.004841657968910595 28.08453617109 21.985698544859666 21.310837321182525 0 0 0 190 1 0.0048153423001234714 28.214029649870298 28.45490259152277 21.29063796682342 0 0 0 3849 1 0.004857562548887865 21.744201718099045 22.00572745877134 21.34320737707158 0 0 0 3851 1 0.004692821824966938 24.91474421510852 22.090924205877734 21.35272013414126 0 0 0 3858 1 0.004830635650089508 21.762121630073423 25.28716036757646 21.302668855031158 0 0 0 3236 1 0.004819071601944546 20.20676963172463 17.281848118263667 35.680818334272885 0 0 0 3947 1 0.0046202582114734415 20.15371690237335 20.498272928735037 35.60993079606848 0 0 0 3945 1 0.004803007132542761 17.021175337064186 20.495930010650703 35.66118856362337 0 0 0 3234 1 0.004728201213916171 17.012766414187716 17.310941425763602 35.581031775913594 0 0 0 3235 1 0.004733690782128541 18.555024615202456 15.611291490824886 34.07963952724766 0 0 0 3944 1 0.00477776815767828 15.387754523726352 18.906823564680117 34.063500497403396 0 0 0 3946 1 0.004895931461136786 18.65691408590604 18.94352077549377 34.03710304880707 0 0 0 3233 1 0.004686409244913909 15.44013431415664 15.75005564394976 34.099025402977574 0 0 0 3209 1 0.005102531981391656 20.182152204822227 17.34271568372955 32.45470770997291 0 0 0 3918 1 0.004783956234736403 16.976360729225746 20.45855769427273 32.42531307083969 0 0 0 3207 1 0.004877716950942176 16.979364777141193 17.20351314824702 32.43837250091408 0 0 0 3920 1 0.004841390096019324 20.217358781961416 20.566901133724606 32.43344026213945 0 0 0 3206 1 0.004742346516348547 15.427970466720684 15.668276055334916 30.77829807517888 0 0 0 3919 1 0.0048899707156089735 18.52042028650841 18.902623555374298 30.81651546907976 0 0 0 3917 1 0.004863174549601482 15.439221738002704 18.858094652522183 30.810531351556506 0 0 0 3208 1 0.0047072274312190115 18.552941987108273 15.602654509335224 30.853368553269362 0 0 0 3893 1 0.004781192863084817 20.109652828484833 20.44727577647546 29.17154067088814 0 0 0 3891 1 0.004644209638762081 16.98139400646205 20.484902913811656 29.21692764941859 0 0 0 3182 1 0.004970814898613609 20.201134204244486 17.22665203099265 29.285086393750603 0 0 0 3180 1 0.004754686682223525 17.074908780665865 17.231595865511892 29.27544369352871 0 0 0 3240 1 0.004884147048177001 26.599220906742524 17.227057567177674 35.743602873218585 0 0 0 3951 1 0.004719995320169854 26.514358721247124 20.505918476461574 35.597364519589455 0 0 0 3238 1 0.004832843404958775 23.41555400403462 17.267145195145478 35.692637752704094 0 0 0 3949 1 0.004687289924376706 23.349372196210226 20.492075886493744 35.6099737133974 0 0 0 3237 1 0.004880528940722405 21.80181038191616 15.691460215743039 34.151495824472825 0 0 0 1756 1 0.004910371203210964 28.123039017895927 18.829025237267174 34.06792240318428 0 0 0 1045 1 0.00489493113427622 28.112058033369298 15.709193717729084 34.064682489783 0 0 0 3239 1 0.004762108804887696 24.945974452197966 15.645375348162217 34.050540447480486 0 0 0 3950 1 0.0049672535207528744 24.98419974537839 18.920228719358338 34.116352395379224 0 0 0 3948 1 0.004910887893468196 21.824226725291084 18.840887446073417 34.14927679001255 0 0 0 3211 1 0.004741857057335231 23.433466213564635 17.29894611746308 32.43423030560046 0 0 0 3924 1 0.004803848587763093 26.6210118853595 20.52351379185814 32.403767537700624 0 0 0 3922 1 0.004804776722750736 23.380063447763952 20.496718590300603 32.382761507081455 0 0 0 3213 1 0.004831674599893018 26.546901899351948 17.140134672686756 32.488421282104554 0 0 0 3210 1 0.004813844296861741 21.822837104114438 15.721691167474525 30.92640367304711 0 0 0 1729 1 0.004753056896202274 28.132112164125168 18.833755478706358 30.83531211626206 0 0 0 3212 1 0.0045788882814236116 24.986685769571285 15.652185616211156 30.916820516724126 0 0 0 3923 1 0.00472046705468256 24.933818148855543 18.849198334311037 30.891939094920865 0 0 0 3921 1 0.004804289510310797 21.830983981935876 18.912739827886966 30.84889809529989 0 0 0 1018 1 0.0047787499619890445 28.202058516594963 15.68128470573959 30.86983208043308 0 0 0 3895 1 0.004677558061485468 23.45496074839139 20.507459822456042 29.29490779415096 0 0 0 3186 1 0.004767628177986262 26.58383569270246 17.303209977662096 29.3121505912096 0 0 0 3897 1 0.004729723768258462 26.66545294787138 20.41555816565644 29.29876012016077 0 0 0 3184 1 0.0047448821222558085 23.37822578753588 17.33474561065114 29.314589722641415 0 0 0 3954 1 0.004841241599068289 16.911692921829623 23.685854050511907 35.653690849119215 0 0 0 3963 1 0.004836282161772258 17.01436811515535 26.725829938895213 35.672366833309106 0 0 0 3965 1 0.00479892450400983 20.19621501677488 26.815366741386097 35.65510166873512 0 0 0 3956 1 0.004721946841575116 20.216977734469364 23.580809986831724 35.66981886277557 0 0 0 3962 1 0.0046151656326881806 15.400849976311974 25.279701867843997 33.98087779005166 0 0 0 2488 1 0.0047448719852207655 18.52612769714616 28.393708015277284 33.927254140779205 0 0 0 2486 1 0.004718770586108343 15.453899664049008 28.410879182325424 33.99613674891025 0 0 0 3955 1 0.004791560464782988 18.598012928454946 22.02141197242719 34.04054196482645 0 0 0 3964 1 0.0047982079229578825 18.607187506484085 25.235121516053816 34.02341058767597 0 0 0 3953 1 0.00481129174815164 15.379361115986015 22.07244808853216 34.0056986563193 0 0 0 3936 1 0.004589653597547788 16.927347276406508 26.838919609731956 32.45854723209361 0 0 0 3938 1 0.004700904259638107 20.178235684299402 26.909236412627845 32.46883499611375 0 0 0 3927 1 0.004855811644586117 16.977641262501606 23.724556096040637 32.46168307916192 0 0 0 3929 1 0.00479539061679113 20.119524904449996 23.645348481136562 32.359190942284755 0 0 0 3935 1 0.0046929793314563414 15.398820898498009 25.310692884624146 30.77532121507474 0 0 0 2461 1 0.004846717413007285 18.6296389923518 28.416538829277123 30.817685658885022 0 0 0 3928 1 0.004658623957615 18.53311344162067 22.010133041918458 30.852174258642474 0 0 0 3926 1 0.0047068493161020065 15.396087683103426 22.086268823909812 30.78769777932698 0 0 0 2459 1 0.004743173875875653 15.40423118688667 28.46199808584258 30.827525702372625 0 0 0 3937 1 0.004794821778444336 18.550519165714768 25.31376826214919 30.858611650075225 0 0 0 3911 1 0.004709959279275899 20.287262422672157 26.826771254393137 29.290854106150384 0 0 0 3902 1 0.004558654611927657 20.121924307443688 23.64601468176544 29.357183122589042 0 0 0 3909 1 0.004808824551295559 16.957656526014052 26.87703534182574 29.19791823511171 0 0 0 3900 1 0.004859241714767572 16.984292790486343 23.60251240994416 29.26833020977483 0 0 0 3969 1 0.004736157098636307 26.613070983158252 26.79446045122359 35.72237092392587 0 0 0 3967 1 0.004740723716457101 23.394498526302897 26.85278855793582 35.61797467169498 0 0 0 3960 1 0.004756452556462024 26.50077044961997 23.60119219199578 35.6029936202275 0 0 0 3958 1 0.004859041396320112 23.408263257781663 23.60460350961404 35.650186774302426 0 0 0 3968 1 0.004795321342732851 24.966918536293985 25.292883449098188 34.069657991185 0 0 0 2490 1 0.004766883590220634 21.811267321526344 28.444885863515704 34.05330037080068 0 0 0 1765 1 0.004645732669904798 28.112713350957 22.094840526038602 34.041119392504264 0 0 0 2492 1 0.004904243816057542 25.03416202738232 28.348071315057233 34.07997391039583 0 0 0 3966 1 0.004894546164008577 21.689535238710924 25.24973148132648 33.98572769912332 0 0 0 3957 1 0.004830826810770482 21.79586921581482 22.048227535324546 34.07936211143761 0 0 0 3959 1 0.004623474087206002 25.005168268228033 22.038952632863147 34.02719673784675 0 0 0 1774 1 0.004764311784804106 28.20589216675797 25.234725434374283 33.991855340783616 0 0 0 3940 1 0.004734195076947948 23.290945516597578 26.796484340158564 32.43992554511102 0 0 0 3933 1 0.004777536270880947 26.60880404173562 23.64456071678055 32.479787828442724 0 0 0 3942 1 0.004745573973291443 26.62904354047687 26.77057527908085 32.434767463394294 0 0 0 3931 1 0.004852776933619695 23.37520216453649 23.74408132552032 32.454018944193606 0 0 0 2463 1 0.004561032921211149 21.797361856315632 28.400777332876885 30.835723300565533 0 0 0 271 1 0.004570679546401786 28.178420964085458 28.462526686605973 30.952594280492352 0 0 0 2465 1 0.004812663180410428 24.982951634323815 28.34737308977593 30.948340021389505 0 0 0 1738 1 0.004641435013364481 28.205500912309382 21.991758632065704 30.807085197760227 0 0 0 3939 1 0.004633284295919136 21.743302784112245 25.162781801245576 30.804691391201075 0 0 0 1747 1 0.004677524723406681 28.190246770150477 25.230869643261705 30.803334221849223 0 0 0 3930 1 0.004794185534081388 21.765182869189115 22.039571435409123 30.780160822943362 0 0 0 3941 1 0.004700282999197329 24.99535284632673 25.23320488948482 30.892907740306534 0 0 0 3932 1 0.0047996962549594815 24.924068867176533 22.115102981465935 30.916900511675948 0 0 0 3913 1 0.0045684835350819405 23.409137664188318 26.813931379276895 29.341412076379275 0 0 0 3906 1 0.004882547495131166 26.677384692349346 23.575927647212662 29.253158944930075 0 0 0 3904 1 0.004632154751058699 23.446481739647297 23.710219146372356 29.24569512765317 0 0 0 3915 1 0.004756215071143401 26.597086739571488 26.7558854031705 29.31031048123112 0 0 0 298 1 0.00472097636004061 28.21648237146322 28.45867141278203 34.10501244393064 0 0 0 3316 1 0.004716370270193717 18.50284843288406 15.7305829598173 43.70011639789243 0 0 0 3314 1 0.004724507958264646 15.308896064420153 15.662525946820606 43.56985614859913 0 0 0 4025 1 0.004835113110401667 15.424115963026107 18.86211680106629 43.65467023074494 0 0 0 4027 1 0.004767378055743248 18.580351237321835 18.895721697149256 43.64604256471123 0 0 0 3291 1 0.004706046822742145 16.96398963013368 17.220138095475473 41.97384286734255 0 0 0 4010 1 0.004795612825155051 16.914619232126824 20.39772510118264 42.02962231147184 0 0 0 3292 1 0.0047159301746732135 20.121907017438573 17.274398250720296 42.039053724564084 0 0 0 4011 1 0.004668861684908772 20.114753868032647 20.366834969855475 41.994898799147585 0 0 0 3276 1 0.004658584100320077 15.321647964444283 15.657479813496678 40.51258290767735 0 0 0 3997 1 0.004822744015357773 15.434472046025602 18.76560526883313 40.3751995149369 0 0 0 3998 1 0.004676468350065206 18.540777454562857 18.826094078489923 40.426469553081205 0 0 0 3277 1 0.004750586548751738 18.5594731344006 15.677954122399257 40.45115795618318 0 0 0 3972 1 0.0047763933580332995 17.00853996698523 20.520654239466616 38.86867402105479 0 0 0 3261 1 0.0046291668494837235 16.897728704720183 17.273614440302165 38.79917270009122 0 0 0 3263 1 0.004753606878497298 20.180988667554537 17.243156582090155 38.84422613311081 0 0 0 3974 1 0.004605187824539208 20.069594757367835 20.411350276163752 38.88693444554776 0 0 0 3262 1 0.004853530498944167 18.51960935485678 15.697872552341712 37.26475321264639 0 0 0 3971 1 0.00470162463759481 15.462903955987777 18.879973520892094 37.245551301618285 0 0 0 3260 1 0.00469600788614951 15.433152535561982 15.761014705017612 37.28751559350866 0 0 0 3973 1 0.004806754037816977 18.662526106417374 18.833886427571915 37.275369330314774 0 0 0 1126 1 0.004739650354504183 28.194693897702486 15.757874175362309 43.609223960498724 0 0 0 1837 1 0.004810607541997733 28.16983884277779 18.885265079749757 43.59152413215297 0 0 0 3318 1 0.0047701288458341495 21.75700032804733 15.650508273687098 43.664402547200474 0 0 0 4031 1 0.004911403128049389 24.936567356447544 18.794425078933987 43.54071788533784 0 0 0 3320 1 0.004692526847739241 25.015064692871203 15.632838578538598 43.574989473684944 0 0 0 4029 1 0.004805220679234662 21.700677138973937 18.83497094724646 43.637334698985335 0 0 0 4012 1 0.0048096705706974045 23.231121862295055 20.460353441840553 41.993975182875324 0 0 0 4013 1 0.004809268329840279 26.484773603868184 20.43378825521249 41.97537631265267 0 0 0 3294 1 0.004783930139563835 26.525246783910973 17.213249045024163 42.03239349112196 0 0 0 3293 1 0.004746906073248252 23.25133436791184 17.207578878384805 41.98080988924657 0 0 0 4000 1 0.004882260812740069 24.921650959186014 18.855480305812108 40.35410829055264 0 0 0 1091 1 0.004604273417063841 28.064682311973733 15.646611801764594 40.3374405487811 0 0 0 3278 1 0.0047647667619787944 21.72226413503548 15.64848014651552 40.52761789522102 0 0 0 3279 1 0.004771829336405341 24.88414496990307 15.66206967453935 40.45805191012819 0 0 0 3999 1 0.004620251146516038 21.757577603388622 18.849187151300576 40.47094877435253 0 0 0 1810 1 0.004950252018308182 28.138290834891638 18.918237885324498 40.4308080835308 0 0 0 3976 1 0.004662513319002304 23.246434289434934 20.489173577797903 38.809623561439906 0 0 0 3265 1 0.004652501047088108 23.35504311781894 17.25726346620733 38.85784834942222 0 0 0 3978 1 0.004810752598330545 26.578714873549487 20.451612809019146 38.83563672727336 0 0 0 3267 1 0.0047268610593647065 26.52385458230579 17.21962767179133 38.881357359682525 0 0 0 3264 1 0.004790792550381215 21.773838272567268 15.660984832465367 37.32645124592789 0 0 0 3977 1 0.004856687154637289 24.877001322557195 18.892697954595977 37.314582859847505 0 0 0 3975 1 0.004735058260699823 21.74251178486328 18.888816111453163 37.35009911071139 0 0 0 3266 1 0.004727883810629189 24.9271265793001 15.61636393850713 37.23238885161821 0 0 0 1783 1 0.004984405579337941 28.128902948025285 18.76540015442459 37.23727527346823 0 0 0 1072 1 0.004678430148943567 28.178038901100255 15.611039547271929 37.362592625583034 0 0 0 4043 1 0.004857646545659185 15.41725074152241 25.286755939215823 43.50903576941241 0 0 0 4034 1 0.004784801512025113 15.438685619474917 22.095326813806803 43.54687469798027 0 0 0 2567 1 0.004778178270289982 15.452095783871856 28.408925442465627 43.629513503481895 0 0 0 4045 1 0.0048164962314568086 18.64826597266493 25.251289500608664 43.5868145609622 0 0 0 4036 1 0.00482072706097969 18.70477166295929 22.06860875707186 43.699566574215545 0 0 0 4020 1 0.004609896011703141 17.022619480429334 26.829509439227536 42.00879409429585 0 0 0 4021 1 0.0045921392589587575 20.124656358606014 26.83494789009555 42.070595808167 0 0 0 4015 1 0.004677368216720665 17.057859477738788 23.587940665436147 42.034211484799904 0 0 0 4016 1 0.004667817269074668 20.197851140772823 23.599346901810787 41.99078925520441 0 0 0 4001 1 0.004742719074125304 15.408239763922136 22.062257066383687 40.46954040387908 0 0 0 2540 1 0.004729845366983031 18.55780446928763 28.4266859772216 40.46790949187167 0 0 0 4006 1 0.004681608542013266 18.65340784646525 25.239761026018716 40.4549035586008 0 0 0 4005 1 0.004770597437355816 15.464137424109522 25.25775157124387 40.48056971257198 0 0 0 2539 1 0.00478060463551493 15.388606720488665 28.42962657367971 40.408841402300226 0 0 0 4002 1 0.004676468473338052 18.63249912198509 22.017085136152442 40.51331089939836 0 0 0 3992 1 0.0049009577693577035 20.085361062776716 26.776853222930686 38.81469773170471 0 0 0 3981 1 0.004878821137129655 17.035141498107187 23.6834382977325 38.92849051520131 0 0 0 3983 1 0.004704545977334445 20.17718604765628 23.642402432587687 38.85760084251892 0 0 0 3990 1 0.004966094523260961 16.960634749045596 26.815306441829115 38.796597294188786 0 0 0 3982 1 0.004750299934842913 18.54553967324584 22.061027588308495 37.243150659938856 0 0 0 3989 1 0.004783610221368112 15.287717464068166 25.23541304724833 37.2407115857151 0 0 0 3980 1 0.004764959391746681 15.42781183687227 22.07330834242885 37.28481309219449 0 0 0 2515 1 0.004835018619373207 18.578241144240756 28.438911960909138 37.125286811852 0 0 0 3991 1 0.004709357055772719 18.609435458555417 25.143397209428432 37.16490388226488 0 0 0 2513 1 0.0047596350806843445 15.378216005916608 28.45796932307234 37.21801949041645 0 0 0 2569 1 0.004614482742781147 18.558413927947658 28.456937248018555 43.599769816932564 0 0 0 3993 1 0.004703747224791955 21.733544703221206 25.166995046257146 37.230843951923674 0 0 0 325 1 0.004579550996823891 28.230192173556546 28.474518731399833 37.21584722978185 0 0 0 4049 1 0.0047235864859564314 24.9823475473354 25.18043463471972 43.54991441527523 0 0 0 1855 1 0.004765733345214865 28.13169343131567 25.242963694546212 43.59223867497547 0 0 0 1846 1 0.0048307306179840095 28.1713703215126 21.992204634625253 43.65781447478917 0 0 0 2571 1 0.004740144981722941 21.736518154906694 28.365017944237398 43.68074739550416 0 0 0 2573 1 0.004699580804954969 25.027007218643714 28.374426379896885 43.58946600249733 0 0 0 4038 1 0.004856407985237931 21.758714274235 22.06136904653852 43.65117268984808 0 0 0 4040 1 0.004692115707431879 24.99932543828532 21.95266211928411 43.52990555799699 0 0 0 379 1 0.004788350848614337 28.18899395628166 28.39750092350933 43.457806079901204 0 0 0 4047 1 0.004832622487459271 21.72880440000417 25.20503560738257 43.57176302408442 0 0 0 4018 1 0.004833283211909524 26.59648445231392 23.57045546884226 41.95914455396598 0 0 0 4023 1 0.004739556077079349 26.453940690838802 26.72698679876934 41.87626000359498 0 0 0 4017 1 0.004770863909475061 23.36224147416703 23.606769031473547 41.982343672346346 0 0 0 4022 1 0.004762334014383012 23.351861024489814 26.873636131671695 41.98366512606386 0 0 0 4004 1 0.004860875035866571 24.895678595564547 22.128179016338812 40.411398154057515 0 0 0 4008 1 0.004659604582234996 24.956459602324877 25.243058286417007 40.34666147758831 0 0 0 2542 1 0.004705366078766553 24.84435608908729 28.39666760155403 40.34920869769102 0 0 0 352 1 0.004809384663977005 28.062255334791114 28.355170841124732 40.309675405167155 0 0 0 1820 1 0.004696012809573418 28.174585656272843 25.16582913822204 40.41506489426839 0 0 0 4003 1 0.004737668512011553 21.750304584342384 22.02656944664655 40.37515698769439 0 0 0 1815 1 0.004753411935166601 28.235164449605517 21.968888144476892 40.39182953178219 0 0 0 2541 1 0.0047132617831699905 21.672370463651475 28.37122773118718 40.542090372645795 0 0 0 4007 1 0.0046948046836136435 21.828240542406903 25.24862046797911 40.43855355301065 0 0 0 3996 1 0.00475775832944055 26.614765115006684 26.75736125030537 38.809151258196295 0 0 0 3987 1 0.004876855603953737 26.53851253169267 23.57278164964127 38.76499448730056 0 0 0 3985 1 0.004628026831372209 23.328862988063822 23.785006984823447 38.785890484508585 0 0 0 3994 1 0.004710111351969982 23.252458898864795 26.80727891878772 38.80900127911275 0 0 0 3986 1 0.004761121739648747 24.887383475773014 22.0082737889531 37.281769277043466 0 0 0 1801 1 0.00470623203736042 28.223102030510223 25.184091775026953 37.166206635466246 0 0 0 2519 1 0.004709820581920958 24.989305778328543 28.29605852193762 37.24397344375997 0 0 0 1792 1 0.004703872785222482 28.113331171138952 21.983653954381506 37.17204073881155 0 0 0 3995 1 0.004697672577640102 24.943456387125295 25.2071023060256 37.207005836807795 0 0 0 3984 1 0.004717046852669578 21.67975518399655 21.991824670396703 37.25305801633649 0 0 0 2517 1 0.0048307237756262805 21.770667820286562 28.378985476032252 37.21053581911555 0 0 0 3372 1 0.004766763105429943 16.91930823705177 17.324230972334366 51.645767232701075 0 0 0 4091 1 0.004769455396789543 16.94312499145431 20.428768766680236 51.58693813720102 0 0 0 4092 1 0.004793179572982965 20.036633257895016 20.48854333189068 51.55814572477884 0 0 0 3373 1 0.00481321987912766 20.14948516497263 17.227330134688966 51.61318713442213 0 0 0 4078 1 0.004773873867073768 15.35503713216151 18.80954393664193 49.975365736040764 0 0 0 3357 1 0.004667982958871435 15.264924234814565 15.722997333842093 50.03083519557444 0 0 0 4079 1 0.00480090311214555 18.475755094283777 18.809990045271753 49.97490230274001 0 0 0 3358 1 0.004831141281572287 18.452330138073805 15.710787893922896 50.00891591349387 0 0 0 4055 1 0.004767621543994143 20.181467911750172 20.399602111319503 48.443300222522375 0 0 0 4053 1 0.004846273434651917 16.912666891050925 20.424243237967147 48.35424906914344 0 0 0 3342 1 0.004712913080345372 16.868249509415737 17.193492116569562 48.395931204804604 0 0 0 3344 1 0.0047605610490722775 20.1921334977714 17.287181705394577 48.46728435286692 0 0 0 4052 1 0.004748583673056132 15.292076093361446 18.866124467111707 46.85664823618043 0 0 0 3343 1 0.004916178668491644 18.609705972186685 15.723033929909649 46.75828050080314 0 0 0 3341 1 0.004764983728469627 15.354139097239685 15.667729554148124 46.777681764518384 0 0 0 4054 1 0.0049451581987593266 18.51992877697552 18.89293270442888 46.86892511928771 0 0 0 4028 1 0.0047827031299438015 20.163034594562575 20.416361268857987 45.24034530047183 0 0 0 3315 1 0.004818546282104335 16.85062325589244 17.256377214567745 45.22102507548383 0 0 0 4026 1 0.004841812679560208 16.976362234329184 20.505016292889444 45.11817444343089 0 0 0 3317 1 0.0047462859886193455 20.113339088319908 17.218583517320774 45.243392251966185 0 0 0 3374 1 0.004787814476413969 23.313073789830003 17.318604673480465 51.52441576105579 0 0 0 3375 1 0.004711894173464329 26.489278775013776 17.2707084854436 51.537259889459236 0 0 0 4093 1 0.004704383471950877 23.25639537540982 20.53946174228162 51.61303860609767 0 0 0 4094 1 0.004670582235857477 26.465292908312545 20.543342173885534 51.55219512569264 0 0 0 4081 1 0.0047531365467015935 24.87619341831735 18.898211620495136 50.0740449275354 0 0 0 3359 1 0.004745419533749412 21.70826595382323 15.656028831300208 49.99514860524831 0 0 0 1172 1 0.004859522829127643 28.11181498260077 15.713584050604851 50.00212473970636 0 0 0 1891 1 0.004859131434891362 28.09626266425869 18.9288678006313 49.925599712831506 0 0 0 4080 1 0.004767067052699187 21.698795001936745 18.91933205258589 50.00527436748701 0 0 0 3360 1 0.00474876981438584 24.863909379192172 15.660822201844056 49.94136871079834 0 0 0 4057 1 0.004858600943984392 23.43477423969137 20.539243162338067 48.38171078132116 0 0 0 4059 1 0.004794968480291342 26.440156407711733 20.41682730382255 48.3214017833075 0 0 0 3346 1 0.00474469342968422 23.382172867466696 17.285485857951322 48.38371388252069 0 0 0 3348 1 0.004763212417455198 26.5748973153629 17.22722520075953 48.459953978991415 0 0 0 1153 1 0.0047267062353994575 28.175170316696605 15.658749018031418 46.871917106811104 0 0 0 3347 1 0.004711387026935595 25.048499877932144 15.584057979647381 46.74832632517906 0 0 0 3345 1 0.004716772075075192 21.811400513040002 15.717299158039882 46.841082744066185 0 0 0 4058 1 0.004808174863634622 24.941556740365197 18.750727291385772 46.870158333421536 0 0 0 1864 1 0.004703143194507913 28.0990512431554 18.808214470428556 46.70074264197621 0 0 0 4056 1 0.004917819201663565 21.76717601934956 18.816346061702866 46.87123880559579 0 0 0 4030 1 0.004980447107286569 23.417191491311304 20.373660188747117 45.13533624988821 0 0 0 3321 1 0.004732516237562084 26.57133257937322 17.178582234444267 45.2268122292801 0 0 0 4032 1 0.004782198589422013 26.542616665557745 20.42690015609857 45.19575489379936 0 0 0 3319 1 0.0048610458763941895 23.417224974614005 17.203708108273993 45.16724622090188 0 0 0 4096 1 0.0046960686819726965 16.940621968421066 23.623168103108586 51.53779106494355 0 0 0 4101 1 0.004847033955742779 16.886176093717967 26.763048867725168 51.592693152053926 0 0 0 4102 1 0.004714863990636501 20.125821206992676 26.844494098445402 51.605526108825984 0 0 0 4097 1 0.004633678966835409 20.174992272624454 23.676225407576077 51.485945480743275 0 0 0 4086 1 0.004653807069312002 15.384828293636897 25.24122174009475 49.915754939633985 0 0 0 4083 1 0.004831501029176016 18.497039444299308 22.12545249028158 49.91909832382732 0 0 0 4082 1 0.004996996796942134 15.35160908188833 22.02688318719854 49.95948505533058 0 0 0 2621 1 0.004910290789004701 18.528483081515212 28.473706729180854 50.00925161061334 0 0 0 2620 1 0.0048183135788664976 15.431892733904832 28.47075308403052 49.9085496299607 0 0 0 4087 1 0.004760945264297704 18.548856310975726 25.219894280557085 49.979072313967066 0 0 0 4062 1 0.0047342127179592405 16.956345166100963 23.704710385639473 48.2864234692179 0 0 0 4064 1 0.0047611403724140255 20.159606238054838 23.624700304387108 48.3570683449567 0 0 0 4071 1 0.0046785549910035775 16.95519725715385 26.835092395107903 48.39533290315612 0 0 0 4073 1 0.004870005332214225 20.171574706876537 26.874929344414475 48.50429010185323 0 0 0 4070 1 0.004703443193954878 15.425109307959726 25.26776707438504 46.754158503712134 0 0 0 4061 1 0.004787257821153988 15.33842058851075 22.055149845430222 46.70674424444555 0 0 0 2594 1 0.004648160200541368 15.342145543632403 28.43112588597341 46.7528222816072 0 0 0 4063 1 0.004884582671830687 18.586981411931337 22.063766446514425 46.8185234269551 0 0 0 2596 1 0.0047845741521152126 18.531535251388068 28.413056322280806 46.77252517132861 0 0 0 4072 1 0.004756904642948508 18.595782784997937 25.33223885668683 46.79768038663559 0 0 0 4044 1 0.0046951575987815245 17.049799188313205 26.846408671092725 45.24473169810621 0 0 0 4035 1 0.004839390444270338 16.975668013657753 23.72337006505293 45.194724556226284 0 0 0 4046 1 0.004716982733585128 20.26059249207722 26.923726697787746 45.23407194840058 0 0 0 4037 1 0.004718756158057327 20.223506259543893 23.720321857806404 45.27448197021251 0 0 0 4104 1 0.004800318577772649 26.48070002222391 26.801333349135614 51.57415017833253 0 0 0 4103 1 0.0046503633819628375 23.302914287790347 26.875356252561467 51.48010903390171 0 0 0 4099 1 0.004760435783022257 26.5984179308702 23.65451738721807 51.561193365416464 0 0 0 4098 1 0.004792368509586862 23.330387170953973 23.686949919395378 51.62495630291688 0 0 0 433 1 0.004678953365406706 28.105606497571838 28.367601736191393 50.00431570124899 0 0 0 2622 1 0.00463451640724249 21.81288226406032 28.544576837149084 49.92919407496888 0 0 0 4084 1 0.004852838746088288 21.739651792394856 22.100153370435788 49.92945775795326 0 0 0 2623 1 0.004775723458908952 24.97297425040673 28.38091801946796 49.99991405808445 0 0 0 4089 1 0.004873954013348005 24.877185343325362 25.220324554001852 49.930038422758734 0 0 0 1896 1 0.004730097508987917 28.099764208939284 21.976104894006678 49.95526751308442 0 0 0 1901 1 0.004682315529335613 28.144406056503446 25.21059830038769 49.9353116636406 0 0 0 4085 1 0.0048198818152248475 24.967877232472905 22.111533815446183 50.01764200397649 0 0 0 4088 1 0.0047518509437731345 21.73045010796886 25.344233640070158 49.97689971821414 0 0 0 4077 1 0.004944218387887245 26.59265912067435 26.784069352127695 48.31182684636321 0 0 0 4066 1 0.004826965100193002 23.36459111090318 23.689043924314042 48.32734357136018 0 0 0 4068 1 0.004919515902653732 26.604820345666685 23.675296255578967 48.291454045468164 0 0 0 4075 1 0.004736301346141433 23.44196113927198 26.90162477058535 48.35387953313419 0 0 0 2600 1 0.004614100033065617 24.919182320394057 28.528146427245936 46.75018968247526 0 0 0 1882 1 0.0046954836481038036 28.175094112243567 25.254501930055294 46.724671347623875 0 0 0 1873 1 0.004806247947301256 28.098126982293024 21.997333973807464 46.784086607427014 0 0 0 406 1 0.004777246797999861 28.236044723644007 28.425907421581087 46.70453166565846 0 0 0 2598 1 0.00479027645649556 21.78470854785641 28.399283258233243 46.858168225625384 0 0 0 4076 1 0.004737395902655411 24.931031391651377 25.244688994753496 46.6479204416896 0 0 0 4065 1 0.004914091231627071 21.79145053151671 22.044947813941633 46.76347952015441 0 0 0 4067 1 0.004751846279980808 24.927835871722387 22.098457849652746 46.7428197140777 0 0 0 4074 1 0.004881199358239297 21.807850553797103 25.262420972297754 46.78617356653291 0 0 0 4041 1 0.004693066122643582 26.49150170075663 23.611343340510047 45.121028391038465 0 0 0 4050 1 0.004854908801360972 26.562997647916244 26.84740605952828 45.131155770671114 0 0 0 4048 1 0.004740249130862772 23.425333236652776 26.929624291380478 45.155286107417176 0 0 0 4039 1 0.004710508889014446 23.43477961926405 23.687451064371782 45.103242497762785 0 0 0 4160 1 0.004821048517149143 15.224089484869992 18.822430229796883 59.493130006961046 0 0 0 3449 1 0.004762264731750121 15.298034089971749 15.690907731376218 59.4845091346969 0 0 0 4162 1 0.004966578377505091 18.566194766162894 18.827448366085015 59.51722225031021 0 0 0 3451 1 0.004819882998163655 18.5509263273956 15.701283287344378 59.49880765982051 0 0 0 4134 1 0.004869211675212154 16.81654286969527 20.424288314699798 57.92663413648718 0 0 0 3423 1 0.004893024107249726 16.861371440777994 17.258763721883142 57.89927128709228 0 0 0 3425 1 0.0048516097534607484 20.156585748838168 17.24548810164994 57.87909007126806 0 0 0 4136 1 0.004816728374308549 20.086143814777234 20.481423704276907 57.984327032451 0 0 0 3424 1 0.004859826593853599 18.485113921048015 15.665446960419526 56.294732048610406 0 0 0 4135 1 0.004832787237130503 18.546568850756344 18.895052438964914 56.341823475333506 0 0 0 4133 1 0.004758116803327462 15.329291766696215 18.803027718593025 56.35870139378075 0 0 0 3422 1 0.00466074929028509 15.33294911730349 15.68678932090542 56.248231303548806 0 0 0 3396 1 0.004718506516826851 16.927683709884388 17.250650699025993 54.73275467041605 0 0 0 4109 1 0.004726766635679331 20.144170648178765 20.43657179913881 54.75682086214261 0 0 0 4107 1 0.004750994237929884 16.948430044176323 20.430301575148224 54.77682374673507 0 0 0 3398 1 0.00465078620529987 20.09338251094865 17.19979875277628 54.68514756742974 0 0 0 3395 1 0.004696052031457849 15.256561467633972 15.741182563621281 53.16841662651417 0 0 0 3397 1 0.004746789002405508 18.484503560152405 15.61369849885591 53.18637737331154 0 0 0 4108 1 0.004705989490432116 18.555198877043726 18.87178165152487 53.21832108131643 0 0 0 4106 1 0.00477787097184006 15.290896275300796 18.957736942387964 53.122282385429585 0 0 0 4164 1 0.004851545083029147 21.640711380918418 18.996870859263453 59.512429207910245 0 0 0 3453 1 0.0048610290608739025 21.66773826622986 15.653761845982748 59.487287380085206 0 0 0 4166 1 0.004877220727518417 24.786185029184107 18.82745125192988 59.53733073225743 0 0 0 1972 1 0.004870936552047227 27.97097904597139 18.892797838508965 59.54612426963927 0 0 0 3455 1 0.004842501978322859 24.833329698481368 15.64415673957887 59.58409903915628 0 0 0 1261 1 0.004684980303083092 28.002571332422534 15.703710990642778 59.53079545503502 0 0 0 4138 1 0.004826620902007708 23.265382170965058 20.47761086677219 57.85495926109214 0 0 0 4140 1 0.004672893968773809 26.469453833956187 20.401800351187514 57.871044803701125 0 0 0 3429 1 0.004750885718538843 26.409595998640985 17.23365575657283 57.88708351185572 0 0 0 3427 1 0.0047626016617862005 23.29764715941057 17.19728319780023 57.84309091469564 0 0 0 3428 1 0.004567097347444286 24.92762016013185 15.663986175543071 56.34580925224378 0 0 0 3426 1 0.0045454793738650655 21.769476342892652 15.680381678075905 56.37183367214553 0 0 0 1234 1 0.004483510934388058 28.078451019941028 15.725172476179454 56.317556687513694 0 0 0 4139 1 0.004825290396077724 24.884301227031376 18.846233084755184 56.3719243234007 0 0 0 1945 1 0.004721912759168452 28.1145785458898 18.938134025669036 56.31525968478896 0 0 0 4137 1 0.0047970218529443266 21.717069101997616 18.811398061538455 56.335978021629536 0 0 0 4113 1 0.004879129693789504 26.45398851720694 20.365142130385816 54.706988536988625 0 0 0 3402 1 0.00481788114353458 26.513765458022235 17.25102982994723 54.66828722613935 0 0 0 3400 1 0.0048084822334939804 23.233370492103592 17.261597991692764 54.746127752366704 0 0 0 4111 1 0.004874008465136255 23.27373116307348 20.559165526743982 54.630316696582845 0 0 0 3401 1 0.004755488806774878 24.932799202420608 15.655334005443255 53.1712161662036 0 0 0 1918 1 0.00473714605921121 28.07780492300015 18.864001203913336 53.01398749318895 0 0 0 1207 1 0.0046363191235356226 28.07163162165969 15.668436891334268 53.12326553384689 0 0 0 4112 1 0.004796903545616812 24.86803946553274 18.81529748298323 53.13188725869041 0 0 0 3399 1 0.0047290246367683135 21.656472109232315 15.679751144490927 53.15304582212749 0 0 0 4110 1 0.004708300864118855 21.686206178396883 18.89871840695097 53.14631823693253 0 0 0 2704 1 0.004807633363330307 18.539008511328355 28.38650905274364 59.45487757497374 0 0 0 4169 1 0.004679348077977107 15.332227633171627 22.027533753834547 59.466787509883915 0 0 0 4178 1 0.004940348105692107 15.427937177025067 25.24078646157062 59.51281559530555 0 0 0 4180 1 0.0046742853731869954 18.648082659456247 25.19268527185129 59.53484689599278 0 0 0 2702 1 0.0049790391235769085 15.368353756726966 28.407160536076812 59.609531323858754 0 0 0 4171 1 0.004800929412195273 18.50751136254925 22.115533901067877 59.59218120452413 0 0 0 4143 1 0.004771455117343778 16.94343347831825 23.634264672281684 57.99610954443025 0 0 0 4154 1 0.0045033391081363595 20.149794790012212 26.81410602107451 57.952026866529636 0 0 0 4152 1 0.004735403646883544 17.089582646459544 26.740834086786492 57.99422376470429 0 0 0 4145 1 0.004667114823593041 20.10908215952975 23.62436100025324 57.947543788485376 0 0 0 2675 1 0.0049345969837928 15.437418332050953 28.367174375577665 56.44003863706063 0 0 0 2677 1 0.004637040520381077 18.59005599766571 28.450697591527224 56.29682204141443 0 0 0 4151 1 0.004842773285997618 15.377174765535585 25.231384377379168 56.39086276495506 0 0 0 4144 1 0.0048891987154943 18.479535430912986 22.058240597896035 56.37947400938482 0 0 0 4153 1 0.004834460242619309 18.612134264480872 25.243208354001343 56.277825486346394 0 0 0 4142 1 0.0046470480962522345 15.3068491633953 21.97764810034588 56.264445981729615 0 0 0 4125 1 0.004864490487925879 16.991834808272525 26.87311579013557 54.75536627374053 0 0 0 4127 1 0.004707627559607127 20.145759756944102 26.88115040327143 54.67830998505198 0 0 0 4116 1 0.004802588691181204 16.889682887357267 23.64351829453271 54.82373684663631 0 0 0 4118 1 0.0047701859065694095 20.138317592992493 23.621673648606304 54.60432357754285 0 0 0 2648 1 0.004811415099295011 15.352504494884228 28.386740329588058 53.17560494610243 0 0 0 4126 1 0.004806072074422877 18.508317902490074 25.134608047346052 53.157819244788115 0 0 0 4124 1 0.0047329199864346895 15.342131319471061 25.22589142512196 53.168612259747675 0 0 0 2650 1 0.004673914326023605 18.557107531806565 28.44973658422386 53.11798188738069 0 0 0 4115 1 0.00477031825666621 15.30896251861081 22.09767609585126 53.096131851203296 0 0 0 4117 1 0.004781573770646226 18.49727863556628 22.040488010538503 53.14390379265308 0 0 0 4121 1 0.004658082340926944 24.88618698545976 22.091904152955056 53.137922555255095 0 0 0 4128 1 0.004694450233139755 21.714702116158154 25.25074633284612 53.08981642618932 0 0 0 2706 1 0.0049305435633255155 21.703578959879124 28.37599211938284 59.52731943042148 0 0 0 514 1 0.004817249645211366 28.098670066639645 28.38953665761587 59.54366919167579 0 0 0 4173 1 0.0047841221635478975 21.703446133695785 22.141829685957514 59.53956671371963 0 0 0 4182 1 0.004872913285238289 21.716179022743862 25.285634008320525 59.55961413377087 0 0 0 4175 1 0.004662574712460501 24.893740313909962 22.01866281314109 59.49356233513993 0 0 0 1990 1 0.00475970524712669 28.115566176760407 25.185341856234295 59.57176265358206 0 0 0 2708 1 0.004722852873636003 24.871328853216436 28.43112432694875 59.56482960502719 0 0 0 4184 1 0.004884876471265353 24.905815440086627 25.241683831634987 59.55463617017419 0 0 0 1981 1 0.004684614705475577 28.135942470752727 21.99788661552238 59.550057363130335 0 0 0 4147 1 0.004648833081739323 23.30827793868392 23.623763550003602 57.95333931350045 0 0 0 4158 1 0.00467338272014324 26.513292292445396 26.87025331328485 57.94667436255125 0 0 0 4156 1 0.004625368540908737 23.345206033920235 26.824992443236773 57.864597221375675 0 0 0 4149 1 0.004710546368076626 26.591601880768916 23.66581471692118 57.93666535340775 0 0 0 2679 1 0.004708374547916418 21.643940798874453 28.386950525693255 56.37049678010167 0 0 0 1963 1 0.004796193615404858 28.10959428277907 25.205833337087576 56.40009573563258 0 0 0 2681 1 0.004724094433811287 24.903054390444662 28.41711572561677 56.38763569764586 0 0 0 4155 1 0.004851320432649775 21.707292131310805 25.22956792783362 56.348253354323596 0 0 0 4146 1 0.004815804727410323 21.6482387297927 22.08637119496738 56.3084898730816 0 0 0 4157 1 0.0048585072761558185 24.957674148556688 25.244051125073398 56.41744250813436 0 0 0 1954 1 0.004735653432129368 28.071044238575762 21.942446085120807 56.32933090569353 0 0 0 4148 1 0.0048729778845162715 24.874740314139906 22.094904618710107 56.3174218277366 0 0 0 487 1 0.004890812830184594 28.09127771567709 28.498867587654033 56.338521054132706 0 0 0 4122 1 0.0048208818823163874 26.55858207469793 23.54255311222863 54.737661098366786 0 0 0 4129 1 0.0049187425071424585 23.336107157328126 26.79128081396817 54.74364282222514 0 0 0 4131 1 0.0048884891488243844 26.551584617277488 26.91149061912961 54.772223733977974 0 0 0 4120 1 0.004903701219556059 23.315586456091335 23.66445416600988 54.74271132456296 0 0 0 460 1 0.00472190610421061 28.075215073389348 28.443080069929497 53.139802476185366 0 0 0 2654 1 0.004902438607212638 24.952368693483493 28.42209919092346 53.232129528879916 0 0 0 1936 1 0.004688189013474824 28.14912812252766 25.18970874569141 53.276973660907956 0 0 0 2652 1 0.004691524376721981 21.77292593318001 28.339935085033915 53.10509141194841 0 0 0 4130 1 0.004923812466904374 24.994005838341053 25.271090590892758 53.140175598501294 0 0 0 1927 1 0.004572938788289519 28.112720943370352 22.051825262762275 53.17059961271213 0 0 0 4119 1 0.004548974253800847 21.612235138086017 22.052430627333766 53.10780700724326 0 0 0 4241 1 0.010722382671134872 15.22700519675153 18.89772921715169 69.08458118927824 0 0 0 4243 1 0.006838299059162719 18.339024995104964 18.815597075378182 69.0876036620547 0 0 0 3530 1 0.010792779055636251 15.268412774179614 15.680703669557206 69.13171987734596 0 0 0 3532 1 0.007728147655805398 18.440414706724187 15.616919185833943 69.17911976235821 0 0 0 3504 1 0.0013716567165236223 16.83576281586404 17.268991647472223 67.54228713935201 0 0 0 4217 1 0.0034781956440052015 19.98055294468104 20.442221790418603 67.45963418144673 0 0 0 3506 1 0.001953483326094095 19.947970956903358 17.286373099297844 67.49818371656939 0 0 0 4215 1 0.0013425267123725639 16.840164441756894 20.47560447235287 67.59990366990922 0 0 0 4214 1 0.004666390588015112 15.316375642872588 18.896098857011573 65.87239244529404 0 0 0 3505 1 0.005409404242023349 18.403811028506436 15.68389768019334 65.99200840384358 0 0 0 3503 1 0.004752874851185113 15.266109792102807 15.680875396195887 65.85915020938144 0 0 0 4216 1 0.005589489202598828 18.39846473677432 18.937638994263292 65.86988874201644 0 0 0 4188 1 0.0050688397684224545 16.8917163084676 20.517198526391734 64.34558299295162 0 0 0 3477 1 0.00541632396415022 16.790968942141028 17.355806219101698 64.31512152417315 0 0 0 3479 1 0.005595326722093771 20.081012491827455 17.296386150902777 64.4075789395868 0 0 0 4190 1 0.004948610103338618 20.063502284372948 20.423955457927118 64.31120822147618 0 0 0 4187 1 0.0045332260313989525 15.28553428131765 18.870281286001685 62.62236373391556 0 0 0 4189 1 0.004694388905791722 18.472279344223534 18.818376623770835 62.746726730388644 0 0 0 3478 1 0.004676201817047858 18.531815861401274 15.652199870396757 62.697985234425744 0 0 0 3476 1 0.0045629577850759395 15.32117150796978 15.642192721770803 62.67974087758205 0 0 0 4161 1 0.004786457484505867 16.928503162074804 20.436204358288652 61.07706666462429 0 0 0 3452 1 0.004558008420852324 20.10965631930509 17.261909522189022 61.02319274356268 0 0 0 4163 1 0.004685299473449454 20.159490954287502 20.49377347298968 61.113806464747874 0 0 0 3450 1 0.004719235169641945 16.846198087306263 17.256890912295788 61.144867806489806 0 0 0 4247 1 0.00218296787999369 24.896342276299478 18.852532356818863 69.20152858190896 0 0 0 3536 1 0.0003940843253379851 24.84834789870186 15.610920055494269 68.98415246815105 0 0 0 3534 1 0.0021041136392736266 21.538820822673305 15.659105824243627 69.0892567195612 0 0 0 1342 1 0.0031680169377183657 27.966504266372464 15.557492176346585 69.06167658780879 0 0 0 4245 1 0.0027882404266256437 21.599437503157244 18.7879279962903 69.04030270711608 0 0 0 2053 1 0.003908879566919514 28.02989794743736 18.812999213115365 68.99562262314268 0 0 0 3508 1 0.003207355465898761 23.23310016410824 17.20047510891046 67.5276016899631 0 0 0 4219 1 0.005315264355884402 23.258815613113352 20.383292593561343 67.5445613487134 0 0 0 4221 1 0.006434142312133956 26.393860473923876 20.44571520876223 67.57645543004051 0 0 0 3510 1 0.006107088759152586 26.555584978449655 17.188032640795317 67.47888826529942 0 0 0 4218 1 0.005878336133139277 21.7128071975504 18.83554060045645 65.95382808892431 0 0 0 3507 1 0.006413902982251059 21.615253908205116 15.678494188151229 65.94902901045283 0 0 0 3509 1 0.006171359854358153 24.834038343649528 15.64588895826795 65.8459601810655 0 0 0 4220 1 0.005614546671670202 24.866273539301353 18.740952475869737 65.96067610225504 0 0 0 1315 1 0.005073341550923314 28.065861637191684 15.60293074996653 65.82898768515133 0 0 0 2026 1 0.004667155425861214 28.06204035476899 18.854892260706823 65.78150311743363 0 0 0 3481 1 0.00493825579771516 23.288799129224863 17.318873417573347 64.32374926479523 0 0 0 4192 1 0.004523172854719695 23.18060039979117 20.38430749457092 64.33432153860244 0 0 0 4194 1 0.004320754581293541 26.40953413032913 20.39496419684126 64.30425368752942 0 0 0 3483 1 0.00437263278570686 26.52652236935999 17.20001674466301 64.29126701319136 0 0 0 3482 1 0.0045373975912338365 24.77551514225108 15.79255898574096 62.668971129397484 0 0 0 4191 1 0.004535566597327144 21.61060369176148 18.818578634448222 62.72661068665911 0 0 0 3480 1 0.004549822741327094 21.618867284138673 15.606160375004361 62.7172294316251 0 0 0 4193 1 0.004668573249322374 24.81599912142149 18.893204663487484 62.68947177386181 0 0 0 1999 1 0.004772283457202278 27.972561056202583 18.855118923708353 62.660528479306755 0 0 0 1288 1 0.004458173922520863 28.033320749759138 15.621585130254475 62.680292647938856 0 0 0 4167 1 0.004939334111485822 26.459338559641527 20.478930477994254 61.0465354342648 0 0 0 4165 1 0.004817404958053351 23.358598113961524 20.505452604252646 61.08440257433899 0 0 0 3456 1 0.004733474445587867 26.450171236195477 17.207811702911762 61.09797226545732 0 0 0 3454 1 0.004622393735234327 23.221166844493165 17.320024630481804 61.10811282870791 0 0 0 2783 1 0.000782350465838532 15.291545593322802 28.382140281247665 69.12784754888416 0 0 0 4252 1 0.002369474440512224 18.446781129807682 22.091428745206446 69.10603955208029 0 0 0 4259 1 0.0010613591349287934 15.223876322370305 25.32621301619795 69.10641694445363 0 0 0 4261 1 0.00043429584049531345 18.406388145060745 25.232371608992068 69.05773628932029 0 0 0 2785 1 0.0005896797030112855 18.427249572727327 28.45672050850751 69.13249237925099 0 0 0 4224 1 0.003068415260878702 16.911644301711927 23.68727749575565 67.56649686385173 0 0 0 4233 1 0.005695095633725932 16.804836957503447 26.86712920063055 67.48251559910308 0 0 0 4235 1 0.007357431890356463 20.04806835758706 26.869476575619434 67.55412592493185 0 0 0 4226 1 0.005154764658959631 20.088756867953983 23.601004908178798 67.43760048724778 0 0 0 2756 1 0.005657795925976476 15.341751036273369 28.47119595628105 65.89589371935065 0 0 0 2758 1 0.005960960751223843 18.500749997654104 28.44363249250375 65.88016274375565 0 0 0 4232 1 0.005866626731817079 15.266123104037424 25.195118741295158 65.87909246069793 0 0 0 4234 1 0.0060132587600074654 18.41125417114888 25.240224632485916 65.93981973788162 0 0 0 4223 1 0.005219050084394822 15.29618151931612 21.95124297402264 66.02081787236244 0 0 0 4225 1 0.005659920483027783 18.431678086480495 22.10756292681231 65.93615829668416 0 0 0 4206 1 0.004307526292940636 16.853031192684533 26.81427563641244 64.30116490613412 0 0 0 4197 1 0.00504553671453228 16.84530295879924 23.59927682633494 64.26312187660163 0 0 0 4199 1 0.004589662771025384 20.180795185164122 23.713746781461733 64.36241795960723 0 0 0 4208 1 0.004099248787455949 20.06030499948268 26.854735858167462 64.41032762541693 0 0 0 2731 1 0.004277561506859751 18.49391681525099 28.32724487463359 62.750000757471746 0 0 0 4198 1 0.004759147930105845 18.521178550675714 22.018487074171475 62.69322222478096 0 0 0 4196 1 0.004563432056819763 15.311619352987195 21.942109594366592 62.74593786488534 0 0 0 2729 1 0.004337495095189964 15.328689395111615 28.401961615272445 62.756618354193535 0 0 0 4207 1 0.004464587748307259 18.478956041596337 25.22074300445022 62.78896583749463 0 0 0 4205 1 0.004450421499729613 15.351497054742254 25.21720404466124 62.779672862680634 0 0 0 4181 1 0.004835479684617646 20.12144078557141 26.824947452824514 61.13041055871286 0 0 0 4172 1 0.004792989696987882 20.143132462480473 23.784888127601636 61.18814672618596 0 0 0 4170 1 0.004680260634320985 16.96760515715101 23.5919542529777 61.15623996167551 0 0 0 4250 1 0.006621614072271723 15.242459882172538 22.024284972594455 69.19342299252457 0 0 0 4179 1 0.004748441810562573 16.966780122145426 26.78277059083822 61.18078192851228 0 0 0 2062 1 0.005235055564259841 28.110188821581527 22.011232071491634 69.13476044270081 0 0 0 4263 1 0.003293139381061171 21.60412930270722 25.156594511189983 69.13134515751358 0 0 0 4254 1 0.00446317736713815 21.633081039041446 22.045887013986142 69.00404242722256 0 0 0 2789 1 0.002328494613031048 24.921738253570826 28.488196079235422 69.11215501848025 0 0 0 595 1 0.0033297642826764645 28.07029373044258 28.373403930423112 69.07676209157671 0 0 0 4256 1 0.006516636927918349 24.960011031502773 22.046502400928237 69.13052112468728 0 0 0 4265 1 0.005513788831211045 24.900802844430867 25.216395764475237 69.17048469675134 0 0 0 2787 1 0.002166642201368984 21.67931689896417 28.39885458693422 69.11307200756792 0 0 0 4239 1 0.007663257225609831 26.48423538869363 26.800577304213018 67.52287023452672 0 0 0 4237 1 0.007977904260663759 23.27118979375815 26.830042232859427 67.58078617354377 0 0 0 4230 1 0.006764758019812968 26.596411952567344 23.678828467513068 67.48704288656819 0 0 0 4228 1 0.00666563843646392 23.286255667498153 23.69306261746919 67.51120695745566 0 0 0 4227 1 0.004930978275746241 21.59430138136824 22.03438483959183 65.97634033095893 0 0 0 2044 1 0.004508130659238267 28.05687448825918 25.187257063940432 65.91737507559283 0 0 0 2035 1 0.004572566774510924 28.045359669649333 21.99889005811429 65.96028909172198 0 0 0 4238 1 0.004559018512100809 24.85531533735496 25.144808269268207 65.97519280657937 0 0 0 568 1 0.005319649497445929 28.098284533562534 28.509636080280888 65.85155741789089 0 0 0 4229 1 0.004545586652489265 24.845212890727332 21.93498244247901 65.946980253309 0 0 0 2762 1 0.005529570340205885 24.79635015755137 28.420341975392276 65.96001281989749 0 0 0 4236 1 0.004998097457156823 21.62761361364641 25.264164882765847 65.99490174897088 0 0 0 2760 1 0.005458271536155693 21.736346904143787 28.416331430133912 65.97650730614652 0 0 0 4203 1 0.004011285412435806 26.551374167878176 23.587182837474522 64.36571659172552 0 0 0 4212 1 0.004160213725314452 26.493981904897193 26.797218867060344 64.37016550086538 0 0 0 4201 1 0.004145977789007096 23.322575521667822 23.58133587214786 64.40454306248581 0 0 0 4210 1 0.0038556834701177316 23.27626931081975 26.779240638063055 64.43665659563035 0 0 0 2733 1 0.004511991084851652 21.68534422604031 28.359871325865612 62.80245379788907 0 0 0 2017 1 0.004751061610827528 28.151196443051447 25.171669266636975 62.73966402006446 0 0 0 4211 1 0.004812002191562952 24.87239362244813 25.272036977487005 62.853311983992945 0 0 0 541 1 0.0046081334423620935 28.05901329565058 28.434354903768423 62.73322035211133 0 0 0 4200 1 0.004868145525199069 21.685004855605886 22.02155166174381 62.76976972825654 0 0 0 4202 1 0.004804224025306643 24.917890336653745 22.052285487506126 62.778763306723306 0 0 0 4209 1 0.004695067893122762 21.69241580245745 25.247649023287995 62.771801642503945 0 0 0 2735 1 0.00448907181555336 24.906146826225083 28.43458482649574 62.77891803485795 0 0 0 2008 1 0.004814667129091767 28.052884961839315 22.051418453309935 62.70080971298914 0 0 0 4174 1 0.005205304106837116 23.39933371691317 23.540084199851915 61.096756005236394 0 0 0 4176 1 0.005214625712352705 26.474222776395976 23.604615571339775 61.1509407024852 0 0 0 4183 1 0.005206826656743154 23.367534943053485 26.79874147326195 61.15756622043051 0 0 0 2071 1 0.005147827537487005 28.014123591405596 25.21079825030092 69.17657936391377 0 0 0 4185 1 0.005164659427716538 26.465977436992052 26.84227978308698 61.184502760297356 0 0 0 4307 1 0.25912999701765405 16.762661466003905 20.415657593307934 77.2335678059468 0 0 0 3589 1 0.0873713270405672 19.979656745701547 17.206820391407742 77.08282500844192 0 0 0 4308 1 0.11433679090375634 19.96802299937571 20.35800516054164 77.00918972237422 0 0 0 4294 1 -0.08004247225577765 15.207906160390074 18.827463884458048 75.44938655158134 0 0 0 3573 1 -0.01436570625011457 15.24551346296331 15.655106002089306 75.48271935559045 0 0 0 3574 1 -0.07818286587732243 18.48350729846027 15.673983418431211 75.40566970049761 0 0 0 4295 1 0.013267713378098197 18.425110622374163 18.799803806876064 75.43191793606414 0 0 0 4269 1 -0.005754058426926088 16.91118092769131 20.40108611421272 73.90866634739905 0 0 0 4271 1 0.0011442174531362762 19.962564900035538 20.38131551547606 73.92174372896653 0 0 0 3560 1 0.00647125103688442 20.051650963343892 17.29433295059383 73.83720009562387 0 0 0 3558 1 -0.012927768540289743 16.778810341131237 17.221411304509747 73.9044985317068 0 0 0 4268 1 0.011477220917140575 15.244793498654966 18.96159531246347 72.28094325864274 0 0 0 3559 1 0.01646103031600455 18.390931663799705 15.700590039759312 72.2306572843339 0 0 0 4270 1 0.00463681707801304 18.437290068156102 18.94542943987833 72.26195485208564 0 0 0 3557 1 0.012621691016850399 15.23263549619303 15.612351328279454 72.31621539117256 0 0 0 4242 1 0.007997571807444377 16.89157011441932 20.495135806277663 70.74212767779127 0 0 0 3533 1 0.00692476860410823 20.00040621281421 17.245579321055573 70.64032610694932 0 0 0 3531 1 0.00043033159324875996 16.820086520540542 17.353043912380024 70.73057526639747 0 0 0 4244 1 0.008170875079306484 20.03661483402033 20.462820355862082 70.64554065296448 0 0 0 3588 1 0.5783262152215792 16.9922960342259 17.20214389358406 77.44056492170637 0 0 0 3591 1 -0.057242352737796987 26.40673150416406 17.15806057399714 77.02297824834902 0 0 0 3590 1 -0.10345761961509835 23.322762119234874 17.236193811025085 76.90051668452759 0 0 0 4309 1 0.0543091240459789 23.266102583441207 20.377351365787362 76.99416676895522 0 0 0 4310 1 -0.014734401510990262 26.48421910046361 20.441870885573636 76.96053073644168 0 0 0 3575 1 -0.053964269500113654 21.53685572241772 15.626804304117586 75.53772779713222 0 0 0 2107 1 0.015747058423457125 27.985706884086593 18.710574495028414 75.51052768157261 0 0 0 1388 1 0.007385539933185215 28.018300558658108 15.516635557961317 75.46275525704567 0 0 0 4296 1 -0.041309621714560735 21.62891650397899 18.90991652629065 75.57756189227372 0 0 0 4297 1 0.0038162073954190155 24.838912674234756 18.864250224497763 75.58006877210438 0 0 0 3576 1 -0.009210894043290726 24.726696886795203 15.663226293910638 75.42985496013024 0 0 0 4273 1 0.004483563521943472 23.175110267483547 20.399762527632944 73.79438393212683 0 0 0 3562 1 0.020014324108308647 23.135660961889705 17.29346290209512 73.97862494130041 0 0 0 3564 1 0.008113898644629936 26.382847899865016 17.221335411626853 73.91490626748849 0 0 0 4275 1 0.005549200603282652 26.42950060289315 20.41543014111443 73.86018279391904 0 0 0 4272 1 0.005662710229102827 21.63729044705211 18.833228099070414 72.2918896653511 0 0 0 4274 1 0.008476137702367735 24.87045787637901 18.790333955061364 72.2042132633373 0 0 0 1369 1 0.009124413264522818 27.94037380778302 15.665770794011017 72.24240933850241 0 0 0 2080 1 0.013468647017427527 28.116558821763757 18.89291446555136 72.35023506226437 0 0 0 3561 1 0.010273170560370805 21.60109969204321 15.560988352720802 72.29775480010369 0 0 0 3563 1 0.0077553151108499686 24.685406872118023 15.67958441737365 72.27881915981807 0 0 0 3535 1 0.009656855786976181 23.286525021405808 17.238996211095653 70.58190458124811 0 0 0 4246 1 0.004077329568614953 23.202374865742605 20.4660521277372 70.67514748511562 0 0 0 4248 1 -0.00031193556249937623 26.49681886695119 20.430026145787703 70.7499438376078 0 0 0 3537 1 0.0034816046266560007 26.46816872393112 17.25885783232713 70.71116645879681 0 0 0 4313 1 -0.06584017989353964 20.06117100129591 23.56392879168188 77.27715731701784 0 0 0 4317 1 -0.037746129445787556 16.865228919540517 26.797939654872554 76.93025112591009 0 0 0 4318 1 -0.06956196275921646 20.068722164775174 26.695986739344402 77.06518648144373 0 0 0 4312 1 -0.02696164785034356 16.788991015118278 23.657374841865472 77.0238899437767 0 0 0 4302 1 -0.02117451923292642 15.31603929882936 25.185982446914334 75.48128809710332 0 0 0 2836 1 -0.008508778092059967 15.296257362509175 28.450506401219595 75.4258048511093 0 0 0 4298 1 -0.06401231153041143 15.220105351579845 22.002994775716513 75.51749019943968 0 0 0 4303 1 0.00022168203136219491 18.49806517956141 25.232952962122745 75.58858528621111 0 0 0 4299 1 -0.032452659316297004 18.412455148334573 22.095636895593437 75.63281096648987 0 0 0 2837 1 0.0017670267660052485 18.494091625701156 28.400599994708944 75.51364065580354 0 0 0 4280 1 0.007083079007549169 20.03211917155312 23.510585594036442 73.97303192519512 0 0 0 4278 1 0.012281868845199903 16.85981772748273 23.442623442113007 73.9470207568444 0 0 0 4289 1 0.017782504778354524 20.10377814068946 26.782685583543852 73.95222490855619 0 0 0 4287 1 0.018695822242548676 16.888541926791476 26.8421244490643 73.86567362602415 0 0 0 4277 1 0.003682598393782469 15.212473394966265 21.96855066423118 72.29077984531989 0 0 0 4279 1 0.008764584040663548 18.52010321458459 22.060561156063848 72.3060207546097 0 0 0 2810 1 0.0037776412742941898 15.360754391413757 28.355672296242794 72.31439987057752 0 0 0 2812 1 0.0020304449223842343 18.52752901291887 28.396821019007017 72.34987538973343 0 0 0 4286 1 0.0020715197372514395 15.21757234671613 25.219127919257744 72.38038629388805 0 0 0 4288 1 0.00969656512624243 18.421170089442 25.151330953083757 72.37621457465735 0 0 0 4251 1 0.01040401696321847 16.858322909692717 23.55429423813518 70.78154379807178 0 0 0 4262 1 0.001527229443413285 20.06095264244409 26.77363844644154 70.75191716090139 0 0 0 4253 1 0.0048091851482397075 20.034765354408748 23.6582986971614 70.69097694006231 0 0 0 4260 1 0.0076324189342603915 16.84085759889705 26.714311351184545 70.75841983373186 0 0 0 4292 1 0.007829779763833452 24.775008076585436 25.189800189805823 72.31643522428952 0 0 0 2089 1 0.011867614426766867 28.160464230867753 22.027557670636735 72.36838183318433 0 0 0 622 1 0.008279385206219883 27.986205962841932 28.360026819641494 72.32644542554925 0 0 0 2814 1 0.005950970917316096 21.581671610879745 28.474496242369757 72.36627933976285 0 0 0 2098 1 0.008579871057787267 28.017944851332913 25.172871841221305 72.2791246118493 0 0 0 4266 1 -0.004460826034016586 26.384535179556465 26.926474694093226 70.69804315304853 0 0 0 4264 1 -0.004273330184882868 23.231432452570303 26.827683406336728 70.59758699579425 0 0 0 4257 1 -0.0030204096725160584 26.489221377136694 23.528853997738963 70.67439985564393 0 0 0 4255 1 0.0008584769350587704 23.284201644748336 23.634670518574584 70.62770894457685 0 0 0 4314 1 -0.04396197257835806 23.112005808799022 23.508231412553915 77.30431554624786 0 0 0 4319 1 -0.0006716092159903056 23.24564340002625 26.704293017160932 76.98443605689283 0 0 0 4315 1 -0.007063801500055339 26.341006421599207 23.58028447037878 77.13830332689797 0 0 0 4320 1 0.0034908902407993388 26.431026373549837 26.747174906461602 77.09534298816581 0 0 0 4300 1 -0.013440381035468855 21.679238253590587 22.097218685241952 75.47639450974452 0 0 0 4301 1 -0.0027880539708316082 24.878177760156643 22.054407700594215 75.49658758965528 0 0 0 4304 1 0.016389822859028666 21.654087610421236 25.16260141851918 75.52172608218383 0 0 0 4305 1 0.020341374136510857 24.80629951769268 25.159615865982058 75.54972532946906 0 0 0 2839 1 0.011237856398045863 24.873938163492536 28.2566047164712 75.43471768069462 0 0 0 649 1 0.00028679246985134285 28.020806167845187 28.384187856257867 75.50136734465342 0 0 0 2117 1 0.005164533074533028 27.95875508932658 25.133624490525193 75.44285173417106 0 0 0 2838 1 0.010665762213033125 21.65689863899648 28.350556158802497 75.51728065303246 0 0 0 2112 1 0.00858310495183539 27.96188551434524 22.04013075972599 75.47269888594776 0 0 0 4291 1 0.014159061496382536 23.27164756550937 26.782295272160226 73.80566799015412 0 0 0 4282 1 0.008433137670024307 23.210585416580788 23.612342691000077 73.9040463086981 0 0 0 4284 1 0.011457277369629912 26.42425304172546 23.572274158990485 73.80116821441666 0 0 0 4293 1 0.012644138883574175 26.405745148138934 26.737299811963464 73.80487376722166 0 0 0 2816 1 0.012655998025600551 24.83890802598359 28.43437601462109 72.29278232186206 0 0 0 4283 1 0.006305238235900887 24.865953441508267 22.03976931347971 72.41850049981264 0 0 0 4281 1 0.006583871415587306 21.66738601363346 22.019909267133567 72.22303894562668 0 0 0 4290 1 0.009019404185274174 21.649807064893057 25.223357296088885 72.31450463323526 0 0 0 5388 2 -0.7087765488099278 16.96173657861265 16.410016755606886 85.1201296768216 0 0 0 4871 2 -0.6608949347568989 15.331776999969746 19.405541211975414 84.933825552964 0 0 0 4569 2 -0.6588015459685624 20.64224215852309 20.26463474581026 84.65069752860109 0 0 0 5120 2 -0.65992452464426 21.34481610944094 18.15037066189898 83.48765226430984 0 0 0 4477 2 -0.7278398913968654 17.549777464036612 14.958750444846295 83.92926366409809 0 0 0 4924 2 -0.6242700436925068 18.517568482171164 20.334223983689803 83.28906502990094 0 0 0 5155 2 -0.6818355970091647 16.944769574915245 18.26560038059068 83.25361578182572 0 0 0 4323 1 1.6333910351330783 16.835827516816064 20.3308352599268 82.77833629444255 0 0 0 4325 1 1.665680046808956 20.643768810748504 20.702356119852464 82.68594098476648 0 0 0 3612 1 1.7411747347375608 17.274326081070818 16.594396737266923 82.81723849324854 0 0 0 3614 1 1.5363554986858443 20.90382554049781 17.271042889317727 81.8971926548767 0 0 0 4722 2 -0.7894687103095769 18.77795161223263 16.568968288136972 81.83677432137608 0 0 0 4487 2 -0.7387769799015619 20.007086490594435 19.48140115748176 81.60013778010769 0 0 0 4863 2 -0.7672968407192452 14.816381858130205 20.050239057098064 81.95360086493208 0 0 0 4441 2 -0.83500640879127 16.05232020722141 16.241860239672384 81.64096363840943 0 0 0 4380 2 -0.7603475693711641 17.098513681713023 19.11547563243413 80.80315077352047 0 0 0 4322 1 1.5241987408175628 15.41988223122245 18.86316244205046 80.23820873655959 0 0 0 3613 1 1.1402363045965676 19.192835692279324 15.670187571208663 79.86040524805104 0 0 0 4324 1 1.4690147444129489 18.936002886788774 18.983268005499756 79.76489870426539 0 0 0 3611 1 1.5948475327106737 15.6553308283616 15.488898062758656 79.6974176162658 0 0 0 4963 2 -0.731758608041945 19.787203205490453 20.5026751558243 79.47449957782801 0 0 0 4422 2 -0.8521446277704656 19.87970479056603 17.338604277059883 79.51859475358084 0 0 0 4588 2 -0.8036186696282018 15.618686796800334 17.539646212066497 79.15386469376298 0 0 0 4844 2 -0.7652481760410937 15.118948970416671 20.086777599686396 78.960225959354 0 0 0 4565 2 -0.8012778132916043 17.60837280278406 15.757859598544922 79.10184477379474 0 0 0 4734 2 -0.7459441985378775 18.036084017032252 18.854523354104167 78.19096888610964 0 0 0 4653 2 -0.7604931132955584 15.012594384533225 15.501094383124132 78.07734906655837 0 0 0 5171 2 -0.6498750848599303 15.836092332530036 21.285777565947743 83.98900033686976 0 0 0 5167 2 -0.68098631213466 15.039950904155816 16.828279656084536 83.61381991681061 0 0 0 4688 2 -0.6730279819761266 19.657210613949452 14.593588000992622 85.16302539938098 0 0 0 4349 1 1.6948383945733172 15.466153060927278 17.79153623055075 85.61765549893823 0 0 0 4358 1 1.7509797805558098 14.551235182322888 21.32184422064477 85.66804261989613 0 0 0 4736 2 -0.6324002190342933 26.368428404601758 18.263122908131702 84.13906222627516 0 0 0 4786 2 -0.6989005835804621 23.533255594023643 17.62942578457392 85.11705787842257 0 0 0 4362 1 1.7082375406480625 22.662666712402157 19.11284494926068 84.7709652265766 0 0 0 3644 1 1.6748335343446232 27.780899791262367 14.92766636866202 84.89560770006945 0 0 0 4508 2 -0.7900331839911 23.848686825924005 20.571148483474776 84.62581198053489 0 0 0 4478 2 -0.7027894707655901 27.707722359718968 16.469351135370975 84.11535104401754 0 0 0 4355 1 1.5881112062272542 25.145384991777913 17.10937162043928 83.49910824803355 0 0 0 4752 2 -0.6463278465555818 24.609717123680475 15.652585639327686 84.43021468585316 0 0 0 5224 2 -0.7046716591325455 23.96946269742195 18.23748192949974 82.89229232980072 0 0 0 4780 2 -0.7544796062749979 25.94270050193713 15.893567733308558 81.89903468208104 0 0 0 4413 2 -0.8664713201353447 22.409312097468984 20.556735526123827 82.4893077550505 0 0 0 3607 1 1.6061795721184589 23.18712801021381 14.357569290518134 82.08095512051857 0 0 0 4945 2 -0.6939609053749591 21.37319546715831 15.617620782454004 82.00724332041804 0 0 0 4592 2 -0.8085573293536373 27.908952002286757 19.211907459397025 82.0029151957279 0 0 0 4679 2 -0.7441940169162745 24.98540551154031 21.213756768293205 81.44745480483043 0 0 0 3616 1 1.429559610461928 23.567288548645124 19.3981339484598 81.08792660425492 0 0 0 4463 2 -0.767798773945885 22.125104992533586 18.02284020150495 80.86346836053681 0 0 0 4526 2 -0.7566063159191606 28.28061568931723 14.915291780442168 81.06880677417952 0 0 0 4486 2 -0.7075653982325816 25.28861725996827 18.716103426240466 81.12313157252164 0 0 0 4329 1 0.7251519056309355 26.717752100613918 20.433498764937998 80.75154126464805 0 0 0 4582 2 -0.6786038770759788 23.45018750102832 15.264752406689142 80.46953085441288 0 0 0 3618 1 0.5305864661120775 26.83260028492094 17.486203132986105 80.61238647972031 0 0 0 4449 2 -0.7931918033466436 23.1966785798054 20.201873016289092 79.55834476454764 0 0 0 3617 1 0.36203178464373403 24.88712205412265 15.80340191028831 78.85986378417874 0 0 0 4326 1 0.4269642277356708 21.783537019853455 18.543189649570717 78.67149477641378 0 0 0 3615 1 0.261673748489074 21.85591298414992 15.770777979104968 78.95459884421086 0 0 0 1423 1 0.05645002491794911 28.075934020929726 15.64138680125687 78.7535272307387 0 0 0 2134 1 -0.14411403460973835 28.019351192719647 18.758412858767535 78.64171966404207 0 0 0 4328 1 0.10523786416899779 24.971733009328794 18.81404218604278 78.6389019411113 0 0 0 3609 1 1.5955847782343184 26.65236591644886 14.349527921062391 81.4738278695001 0 0 0 5145 2 -0.6125881720965363 24.008674173275864 21.643590779567603 90.73395086181733 0 0 0 2161 1 1.6353412686945121 28.38324520678515 18.427598121699628 83.4283407767908 -1 0 0 4909 2 -0.6722142267033403 17.618978341305507 25.38516862641661 84.85391074463337 0 0 0 2893 1 1.6651922849720449 16.801784921758898 26.912802776483865 84.7301493477922 0 0 0 4369 1 1.7054374158718575 17.726389261219296 23.193441846992464 85.07031599001276 0 0 0 4437 2 -0.8013001107745199 16.67237269295184 27.52496533785212 83.09188921183177 0 0 0 4500 2 -0.6858043540675469 17.624587733460793 23.507308246092677 83.33386108314586 0 0 0 4573 2 -0.5967174514808492 20.476549407874003 27.44916512685911 82.89677856174482 0 0 0 4626 2 -0.8049845529639073 20.4247512356403 22.420691909122674 82.34522047043889 0 0 0 4545 2 -0.8304171492840706 15.260881670844855 24.80336122321486 81.63955981038619 0 0 0 4587 2 -0.7583028035708373 18.395384948716785 25.53975619603274 81.41702232374448 0 0 0 4341 1 1.130278489079518 16.71997464385598 26.31205856111206 81.39686626745693 0 0 0 4528 2 -0.7140104999474918 16.753788389949214 21.6775064792007 81.3004195689236 0 0 0 4332 1 1.1830983318353785 17.144575566093483 23.592819028911457 81.23410546074292 0 0 0 4343 1 0.7865783039276902 20.10584424918605 26.538827549587026 81.16335014675536 0 0 0 4334 1 0.2601851882438953 20.040078524316918 23.69761258610666 80.49560964856657 0 0 0 4427 2 -0.7694806337859549 16.859075787827823 27.30684242519746 79.94947882046453 0 0 0 4899 2 -0.8275976009106694 16.817395048030363 23.963172719856455 79.60045865785264 0 0 0 2866 1 0.38263496333248925 18.56429896862475 28.368108852212444 78.92525894606756 0 0 0 4333 1 0.2518069167575019 18.3406777429708 22.176531687260937 78.78086258317697 0 0 0 4331 1 0.7210725908302389 15.41187309057701 22.13730926442284 79.1424265043697 0 0 0 4340 1 0.5536107699307187 15.19952730027515 25.16843581753507 78.81514074940588 0 0 0 4342 1 0.1895612552426445 18.450886255828113 25.388354051198128 78.81536645836107 0 0 0 4980 2 -0.6153057984723459 15.159492098999628 25.484073886863897 85.01301410952789 0 0 0 5327 2 -0.6333675704799555 18.88651269632411 21.947649206799102 85.46412303496608 0 0 0 2864 1 0.29451608750542535 15.374319553262833 28.38178395996468 78.76561802251018 0 0 0 4676 2 -0.7590188496398141 21.132248907306433 25.195028254840903 84.44776881255942 0 0 0 4813 2 -0.6497665784260092 17.521137723523722 28.038511865008687 85.90978047293787 0 0 0 4425 2 -0.6888447743650811 24.63683762141207 23.539818697507297 85.17777508568105 0 0 0 2895 1 1.6299983387873873 21.582073475575328 27.494969242231182 84.60479171065086 0 0 0 4596 2 -0.667454483997152 23.144659590625093 28.076322838873168 84.02277026538336 0 0 0 703 1 1.736142634355784 28.05115120800615 25.97005540685022 84.32796061810225 0 0 0 4645 2 -0.8054000023785027 26.057907777602285 26.392749629639134 83.93433940542094 0 0 0 4591 2 -0.7531131338530328 27.032980795779952 24.08432518825618 83.53383067175437 0 0 0 4405 2 -0.7214350879452697 26.068821108077184 21.814804254595828 83.75896539363171 0 0 0 4373 1 1.6136166612750475 24.999376838940943 24.61219827469254 83.41454122937392 0 0 0 2897 1 1.6457258749313077 25.15996375782225 27.84706042638781 83.44394143622115 0 0 0 2179 1 1.5897709258647723 27.671234801905744 22.469064622223815 83.28277046630132 0 0 0 5320 2 -0.8038643942031003 23.087598060687444 23.37447491385441 83.17465520926959 0 0 0 4371 1 1.415314450763893 21.49271068372116 24.20980596736361 83.00237703094695 0 0 0 4327 1 1.348375187060381 24.109216095705094 21.751153110531863 82.91895849232522 0 0 0 4880 2 -0.7129486152235315 23.962808668100976 25.820241456013353 82.76592529469808 0 0 0 4514 2 -0.742149233247852 25.08192739542856 23.6717956895718 81.94633676177641 0 0 0 4409 2 -0.8052677094073442 25.08750338030726 27.828734871565498 81.62555147954258 0 0 0 4506 2 -0.7897434304972415 28.152212311593594 22.14968892794689 81.53292440534638 0 0 0 4622 2 -0.8287161508226456 21.696744258316343 25.167231217477887 81.59525868615265 0 0 0 4336 1 0.28746320125109387 23.206583765834026 23.540383395792983 80.4740660063267 0 0 0 4345 1 0.6584518880756409 23.285938323017174 26.519129327281277 80.87220942650428 0 0 0 4338 1 0.339454397705144 26.45435644629521 23.671117638429653 80.34114688365887 0 0 0 4347 1 0.3632977153251702 26.50242171780261 26.713391723058194 80.47563366180563 0 0 0 4335 1 0.37056989219880715 21.6432399117706 21.623794211192223 79.08875927489778 0 0 0 4344 1 -0.08704247256589584 21.60763860826387 25.335266062583337 78.91430308702732 0 0 0 4337 1 0.14464154207982008 24.764534497325368 21.81181401099004 78.83028055085985 0 0 0 2868 1 0.03912552028922528 21.779464616196016 28.23978266536945 78.85707884324793 0 0 0 2870 1 -0.11856574209339618 24.83862397332678 28.250307824830923 78.72811528632872 0 0 0 676 1 0.07678514882927476 28.072531275235683 28.35758604385462 78.72879188107048 0 0 0 2152 1 -0.13637964954756399 28.03164816730595 25.232535991728906 78.68146518454195 0 0 0 2143 1 -0.091739757557463 27.99076812168173 21.836748759316414 78.6903814002718 0 0 0 4346 1 -0.1154678238183248 24.73084641902137 25.160260830528763 78.75588877405717 0 0 0 4629 2 -0.6457500379139275 28.14776055189823 26.180322089206555 82.2019906399625 0 0 0 4348 1 1.7082626934107887 15.72027321116916 20.766629017603208 92.81144038766045 0 0 0 5470 2 -0.3675638810036325 17.42658814718445 19.45738836657626 92.31067713574491 0 0 0 4352 1 1.6853618041118457 19.374690725016567 18.93983420087702 91.26501697279623 0 0 0 5242 2 -0.4127293322445995 18.937451356796625 21.07280079231716 91.14992085979561 0 0 0 5081 2 -0.6259085542726613 19.739224403943087 17.369473167432115 89.89104328678792 0 0 0 5179 2 -0.5854304835009264 15.068748658576444 19.609362957139158 89.39173411284267 0 0 0 4691 2 -0.6308205731992981 17.707382888161 18.864789299446148 89.92448475550256 0 0 0 4696 2 -0.6685261734854072 14.659386395170511 16.91362184555545 89.27953015599377 0 0 0 1458 1 1.7149457891277775 14.896809705540422 15.29400625011345 88.6539930804371 0 0 0 4359 1 1.7438880185701962 16.665639773889286 19.634048935241704 88.67566316061274 0 0 0 4351 1 1.7514538282832932 20.435575397966097 16.900274336901674 88.29599585646618 0 0 0 5301 2 -0.6613249804630074 20.83467486495688 14.676800414521766 88.67507551606656 0 0 0 5184 2 -0.666035958225497 15.933679961428737 15.410219613818072 87.29046840381721 0 0 0 4530 2 -0.6503708061740595 18.730758051288632 15.882180706659861 87.35048363613903 0 0 0 5019 2 -0.6085889493998277 19.811952466099992 18.217377735937557 87.22834769405634 0 0 0 5108 2 -0.5376034664723541 15.24019744210159 20.779675968818296 87.22854576824092 0 0 0 4607 2 -0.5903980958400877 18.147554267850463 20.160504618753606 86.91309659551281 0 0 0 5312 2 -0.6664543198025843 16.30435859430766 18.230705645861708 87.14683427058199 0 0 0 4360 1 1.71548653768058 19.855770496909226 20.305934840974224 86.61133195960204 0 0 0 3640 1 1.7727551835775586 17.77388113101251 15.121887440222933 86.11268095448129 0 0 0 5364 2 -0.5622229413598407 20.759510966436377 19.42323751559229 90.28866681188316 0 0 0 5428 2 -0.47053350343380684 19.695844851665615 17.11524020995771 92.60434811582097 0 0 0 5512 2 -0.5026491227770785 20.029058892254422 19.147775589691424 92.96360371833688 0 0 0 5509 2 -0.37475695864186637 14.941434301218022 18.888762452903844 91.90172163386791 0 0 0 4419 2 -0.5885205318076944 16.291581373205236 14.43956125883633 89.77411413567815 0 0 0 5185 2 -0.5918041036683495 17.16722525927581 21.340481208641876 88.95291829986185 0 0 0 4983 2 -0.21553993339775082 16.996106094183165 19.011937733919115 93.59891550556485 0 0 0 5455 2 -0.1900433981004193 14.878809007059775 17.481918904783203 91.8925945279502 0 0 0 3642 1 1.7292415165285315 23.115542535447887 15.606247202033991 86.01609835003346 0 0 0 5335 2 -0.5848116021944032 23.264901190350365 17.32252735438114 90.68312597889887 0 0 0 5495 2 -0.5196688208244472 23.91679563902762 15.87922802109521 93.6695489302122 0 0 0 4650 2 -0.6397666202293972 27.93478983737772 18.941267757869014 93.46860836531987 0 0 0 5041 2 -0.5448978858686251 26.007983280508316 17.070091699706023 93.35151220547635 0 0 0 4712 2 -0.6119259766262994 26.174656832539693 20.78452803768533 91.9099887570335 0 0 0 1468 1 1.67498381867225 27.80930799485129 20.14459026741405 92.19030848202311 0 0 0 5075 2 -0.5341792778542768 26.319195550949356 15.13111256764736 91.82503125994374 0 0 0 5058 2 -0.5594045761965737 23.61077045729581 19.651071516636424 91.68759341710117 0 0 0 3634 1 1.7035242914493065 24.761757552979507 16.017985350146706 91.70828741905008 0 0 0 5049 2 -0.6375185203137002 27.50692601284108 18.77237432608449 90.44993568261252 0 0 0 5243 2 -0.5612815891797319 25.543432373684055 17.421617772091164 90.86065057176333 0 0 0 4353 1 1.703467375412944 23.114525407606042 19.047715432308117 90.07051162681174 0 0 0 4936 2 -0.5832364949648101 24.941896980023255 14.858804678704445 89.84768925352937 0 0 0 5175 2 -0.5114953458334439 22.760241024199033 20.526969964065483 89.14328679749525 0 0 0 4772 2 -0.5642760069842495 21.98835147325785 17.594937433190612 88.66493545686977 0 0 0 4809 2 -0.6321016399495772 24.892131260079722 18.910361707437396 88.85720984695244 0 0 0 4356 1 1.652562223177046 26.55253594597889 18.266179264657254 89.04693183909352 0 0 0 5042 2 -0.5902189880092814 26.525400946872363 16.560564459078716 88.57543706490401 0 0 0 4767 2 -0.6246309515065431 27.96817166904197 18.909810531702124 87.53296214001954 0 0 0 4507 2 -0.6395121447988882 24.419535373257602 15.77031276719746 87.13218308860534 0 0 0 4665 2 -0.6549208788936267 21.69518652877334 16.35293168916198 86.58849544729743 0 0 0 4675 2 -0.6190601593898836 21.780451572556288 19.38268257925533 86.22146766447905 0 0 0 4621 2 -0.6361195791533837 27.04753967712032 14.915633296309197 86.45759297640369 0 0 0 3633 1 1.7711935854689718 25.776260355409363 14.473012635509296 88.32326894722446 0 0 0 5044 2 -0.5186794360291341 23.455044446909994 14.40863511811229 91.79442410799896 0 0 0 750 1 1.736795823605475 28.430062507918414 14.67401187584866 92.964725892824 -1 0 0 5336 2 -0.561407702078293 23.034922193975017 20.637176554609006 93.81784803477423 0 0 0 4920 2 -0.572259062614286 16.200800334670667 22.71752313975358 85.8496849396515 0 0 0 5290 2 -0.6111870176586643 16.36659149447996 21.510933483196016 91.39039302034791 0 0 0 5188 2 -0.4962153642028789 20.58226270540908 21.393673778984564 87.68601312410316 0 0 0 4873 2 -0.5810178584151573 24.808668999926507 28.393451427649133 90.54759247431879 0 0 0 4782 2 -0.6196450932525638 15.253086124748135 26.88477554389484 93.54932606300149 0 0 0 4952 2 -0.6528909276355209 15.4209336170744 27.537498035694263 86.31782301442239 0 0 0 4996 2 -0.6514933709524899 19.013806235883976 24.156404218644894 86.54548220426936 0 0 0 5497 2 -0.21911651810733596 19.09970341360958 22.125708033859134 92.09486579656344 0 0 0 1485 1 1.730330190713955 16.381696005558805 25.01302471373026 93.03878702823236 0 0 0 5305 2 -0.5960744588682063 17.52104532666204 23.99070955163513 92.11624907202338 0 0 0 4410 2 -0.5947492569223686 17.745816320864808 26.410419614936885 91.84825483646684 0 0 0 5235 2 -0.6091093834629476 15.080207160009026 24.888718589689436 91.783615717966 0 0 0 3667 1 1.7809139049866498 17.857172580053756 22.76414813465701 90.34936355168837 0 0 0 4368 1 1.7234336169637863 17.741710015756876 27.768400670778046 90.67403441999618 0 0 0 5247 2 -0.6062427517000276 19.357767932380746 23.358508445399124 89.68074953772467 0 0 0 4788 2 -0.5696722458940148 16.884196055035073 23.966864541596912 89.58538577778442 0 0 0 4361 1 1.740631973460307 20.614905022518116 25.157103143618876 89.99674534971271 0 0 0 5089 2 -0.6177921240492933 19.34218636802977 26.367343652287428 89.80880701865448 0 0 0 4367 1 1.6995434865748391 14.974982527559272 25.291671473954576 89.64097262850068 0 0 0 5087 2 -0.6051335222528275 16.426230230831138 26.33674573436009 89.55347251091511 0 0 0 4370 1 1.5767763154851633 20.248128412993474 25.349161671935562 86.39405309995048 0 0 0 4550 2 -0.7449666252486938 19.773446911169515 27.036334595221646 86.00376215985584 0 0 0 4806 2 -0.6049035253425713 20.86482332234666 24.85371765471525 91.72729155729084 0 0 0 5165 2 -0.5893297820290189 14.679741765405655 24.796902623091057 87.46393493417885 0 0 0 4631 2 -0.7193789575482558 21.167509604936697 25.542752327411208 87.88957772172829 0 0 0 4411 2 -0.7790555144522263 22.249647981785824 28.589153323446368 81.21444082796556 0 -1 0 4830 2 -0.60856496405878 18.156524907186615 28.491893023456548 88.56415812994993 0 0 0 3671 1 1.6497753496748289 22.984496269872984 27.50022539689415 91.33737104733986 0 0 0 4802 2 -0.547515498831743 23.784662282602373 28.29905120128804 92.67645603067416 0 -1 0 4559 2 -0.5856618263032557 21.99589900102564 23.390383533405643 89.71709309591975 0 0 0 4543 2 -0.6083158682354695 24.01575962669513 26.891718070651407 89.28876493475587 0 0 0 3662 1 1.732223283235998 21.777813269641523 24.55240782358618 93.68857546722982 0 0 0 2170 1 1.677043203222014 28.248499929612223 22.328579534885346 87.75478025393328 0 0 0 4372 1 1.7532947590830132 23.260448500029366 26.163950514333433 87.90934738375326 0 0 0 5028 2 -0.7411155507217598 26.822114974915614 28.12480607659096 88.39373326020504 0 0 0 4812 2 -0.6181986893762693 23.441875651987136 24.44264421959827 87.78093174325498 0 0 0 4404 2 -0.630409386673882 28.222076553329142 22.96785772310677 91.43806437730525 0 0 0 4363 1 1.7310932505465542 23.625508768433313 22.748195333786605 89.34219029218485 0 0 0 4601 2 -0.6487930112514922 27.37006802576904 22.82271503042398 89.1774169528272 0 0 0 4633 2 -0.662235195930185 27.249078680190227 25.33430509442683 89.39242600409403 0 0 0 4406 2 -0.655150002555499 24.215653808641477 21.838001061826688 87.51416074494578 0 0 0 4522 2 -0.6154421199259363 22.346053324278977 26.266281939115288 85.98300776767987 0 0 0 4412 2 -0.6150467646367968 26.66233227269177 21.816113395878226 86.30267256219656 0 0 0 4505 2 -0.6594058596580938 23.500176423205534 28.035247019901043 86.84550835152875 0 0 0 4377 2 -0.6127570456056284 25.3800842955948 26.07928631866475 87.2921933023408 0 0 0 5021 2 -0.705235651371586 22.072237228856224 26.16999147085459 89.71204576066162 0 0 0 4600 2 -0.5882985242863006 27.401809437292314 25.66888001964361 86.0406617799261 0 0 0 4702 2 -0.6203375964296932 27.60417906568891 27.810113788926433 91.36182523592385 0 0 0 4354 1 1.775761841267624 24.25126412666726 21.48764238050355 92.86947832857066 0 0 0 2195 1 1.6748268117263032 28.01561881163692 26.710179728983935 93.29080106689602 0 0 0 4808 2 -0.58656601256379 22.869572415624262 26.08765483642221 92.48331788944381 0 0 0 5476 2 -0.5426233553404335 22.980737976440697 23.108345537679643 92.83756822653915 0 0 0 4364 1 1.5525436658420837 24.88128961631328 21.96362438994944 85.86514609875519 0 0 0 4913 2 -0.5850852605785959 25.657014834342156 23.07516748465207 92.17025251004272 0 0 0 4877 2 -0.6353406398174853 26.782335718933197 25.39822336397163 92.04042365629816 0 0 0 4957 2 -0.6568983182311021 24.945587148600154 23.764086339297346 89.82016174640856 0 0 0 4374 1 1.673642188593282 26.94401017631464 26.342576300820333 88.00321974893826 0 0 0 4365 1 1.7533314089651943 26.75541813277408 23.9119093981486 91.03470804689086 0 0 0 4641 2 -0.7008612363953697 22.02608077885912 14.412779202210706 83.80190125510208 0 0 0 5420 2 -0.5527027678001797 14.539201543825921 23.61094741411886 89.94391633146077 0 0 0 4540 2 -0.5481068316524652 20.749779771788237 28.45467604663806 87.8240144183399 0 -1 0 4376 2 -0.6196848589521674 28.369595547069927 21.578814340670537 93.819381252196 0 0 0 5007 2 -0.5537275943779072 20.504949480006168 20.659950572474703 98.63946653168543 0 0 0 5418 2 -0.2035120951459885 16.665012994150914 19.189787814085058 98.85398875621166 0 0 0 5391 2 -0.17287195536747338 17.141488449072305 18.08720973814775 98.24663016373825 0 0 0 3649 1 1.6091750866772543 18.628532152342263 19.908709619309136 97.66788276536799 0 0 0 5294 2 -0.4291613159811153 19.219264732853205 18.766027581924707 98.89542918482483 0 0 0 3638 1 1.4092077733999027 20.029400489665786 17.290979653938948 94.62924230427046 0 0 0 5404 2 -0.46837555762469935 18.92782919212694 18.377427367617607 95.97533604856315 0 0 0 5285 2 -0.5923702450399246 20.173528406121438 20.967033435715813 96.4301565018866 0 0 0 5422 2 -0.17274627701733924 19.06735721020102 15.249388013317969 95.19528437912473 0 0 0 5466 2 -0.15826063416490305 18.11474567056485 16.159281400990178 95.23690439892995 0 0 0 5241 2 -0.4642919877299657 21.38134872440549 18.867099277755166 95.07703418011936 0 0 0 5463 2 -0.42330615574515096 18.094942848044077 21.354067364205562 98.55395921720708 0 0 0 5375 2 -0.4804147671359618 20.532037276058936 21.652396119662047 101.20560293635972 0 0 0 5374 2 -0.5113072138249607 20.873244621132887 18.98386642014543 101.21312666231069 0 0 0 4350 1 1.5693906618218287 21.460248206587824 20.69384156751456 100.13951503326206 0 0 0 5454 2 -0.4934802409519104 21.462306789494644 15.886290399249512 95.23408839072508 0 0 0 5141 2 -0.5590560155684405 25.453479901318165 18.524267309042312 101.6399109944406 0 0 0 5086 2 -0.6011896923455806 24.441864617348575 15.759920943738912 101.27097164612458 0 0 0 4962 2 -0.5670892538444929 22.101336416488643 16.60258490014805 100.4582086241408 0 0 0 5360 2 -0.5795583656858468 23.262741521079498 19.701530444278447 100.24718177220738 0 0 0 3632 1 1.6171237136780818 25.257055011568816 19.118068011508285 99.9738795262305 0 0 0 2931 1 1.6328746552182023 23.64622855121624 15.657740607012636 99.71215387827205 0 0 0 5213 2 -0.5778962996507075 24.507668644947906 17.69324627942095 99.22982853976323 0 0 0 4718 2 -0.5972407054735479 27.412622911457284 18.593628327712896 99.79168006048948 0 0 0 5279 2 -0.5754535856222611 25.818337964072747 15.470480817109006 98.95178617185024 0 0 0 4959 2 -0.5752826229361538 25.029976143858466 19.614761721363116 97.7561900399638 0 0 0 5323 2 -0.5130097633673828 23.258114416364315 15.8227982890967 97.62198275060955 0 0 0 3636 1 1.6560468667122965 26.879988933868926 14.85312992568804 97.66152932587289 0 0 0 3651 1 1.7268142713484627 25.440940638866834 20.79572847498861 96.47190122107911 0 0 0 4960 2 -0.5943347332780687 23.25914438691024 20.829052812815046 96.35499188611425 0 0 0 4466 2 -0.6015857850113255 27.199841537853132 16.21844940144277 96.61475216796633 0 0 0 3641 1 1.5444771766083476 23.59249534404424 15.212821127893893 95.61758448536625 0 0 0 5035 2 -0.48295521311783435 25.011609258143377 16.697733171526387 95.60606187949087 0 0 0 4783 2 -0.5828689889243805 25.709198044356437 18.989409343547273 95.0749912892802 0 0 0 3643 1 1.7152747744457477 26.80903807889206 17.606713858041996 94.85115000701451 0 0 0 5346 2 -0.23295417601473567 26.48973040374956 21.06188576213758 99.50011137860243 0 0 0 4379 2 -0.5239001187729099 28.397920775652455 18.274173440624104 96.0346853538079 0 0 0 4991 2 -0.6243949629540946 27.191979124055244 21.064651830977507 96.4570400426606 0 0 0 3658 1 1.6985711363538218 21.660877035903493 21.14431569925415 95.52903950692328 0 0 0 5252 2 -0.5878145472047455 28.261635834445727 15.93451404474234 99.08032808297804 0 0 0 4444 2 -0.44736941535366165 20.076043871334445 24.652241308060496 94.01904228228507 0 0 0 5144 2 -0.6158344354844865 25.22203232041611 21.46170141957537 94.33222661502593 0 0 0 4567 2 -0.3603669443229898 25.16367928845133 21.341165384330964 99.82324535599727 0 0 0 4493 2 -0.6439519205012558 27.901779209335984 15.746279209595528 94.24157656761777 0 0 0 5074 2 -0.5456024559534572 17.219123427278443 21.18540094241145 96.36381345321111 0 0 0 5151 2 -0.4496970651896552 18.73514676601074 26.005744482387044 98.15159165287221 0 0 0 4947 2 -0.5820897708893341 18.585183033111885 28.242269912546504 97.50392559125632 0 0 0 4999 2 -0.4591576884656312 15.907231872624946 26.5252569712577 97.80885152485234 0 0 0 2191 1 1.5635362456530206 17.455492634367648 26.352139767243084 96.99975768689251 0 0 0 5134 2 -0.6044865239536067 21.22651507004307 27.49720278911195 96.71972960307909 0 0 0 5237 2 -0.5558993072096342 17.34226449057405 24.119817813865957 96.74201776848803 0 0 0 3656 1 1.623297256617283 16.23991684148301 22.73600191700154 96.32014682678613 0 0 0 5504 2 -0.2552923008986581 18.210025164590487 27.079658601873504 94.96666909057774 0 0 0 4848 2 -0.38777318089775265 17.31136109554839 25.9862568307657 94.86218987358299 0 0 0 5297 2 -0.590329253385566 15.94298741215156 24.10127625842858 94.47645353369703 0 0 0 5448 2 -0.434197079720583 15.17919752172565 22.71619803217623 97.75084338953926 0 0 0 5240 2 -0.20167483015412616 21.258145202143893 23.223223686243816 96.72828371367477 0 0 0 5036 2 -0.578094394927999 21.47358611838445 22.463903810769203 94.35437713456024 0 0 0 5503 2 -0.5663921914182198 16.359138867885946 21.79973535209761 94.09922906546419 0 0 0 5253 2 -0.4573396547443839 23.287455382221214 27.560975197959095 100.45219202342052 0 -1 0 5357 2 -0.43287625787849315 24.965126296341374 24.058852820368816 100.29397229987056 0 0 0 5456 2 -0.5930670202538811 22.84853974153566 22.506203400905335 99.75916184283221 0 0 0 3660 1 1.6635820731164292 24.122788471811244 23.38299203718859 98.89577298547269 0 0 0 5501 2 -0.5753319982585317 23.244168780136384 25.12810000183089 98.1759072469846 0 0 0 4589 2 -0.5536287019036108 23.326963556704825 27.949239934691636 97.8149555957214 0 0 0 5026 2 -0.5691402503984918 25.90724013201258 24.384980062598466 97.96035121657343 0 0 0 5299 2 -0.6152282319516724 25.13184297655404 22.346808826139288 97.34508433652681 0 0 0 5125 2 -0.3043647953658295 22.43429458748187 22.699666346025445 97.26195157518346 0 0 0 3669 1 1.7219613364844097 23.24844352978213 26.564371103431 96.75116550303048 0 0 0 4865 2 -0.531959363835855 26.963186567757692 26.916262720448422 96.5346546375575 0 0 0 5325 2 -0.6235476340025885 24.854671281891637 26.260720753758996 96.20534808599508 0 0 0 2942 1 1.6398986239202502 26.53883337944972 24.853642032839005 96.34526021465429 0 0 0 5250 2 -0.6220114421903964 28.27058372858062 23.57659360719336 96.27962385310713 0 0 0 5148 2 -0.500230333622698 25.685655991493274 23.916096380093826 95.18886466174966 0 0 0 4807 2 -0.6106366028424085 22.559434578593486 25.396614037164788 95.03091621582783 0 0 0 4816 2 -0.5968559842895549 27.678114151707092 25.462586552425208 94.44818237919111 0 0 0 4992 2 -0.5922782599748608 23.027993338069543 27.92076718430255 95.01114927531101 0 0 0 4590 2 -0.5948718853427315 27.208171237764034 27.97158546409601 94.1955888635413 0 0 0 5427 2 -0.31910680093194477 21.44943623803773 28.384412475925874 105.62016842435459 0 -1 0 5278 2 -0.48844615098306576 20.231124079812304 15.920734301497154 101.97084989717999 0 0 0 5432 2 -0.3082889298602804 20.177459556224004 17.682998143366436 104.28507106764036 0 0 0 738 1 1.5310210632222614 21.316197114629773 17.22387346704965 102.3936385273538 0 0 0 5458 2 -0.26246844601589553 20.728982411349264 18.907393881396345 103.99493652153328 0 0 0 5025 2 -0.4720951377111816 25.786567505537423 17.97208903422826 104.48505002388026 0 0 0 5126 2 -0.41358211515537807 26.796947184135266 15.869334377871093 102.58372821995764 0 0 0 5482 2 -0.5976659518418389 22.814775408776146 16.932967174875984 103.28296022381829 0 0 0 728 1 1.4395654719226525 25.19702380428621 16.588926445606816 103.32638784479205 0 0 0 5140 2 -0.45824221652144725 24.529792007156225 15.198406050485703 104.44807074677482 0 0 0 Velocities 41 0.0013691033287171867 -0.00028627420729682173 0.00029704108243070284 48 0.0003748735944712144 -0.001731876937042355 -0.000734540354762748 50 0.0005809274802019534 5.0492012283697785e-05 0.0012664125160707367 39 0.0006782512089098939 0.001732736055462389 8.828084944727949e-05 11 -0.002056889648080851 -0.0017241310109934278 -0.0009819971146477393 13 0.001405326094366696 -0.0003061927322065578 9.69059385224195e-05 4 -0.00029704007524130596 0.0006969816398631375 9.43960659296328e-05 2 -0.0009902976276396198 0.0012842940876331885 5.3167467978478304e-05 23 0.0017691981643810444 -0.0002247139910810747 -0.001542965218769036 45 -0.0007561875824929614 -0.0015295371214741173 -0.00020993371764769977 54 0.0016331196475034165 -0.000538720448911056 0.00099276581297507 52 -0.0013419781495321477 0.0020152374654750717 -0.0014052134807552002 43 -0.00047822661873688085 0.0012155175572721175 -0.00041533218485778015 2188 -0.001424345784874383 0.0002741963498160997 -0.0014448447764347692 8 -0.0005978396843674274 -0.0009728548325924754 0.00029475017099171415 2197 0.0012698746401966915 0.0020439048571708734 0.00019266964597994816 6 -0.0019378728513811685 -0.0003703972013344237 -0.0012732780815200792 17 0.0013241866505142362 -0.002004146864281896 -0.0004434577920721315 15 -0.0010252599740240695 0.00027930844959991397 0.0003443291578769032 25 -0.00168561141553847 0.00042999204658819313 0.00123953049192288 761 -0.0007110607378889376 -0.0012233682398943655 -0.0019841949729559865 759 0.0017767936423685152 -0.001993799229475835 -0.0019251148436963215 770 0.002253751418559681 0.00046735544391544523 -0.00070706391906402 768 0.0018638014776715193 -0.0017435745385464205 0.0009404840385350136 20 2.3968631107446113e-05 0.00036239354145987176 0.001550435508037256 733 -4.277515564755745e-05 0.0019207651557481117 0.0013864846903744853 731 0.0017798991610885565 -0.0010350743779224936 -0.00086393976625697 22 0.0006355519159302065 -0.0004551812092817625 -0.0022209795910333825 742 -0.000508016006793381 0.0012248215696614214 0.0013677056663103742 740 0.0006618250563608732 -0.000417424242587907 0.00044870864331262423 765 -0.0007004441125015907 0.0021428262391362373 -0.0010602655486453832 772 -0.0018822619614339187 -0.0001578698763881291 0.0008073578774935898 763 0.0011402687346299277 0.001342291644149989 -0.0006565459486386695 774 -0.0015241852737960405 -3.352338238444641e-05 0.0016071331255386081 2926 -3.0492807272114518e-05 -0.0010263697753380525 -0.0016154176850934066 735 0.00015952848718533638 -0.0009901708498819793 -0.0013170640652917281 737 0.001097124516278757 -0.00036321608715618177 0.00026798440686640144 24 0.000215351000989073 -0.0005022673928908772 0.00035046781231154065 2917 -0.0010865261725598837 -0.0006549443875883492 0.0019168966585732493 26 -0.0005773135146824605 0.0019199405321446512 -0.0018475570515190606 2206 0.00035395369540733843 -1.2671879511930964e-05 -0.00037873420012990607 746 -0.0007537713244924243 -0.00017753042054695627 -0.0009076867048341613 744 -0.001890808694473597 0.0007910766822181968 0.00034153085486334075 94 -0.0015803397440848118 0.0013654647208494641 0.0008110401331356285 83 0.0007374538042884949 -5.361157445625325e-05 -0.0001626934965269721 85 -0.00047131257424368514 -0.0006636802036824453 -0.0014659554097714764 92 0.00037578601367101996 -0.0006564953506062367 -0.0008921390926266406 102 0.00047448055670477434 -0.0001471070556646857 -0.0002327270373832477 95 0.0005294793119210535 0.0016492136889883562 -0.0006732575509805636 93 -0.00036376571376184205 -0.00138600259411362 0.0010905144418454176 104 0.002050105608758564 0.0016171291491883487 0.0006157425205478456 56 0.0011176164978714818 -0.0007540867039236847 0.0014443881956892062 58 -0.0005249756527033133 -0.0002869749030998146 -0.0005248302032689596 67 -0.0005426105146435512 0.0004995690794854244 -0.00021116029831542093 65 -0.0013301681356655349 -0.0004580807230198733 -0.0019937498313993265 75 -0.000295967015187509 -0.00027144154425873344 -0.0010868308108449272 66 -0.0011848699921287236 0.0006272523996242502 -0.0011899314351630909 68 0.0005833828424915586 -0.00018864954153258173 0.0019307364772912401 77 -0.00038285952095762626 0.0004943496667332344 0.00032056518698191696 31 -0.0005422975317080534 -0.0003214238817663539 0.0005636966031672382 29 -0.0016962946130190011 0.0007091920706446908 -0.0002221899037624287 40 0.0014541383764643712 0.0010620100608653088 0.0006422281273183038 38 0.0008208995432454117 0.0011390298393176507 -0.0012358172478423224 2278 9.384560972651261e-05 0.0016846876909671824 -0.0021248697388130946 96 -0.0015472375983438668 0.00036388837178758724 -0.0018028062298584863 98 -9.005300222519668e-05 -0.002066026722667427 0.0006863176169436308 89 0.00040491532995658554 0.0013294508089835926 0.0008935051227625852 2269 -0.0026180984595632686 -0.00015053506078072326 0.00023996431931070186 87 0.0007348168331922371 0.0009715774497831421 -8.762342249251905e-05 108 0.0025904179482443375 -0.0013590969540995539 0.000587406997242697 106 -0.0007249530451020694 0.0003077844260999877 -0.0005097745117395417 97 -0.001603767884622031 0.0016906969498856335 -0.0007393892505348104 99 -0.0007417136132172219 0.0016272476993186768 0.0014987473952862798 2251 0.0006322827449039639 -0.00030988236480569437 -0.0005234340600778325 69 5.379991030551911e-06 0.0001149057901890804 0.0006226027239022193 62 -0.0007184878772585478 0.0009598550873781628 0.00015802249622417738 71 0.0004581495048707374 -0.0006984177556957705 0.0012249010545885184 2242 0.001039432943677035 -0.00037610765629428507 -0.0002872200274880777 60 -0.0008166283229908825 -0.0015984202970928134 0.002275852637279389 81 -0.001499362587375721 -0.0005375365212559034 -0.00035535834363456704 72 -0.0005924295745105923 0.0009576979482333247 -0.00012667847104485603 79 -0.0011988353176265061 0.0006472301844282991 9.766900284734171e-05 70 -0.0022293726440441816 -0.0019851121710553967 -0.0002866876405453122 35 -0.0014565188649986746 0.0020555937064002184 0.0002409166758860832 2224 0.00015469211821277778 0.0017833248879204375 -0.0010185844458111297 42 0.0008839357945129595 0.0004897353777156212 -0.002153628285908138 2215 0.0010907364395466939 0.0009158389665012933 -0.0005161705211835811 44 0.00032989146978543995 -1.8533799883450972e-05 -0.0021245143776936547 33 -7.443582323688716e-05 0.0008620538410779616 -0.00036272190802780387 769 0.0007778460620462418 0.00034893432300344774 0.001004855061026415 103 -0.0018427105159334735 0.0004451018338159122 -0.0020361812171354 814 0.0005740267880344787 -0.0020894362521153994 -0.0010387035795051162 812 0.000756439246322517 -0.0007839293369054667 -0.0009339683709976786 101 0.00026051683603834806 0.0014094479593070672 -0.001102519029368466 823 -0.0004876094459385698 0.0017917451304209817 0.0007714221770039494 813 0.0011034739310098126 0.0006025891063495073 -0.001057126007073968 815 -0.0014028057857581751 -0.0005682776469987315 -0.0019479787410440447 824 0.0008977320331320067 -0.00037012446051343023 -0.0011615903055340558 822 0.0005658189185548143 0.00029742467212653446 0.0003436792749303623 74 0.00043939201474435584 0.0013336647438305835 -0.0008016017048100097 796 -0.0018660911190483587 -0.001196159691030628 0.0009222896931003174 76 0.0025089029694632197 -0.00020875894748054852 0.0009305656230267031 794 8.121910899485285e-05 -0.0017192437278167082 0.0007579867037795595 785 -0.0018729822000005743 0.001120796951228623 0.0014672243535493342 787 0.00042571936689314116 -0.0010437317195904528 0.0008017055314905232 795 0.0025084098279865973 -0.0007419621180241426 -0.00096830859533597 786 -0.0017206144144126315 0.0018939516217555232 0.0006256884778274103 797 -0.0016106555740728755 0.0015732946633084245 -0.001301500396966087 788 0.00041330128345778115 0.0018147410096565268 0.0011254234256125313 47 -0.0016879789487392913 0.0010144838090299626 0.002144846615547391 758 -0.0011014191758626055 0.00020270945806470566 0.0012996168360441414 767 0.00032517929162467676 -0.0016288210026543918 -0.0001258011815516106 760 0.0010947731335163025 0.00047030001328760137 0.0006315147556451011 49 8.491160634469279e-05 0.0005932107707346417 -0.00032364791152000665 821 -0.0011931754382001497 -0.0010591080267516122 0.0013842208559871583 771 0.0011155890979517625 0.0009941559027226061 -0.0003514334447278157 762 0.0015102647805029959 -0.0012075674669165088 0.00017518770362765792 2953 0.00093879789379006 -0.00102761928852775 0.0023839344423388915 51 0.0019424718444387892 0.0014919123283392145 -0.0016403066612507102 2287 0.0005551554347378762 -0.00018693587535823487 -2.897061963033447e-05 105 0.00035920494293044814 0.002312168256756743 -0.0008597174891857614 818 0.0007584831886388811 -0.002386801517248451 0.0014647859504187178 107 5.408765533815947e-05 0.001690568498106224 0.0022134622483306133 2998 -0.0016849464147361498 -0.0015596137217910285 0.000980177001221036 3007 -0.000537568560038784 0.0005179082252624042 -0.00034406830801929605 825 0.0002153750339036831 0.0009865937899736523 -0.0005632892176376665 816 -0.00010547875181792215 0.0002536008294709404 0.0007659658661489714 827 0.0005014849882258781 -0.0023244740973206858 -0.0017857056407292753 817 -0.001500269683103359 -2.371951313071539e-05 -9.977802361480523e-05 828 -0.0012519910602932082 -0.0010539132549436106 0.0006248087029373766 819 0.00015997719695985668 -0.0004909417525161982 -0.001128383801221548 826 -0.0016978933640751028 -0.0009292090518365635 -2.0315686889682473e-05 80 -0.0012579129184218238 0.0006687593160255824 0.00010017930689458585 2260 0.00044960457930722105 -0.002635582909816323 -0.00033940297485170645 791 -0.0012647611460816206 -0.0024869667118671344 -0.001550735841604796 2971 -0.000513161857523863 0.0010654815892281416 -0.0009713224984183918 2980 0.001504945829419021 0.0023989657392524217 -0.000667752344486742 789 0.00039192595795980913 -0.0013583283153913123 -0.0025014780805395396 800 0.0001743422486472682 -0.0009899215148278678 -0.0009232160027867791 78 9.187948467486736e-05 -0.001031710767631765 -0.0006805521880841629 798 -3.396232953104157e-05 -0.0013858967441787362 -0.0020523370833112602 792 0.0004123413687959132 0.0008562802779220698 0.0009330707766731697 790 -0.0003512339762956711 0.0010414696949034628 0.001156425146766653 801 0.0003789374543850504 7.718078914991316e-05 -0.001478035966899126 799 -0.0006249573077453098 0.0006279634273894849 0.0002755551100739604 2233 0.0011069647047976827 -0.0012386628329942404 0.000870481022768897 773 -0.0013367543149330667 -0.0012262030111458513 0.0006553762864541198 2944 0.00046377500206318603 0.0019177581485750228 0.0018755661355338588 764 -0.0008847261537517615 -0.0004166616651644329 0.0005264928667475346 53 -0.0009186998088635989 0.0006658745486907082 -0.0015156644352918361 174 0.0008563349602831905 0.0008647896822428872 0.0005852629683682173 185 0.00027215613493713077 0.0009210557543748263 0.0006076820757781837 176 -0.0010446138344892498 -0.0008991551591138061 0.0013033346030562416 183 -0.0005327788662997207 -0.0005513197248547155 -0.00025164458093772726 151 0.00011133541894634523 -0.0006162035457041597 0.0003465348257846877 155 0.0017061646199544775 0.0008864366821882859 0.0004691166926325779 152 -0.0009463382657209222 -0.0004161090764489262 -0.0007525041513150937 156 -0.001119202614657791 0.0013153849034696645 0.0007913693718197537 142 -0.0002935655496757389 6.708904566980105e-05 -0.0002109959905549993 148 0.0017418246538382486 0.0005875540150309666 -0.0020089554311755733 143 0.0004250149835557955 -7.716031394352293e-05 0.0011412711646798276 147 -0.0002734746331324498 0.0007228690526644955 -0.0012182837804989358 110 -0.00043629910820233654 -0.002155680245062178 -0.0008888117983696809 121 -0.0008471818072600076 0.0018423920142696568 0.0008103646980178092 119 0.002013135097019566 0.0012106583255004275 0.0025547761171071425 112 -0.002159546611053096 0.0022200400295081858 0.00042731570835969197 122 0.0020908077635108584 -0.0008434273217999782 0.0015091159330888901 131 -0.0021570760869049892 -0.00018336445175494496 -0.002312242004530034 129 0.0010779356689162962 9.061732994855229e-05 -0.0004063219450170124 120 0.002210779183498985 -0.0009073877820020905 -0.0014913329237678352 166 -0.0010893375352152915 0.0011426729800240924 -0.0008404556752417411 175 0.0011944904737945777 -0.0017690591996424947 0.00040267357110312083 173 -0.0004321735604992436 -0.00014274085605958512 -0.0009258230033328397 189 0.001205931611723287 0.0011026151310829266 0.000993650886759902 180 0.0015457533752301004 0.0022420247239402624 -0.0004613685552004572 187 -0.0001786132562183549 -0.0005547590113710149 0.00014014777549969373 178 -0.00047499103634926823 9.090023593988231e-05 -9.497145480511892e-05 2340 0.00010764936447863979 -0.00024504873454947625 -0.0008660226217933087 153 -0.0007899875220591419 -0.0014349609283387443 -0.0013029246455015231 158 8.752787364084717e-05 -0.0011393419078381663 -0.0010839223853000004 154 0.000931378375815852 3.412600173840477e-05 8.19347706530354e-05 157 -0.0012646472034550534 -7.412369621902833e-05 7.438122746599406e-05 2335 0.0007684890146508303 -0.000795365828433015 -0.0003435468451183858 145 -0.0001419088737416856 -0.000868311315215116 0.00021168699987784588 150 -0.0023895457124437046 0.0014512430041403335 0.0015175926101791259 149 -6.243297288669554e-05 9.466333959820723e-05 -0.00038069731464878374 144 -0.000577358903237901 -9.705901165110546e-05 -0.001721594004873317 123 -0.0004216999916022701 0.0001610122869448818 -0.0007466663480529398 2305 0.0011183916629462166 -0.00018649036273976887 0.000833760156935601 114 0.00013973253844022432 0.00015741059942175743 -0.0006234497753347355 116 0.00018025400114778187 -0.00012422783297644604 5.423884878128296e-05 125 0.0004100007950223715 0.00010334438131984832 -0.0012651710150520363 2296 -1.4715278311590568e-05 0.000943633867276025 8.345894908360951e-05 135 0.0004395360479030649 0.0002566333796659515 0.0005481469544861993 133 -0.0018717724617966893 -0.0004997572949055186 0.002052912113343227 126 1.3556558615541048e-05 -0.0012155676421066906 -0.0017663180564802352 124 -0.0014766172188075376 -0.0007102189521431762 0.001524900261430174 2350 0.00015521560883430307 0.0003534607313246056 0.0004932513852889482 177 -0.00014931249382712543 0.0007636711329742389 0.0013882645506979089 2359 -0.0013251469713426753 0.0018518290055896693 -0.00030914802419913963 179 -0.001971170251454482 0.001093683134499612 0.0006277174496171587 168 -0.0009267620232920404 -0.0011787352813499596 0.0010308954969684445 184 -8.480538350606132e-05 0.0004231337163187565 0.0008998444264367374 903 0.00019123184745279635 0.001081013777246381 -0.0013015847107755729 894 0.00019482008291096017 -0.0005509858371028414 -0.0009145498988925628 896 0.0004111250116081955 0.0010727340899777265 0.0009462500305824789 905 -0.00017711829527931812 0.0013391270414625078 -0.0005136927001891671 880 -0.0008749813626627142 -0.0016251606373143743 0.0011373619826903487 884 0.00014159737506902297 -0.0009983651907155223 -0.0007240891840668636 885 -0.0005274819457054033 0.0015010472600299836 0.00017827649400453563 881 -0.0008913711308513779 0.001515524659143992 -0.00011857589780172272 159 0.001507401970746334 0.0022589967873304496 0.0013538293657022755 160 -0.00023644841741552814 0.0018551800012964375 0.0013877215255575653 872 0.0022297427850509564 0.00018677312475247755 0.0006552563687070195 871 0.0012022351616018732 0.0008073641023072051 0.0013822174279367778 867 -0.0028692555782959647 -0.001999664229211421 6.127232224133628e-05 866 -0.0003598412511181359 0.0018643381267269374 -0.00013549282490697917 850 -0.0020291316016659232 0.00029026214718526084 -0.0006718235099485274 839 -0.0010863359548674545 -0.0008172909461117994 -0.0004281540615213033 848 0.001499825607137555 0.0008062213871180425 -0.0019891194610119033 841 -0.0005542447387233883 -0.0008288550560665584 -0.0011104254078249162 130 0.0007449517541425386 -0.002620884455715595 -0.0012743028620448363 128 -0.000985790204824217 0.0015309513705125761 -0.000869935820639969 842 -0.0022963831332914442 -0.0013890556705898037 -0.0014314689400411035 849 -0.0010535351171474113 -0.0009272870814073428 0.00231115104052914 840 -0.002293980140707935 0.0009981667544142127 4.714331053268575e-06 851 -0.0014432452916682556 0.0008416421009801126 -0.00011589084640365496 904 -0.0002949052725948788 -0.001977099962041395 -0.0014275829824468463 902 -0.0003237448860011554 0.0002745621638106169 -0.001084853637964971 893 0.0013589150154007547 -0.0006299589526664023 -0.0010451394476837224 895 -0.00016334919589761077 -0.00048740974249067925 0.00010241105323487696 182 0.0018633656440113556 -0.0006431962832097017 -0.0003773054190092046 3088 0.0010953585913413232 -0.00032311513150202185 0.00124254778249611 900 0.00014032057172644785 -0.0012517321165354351 0.0006233884009466024 909 -0.001693398730711183 -0.0011087956729799353 0.0019281814252519246 907 0.0018805041979078957 0.0007534366957916759 0.0010568970184176576 898 0.00022935109606671606 -0.0018818016618303698 0.0008877896663090918 3064 -0.0010979877772948957 0.0007367437389965542 -0.000957553480738355 2345 0.001735800245373991 0.0020715682392619585 -6.126828599503246e-05 3069 -0.00045901645216138 -0.001651053928473242 -0.0012634472121288585 882 -0.001324534686301536 -0.0005308435082271082 -0.0015166991217543447 887 0.0005582454740624117 0.0007765294401103518 -0.0009428733160777114 883 0.0014835004756873966 -0.00012421461719910247 -0.00107041564899617 162 -0.0015652368848608049 0.0012048680862018551 0.000236726118774347 161 0.00010487622586572896 -0.0002679201603909447 -0.0003604627039863925 886 0.0011539942773581946 0.0013363864285968533 0.0016113270977999002 869 -0.001061946852532047 0.0004382837180582828 -0.0004690862590918986 874 -0.002073601186881671 0.0012405759352175853 -0.001048475768696313 873 -9.192327411258663e-05 0.0002597406996459597 -0.0017328314060600961 868 -0.001076061830257265 -0.0006312737091378315 0.000700914036401443 3025 -5.300288266491806e-05 0.0005058348215320093 -8.963772518068031e-06 2314 9.181878132468314e-05 0.0011237868303039249 0.0010715748164886764 132 -0.0011068945756002213 -8.985202591588626e-05 -0.0018797387431336871 3034 0.0009183610881344909 0.0012203805276147055 0.0015348430973400858 134 0.00023241576236557055 0.0003932558140412846 0.0007141641873884424 845 0.0011340459353843797 -0.0003036776991620668 0.0006309121563533907 843 -0.0013054292509527528 -0.001373938280492697 -0.0016273760200423105 854 0.0009169636797523222 -0.0024758596393013896 0.0015071408121082063 853 -0.0009200679562569511 -0.00018939570526191557 -0.0017356978469786465 846 -0.0009863607442023598 0.0010934664654654578 -0.0016637501695226412 855 0.0008324472315500847 0.0012099428435947595 0.00016723333563642894 844 -0.0005980464765704806 -0.0017752209635667044 -0.0006970307285476292 2368 -0.0014999026630101164 -0.0018281608938419507 0.0004067293232610414 188 0.00017517865513335795 0.0006795894601530001 -0.00032014792040588764 908 -0.0003024690830934971 -0.0022927449032326954 -0.001331474167556428 852 -0.0016201834738828152 -0.00022445847319356796 0.0005257698929249683 3079 -0.0009725088774171203 0.0006319722799884431 4.577612227246166e-05 906 -0.000781150074236447 -0.0009882604189235824 0.0006139098492282237 164 -0.0019100419716246888 0.0002425669918175164 -0.0002796240531017694 266 -0.0010626639769049562 0.0018468132948315872 -0.0008564306525759386 255 -0.0005895723415284102 -0.00028513369175465434 0.0026284128481370984 264 0.0006788350588300341 -0.0005194252282943248 -0.0009392782253340572 257 0.0001137923929152105 -0.0018741049689071114 0.0003617676700716616 232 -7.313579207490241e-06 0.0020898139937204113 -0.00022171572525491606 236 -0.001850727060266972 -0.0002537103899408645 -0.0009534822640260275 233 0.0005197543583524661 -0.0011485780265170198 0.0005255191530857135 237 -0.0005283968205616473 0.0005963926868521974 -0.0007009632319420385 223 -0.002527091142389852 0.0001385502632183836 0.0005720443102471887 224 -0.001454239622809993 0.0016533807378182564 0.001185884089877047 229 -0.00028058413523940687 0.0013343573117744537 -0.000785056275963201 228 0.0004164584054530032 0.0010755682243013326 0.0009819707013752935 200 -0.0013847218203552683 -0.0012859849252893339 -0.0012769690185228035 193 0.001865441546275239 -0.0009381066892546776 -0.00024717814707045805 202 -0.0018515890292768716 7.023052623638987e-05 -0.0017025030716501268 191 0.00137597901721731 -0.0003513416184127635 -0.00019740996071978146 201 0.0023833245028210574 0.0004318076056288229 0.0012826969265522553 212 -0.0002709952663198802 -8.376954302963973e-05 0.0010078667168562075 210 -0.0006536895682227861 -0.001665588700992707 0.0008278053950295766 203 0.00031197514047610463 0.0012489603217790601 -0.0022948109214301314 170 -0.000759909025969814 0.0013627214710774918 0.0009555375079251958 261 0.00045417477950187267 -0.0009835004016562295 -0.0012729541266931195 259 -0.0013291229788688986 -0.0015542911338425715 -0.0024605434217377965 270 -0.00023657132417923303 0.0017885771814504202 -0.0009022469414924091 268 0.00046975417621650115 -0.0007519484929770911 0.00017141591641870835 2421 -0.0003323080245303588 -0.000393377128010403 0.0006897592071441689 2416 -0.0003356144376891278 0.0008738846111368301 -0.0019238604427309505 235 -8.425698286466325e-05 -0.0011243999260336314 0.0014735072079112594 234 0.000831469734464465 0.00026595301360740446 0.000232496946049174 238 -0.00039789405649896456 -0.0012648270219562632 0.0004998045323590587 239 9.700082192300608e-05 -0.001778699016733959 0.001128824405115862 231 0.0011379446037912563 0.0020622869771142454 0.001379357079347836 230 0.0011670223931234997 0.0016189620510276364 -0.0012118146907751021 226 0.0016320029488730826 -0.0012072458901674888 -0.00018628535767328003 225 -0.0024906564858185884 0.0016806164099505204 0.00025078426516131 2386 0.0009873669118074988 0.00010527745783728618 -0.00019886876785482686 2377 -0.00045126133936996323 0.0018374813211287637 -0.00016925868687419797 197 0.0011033744811966464 0.0007741488193769654 -0.0007759083473386039 204 0.0021328639268701818 0.0015214177810913205 -9.543125482517267e-05 195 -0.0008768603652624244 -0.001522846775422908 -0.0008258959412055399 206 -0.001634373418215223 -1.7008953206332656e-05 0.0006441612418489642 207 0.0011321607664325395 0.00090516767574787 0.0008224816671511849 205 5.433969369618408e-05 0.0003834579933296295 -0.0005469015870900725 216 0.0001813881991958002 0.0006206345055329804 -0.0017392555204707363 214 0.0008840822132365141 -0.001996995059752978 -0.00026146592255543114 984 -0.0010353183424401781 0.0005224926526522949 -0.0009479833023138551 977 -0.0014526205717293396 0.0005877618675588457 -0.00043416300167530746 975 -0.0021077318794792185 0.0012751084976172847 -0.0015658687908465278 986 2.9363081469153604e-05 -0.0003004218509163384 -0.0009060126978926202 240 0.002523384494355879 -0.0014913685112530588 -4.133543592765485e-05 965 -0.0012662765525336005 0.0002816804201626143 0.0011874682669265838 961 -0.0013647353646104817 -0.0009157749028914791 -0.0009412170826041096 966 0.0005404384303504395 0.0020306409935339576 -0.001918158142636943 241 0.0012379159010400043 0.00011750271141835501 -0.000633888150554814 962 0.0008870563771995559 0.00019340183139172733 -0.0007086320621283804 952 -0.001609006216440564 0.0002680344382773569 0.00040676756388998044 953 -0.0017595307749454713 0.0006147633367443288 0.0007154480653511549 948 0.0017543648229329707 0.001926125296688769 -0.00029895989782565324 947 0.0021848743056442953 0.00042028659671678977 -0.0014640250891253229 920 -0.0003320796626520386 -0.001376445359181589 0.0009343686870332461 929 0.002610228912195518 0.00011603052587523185 0.0005430671739555527 931 -0.0012668581993738836 0.0019685188355629425 3.069645092405892e-05 209 0.0011830869654726418 0.0001063722404616549 -0.002158376977952979 922 -0.0006988127065389012 0.00031560437838811396 -0.0009386332759059766 211 0.0008227293726742597 -0.001485782408943339 -0.0004337729210069142 930 0.0005518565896698961 -0.0019291455803938375 -0.0010917447739373254 932 -0.0022127563600395986 -0.0010425704533983224 -2.8115012637336487e-05 921 0.0003717241532017881 -0.0014474034006110147 0.00012274409457497263 923 -0.0014409450756763856 0.0008178399612408759 -0.0006896566787604935 899 0.00015958530022319717 0.0001342538556571895 0.0015157765595170836 897 -0.0013858693387790522 -0.0005934031123416505 0.00201915902111806 186 -0.001580073040313196 -0.00020921141670663312 -0.0014538263289559897 925 0.0008635130858852616 -0.0005923177812521073 -0.00020450512223762346 935 -0.0009624864646227405 -0.0024132452833087368 -0.0006696511327289115 990 0.0004891939829626706 0.0011700150753423937 -0.0002991917175870207 988 -0.00045077810994638466 -0.0004218986022690549 -0.0012650942586466816 979 0.0007279955277316617 -0.00010658466636198844 -0.0012051834189776857 981 0.0015805833542532584 0.0020464992889754926 -0.00047597149280582864 3150 0.00013929443982123877 -0.0015432359406066356 0.0014935787254279891 968 -0.0009459121068167449 0.0005916590725640436 0.0022278124613905543 964 -0.0017383941985082735 -0.0003350047463198983 0.0006612502513863893 242 -0.0001805151771314584 -0.0005657286791554724 0.0009800482298975982 967 0.00014691024316658245 0.0001054231604142382 -0.00023307161401084917 243 0.0009989949464824237 -0.0003747351018797574 -0.0005777651782498383 2426 -0.00013458221808900807 -0.00024130730087863197 -0.0006633698906936172 963 -0.00018693214426129465 0.0017722829490337568 -0.0009227521801107539 3145 0.0010397187627224527 -0.00043772469571933025 0.0023483366801613915 949 0.0019627947725139954 0.0017328203686973903 0.0014820040719467694 954 -0.0013411419439427164 -0.0014659264418179561 0.0004117616702770581 950 -0.0004554193919702038 -0.0007182217578940711 -0.0010607948172795718 955 0.0018045412541039764 -0.0003663284088315452 -0.0011853899969080871 926 0.0005929364060404119 0.00023087089904407594 0.000715028156719034 3115 -0.00203126242537017 -0.00022200849038751715 -0.0016704818992650447 2395 -0.0006674787469381607 2.3596531938186935e-05 0.0005473387061628464 924 3.7804790220324295e-05 -0.0005384473253393094 -0.0015908056715177644 3106 0.001043511341153036 -0.0005195998769283862 0.0006950719606465643 215 0.0016356516291952427 0.0010958241703841328 -0.0015883020520737654 213 4.009334276192263e-05 0.002411780834154268 -0.00029655552562135156 933 0.0006933474549140326 -0.0005809137079367429 0.0007557968265622284 936 0.001370038433353699 -0.0012039698226692635 0.0005798756792442798 927 -6.103890355702035e-05 0.001194426016218547 0.000703621984179644 934 -0.001103718972976438 -0.001071021630691261 -0.0005298641250607661 299 -0.0007911968179607188 0.0002178471697523584 0.00014629318286559488 310 -0.0011226256274937403 0.0013919507546156038 -0.0021517763053774492 308 0.0005567060351371455 -0.0007699685849282285 -0.0020918748949193835 301 -0.001599563031043297 -0.0008252339513517635 0.0020031073247757723 318 -0.001675596565662243 -0.0010385679962339486 0.0010792136549438616 309 0.000623011205643191 0.0007573202337335893 -0.0013864666549802138 311 0.0005551411444397378 -0.0004926649699142977 0.00026472780734255216 320 0.0014748119762067274 0.0015144989085477392 8.531828762590316e-05 281 -0.0004532370081969544 -0.0019859964494066914 -8.218800425008289e-05 272 -0.001269004484442629 0.0006669230973703669 0.00041246585841313364 274 0.001217128069323848 0.00027964827790394006 -0.0015255497199208265 283 -0.000693726949194893 0.0010575270597865585 0.0008308460618277273 291 0.0003892943931098098 0.0010693533646654828 -0.0002489996190638277 293 -0.0008366943537931246 0.0009217689549712691 0.0006336190081496112 282 9.245208928257247e-06 0.0007505312332987725 0.0014706097590421368 284 0.0007739640856244263 -0.0011760402975794255 -0.0012793805991973526 245 -0.0013955708671911178 0.0022426867880554415 -0.0009311328439193325 254 4.3129375549716365e-05 -0.0008934432443089199 0.0017496840447842857 256 -0.0019520029574284985 0.0007421270145423424 0.0024873955148341635 247 -0.00111502068503293 -0.001860302590812812 -0.001360983604805379 2485 -0.001596245809625941 0.0011516283360380668 -0.0001873464499770577 305 -0.001252344583727956 0.00042791980768897204 0.0017817969907883784 314 -0.0010665185188211985 0.001311008873002274 0.0015055446116175007 303 0.0015128762204341323 0.0016979979862796163 0.00110719199816597 2494 -0.0002239233996318452 -0.0007133592005765596 -0.0002462469183599717 312 0.00018865649974245737 0.000210768424729962 -0.000331219574416371 315 0.0019937692475748645 -0.0012212891689124957 -0.002249967437534439 324 -0.0013856127159702029 -0.0003312269987902042 0.0002326298843544268 322 0.0016547282533196342 -3.126916759168451e-05 0.0007330181364604924 313 0.00018689783309365916 -0.00026264637605958306 0.0005167154036987905 276 2.9103447782766103e-05 0.0008417454402502287 0.00011544636591027686 285 0.002344420196159975 0.0007454026975412995 -0.0003706163650732219 2458 0.0001622738823267119 0.00014704803125054067 -0.000409326787555603 2467 -0.0006364618571207859 0.0011633483746056792 0.0003925672795967504 287 -0.0006084545228638157 0.0016726586459003016 -0.00227506975404182 278 0.00041945134376496836 -0.0016955157077250434 -0.0016303264239405047 297 0.0005442460306526219 -0.0007020657118596799 -0.002454336662568665 295 -9.735622089248588e-05 -0.0004821008911491641 0.0004119108837986425 286 0.00012564768710129947 -0.00218328889348871 -0.0012358502156097628 288 -0.002210199640549834 0.0006232904025622358 0.0024297849833527273 2431 0.0012179487354877748 -0.0017813878658745968 0.0012728681305838741 2440 -0.002282182445233107 -0.0017508770719606485 -0.002185046323065033 251 0.0007617123460859647 0.00021362841906844184 0.00015202610021025582 260 0.00038566889573533273 -0.002008850868366617 0.00013813282344137 249 -9.250053950979234e-05 0.00028813219259514705 -0.0014264840954574954 258 0.0009502697665000476 -0.002217814720510736 -0.002515765691639852 1039 -6.294985144582235e-05 -0.0016152509772186631 -0.0012437548403128646 1028 -5.3180386346527255e-05 0.00016597292229543763 -0.00017112165187017437 319 -2.438262939497479e-05 -9.773270280019337e-05 -0.000506616697851128 1030 -0.0007182962040744494 -0.0003910144264670849 0.00021324287118148382 317 -0.002202980391372264 -0.000298577133336142 0.00028692405730447294 1037 0.00014587339803101898 -0.0006095911425696222 0.0009703314462669411 1029 -0.0010445500875337775 0.0010021758633200952 -0.0018704449764266017 1031 -0.000698496306698236 0.0013958746723595457 1.500957996595836e-05 1040 0.0009022700216253102 0.00013233508299016587 0.0001310575873085646 1038 0.000289306230955977 -0.00028513157078203675 0.0013034976715361251 1012 -0.0018144353353075175 -0.00030604174836898696 -0.0007029362712551418 292 -0.00012757944724020196 0.001601964412072159 0.0010643698354070496 290 -0.00102117486149279 0.0008681542817149049 -0.002262305932494544 1003 -0.0007572344005695265 -0.0001637377381611938 -0.00179141216626733 1001 0.0015436361081996028 -0.00026634297980627553 0.0028487825400006104 1010 -1.826100630489963e-06 0.0003428579263760772 -0.001135473419368247 1004 -0.00044731997866003436 0.0025120298032511377 -0.0013440846295275609 1002 0.0023875426957406126 -0.0004511206710484806 0.0005004317254638172 1011 -0.0020071474929432053 -0.00100919194444847 0.0002294836147884678 1013 0.0013699280489174843 0.001615845681522754 0.0002989040166759822 983 -0.0008030675896911867 0.0013260368786380755 -0.0011128267175091505 985 0.000743185029042807 -0.0011726507678176035 0.002626676289527226 974 0.0017738728051978968 0.0019148079807779004 -0.0017921016454346516 976 0.0010176528540469416 -0.0015707545547524757 0.0009117506436375481 265 0.00014384689606020237 -0.0011134627230104629 0.0008110424295458352 263 0.0011031823323192278 0.001666215565583632 0.0011671873071232852 1043 -0.0002072347882975834 -0.0019417450098213284 -0.000912323376551755 1041 0.0012354124510924201 0.00024077702483332503 -0.0014536350392223834 2503 -0.00023524243477446045 -0.00024707723782252183 0.0007230305590853554 323 0.00015127619730524147 -0.0008480438862476907 -0.001848805310755029 3223 -0.0010995268890253954 -0.0018291842113570627 -0.00043580283989461577 321 -0.0011696592586747695 0.0015709593008359673 0.0005989887631619918 1032 -0.0018205537430897494 -0.0004796605819683225 -0.0004266076625811546 3214 0.0006209627853995402 -0.0015260608299054064 -0.0006864772232784429 1034 0.0016243517207613933 -0.0016580061452379474 -0.001525209752263927 1035 0.0014184609463940906 -0.0006505360031004736 0.0003174420108697046 1033 0.00044585997825549967 9.301688560568473e-05 0.00216118827306441 1044 0.0009666831653543581 -0.0005292441291260416 0.00034788766051583307 1042 0.002403315559038089 -0.001680110810417192 0.0017554466865242343 294 0.0002518327248848735 0.001227507007108706 -0.0008130830133451245 3187 0.0010987077807895012 -0.00012185381026697667 -0.00019693869782679902 2476 -0.0012183730438314589 -0.0005871682931799143 9.113537775303675e-05 1005 -0.000709546250734465 -0.0011085945909170632 0.0011384141002958742 3196 -1.1453346028913666e-05 0.001774792868958733 0.0004477820434865339 1014 -0.0014455683936216005 0.001353488929021192 -0.0007828623731859568 1007 -0.0006887870720322744 0.0007945707990257309 0.0011912014950648453 296 -0.0008941684496969162 -0.001357114655100963 0.0013069216987153798 1016 -0.001682305565791516 0.0012559084945655513 -0.000769637825232438 1008 0.0015865735398510276 0.0007819956310661179 0.0025535174437807838 1006 -0.0007598327317903536 0.0010718583382021305 0.00030416800228062833 1017 -0.00026611462364532876 -0.0011587986022731636 -0.0013466507710541004 1015 0.0005077951434966834 -0.0001352939570931425 -7.390239744807818e-05 267 0.002227695817098087 0.00013270068633481442 -0.0013315177526511267 978 -0.00045680868234749996 -0.001241360968144649 -8.106332682779327e-05 987 -0.000960592518633824 -0.001148991051970331 0.00021964341266752499 3160 -0.001853206320925704 -0.0020908883082102533 1.931467310212426e-05 269 -0.0006845206049853349 -0.00041774132788005396 0.0007107396020108632 989 0.0015239819094959293 -0.0008645341926569467 0.0025813455885461347 2449 0.0019168660607075236 0.00024736742237533573 0.00033414012570381793 980 0.0015489522872907846 -0.0013458371921168202 0.0012468709801952322 3169 0.0026655932548202152 0.001824779505291945 -0.000601335137742718 392 0.0007173085890969152 -0.002093806775416392 -0.00037535646257628097 399 -0.0006346479058781894 -0.002294414463501573 -0.0005296002109975422 401 0.00120637106941417 0.002341879386004262 -0.0022326237046391578 390 0.0013797757737791677 0.002441477823598965 -0.0006293010166781573 372 0.00012004871508157662 0.0009849821252952025 0.00020771679772307742 371 -4.128430017872448e-05 -0.000569621848736507 -0.00047584073320716116 367 1.783678265005709e-05 -0.0003466600205930188 0.001820129285698914 368 -0.001108426667435517 0.0012275841478284941 8.825415041268454e-06 364 -0.0003168740040909426 -5.31925622306934e-05 0.0009334977261179605 359 0.00029315076993142184 -0.0007027124963112003 -0.0019012323179650856 363 0.002750452727346569 0.001832258692533434 0.002081242657717045 358 0.001328588293635761 4.994387210783646e-05 -0.0002444393235518772 337 -0.0002966663786162221 0.00018086650060927497 -0.0013037343249448692 328 0.00024207396069665676 -0.0019594604073457115 -0.0008586189631680171 335 0.0003958058552158278 -0.0019733315325603834 -0.0002765209926873088 326 0.00013057231053093064 5.3245256674132845e-05 0.0006094918825664286 338 -0.0016296740051554588 -0.0012490087055568757 -6.824646181875262e-05 336 -0.0005469373808352232 0.0004794189543671241 0.00031756166822383434 345 4.66406144227769e-05 0.00018757835435494587 -0.0016278374395725013 347 -0.0007003024099890072 0.0010808375260766665 -0.0009480787795739889 403 0.0011942186945336742 0.001402524483506243 -0.0013855966370053146 396 -0.001366292475433492 0.0016329302619067692 0.0001970311041194705 405 0.0004499541544252196 0.0004597721245210028 -7.428028951735857e-05 394 -0.0001140349297706158 0.0015076177158433687 -0.002472038962957281 2556 4.042687364791105e-05 7.686355083615201e-05 0.0008443703395385946 370 -0.002324716607720851 -0.0011833397607733528 -0.00038294876771184216 369 0.0002545087274705573 0.0009141588844576653 -0.00013967169625721812 2551 0.0010650436848474787 -7.9277782406054e-05 0.001504061539747642 373 2.0392954086489166e-05 -0.0004944079975412052 -0.00019741654392995195 374 -0.002333763024539035 -0.0006190801751722836 -0.0005965312022113184 360 -0.0017665637633906004 0.00024699225384866564 0.0019426352678198187 361 0.002256473190095061 0.00022324359679860503 0.0019535633759343723 366 -0.0006582605787432153 0.00037890512667114115 0.0014677582121527212 365 -0.00024855272080048546 -0.0005963210026068218 -0.0020575232163405756 2521 -0.0005190016096401143 -0.0006618717813875328 0.001273467672482269 341 -0.00036810911547265675 0.00015655036788634946 0.00018301273954748377 339 0.0001312703063230552 -0.0005364060863734749 -0.0007097485919195063 330 0.0004564169064801046 -0.0007214803962311725 -0.00036605336403189195 332 -0.00183102019645627 -0.00031016299065746687 0.00021389253310056307 2512 -0.001947105141581687 0.0010478874095495385 -0.00014998026579209154 340 0.0006790895764068239 -0.0016422930837226195 0.0011421293938349195 349 0.00021188819926311504 0.00015320564357278416 0.00017650950210405976 342 0.0012069314499575717 0.0018762478321884854 0.0017963036231431482 351 0.0015853302348435533 -0.0003380036554319686 -0.00013801914830600644 1112 0.0008765940927457404 0.0009824888849775733 -0.00025482458244029463 1121 -0.0004764804120626397 0.0008331084080633845 -0.0005886630955020823 1110 -0.0011358568237004455 -0.00046480292640680224 -0.00042918137561711884 1119 0.0011831178309454678 0.0019647642789748926 -0.0010347283498780401 1096 -0.0018428302203172165 -0.00033191255230755545 -0.0006344529533380354 376 0.0018169214687126997 -0.0004215656363940547 -0.00019464689672421824 1100 -0.001217042687504201 0.0008876101789479783 0.0020635686762179657 1097 -0.000901835334800689 0.0021546682583267994 -0.0019531157273345802 375 0.002447016206010452 0.0015291324097680813 -0.0013232522432603312 1101 0.0001722747028672022 0.0021651787087431564 0.0019940390745487586 1083 0.0006913609282606179 -0.00016615977804642994 -0.0007245166749890937 1088 0.00038353126885023146 -0.00010971067815191294 -0.00032810855738073783 1082 -0.001357647352854074 -0.0005506006165094599 0.0006774031913603885 1087 0.0017224405281345426 0.0006201782312875233 0.0014798929436965922 1057 0.00027985911802999716 -3.909134677338713e-05 0.0004367336848217629 1066 3.097796034726857e-05 -0.000562228551146677 -0.001759233235000126 346 0.0001237949219051568 0.0004922893862538708 -0.0004051838418827876 1064 -0.002147832793415427 0.001833224026938389 -0.0006537759907648169 1055 -0.0008263344094619682 0.000306719298580686 0.0005095597299328169 344 0.0004855772099010221 0.001436541775532093 -0.0007493883878278823 1058 -0.0008600973026583211 7.716618692972792e-05 -0.0019066266461889563 1065 0.0003747569571252115 -0.0006992361749464013 -0.0009504639419435004 1067 -0.0008548703314663886 0.0008967459006890023 0.0008250621438315956 1056 -0.0022488283030740303 0.0009201482646313688 0.002706215908627978 1071 -0.0013499383674463105 -0.000667033899613118 0.0004328011381110907 1116 -0.0015831537960496315 -0.00042713746652480795 0.0005337332721596691 1114 -0.001758536667249503 -4.531803510843908e-05 -0.0005647225161925943 1123 0.0007973060060464305 0.000830584347182914 -0.001143449435825669 1125 -0.0008319831538414729 -0.0014089129643366854 0.001348607242819661 1098 0.0011579642170800493 0.0016119092682196478 0.0011959589997483783 2561 0.0009440291589004673 -0.0020156005807296855 0.000605503129909681 377 0.0004033235519332477 -0.001045660370750608 0.001554579247576888 1102 -0.000575570508807887 0.001142046637107823 0.0012070994648817864 378 -0.00028445425797535805 0.00029179171962573445 0.001493766983447012 1099 -3.227181201065268e-05 -0.001070932265453093 0.00028400805825043956 3280 0.0013372625861793543 -0.0008646238699539695 -0.0014017547639799818 3285 -0.0026351758696016455 0.0009001768644293707 0.0012097097409504982 1103 0.00010745640726494044 0.0005780859390877287 0.0014469302829684583 1084 -4.825502210341836e-05 -0.0012574965168745467 -0.00030849504045873293 1085 0.00039953052421692415 0.0004617943887660885 0.0006227335945902048 1089 -0.0007215744768935863 7.060894752407076e-05 -0.0006446765056887108 1090 0.0021046449395140266 0.0007477837576438378 -0.0001679839306592346 2530 -0.00037977378704744135 0.002270129652265256 -0.0014409822072448271 348 1.3224724476300397e-05 -0.0009624423240992917 0.0011805756594302271 3241 -0.0006891332004591874 0.0004243381374398408 -0.0002596077667872379 350 -0.0006771375013739262 0.0012270821578278495 0.0012752288243358082 1068 -0.0019855768150568824 -0.0012906287464451794 -0.0012304557118521392 1059 0.0002801279607456226 0.0018611772470587943 -0.0021657037564852197 3250 0.00027334895489049347 -0.0014897720824881874 0.0006049367363912307 1061 0.0008557597008491897 0.00019058190263448592 9.086027521414608e-05 1070 -0.00046958147224586064 0.0018840131832229797 -0.0001364019632080853 1060 -0.0017662153908300391 6.951453925353843e-06 0.0014321759819739639 1069 -0.000948305141696636 9.134537048688125e-05 -0.001078322831125199 1062 -0.00034487428337533275 0.001858250375825776 -0.001444082783928602 449 -0.0008463437667548756 -0.00019790993724492405 -1.9305383946238578e-05 453 -0.0007993679369837383 -0.0018345785010598008 0.0019596614680724386 452 0.0010105878698314227 0.0005972336166015322 -0.0011340307755977226 448 0.0008837760019458959 0.001482628975241497 -0.0018061704002492718 445 1.0759775383866973e-05 -0.000360961176089782 0.0010922694885303048 439 0.001019367269754851 0.0001890904800257515 0.001374182155156309 440 -0.0014604126357313316 0.0004549500147889309 -0.0008882804588627091 444 -0.0015158912339939949 8.812339614409155e-05 -0.0003381943187767795 416 0.0007369460635655912 -0.00041042876388402625 -0.001896160654525782 407 0.0004495360932526321 1.6919946257978446e-05 -0.0003473712103773431 409 0.0002370365631102619 -7.218613095746028e-05 -7.809785008974464e-05 418 -0.0019218454764114569 -0.0004039985302502411 0.0019534857220273407 417 0.0022094955733483633 -0.0005074274845306428 0.0012489731134625408 428 3.779002373462321e-05 0.0008857499261319704 0.0004579890296609909 419 -0.0006436307975337815 -0.0004699252884573982 0.0006278750872605494 426 -0.000958558490985152 -0.0016320411834714037 0.00012361252089849962 380 0.0017171278671324632 -0.0001965624742418222 -0.0018483009500852828 382 -0.0011172101326519458 0.0008312340937639666 -1.728217433372744e-05 389 4.990960456061435e-05 0.0011653135119106457 -0.0014966687224452812 391 -0.000845558507173327 0.0007522532482441007 0.0005525442240048267 2637 0.0021674075687937366 0.00011368843025135172 -0.0021602162510403105 455 0.0017065392316002784 0.0022289370619418144 9.726022727585477e-05 450 0.0025043020530065496 -0.000398825952704488 0.0016047819998147217 454 -0.0006727858859860579 -5.3681411037436485e-05 0.00029053142065486675 451 -0.0003515181679093777 0.001070553386245927 -0.0009059071345932101 2632 -0.0007931310268563644 0.001049304442394334 0.00016022505173530783 447 0.0004862560555236556 -0.0006861000686292956 0.0008445029640117589 442 -0.0007611541661041982 0.001674135878480039 -4.253533775850149e-05 441 -4.170652421667167e-05 0.00019145676246105174 -0.0019592744603324965 446 -4.389548755866755e-05 -0.0009224396443006029 0.00028359361250787033 2602 0.0006179126351347277 -1.7659891249773745e-05 1.5946054645642367e-05 2593 0.0008784804574703304 -0.0005112622887326582 0.0004185778194386595 420 0.0003127741655996547 -0.0009481734285315014 0.0014888231657273685 422 -0.0008838648560949419 -0.0017847492861160963 0.0005873776011996965 413 0.0007895415615106879 -0.001175807207748215 -0.0022219418980558552 411 -0.0006094040348215651 -0.00016263688012502176 -0.0007685368153113657 432 -0.0015725190394440763 -0.0018441536343896453 -0.00152015097572652 430 0.0020943748289267263 0.00017378271440916413 0.0003817072799933163 423 5.645998047738073e-05 -0.0026445747364000592 0.0008086105901377327 421 -0.0007873039508816165 -0.0020123517685015258 -0.0012155849831283825 2566 -0.001074758156322604 -0.0022574658480918573 -0.0019236122489476063 386 -0.0010712691455252651 0.0015301452498344766 0.0009221451908607853 393 0.002328524250492574 0.0011309440169921274 -0.0003821264453715104 2575 -0.0006070736054461514 -0.001270862679772315 0.00032660038639556097 395 -0.0009646552289011802 2.7425004847784692e-05 0.0004342577407446637 384 -0.0012001810260397062 -0.0006890085751977656 0.0010054832804569495 1181 -0.0012590200467152088 -0.0001574945859717184 0.00032759315007010624 1182 -0.000927779850629756 0.00043762719599124244 0.001807191212128661 456 -0.00029798992802602866 0.0003124083132017405 0.0007811981428827699 1177 -0.0008713834600974297 -0.00040691275671160543 -0.0022357259028129763 457 0.0010893132175655114 -0.0006419329637095527 -0.0006959401477554401 1178 -0.0007741842223767388 0.0007235446499954321 -0.001154172968586649 1169 0.0003998358683239946 -0.000807011505722373 0.000366339633224253 1164 -0.0007326111280423642 -0.001574387214073584 0.00029495444648375 1168 -0.001976620832245751 0.0008997567111743792 0.0018241122103063315 1163 0.0020560794826706137 0.001365427370276052 0.0012298691310138016 1138 0.00023093032945399128 -0.0011583099972666273 -0.0016779776508963704 427 0.0011100715030333288 -5.03499525682878e-05 0.0009406071345623644 1145 0.0010997274071971501 -0.00015813998766208456 -0.00017430763621601418 1136 0.00039181553408987324 -0.002057134088097867 -0.00025695798184765265 425 -0.000649409677959046 0.00146451525933294 0.0005385116335310668 1147 0.0004354263953893322 0.001045272319964128 -0.0028174048850849597 1146 0.0009883635922064485 -0.0005143047681496885 -0.0023775350468767235 1139 0.0015408124699372492 0.0006172728966848112 0.0006701626431363109 1137 -0.000531431443316482 0.00010110590849581535 -0.0003900495277812848 1148 -0.0017267529680355144 0.0014217528956859487 -0.0008383447343051872 1109 0.0012012573184704348 0.0019351644952057077 0.0026939434904690177 1111 0.002270030691618188 -0.0005740980542093838 1.942399519865544e-05 398 -0.0008091911583437072 -0.0007622092110401968 0.0005421230649511154 400 0.0006266929181163396 -0.0004738662202276562 0.00015479619273024524 1120 -0.00036123363543920763 0.001525381320492679 -0.00039854237179746477 1118 0.0003582168968241043 0.0020011878736287798 0.0014624222360557395 2642 0.00220717048528963 0.0014619174758834608 -0.0018543431866136042 458 0.00019551924615396994 0.002234027280954506 -0.0019995846790267628 1180 0.0016724884742319733 -0.0018983065254810376 -0.0005936230189982736 459 0.001697872026572289 0.0007225429547009649 0.0002015004650943352 1179 -1.1949532839334101e-05 0.0011154763374694708 0.0011407904609427525 3366 -0.0006337133343186023 0.002381311192691171 -0.0008828986221619682 1183 0.0008474869579980688 0.0013845659648928728 -0.0013817816762901973 1184 -0.00020089038802105985 -0.0018617770799814282 -0.002111968656638378 3361 -0.0009266723809459851 0.0006381153566087986 0.000350710722424506 1165 -0.0017717088691714684 0.00023835494240885514 -0.000539251871568173 1171 0.002332524656696856 0.0010157624378404639 -0.000514685505858935 1170 -0.0016399522902838947 0.0016162719184178898 0.000528435707991967 1166 -0.0007146461932078818 0.0013412651570360277 -0.001521908332986351 2611 0.0013475476624571678 -0.002078832890368088 0.0011691237510190473 429 0.0005098803843786102 -0.001040518520458474 0.002065549312075763 3331 0.0001884939541734569 -0.0009899066956121868 0.0007596043492720411 1142 -0.0006281451722768133 0.0007727421307107197 -0.0004750932535790962 431 -0.000102482348777078 -0.000765840615523355 0.000415231283540933 1140 0.00016347622012995015 -0.001176944368011385 0.00034085960485091306 3322 0.0017525401643334753 0.00043076177458832094 -0.0019651448353227227 1149 -0.001037400988016177 -0.0008437984965527724 -0.0010468986798225755 1151 0.0005685891945933081 0.0015998489761865234 0.0006383118028747345 1141 0.0005554453538603326 -0.002141282175575289 0.00011824673674127044 1143 -0.0008243101546725267 0.0008045546670907913 -0.00035164632074878317 1150 -0.0005267773564931722 0.0014776527173987813 -0.0014002075637689869 1152 -0.0015070606190317154 0.0012961815875295723 0.0008989649735619389 2584 0.0005374009673813421 0.0005184834123531795 -0.0007478611338465888 1115 0.0009808705913896616 -0.000982777895842385 3.119429351038433e-05 3295 0.0001302302023164911 -0.0002473613140859046 -0.0016511065110565268 402 -0.0003872450653152518 0.0007663991885237299 0.000816729801585156 1122 -0.00021575414720788376 0.00026204130333056116 -0.0014445906406234843 1124 0.001210085421903476 -0.0013483749962181482 0.0002825714342533492 1113 0.0006795177427909154 0.0002627334058934573 0.00015095840077166604 3304 -0.00043103554731256503 -0.0016921793407271887 0.0007557005072131974 404 -0.0001160186805261186 0.0018255409490403134 0.0019784265579004283 527 0.0004685788853777633 0.000403338069235338 -0.0007620118298765851 534 0.0013664209891567146 0.0008862437784014478 -0.0006216315792642116 536 0.002422101158881156 -0.0024327093694045533 0.0015288704243855019 525 -0.0009109277271327071 -0.00024086211006469488 0.0018104341242738506 488 0.0016442829940453386 0.00016130642979242707 -0.000374098069018218 490 0.0006586195544552591 0.0005084939780476818 0.0017370744286452518 499 -0.000621155049407122 -0.0006588279891371066 -9.618354039107359e-05 497 -0.0007622783373548193 0.001455568796079599 0.001068740800819614 509 0.001723677305564664 0.0008760939253639184 0.001065661865702717 500 0.0003144749834771268 0.00013275736980341278 -0.0004762564846848763 498 6.727670620820412e-05 0.0007509286265254143 -0.00011146984704719313 507 -0.0013409061457052935 0.0005882529974982585 -8.099255154028198e-05 463 0.0008192181141784122 -0.0010236841215892287 -0.0009464914618018893 461 0.0004367005364275047 -0.0020530629023455295 0.0009590899851275483 472 0.001761919186806348 -0.0015933514079971777 -0.0017799554997927304 470 -0.000637028679254293 0.00046961716797429016 0.0021501587998419202 473 -0.0005122223356722421 -0.0019995667315967527 0.0009089979320401457 482 -0.0021294737737208003 0.0012923399119054283 0.0007279450937329789 471 0.0009037415521529232 7.371055971789621e-05 0.0011828600559782 480 -0.0006560440776070934 -0.0001911257386253719 0.00250100820194261 529 0.002359391918121352 0.0014046801677430898 0.0005061985617812015 531 0.001456737518683832 0.00021776240932397297 0.0001288752874865492 540 -0.001836499124477588 -0.00121499541391553 0.0018626994479695046 538 0.00046173641502340293 0.0016401731271057205 0.001197161841119304 494 0.001277701386901264 -0.00039795438006662623 4.019015635684572e-05 492 -9.0936304276046e-05 0.0002909144731943062 -0.0001861980296785934 503 -0.00021170231183041677 -0.00012958062120732908 -0.0009407141460048542 2674 -0.001415890597253237 0.0017699807528170784 -0.0010627051557746579 501 0.00010224898977664345 -0.0009893375222466535 -0.00021137718998105856 2683 0.0008661102305232129 -0.0010386459619929121 7.947627283203825e-05 504 -0.0011625379494785296 0.0002582719019865432 -0.000993386416817435 502 -0.001511983443254287 -0.0017416917536180233 0.0007881691230391725 513 -0.00015109751023940378 -0.0007500292593490938 0.0019335629534737477 511 -0.00028984985127460117 -0.0020211788210448864 -0.0001457361820102794 2647 -0.00040035164061258074 -0.0016186922162168067 -0.0005254536764889566 2656 0.00010445148815085305 -0.0007647874292911833 -0.0009156144947657606 467 0.0010196962337640668 0.0003507982325888432 0.0017729220892310539 476 0.0009187702457971796 0.0018174448641619279 -0.0006846376940102886 474 0.0008246423013420201 0.0006890408744245033 0.00025754751342971504 465 0.0023616976641192733 -0.00032022644316765585 -0.001865687496309085 477 0.0020803467562037865 0.0015259740476819548 -0.000762649618773998 486 0.0005134426023509992 0.0009504234658691368 0.0017139773675620116 475 0.0013082133076967313 -0.0009743656595131985 -0.00011413670307432579 484 0.0024216864770579233 -0.0011618474066113905 -0.0021876250028880564 1247 0.0020397224475037657 0.001446329795502158 0.0003276227274566488 1254 0.0006307532963111186 -7.905676100656298e-05 -0.0010411482465054783 1256 0.0010317472417831334 -0.0003943388771701856 -0.0009431195816080055 1245 0.0024195948328651832 0.0011064589540685887 0.00044260979468776574 508 -0.00019507575051880483 0.001991116386330053 -0.0002577161282305571 1217 -0.001976955325397541 0.0005795936129504185 -0.0015802930131084776 506 0.001222906600731264 -0.0017865685808502864 0.0015895878990383559 1226 -0.0015327712299799778 -0.00035575046350829614 -0.0005924880063496827 1219 0.0004190773386013344 -0.0002515786356520702 0.0006169715647944626 1228 -8.257676391430421e-05 3.985781897331573e-06 0.0005320700241442276 1229 -0.0024408870855366894 -0.000998123490255118 0.0003961231406058233 1227 0.0019076327482507442 0.0007530714623599959 -1.6701501120214377e-05 1220 -0.0009997519547014478 -0.0005211960252995472 -0.0014530726924549008 1218 -0.0004372828872536347 0.0005989754374073531 0.0012914055457727896 479 4.889015042291696e-05 0.0010299590920548533 -0.0012738740550424774 1190 0.0010804681608657324 0.0011770385493628213 0.0005056980884048359 481 -0.0007863296459277383 0.0004687973796899847 -0.0016161299644816295 1201 -0.0011472242953509486 -3.323791912575357e-05 0.00015957581338956134 1192 0.0012668740874039021 0.0013579996513177542 6.0057345249556806e-05 1199 -0.0025958190928543953 0.00024129108110985194 -0.0011741084757967437 1193 0.001904520626778111 -0.002286698898794822 -0.0008521299338778928 1202 0.0016655838301363874 0.000620489560302976 0.00017492175432732714 1200 0.0002684923931227303 0.0008073800096388107 0.00024143193293130823 1191 -0.0008456017142625079 -0.0009494849760217507 -0.0009629343885142514 1206 0.0004800322566008734 -0.0018446776677186888 -0.0006244410945439485 1258 -0.0010316818752163566 -0.00015720775358917514 -0.000144420305224581 1260 0.0003659031382737899 -0.0012546569675834422 0.0019145715552273985 1249 -0.00033379687678496573 0.00023872507918107428 0.0023071426897777626 1251 1.2893118084394625e-05 -0.0003333335506603124 -0.001280135420593236 512 -0.00196227233227024 -0.0010852922680855133 0.0003855234352210374 1221 -0.0021333982549924194 -1.1951305949574548e-05 -0.0011437364806063755 1223 -0.0007412939211815819 9.001111954840598e-05 0.0004632293307437111 2692 -0.0004267587422514365 -0.0011566199321741428 -0.0014570191449034525 510 -0.0001387405991729602 0.002216699936175287 -0.0010117480811021452 1232 -0.0010935297693356733 0.000773000100174147 -0.0007968257873447212 3403 -0.0002632679996272759 -0.0005991534602659847 -0.0004257544104338209 3412 -0.0009918096973431222 0.00020172804644448094 0.0019857503405302764 1230 0.001818143173059783 -0.0013103516034186726 0.0005964107853359778 1224 -0.002308609838853748 0.0025168978574088862 1.5169402728645845e-05 1222 -0.00031835635856974865 -0.00046878587131070934 0.0014685245639437015 1231 -0.0011794238896939866 -0.001242304270631284 -0.0009046395945601542 1233 0.0022582205434750926 -0.0008579418647392034 0.00011344227268241262 485 0.00012141943085253507 -0.0011261978630813223 0.002487122728084491 1205 -0.0010544744091810772 0.0008553937961224996 -0.00020996097182288391 1196 -0.0026583198023144333 -0.0004404806758461767 0.00011865927188437733 483 0.0017260431735542188 0.0007956915945763912 -0.002550316222532343 1194 0.0001951968267898039 -0.0009863237546514315 -0.0004176613587652642 2665 -0.002457714250031632 0.0013210057325779097 0.002307518330060048 3376 -0.001386862726919362 0.00032613616384166537 0.002193156156588596 1203 -9.05042580377772e-05 0.0009412333085154127 -0.0012625476936722463 3385 0.0017118449112822833 -6.710178906576755e-05 0.0006209890849591073 1195 0.0017089155894682438 0.0018020966835757303 0.0013035394652403738 1204 0.0021143457582751602 -0.000560097118477562 -0.00016803081422374225 1197 0.001003672568875014 0.0015705783141736198 0.0023363035408959887 608 -0.0007363277600132532 0.0008214401186845076 0.00035873359159993427 606 0.0005087369891865489 -0.0007061171590132207 -0.0006131523525852644 617 -0.0001222450818367648 -0.0013712687858706291 -0.0012598515320791795 615 -0.0018717547166811255 -0.0015404177995767185 -0.00022984011721655572 578 -0.0014827986077333194 0.0011167608017983673 -0.0012002121848123358 580 0.0019444950627349668 -0.0014105254360944842 -0.000982702079424566 569 0.001986263325941636 0.00010589072783085502 0.0007159776033220298 571 0.00011542363734767325 -0.0015636663229581928 0.001440506862786071 588 -0.0016764147524437288 -0.0012279249196892532 0.0005139437911985277 579 0.0008738478993905747 0.0026141309676174732 0.0008207980319660288 590 -0.0002924658169531492 0.0003141649461483073 -0.0011568492307340449 581 0.0011920512584176661 0.0014425069087608995 0.0003039645116767848 544 -0.0023069076375796037 -0.0022929382449402734 0.00010528322025935949 553 0.0004488690851135902 -0.0026206245986557593 0.0009201424674486107 551 -0.0016651755479323333 -9.146990456871296e-05 0.0009212145617407297 542 -0.0013798144017525174 -0.0004897342963335441 -0.002518582308750564 561 -0.0001823098244777134 0.0018529083723862892 0.00019682397711947186 554 0.001474270599147225 0.0007204202201250738 -0.0011652112499285858 563 -0.00024517097056017814 0.0008100882750362286 0.001247249885184247 552 0.00020246868353686765 -0.0018344749982874455 -0.0012460333879256158 517 -0.00015462990215586638 0.0011222051654880064 -0.0012185341135716506 515 -1.1571493031456957e-05 0.001331979647009552 0.0004943422602100892 526 -0.0010505743184194396 -0.0002926074104033327 0.0009685403820845453 524 -0.000986367891771418 0.0013240705453842617 -0.0025838903221778236 610 -0.0007821067772323838 -0.0019170670445369455 -0.0017391265351846441 619 0.001190239732923692 -8.599507275524037e-05 -0.000708222353649837 621 -0.0002127751621612663 0.0009127709703953988 0.0007139582480120574 612 -0.0010554602421680656 -0.001010313659086646 0.0003423986542413959 582 -0.0008596973929528229 -0.00010632701482332792 -0.0011406357662457098 584 -0.0003790423674401524 -0.00011783469755452785 0.002044404917162538 2755 -0.0008937940234140146 -0.0005607064015892987 -0.0009740808227084528 2764 0.0015190848716471392 0.0007017243181029931 -0.001150834542266373 573 0.0006586858517998491 -0.0005647889232039561 -0.0012545469927446123 575 -0.0005359968423628993 -0.0013487730401646547 -0.0013427462093509287 585 0.0006452361154519674 -0.0015177828195144058 0.0007657115040273126 592 -0.001043793242528521 -0.0007542642775072914 -0.0008761565399303782 594 0.00018977080889710177 0.0027008048271568333 0.00017845084671662794 583 -0.00012531676119195288 -0.0013545160481959488 0.001158667076934993 557 -0.0026921918229991576 7.78654486381584e-05 -0.00048371268141224983 2728 0.0009401957206884949 0.0021506346814006193 0.0013601776187273475 555 0.0003563436003025649 -0.00024910943708179086 -0.0024633918025933374 546 -0.0007245286952021588 0.0018413061857694886 0.0009097102702596983 548 -0.0008328960584354475 0.0015069882324572487 0.001018243125064234 2737 0.00012683194624527055 -0.0021187827235561478 -0.0014091760385139048 565 -0.0007274004932499502 4.969102054322184e-05 -0.00013655952446519249 558 7.453412724249976e-05 -0.0005834382681633304 -0.0005400861544181657 556 -0.001130848589453087 -0.0014401392269599287 -4.973050461938664e-05 567 -0.000243304458034484 0.00039456903163732253 0.0007845401289716032 528 0.001622560638097043 -0.0007779789913342822 0.0013639159792354994 2701 0.00046026661965484846 -0.0013944665340545445 0.0011499048296912682 2710 0.0003742937614668882 -0.0001693180961203891 0.0015193776518860626 519 -0.00026304761283666616 -0.000833272884920838 0.0019097222244705819 530 -0.0024673803138767765 0.001578852998374315 0.0007562519282279366 521 0.002645174523454978 -0.0015888749489645659 0.00020035347108299424 1328 -0.00016772601995997463 0.00033481848891731594 -0.0026755278516089878 1337 0.0005597799621660689 0.00029260076849996165 -0.0002875933141906588 1335 0.0012395245272220662 0.00041245030161041977 -0.0009834180141607956 1326 -0.0004936617086473828 -0.00036800156461255567 -0.0004287542013208744 589 0.0016532221168182157 0.0014324450109462396 -0.0009234984483401675 587 0.0005505222662909753 0.0008956606274483391 -0.001418991100034349 1300 0.000579408673384677 0.0009714651077896673 0.001761833700320601 1309 0.0013310128615181636 -0.0005251849121876489 -0.002148907117746069 1307 0.0015266009783396128 -0.0010387370546308828 -0.0008282547633732462 1298 -9.210223124021105e-05 0.0010381281205447046 0.00076143263054994 1299 -0.00035226314714943783 -0.0002597214324350711 -0.0007175321192150554 1310 0.001382923728095892 -0.0012031408381721806 -0.002216567212445313 1301 1.673590476157982e-05 -0.0009251182736294758 0.00014758808885457445 1308 0.0008476177073965814 -0.0005188440707634132 0.0009422495359899372 560 0.00010753435673027461 0.0006908441965430576 0.0002317791395011258 1282 0.0009420988689784301 0.000604968098305708 -0.001195482281480638 1273 -0.0005231502744029591 0.0008202871404145639 5.341252681126266e-05 562 -0.000176264521080413 -0.002105990987425055 -0.0018944537797723304 1280 0.00032155165840098824 0.0008888704317774415 0.0016752308466408041 1271 -0.0016740613646546712 -0.00028773869830517676 -0.0011384915670384435 1283 -0.00019850013128195116 -0.00043423307550237954 -0.0009098028932368209 1274 -0.0005696444968283248 -0.0018845021781396176 -0.0009722674103604181 1281 1.8781245961876566e-05 0.00045937451003409604 -0.0008716846161418091 1272 -0.0007223921438350707 -8.24913752065946e-06 0.0009303005696612577 1255 0.00014680745524805474 -0.0021084483022480688 -0.0014224690542012468 1246 0.0005618119793124349 -0.0005295202026669299 0.00036639627863932126 1244 -0.00013585428384976637 -0.0021508768141434383 -0.00012705646102068686 535 -0.0016978829777986064 -0.0014185074339634041 0.0003229284248265935 1253 -0.00018718768680326103 0.0008082953856739571 -0.00025545206760348887 2719 0.0017475855315863115 -0.0007703677974026095 0.00032112998943460225 1330 0.0005228674638784952 -0.0024003262546546016 0.0020071996950969426 1341 8.659123795030314e-05 0.002018688594400264 -0.002024253103677826 1332 -0.0008034031543233382 -0.0002959632630661778 0.0020508666697658866 1339 0.0005823424563700702 0.0004067513436350305 -0.0016582594905346893 593 0.00028889043197629955 0.0006613431228555748 -0.0013659167421064536 1304 0.0006579060168222766 0.00029015696522339553 -0.0005650733646083029 3484 5.7366781460621574e-05 0.00010367859841134202 -0.0013169726628372697 591 -0.0004697946970248591 -9.917489164584271e-05 0.0008218450619781776 2773 -0.0001755709965772965 0.001330544097379491 -0.0003185002700754882 1313 0.0007689711562972401 0.0018363869060022467 0.000988623232332164 3493 0.002719367876046684 0.0001441931015423736 0.0018460210507579094 1302 -0.0012510937250759483 -0.0006394068486293919 -0.0012427076597467802 1311 6.176777254399081e-05 -0.0003147662680960261 0.0007174173514419738 1312 -0.0012190240548650034 0.00015600431291516888 0.0005797989051094757 1305 0.0008386657879294057 0.00011891257720674268 0.0010685882011310566 1303 -5.722790371879129e-05 -8.224280965595838e-05 0.0003262544710247294 1314 -0.0005457879555453484 -0.0012194022109018462 0.00010135261758178202 564 -0.0014023951395455885 -0.0009116343207000757 7.210008468773357e-05 566 -4.7813856212651083e-05 6.533751397776026e-05 7.037859246990783e-05 1286 -3.2080957541799626e-06 0.001073712110324949 0.00033262541237727406 1275 -0.0006196420681291773 0.00018931350262774892 -0.0014058015834199338 1277 0.00018589520081596062 -0.0008122715105871646 0.001484695066046344 2746 -0.002178541811946803 0.0006118436440834363 0.0007968354258273919 3457 -0.0012062692070321014 0.0020123359076196635 0.0024182096621314713 1284 -0.0007338439546412158 -0.0013761205964854311 -0.0017117283777525433 3466 -0.0007499114308561866 -0.00012673339425558713 0.00240486580932784 1278 0.0013271270814457325 0.0002752369475152645 0.0002184448872718384 1276 0.0015108870734523965 0.0011122066301272166 0.001386032629147109 1285 0.0006537775038121603 -0.0007486683223846325 0.001858076485754042 1287 0.0009268908844874838 -0.0010300399230320735 -0.000916204173709217 537 0.0005420011718652862 0.0016297972044222746 9.931916532165616e-05 3430 -0.00010976384177750764 0.0006507707825762504 -0.0005366057297673224 1257 0.0016685690939592553 -0.00020993461311380902 -3.40257880668709e-05 1357 -0.0005821885978502298 -7.592526107717346e-06 -0.0013458928311879872 1250 -0.000813947263840276 -9.318797029413866e-05 -0.00028962527751620767 1248 -0.0007720887101469369 -0.0017410199869568612 0.0008420689608349583 1259 0.00045508368413839026 -0.0013296709491968605 0.0019319902408364916 539 0.0008472489952369313 -0.0020294559604332224 0.0003349396962080732 665 0.0007030400719002244 -0.0013975461297295523 0.0011004108025040654 669 7.714181954444053e-05 -0.0009046868722137108 -0.000502236999339584 668 -0.0016370767911456998 -0.0008481948233012008 0.00012886307866051506 664 0.0025894803726279137 -0.0005201583610797264 -0.001141144235500896 655 0.0007282703128324633 -0.001350505690559594 -8.353763869623054e-05 660 0.0019867210102851025 0.0005938816745323361 0.0007724041848939985 661 0.0005360340646313286 -0.0020647509707611674 -0.0011627882938173785 656 -0.000985496958009399 -0.0010344348670032195 0.000347511724247543 623 0.0010021395442761781 0.0020034761568163053 0.0013251702667667004 634 -0.0006008060657385053 -0.00011343145330938514 0.002029602723805903 625 0.00048385711471233455 -0.0005529150011713312 -0.001041908876933047 632 -0.00026471399232527314 2.6536479453106955e-05 0.000647109026053798 633 -0.0005607901105775773 3.430847450806829e-05 -0.0005064616921275199 644 0.00043360706777930324 -0.0006313038453632162 -0.0008288496383010318 635 -0.001363067360921225 -0.0023617010584962303 -0.001226348667535611 642 0.0007603726803566432 -0.001369263672055276 -0.0011365918391912921 605 0.0016377216951998163 -0.0009010647005645049 0.0015364516370694919 598 0.0017382149469696013 -0.0008210309978529467 0.0013445596012681244 607 -0.0014886203537241753 -0.0020586056150441903 -0.0014931091846989812 596 3.405072406414066e-05 -0.00013973391662763313 0.0008302452794505832 670 -0.0006567997464646043 0.0003917756829224439 -0.0002177097581576976 2848 0.0009713607419450786 0.0004002760246817474 -3.725173617413196e-05 666 -0.0007005133844961635 -0.001885672311441578 -0.0012827434329975044 667 -0.000658274262432681 0.0004507115438319967 -0.001222571464353268 671 0.0004817983094230116 0.0028055333395559908 0.0008980316571787969 2853 -0.00022264302772712985 0.000397218754574758 -0.00031465222681158916 662 -0.000860780669042732 0.00046904308110858246 -0.0020629765766464365 658 0.0008202066166952901 -0.0003771187624808214 0.0005524549098838451 663 0.0014577073650589875 -0.00124646221028592 -0.00020178650091314736 657 -0.0005781835149749175 0.002059218834670528 0.00024094563219000358 627 0.001049315101899617 -0.0021947808933945345 -0.002439065051796708 636 -0.0007185281731184944 -0.0002279706654227491 0.00010551672788488729 2809 0.0009461756226017171 -0.0012755729684728468 -0.00032502832710083653 2818 -0.0002525202695534891 -0.00021645706372556668 -0.002092123135939248 638 0.0002184208354382767 0.0006422655244758477 0.0027817178013600477 629 0.0018035111583991797 -0.0010470602314202643 0.0002810235715851963 646 0.0005780991138659216 -0.0012026320350493186 -5.2474315066351426e-05 637 0.0015240679894791918 -0.0009093515895134603 -2.567737683894936e-05 648 -9.566916746969712e-05 -0.002235812537656552 -0.0002047729926653348 639 -0.0005689439950261833 -0.0008327416913112939 0.0006968143961117415 609 0.002138212305558337 4.846619058960426e-05 -0.0002991678684716435 2782 -0.001989318995394169 -0.0008955172237424167 -0.00038457562800784485 600 -0.00021422863409946208 0.0003745113342363273 0.001466129649595432 602 4.66580315803439e-05 -0.0002524359940970413 -0.001127795846410668 611 -0.0007351311740865331 0.0007257292396889536 -8.663140612940359e-05 2791 -0.0004405357960836566 -9.439308717520837e-05 -0.000545241813867281 672 -0.0001793358191608228 -0.0008636780736223767 0.002249642005465307 1398 3.0940860528244065e-06 -0.002187336320550007 -0.00012585115425537514 1394 -0.0015737813385184145 0.00039668958118305425 -0.0003050773558830875 673 -0.000987170369799079 -0.0015981028214581885 -0.0008111231996882681 1397 0.0014269687343003111 -0.0014999226017866256 -0.0008768125242916997 1393 -0.002068132022877552 0.0015504246313781155 0.0013016643922759967 1384 -0.0020170048758264376 -0.001995011272973125 0.0011548319482028247 1385 0.000140047895125849 0.000593332725103491 -0.0014549355702967069 1380 -0.0005640316856746778 -0.0012593371222054132 -0.0018494602437941717 1379 0.000993455850777987 -0.00011837170367246267 -0.0014212272146605224 1352 -0.0001101787428305107 0.001074204001920274 -0.0021001542061049394 1361 -0.0017650272079552658 0.00033859882891660925 0.0004481125129530397 641 0.0018410850521953916 0.00030928645189508275 -0.0006688087160652821 1363 0.0009991846064369772 0.0014201647168632966 0.0007632940280173075 643 -0.0007175320832099787 0.0006174669192702742 -0.00032980892601820484 1354 0.0010918447249520893 0.0006130289913077443 0.0023514877771883286 1353 -0.0014136885453282261 0.0012360325140148218 -0.0020108343028512636 1364 0.0007148691356329819 -0.0006190539081419589 0.002133211427607494 1355 0.0003762422340572 -0.002250506595639673 0.00013239473443977569 1362 7.856985951563907e-05 -0.0023967504489567867 0.0008364189636969278 614 0.001614583629371325 -0.0009398739173418031 -0.0022953044317217393 616 -0.0018132449540742327 -0.0013769123342842738 0.0016091350291932561 1327 -0.0004526924545865728 0.00023947942015439534 0.0010449963608001552 1334 0.0005853047295241772 0.0005205717043253072 -0.0011428867194293443 1325 -0.0021944192953582513 -0.00012105380435118275 0.0008927885108764488 1336 0.0013916905767767497 -0.0005661345190887629 -1.8755813988957475e-05 1365 0.002567229601278132 0.0015250784085860686 0.00023827475668432535 1359 0.0005107965517153338 -0.0012213931462578518 -2.8779116202309104e-05 1340 0.00035472498147068375 -0.001193370436808877 -0.000744249303109391 3511 0.001761261702459546 -0.00010260012360357898 -0.00011525517139965801 1368 0.0017042314334728488 0.001458777999047573 -0.0005823108319451455 1329 0.0004396950545082156 -0.0004315852788275012 -0.0018145974076855963 620 -0.00020693202573875266 -0.0005051364627642668 0.0012874276676746344 618 0.0005355299083596998 0.00014517341783570068 -0.00027540838263440267 1331 -0.0008220446428174946 0.00038642031502895665 0.0010403139935606326 3520 0.0009716786140904013 0.0008845049106098459 -0.0011113483740505079 2800 -0.001037177584499333 6.977138283687802e-05 0.002139713202157686 3582 -0.00019654800079616386 -0.00041293346801325997 -0.0015573014101168048 2858 -0.0023911730184976903 -0.0013265365446277618 3.142678728411223e-05 1395 -0.00019217215271105734 5.921515231902376e-05 -0.00027285423326706745 1396 -0.0020740953849508314 -0.0025283708818741634 0.0024038906180088287 3577 -0.00043824049957530593 -0.00035696119650417625 0.0002638183916179135 1400 0.0006580313371166045 0.002605948114624218 0.002021137562693931 674 0.00256994179611736 0.0001682811560439672 0.0003856957896247093 675 -0.0019528972471975457 -0.0005234932678343238 0.0011446582525193063 1399 -0.0025311675247971168 0.0005186268309445526 0.0001268933053783817 1386 0.002146337434398881 -0.0022670823668505284 0.0006498545421690219 1381 -0.0006296701562468943 -0.00046733752964576904 -0.0005233844353796284 1387 0.00046438741018152267 0.0024074268798761687 0.000310116362003439 1382 0.00047623715559613387 -0.000917248092562116 -0.0011220573656704372 1356 0.0015114393999046487 0.0022790546765530354 -0.00029020977941058624 1367 -0.002044390569600113 0.000881096083316434 0.0019509731064531967 647 -0.0010040767108976548 -0.0003932901820230912 -0.0010789519900893784 645 0.0026379265167971316 -0.0018762000971982438 0.0016990850881689517 3547 0.0010237197075307362 -0.0017534201669721708 0.0014786281054396668 2827 0.0014812137946791314 -0.0007597696145496379 0.0001995506178140529 1358 0.0018896804396115242 0.0004661147476886071 -0.00024177421103154916 3538 0.001505174307071313 0.00033691830824532105 -0.001914686628313289 1338 -0.00032648789653010095 0.0019005010285028077 -0.0023178269238011513 1366 0.0008499840305303632 0.0019089520731760696 0.002003415331444621 533 6.9202520251512856e-06 -0.001437564456418976 -0.00010128448030662421 3439 0.00019950572533781888 0.001723130873395064 -0.0006311431782694383 723 -0.0011506956478921858 0.00042776792391955215 0.0017134675270792613 4919 -0.0023667077635198806 0.00042327161604403026 -0.0035421998630933865 707 0.001132522600612818 -9.527901748234406e-05 -0.0011587483651706023 716 -0.0007499129954903474 -0.0022099813562842232 -0.0012523444198607964 4595 -0.0013474730784445456 0.0019439066110012821 0.006037610760573428 705 -7.678401635585768e-06 -0.0009647546073768012 -7.463405163508777e-05 714 -0.00044496333323648164 0.0007846496186602208 0.0005138724567734814 5004 -0.002829275490265879 -0.0010272793843307164 0.0007119140452393438 4497 0.001287044083808907 0.0020470442276895326 0.004082316220104106 5128 -0.00024738001102757545 0.010502510610807803 -0.003047502033709065 4779 -0.0015556453859332912 0.007791814298033143 0.0007983250039316596 4383 0.0012105767262457368 -0.007932953105322316 0.0018046950424815042 688 0.000923001158173479 -0.0007919567234843987 0.0006007642622156786 686 -0.00025122985229985694 0.00017815702840051802 -0.0027436518304503063 679 -0.0007269028793342796 -2.506130463282444e-05 0.0007545459656450504 677 -0.00024607508207999135 0.001145907058958993 0.00023975271719830878 4822 -0.003437016649572227 0.00044658610877271177 -0.0017859399406066796 4430 0.0036909700878008404 0.005413296879797526 0.0025351178318729515 4683 0.002460635986549314 -0.009733119295750568 -0.002541769779057064 4423 -0.00600259678496254 0.0026525945674107246 -0.0023107097554844165 4396 -0.002783175480622759 0.005796786278252028 -0.0025692769115627967 689 0.00021456637341275972 -0.0002715456511863496 9.87821482327445e-05 698 -0.0012018943048109493 0.0008942989339209206 0.0007148573460391117 696 0.00186721920493212 0.00041296265508706967 0.00020210983383230877 687 0.0008245395564943369 -0.0006912146209063549 0.00032758373351367276 4568 0.0025920270380331207 0.00787339890744398 0.006458604805331379 4451 -0.00643037409375494 -0.008340652842128652 0.0028269111107563625 4649 0.005111862315854818 0.0005184956839691247 -0.0023085770539277265 4828 0.008502417034877025 -0.003626165731538333 -0.007738696068992332 4525 0.0027554775322935912 0.012866434528079932 0.0020926105497987065 727 0.002064919132290103 -0.002179086444994726 -0.00016648736374366788 4725 0.003519373300072201 -0.003145956472583572 -0.004168146000968242 4520 -0.008551974608480475 0.011659976331285194 0.0018386178236799518 718 0.0003018919074714993 0.001892081834835768 0.0005385597604427134 4476 -0.0004166863689175506 -0.005166959020355281 0.009221894816517764 692 -0.0005289514769722293 -0.00202173457132843 0.001836234197077042 2863 -0.000272089166969462 7.701654739501371e-05 0.001660428763976352 4770 -0.011380786006646642 0.008586917418706036 0.005334519386203901 4901 -0.009047124364325913 0.005960963831471638 -0.0008419176147495665 4627 -0.0005526622653163511 0.0015005848202120577 -0.001920914047623777 2872 -0.00016219925502050083 0.0017162635177367233 -0.002327125027667038 690 0.0007772941246136265 0.0015558054042458475 -0.0003722469277896483 4438 0.0027846808629350284 0.007712670306876347 -0.004615279609748171 4461 -0.0011500423289815386 0.0015253672495126745 -0.004430047958997633 683 5.8017223275730204e-05 -0.0005030497817139646 0.002599008893664685 681 0.002141737530142289 -0.00010671365058239794 -0.00023362674359496687 4697 -0.001412198801723934 -0.004952170096045044 0.005399947964575514 4700 -0.004692781070564414 -0.00011890084590872725 0.004900905557329373 693 -0.0010616979986973842 -0.0015423155757999332 0.0014477764042915221 700 -0.00158121467833685 0.0007786581297164208 0.00026793633052126604 691 1.7776477269996257e-05 -0.0008247551452831108 0.0004916818045652197 702 0.00018216611210612917 0.00028565279885497236 -0.0021767231467888773 4534 0.0012406328213823833 0.004422963598579955 -0.0015511640617763489 4666 0.00837612067033683 -0.00036421437304676635 0.008654031524819559 711 0.0011105753964482548 -0.00020821538930351205 -0.000555931254843903 4709 -0.0024951137221763497 -0.005551473851374267 0.00430223361726426 729 -0.001640993236822826 0.0017060780330987433 0.001527156545067632 4762 0.0023629249945256343 -0.00019393760580129892 0.0019728859198389253 4855 -0.0005523451899158976 0.005871873497862283 -0.00022733521890383327 684 -0.0006693963090947703 0.0004988173965703975 -0.00018460241465785576 4495 0.0010488555412378761 -0.001134101704691982 -8.43736328913706e-05 4618 -0.000861997209800935 0.002361212998163047 -0.006720452333229974 4566 -0.0013774129409516909 -0.0079755910858289 0.0002909465255372172 5059 -0.004727286838209712 -0.0009369740648448443 -0.0006132389058289491 4598 -0.003087682297004717 0.0028631762899886475 0.008242064313855891 4576 0.0032721613222625842 0.004080264994165885 -0.004318476913593087 1436 0.001591958320077962 0.0015182706362167413 0.00019645289160036793 1434 -0.0018466932948308843 0.000510163967846661 0.0001537606697075138 1432 -0.0005873262720196908 0.0004487504338925926 -7.240450493238028e-05 1441 0.00035099348446183704 -0.0006342344421088567 0.0009414561482087146 4658 4.1063038823128777e-05 -0.0018492002534222394 0.006902486409738767 4548 0.0050951957672645525 0.007406633584626976 0.0012788154905516696 4825 -0.005490340412335696 0.008145419668793752 -0.004225541988541034 4429 -0.0018440638383334853 -0.0008615560617767491 7.306187876588878e-05 4453 -0.003566287065527381 0.009769262383482857 0.0021756647408797017 4846 0.0014700092441169905 -8.607019549138336e-05 -0.001609523263165883 697 0.0004050911711435049 -0.0008788234027263932 0.00011783361673939168 4464 0.0032602772386476253 0.011372202229648338 0.0008351070961854653 4556 0.003777334626193806 0.002835032720011698 0.0015266372195684957 1408 -0.0013807677864191381 0.0008530873242064801 0.00010700251740954265 695 0.001450700025689602 -7.473264840497147e-05 -0.00015720218728342526 1406 -0.002020828243824384 0.0017331734446153243 0.0002186993428356244 1409 0.00023741356364661984 -0.0017847857307378336 -0.0006774173010491207 1407 9.841008733855452e-05 -0.0002652197889960354 0.0008324701489211251 1418 0.0012933657017663962 0.0017962579864136173 -0.00014287956087185747 1416 -0.0021776084354949384 -0.0003654721771335753 -0.0012215420074889786 1415 0.0010915851553155603 0.00038381407028721237 0.001982581464877441 1417 0.0014957541747685683 0.00012373154824167187 -0.00025576858187845684 4552 0.004435076205724283 0.0001243637676361202 0.0006051183523323308 4917 0.006391784224961299 -0.0012774798102939211 -0.00398125613349069 1410 0.0024969447699379056 -0.0011002043332105145 -0.000657315433287906 4439 -0.0061300831882642815 -0.0028372050950150837 0.00225779260397761 699 -0.000548498375107172 -0.0010979776580508035 0.0015115927169856553 4482 0.0011840808047396342 -0.005282262968604494 -0.0063682312917828585 3592 -0.00015678730821851313 -0.0019042952343614142 -6.1751943607032e-05 4953 0.00040530151826700977 0.002766698370609177 0.0037956306700087364 4724 0.0014223031485070588 -0.0033051648109215085 -0.0029848239603163613 4907 -0.004612773397768056 0.0010182468617936271 -0.005013051431790825 4558 0.0006221825311824099 -0.005529510692044386 -0.00027213410070719307 4764 0.0004448179079852169 -0.005905900121065974 0.006621077238746825 4531 0.002318811357001013 -0.001513666548739092 0.0018645118381645396 2881 -0.000855931475744283 0.0025759422903206645 0.0006740949147239883 3601 0.0015469157249493955 -0.0020284304228193515 0.0009270645841238472 4391 0.00449259833095438 -0.004654062935485095 -0.007090826031987132 1412 -0.0009270906110952961 -0.00032337553240897876 6.104847750515886e-06 4593 -0.008060035229329332 0.0008015268782705463 -0.003446368603199393 4609 0.0066571412743245606 -0.0003961781190329642 -0.0019332764382686241 701 -8.500390731415149e-05 0.0005830786858928131 -0.00023515942560738677 4719 -0.00442625010376873 0.003941961796441577 0.008701377117864706 4747 -0.004851509901072126 -0.0017528294268604376 0.001501458029187468 4614 -0.0019179052572570292 -0.0029195447274266463 -0.004058478826939316 4524 0.004489913366374592 0.0028588955126180255 0.0034551278041189872 1422 0.0006927545944796709 -0.0017176180426332441 0.0015252478242128835 4484 -0.004241522276325357 -0.003961491676751951 0.002874328729846919 1411 0.0021921629480402193 0.0005252682525620092 -0.001085544292969043 1413 -0.0025295611248810834 0.0012058850189439277 0.001546917480943763 4519 -0.000418488075431601 -0.006588542233453185 0.00022190492118409372 1420 -0.0007750312412494842 -0.00018174443892865922 0.0005558823760799115 1443 0.00038138714194501863 -5.851271854093312e-05 0.0018015077955103442 1419 -0.0015518089713878762 0.001643064677197025 0.0009849449817052446 4648 0.004706143053877807 0.0033732084888282235 0.005618850373860581 5063 -0.0034837894825163872 -0.00922829180867119 -0.001577281311791566 4416 0.00219490168104409 -0.001644046934133358 -0.007549404035191924 4479 7.812362498819394e-05 -0.001204347164812573 -0.0025331318914482144 4753 0.00873740841170842 -0.000800502055361887 -0.005323430822066018 4443 -0.0008202090020273633 0.0049289897561983825 -0.0041611467160644145 4854 -0.0020785150384253566 -0.00010056175087223875 -0.0013807135442578042 4852 -0.0068340514959434676 0.014504534510547989 0.005230204086615414 5017 0.0035155025199811625 -0.0024724084579912306 0.0015887405184423255 5070 0.000458010679170042 -0.003116788196995658 0.0027939495160455518 5 0.0019364353345580167 0.00033417549079053395 0.0004097421366208941 21 -0.0007801180369730024 0.001023145864457918 -0.00022377897737978762 4921 0.0010962505746068734 -0.005555049845839968 -0.003797718443242443 4417 0.001229479261076732 -0.007986349808273101 0.0009921302530681059 4973 0.003463092467606981 -0.0010498355155309147 0.0015117003163163708 5273 0.004394028082923773 0.0019608568001727666 0.0024492322561307026 4420 0.011601044898514842 -0.001094776013987372 0.00671470938408191 5477 0.0027600565175539297 -0.005832445488200214 0.0026041645699667665 12 -0.0009279770768000958 -6.720322824455298e-05 0.0013433025213472431 725 -6.67328473741731e-05 0.0002734333311014139 0.0004984774973601327 5030 -0.005130603802994333 0.003766509570610239 -0.00472676147694695 5302 0.006355813318756612 -0.0008528766929515852 -0.0014245778918522416 4868 -0.01070132001367045 -0.0015759601732592268 -0.004973053484058569 5376 0.005216388095093613 -0.010211218331459252 0.004986054965269202 4756 -0.004875520598282673 0.005175169581228046 -0.005672113143788252 706 -6.274423818091682e-05 -0.00032903985865326453 -0.0009119230102994643 5352 0.0003470790877221151 -0.0007400617628086092 -0.0017418531057933995 5339 -0.0008172741136566566 3.9661539418394147e-05 0.004004252982929242 717 -3.781092856869708e-05 0.0008639692873632506 -0.00017973331705890946 4847 -0.0003716822578908039 0.00278868162540455 0.003886553588904887 4894 -0.00041063720030506577 -0.014166147443694634 0.001126962426766942 14 0.0006443417418142692 0.00022906155728717736 0.0010590620166674293 715 0.0018766982742228927 -0.00036390933237705355 -0.002441023074628416 2890 -0.0008200100233672762 0.0015888306073347327 -0.000405061637064183 16 0.0010282658490132265 0.0008190243624880279 0.00013384607922127415 5093 0.0035436504577772763 0.010176385850208906 0.006196994276354644 4998 0.0038486796286376526 -0.005851209611702254 0.001998911358518264 726 -0.0015391258012775405 -0.00048527684937227356 -0.0008418809001155588 2899 -2.4449790233056464e-05 -0.00020151409814727337 0.0008877258335007318 5196 -0.0010550899693202945 0.010035046183042974 0.003436280186405613 4842 0.004962464331326929 0.0009321556167816805 0.0018685806341783026 5275 0.005025339276266846 0.0003348689305873231 0.00533520239303165 5399 0.006516437428489986 -0.0006146646852245354 0.0013695973916899688 5258 0.0015137634330343614 -0.0013626637154773012 -0.002301076704978229 710 -0.001319555733815139 -0.0021956341853954413 -0.00044459495789068326 5106 0.0009732301310953074 -0.0029667733281951124 -0.0063141728562224365 5385 -0.0025252459965251464 -0.00636196707394946 -0.004157800779550642 4851 -0.00036327284958045426 0.01005591388869781 0.0036154164337280866 5005 -0.002408780356051155 -6.056947796191723e-05 0.0038029603307670025 4797 0.009945845633563405 0.0013696059346961092 -0.0021048558674590227 4450 -0.0005188522581438598 -0.008052224552051611 -0.0012855588802517636 4584 -0.005054785730651778 -0.001823891357139352 0.0012597778019101504 719 -0.0014201445820662796 0.0005319132633984022 -0.0003907600464351333 720 -0.0010555173268936954 -0.0010773262419832346 -0.0016983542738914503 5107 0.006565295439421826 0.009601822364220408 -0.0029141423127433566 4529 0.008512605007618844 -1.990937405516068e-05 -0.0012980364742427167 4910 -0.001060388358511428 0.0007972751661625418 -0.009175560809030307 4970 0.0004507585216763865 -0.009476919202103733 -0.005211048308727569 4435 0.010487038981367259 -8.190425904862762e-05 0.0027599007298317944 5211 0.00830919334605108 0.0023170358151985266 0.003255263111217051 5431 0.003870255698220676 -0.009538145066186485 -0.0009402016793662951 5381 0.009627971401570656 -0.0002550739229429305 -0.006857051069560552 5064 -0.001047468542954396 0.01092364397984563 0.00430025752833418 4703 0.000107545098805325 -0.0067248217347577795 -0.005529218659970027 4694 -0.003619580376192417 0.005220963648369759 0.007766561285869145 4895 0.009284011163625204 0.002376834006364565 -0.004863710412693813 1446 -0.00036684969654706746 0.0003943034769052561 0.0012282738671709954 5351 -0.002819024461693104 4.606514271840987e-05 -0.006633508319405967 724 0.0009125162841142277 0.0007432546395824139 -5.5379310296042265e-05 5433 -0.005590591784303589 0.00259397800801855 -0.0001590270937838784 4882 -0.004918789465942873 0.010657447611624555 -0.004607130198578265 5164 0.0036484048542636907 -0.0010507321832571072 -0.0017596186620267385 5421 0.0018653834516652557 -0.003671364991069254 0.01379881001575809 4763 -0.004414368741893586 -0.00046609999437777433 -0.008399468854972551 1445 -0.0016578470637674397 0.0007376121039889348 0.0018373031447529093 722 -0.0002919158354426565 0.0009729378734455053 -0.001470154315375592 4713 0.003508698376322415 0.006679289031109313 -0.002562874520217008 4993 -0.0024392483940684512 0.002858363329466239 -0.00485183264548519 4657 -0.006679506688820944 0.010871941629516874 0.0012023541817278165 4750 0.0027118401430454415 0.0005210368660786047 0.0017332523132157908 5068 0.0011414028804503213 0.0035210989220634285 -0.005969952230974342 1433 -0.0007886387352014235 -0.0007245056860869623 0.0004850374175509132 4496 0.011503586877226564 0.002252880069579576 -0.001192493924720667 5349 -0.003397630912717432 0.006719478518853416 0.0023380205288725197 4579 0.004084765793399627 -0.0027475207053000127 0.002595747090324412 4652 -0.0005240188623368698 -0.004677395187667464 0.008765962738294227 5208 -0.0017742059409101122 0.00354068364517565 0.0034314304472709127 4997 -0.00026549175709138657 -0.009498943157047506 -0.006924637530625498 4721 -0.0049902998868177305 -0.005367405921390182 0.0039056238380879107 734 -0.001092540607917983 -0.0007734610207220825 -0.0009125428490340496 1447 -0.0024137662357529457 -0.0026757229662093813 -0.001498329948538893 4759 -0.0022485380273225427 -0.0010767731728204021 -0.006093845257156602 5461 0.0007986348303565085 -0.005142109129894996 -0.005547060792766733 5439 -0.002049131658589576 0.0005037861418449184 -0.008517373091530112 5331 -0.0008287797974247817 0.0029670967241504755 -0.00557497720446238 5177 0.004264933786468004 0.0026293193325689418 -0.0028441592408798315 5153 0.004391834358371498 -0.003997486994447687 -0.013696214534261727 4620 -0.0028366682518732133 0.0016627828639308804 -0.0059240760454045875 4446 0.0030307473630127933 -0.008563193469494093 0.012323633558214808 1437 -0.0010035409239707816 0.0011311624034781211 0.0005494173929664805 4827 -0.008187380531357145 -0.0013870564396909002 -0.0015605877348405137 1438 0.000527881723702958 -0.0006344635293540778 0.002196453436564969 5286 0.003875983569228423 0.0008940121185916397 -0.002224949430602326 4677 -0.00791019005907216 -0.004829424909653437 -0.003093917777535692 5328 0.005340737706575397 -0.0014914006289762796 0.0033109981020693936 5389 -0.002327283196788185 0.0008156402491106864 -0.001109916626870368 1449 3.442451929965267e-05 0.001654504149735499 0.0002508119908180798 5348 -0.0027395509596469794 -0.00032570029677796554 -0.00581656392302601 1435 0.0009877732013303141 -0.00214988548157583 0.0016649310250073804 5060 -0.005633807600194968 -0.002984084454526206 -0.0060012142944138895 4616 0.0018622815138736493 -0.0027704959591918384 -0.0035142174149648897 5366 1.8209946428945564e-06 -0.001918359820308992 -0.003449643415206873 4930 0.0056035711953219694 -0.0029901202128125187 -0.0028868615798206244 5505 -0.009073469002600558 -0.0006341497952695053 0.008387867949386991 5343 -0.000901319536864364 -0.0027714697120505816 0.0037723088737031682 4581 0.00017900622013860464 -0.005550609493043146 -0.0006407502317231728 1467 0.00030653303360184386 -0.0006098421677763392 -3.472520926691715e-05 4768 2.0458603573028877e-05 -0.006962382711326887 0.005971219089060118 5465 0.008157585669899223 -0.008508938424725367 -0.004560280054471206 4564 0.0008337907078497717 0.0042485577247766805 -0.0031409604132428322 5066 0.0029019168993150617 0.010441679251782748 0.006808319693605076 5276 0.006419987017447833 0.005779721592393252 -0.002880382875963581 5316 -0.004668294740264923 -0.0066885577519967656 -0.004586279603990778 5158 0.0056515354727232 0.004820559579106732 0.0015826003904626119 19 -0.001206550300888847 0.0017854366773497512 0.0013024007094070372 5256 0.00520057196650065 -0.004169200090289903 0.0008872947319514242 1481 1.4389150938409409e-05 0.002388770282775978 0.0006144210077948543 5342 0.0004300403363459175 -0.00016084066367781047 0.001978582573466376 5161 0.0029875001195574665 0.007406945138771284 -0.0005528557261724075 5245 -0.007148376119778421 -0.00044510639815623044 0.005249599778593746 4448 0.005553289581429546 0.001481390646639556 0.006318933328025141 5392 -0.0017993730495478905 0.0006951533679594489 0.007445577225397814 5121 -0.0023957421530992414 -0.0018827815742246568 -0.0007540118121277315 5212 -0.00504276236908263 -0.0013485936783722442 0.00014555721034456754 5289 0.0037645657936672718 -0.005251184853940641 0.002130838369731105 27 -0.0009766459464908746 -0.001200183878663186 -2.175341112154198e-05 4706 0.005143899670895922 -0.004156913795907245 0.00029692894548008513 4602 -0.007932374910896491 0.0020295085884828932 -0.0001255362539039997 5246 0.0013585768012122292 -0.003797078082355404 0.0015854365129056773 5024 0.006657432269160383 0.0006866076680204331 -0.005610201063651795 4931 -0.002574911881530867 -0.005698537071779188 -0.002955087687154035 5472 0.005255165085093335 0.00866924009301792 -0.0020424603964911063 5101 0.0012956322832216511 0.005879869446652304 -0.0007611833382565299 5491 -0.007556545404258467 0.0003409152422211209 -0.008107915980378189 3645 0.00014376136974393388 -0.0022396264246711583 -0.002408787964608312 4538 0.002958959105367967 -6.455547087919311e-05 -0.0034009867224332377 4670 0.009575758111438223 0.00012766915368935704 0.0010658333244667308 732 -0.0006260678472717264 0.0010919334278708987 0.0001720803173415296 4811 -0.0024624780228046468 -0.0003912211153766343 0.009678182989562429 5344 0.0019027389606472522 -0.0038901526843552856 0.006603465686086678 743 0.0005941766714360457 0.002183304692133331 0.0013007865355590083 4918 -0.004070167310881257 0.003887266528203186 -0.00039196153511473434 5055 -0.007227104332798532 0.0077069481840766054 -0.00024091669648569527 2929 -0.0018666713055701613 0.0005787287315800605 -0.0025935054299500624 5396 0.0027697470534749414 -0.0005387768982598195 0.0022924302659046323 745 0.0006451689876685366 -0.0001099383520076166 -0.0005777970914465883 5067 0.0006537948433288285 0.0013567682392832507 0.002821103272275846 5262 0.00422720152667105 0.005708696450599714 0.005001355425529605 5430 -0.009636355459374944 0.006167995125972145 0.0019547369692957776 4465 0.002168257495709129 -0.0041005400215253125 -0.0018974889171046946 5261 -0.001708674062841033 0.003511871899701838 -0.0029009733429728544 5485 -0.001738444957549793 0.0031812380679894434 -0.008299959031421842 5189 -0.0004892064130052025 -0.004334013151696123 -0.003342348271019406 4967 0.007129130382454612 0.0015625482179052526 -0.002851131855991699 5361 0.006316293421618968 0.005079052714222094 0.0007077729746701863 4458 0.001369907312666849 -0.0008164955581429814 0.0033297905433765226 1488 -0.0015035902576505692 -0.0007356264670401944 0.0009109333376428472 777 5.613630414277282e-05 -0.002387497834652445 -0.000333850576792467 1490 0.0024448072290629186 -0.000586116400551497 -0.0005111889173879164 779 -0.00022791604440611078 -0.0018922104730823275 -0.0015215892016799812 749 0.00040067677675788955 0.0008431625364565178 -0.0014649462347913044 1460 -0.0027783472158794003 6.508839885297781e-05 0.0024761759599012884 1462 0.0007005995537258918 0.00205379555550917 0.0007690674968239617 751 0.0002289102433620494 -0.0014109999140780097 -0.00039818511102081706 781 -0.0010649357090900722 0.0008947805190713469 -0.0011279937828451408 783 -0.0008748525492062351 -0.002246408652404538 -0.0021558616217050896 1492 0.0005094523266171518 -8.152513037607174e-05 -0.0006130312501304437 1494 0.0002808475264893335 0.000793967532013398 -0.0011835714945788531 1464 -0.001421143081355809 0.00026739335770110473 -0.00039856591784952146 1466 -0.0008290718683479311 0.00017007663394785798 -0.0010171819821369749 3646 -0.0022374242984802228 0.0005999068136779157 0.00027746002652622977 753 0.001093270025670426 0.0006171176205828893 -0.00016897317943412391 2935 -0.0005709074235705385 -0.0010652497855791127 -0.002093614799052888 755 0.0007204435977390333 0.00031373617912141237 -0.0006515365293145592 1499 -6.582836158701595e-05 -0.0003319730239111534 0.0005073869866387675 1497 -0.0012305823622250664 -0.002411581853994544 0.000863815974036474 1506 0.0006963021360390234 -0.0018527753328234468 0.000357371379181075 1508 -0.002092378781817286 -0.00012847756162163537 0.0009399388463658578 30 0.00040934421669002515 -0.0003448735411807947 0.0010080494854077852 1471 -0.0008548326500573615 -0.0020719114408295942 0.0010198183206357996 1469 -0.00010617303606892973 -0.00045831658758502627 0.001547681795086523 1480 -0.0008231002341391696 -0.001166269070509429 -0.0005488006593117619 1478 -0.00146762989098942 -0.00018555827455860778 9.04132812500073e-05 1479 0.0006468869074929813 0.0013182989677567654 0.0005906757000014575 32 2.8601718289250188e-05 0.0004098157946369474 -0.0004643433029649362 1512 -0.0005538597237858538 -0.000151284510989682 0.00124953241901211 1501 -0.0009710942618072929 -0.0018266310608893146 -0.002486268152934135 1503 0.002255820666211408 -0.0020670374004632935 0.0005054293943185934 1510 -0.0005834023390588511 -0.00037636992433254463 -0.0010325919767474295 36 0.0009317716099712589 -0.002382370071121634 -0.0004929031983261367 34 0.00029915118898368384 0.001126429028579097 0.00043052772389505435 3664 -0.0014792385937687387 -0.0010302074597865023 0.0008007787390734114 1475 0.0003674298911527211 -0.0004141977693034476 0.0020793859781822 3655 0.0002656821650868545 0.00025827356274961107 -0.0002629477356184914 1473 -0.0015413007499725947 -0.0012744009700016246 0.0004219202606467758 1484 -0.000426405335700033 0.001214617468093163 0.0002573657240940556 1482 -0.0018180797382790195 -0.00022363316496559326 7.471742189550418e-05 832 1.719850721828767e-05 0.0008000520264488246 -0.00010279611880978738 1543 -0.0021047326197406358 0.0016197881891172044 0.0011510948649943301 830 -0.0013726361515518713 -0.0009358078822794265 -4.372353654506084e-05 1541 -0.0012851209065738146 -0.0014483026453447109 0.0009917858354687083 1542 -0.0006139545650229122 -0.0020377531604483293 -0.0006852897211025542 1544 -0.0002562843487223473 0.0007548492374194974 0.0013704393974516731 831 -0.001597962617248358 0.0027055809085811473 -0.0005188473693802347 833 0.0002007822295703903 -0.00041749952195247993 0.00210681665734191 805 -0.000709623066324198 0.0016429827370217731 -0.0008355560479591921 1516 0.0016146389700515923 0.00042352513051324063 0.0009152948840615185 1514 0.0007143317415532064 6.632317696750366e-05 0.001069978466311016 803 -0.0015160768995957524 4.7459194478151594e-05 -0.0017389692784076146 1517 -0.0006117620422970362 0.001427289819569079 -0.0019635400320386336 1515 -0.0016363058210820624 0.0001325498212344185 0.00108975143384653 804 0.0005429555492793613 -0.0014179284184637692 -0.0024604992960086548 806 0.0020043429079049362 -0.0007595415755387752 0.00013202367162336553 1487 0.0014499150136612054 0.0006342381738320609 0.00211706542809524 1489 -0.0002676394574616756 0.00015788804838652213 0.0015956316131723123 778 -0.0020299478340768395 -0.00100528181109131 -0.0003373950727181031 776 0.0015839481552308654 0.0011911363455159038 -0.001900756730223536 834 0.00012665047383333874 -0.001843888100665816 0.0007313401068900622 836 -0.000748674082906771 -0.002520177975783195 0.001007491526893441 1547 -0.00018343964931725185 -0.00023383643524887 8.710539652438716e-06 3016 -0.00166273605390276 0.0006453426159896949 0.001149323683926847 1545 -0.00011619525855079149 -0.00020503092597382554 0.001184134606118907 3727 0.0004024189547026884 2.4849905030887003e-05 -0.0013107287295654245 1546 -0.0009423492118750042 -0.0003005020629565699 -0.0009990365336594999 837 -0.0006660973152692682 -0.0006643841060533337 -0.0003099315556279441 1548 0.0014121790806888787 -0.0009661093916265724 0.00021727028270323006 835 0.0001851712759890615 0.00042853926416253866 -0.00011269024472596462 1520 -0.0005499679328584864 0.0014525574142459524 0.00023313546086951723 3700 -0.00011812592695236075 -0.0003881865760693538 -0.0016691126665054686 807 -0.0002916304115515156 -0.0016251580997505215 0.0012123022864279304 2989 0.0012321407476429817 -0.0010659617766163839 -0.0005193522153712471 809 0.00027442638088152546 -0.0018738819483476155 0.0006058468334238644 1518 -0.00022140388149156811 0.000998314765387352 0.0022558354552876096 1521 -0.0004957858691239489 -0.0020571560233046647 0.0003824416128509892 808 0.0012850140483101821 0.0007405182533973248 -0.0006504561632419234 1519 -0.0005480682617095944 0.001845944056820078 -8.272770894983861e-05 810 0.00037429672197809437 0.00039706107679443874 0.0011627688059224822 1491 0.0005783301165049003 0.00019267317015571675 -6.59201846214554e-05 1493 0.0007021960948291942 -0.002109846980176729 0.00044266273779517296 3673 -0.0018239167670413235 0.0009301269433267507 0.0012909471619708163 2962 -0.002256388605896791 0.0019618361897901517 0.00047730418919887316 780 0.0012986367997455952 -0.0012795873037122515 6.598125950353336e-05 782 -0.0016078727608394325 0.0006570974086829644 -0.0002759421431127563 1552 0.0012452945104878639 0.0019638558374426235 0.0014552609554667518 1561 9.690052382789688e-05 0.00017726696356708954 0.00040910771691564764 1550 0.0001400366509635106 0.0016736766542356403 -0.000793043769795669 1559 -0.002495843646003189 0.0010635987648465143 0.0002868283438528769 1551 0.0009509179093432269 -9.17809737306088e-05 2.138259080517943e-07 1553 0.000958096307586895 0.0001682977317302765 -0.00019967447494841908 1562 0.0014200973416360597 0.00023952297928732488 0.00126530246901548 84 2.498476526963361e-05 0.0014656840144416238 -0.0010685263290708745 86 4.179601308612201e-05 8.375132028774377e-05 -0.0015769393145419349 1560 0.00037232958739034623 0.0011856505967531123 -0.0010475986589367416 1525 -0.001887125990012891 -6.0051311066774754e-05 0.0005816494931556622 1534 0.00010957420071953418 0.0012544528884620586 0.001155187161043823 1532 -0.0018536895234020697 -0.0019032845907907814 -0.0015782657824145174 1523 0.0005160339940502266 0.001932177372048502 0.0012571348193842731 1524 0.0001416017912103558 -0.0019126161782619467 -0.0009005788845486938 1526 -0.000710390875510626 6.966499989649686e-05 6.317938108893549e-05 59 -0.0017134958497793428 0.001187071500014311 0.00047160231630062187 1535 0.00031812343582293895 0.0008996644477884865 -0.000667528847987026 1533 0.0019105551503849516 0.001732138282709543 -0.0002472639209367684 57 -0.0016946760776457453 0.0007984946444306768 1.4267582354238716e-05 1498 -0.0017297745594066832 -0.0018412588676862474 0.0007975396694764711 1496 0.0009167113200292784 0.000845417215756712 0.0012483690892059456 1507 -0.00017704273626870034 0.001412265256768404 -0.0003451664186845025 1505 -0.0007985314329314846 -0.00012011382324057795 -0.0012269454362561513 1511 -0.0020957418767215395 -0.0007188773219073176 -0.0008294126728339607 1509 -0.001949171063363737 0.00034942654568821175 -0.0008890679492234579 61 0.0022977119751502587 0.0007341969895867482 3.1037184414501933e-05 3691 -0.001480752764556221 -0.0011125667644075097 0.0022105486653752207 1554 0.001884958431345328 0.0016348743806525066 -0.00010640944876694886 1556 0.0004320250443031698 -0.0002933755699001737 -0.00013642192093832046 1563 0.0024694973051045664 0.0004849932349826324 -0.0015435105075745593 3736 -0.0015309193351435142 -0.000468638082006516 -0.0010602057483019309 1565 0.0003908933751757223 -0.0010945186215048704 -0.0009793275989527076 3745 0.0025551180031248167 -0.0006779314850163995 0.0008804351790047816 1566 0.001264248805285654 0.00010820315937849659 -0.0003248228398207998 1555 0.0005853853121499904 0.0004000440213196546 0.0007605961984343593 1564 -0.002045018465041552 -0.0010438125043691084 -0.0010211113601327493 90 -0.0014906786812639845 0.0006752012370723624 0.0003628369298499019 88 -0.001476947649658446 -0.0006007206802499088 0.00037454271069893965 1557 -0.0014676565976004534 0.00024967102001697324 0.0001883228413002546 1529 -0.00016778448048697468 0.0014456949580728786 -0.001830225973828801 3709 0.0022486803010939157 0.00025305024151684894 -5.3652170376365963e-05 1538 0.00036287086643374544 -0.0018053173961258633 -0.002551665116990541 1527 -0.000604444804023605 0.00016709905822126687 0.0008750500162984013 1536 -0.00014615642922706582 -0.00025090466568072293 -0.0020778096680424104 3718 0.0005170747630005451 0.0005513216244884347 -0.0006349898452111956 1500 0.0004152452501042024 -0.0007325432405049296 -0.000622067756831263 1530 3.8084078170361755e-05 -0.0010567484240584712 -0.0005001698277712192 1537 -0.00021861821263236166 0.0012867082441498305 -0.0014509772471820819 1539 -0.0004618219626600201 -0.001838402332088373 0.00037560792479138623 1528 -0.002414358698611276 -0.001889503012235123 0.0005858979568228744 63 -0.001327115692909352 -0.0017475775687918651 0.0009655493300125954 3682 -0.0013497568483805944 -0.001296460361405851 0.0014747306951279258 1502 0.0005269033293066386 -0.00020374018324605266 0.0002546849590873983 1623 0.00013119980592563973 0.0022248243443351665 -0.0011276041979184329 914 -0.0007010418051711619 -0.001727289324822542 -0.0017286261969344419 912 0.0013255889053086758 -0.0006034320559457709 0.0007922758075556643 1625 0.0014261875692397888 -1.73548451231058e-05 -0.0008017851568807315 888 0.0008238773210716478 -0.0011179683837300898 -0.001955789874051205 1609 -0.00020542355803622936 -0.0020929155080227154 -5.36500372416834e-06 1610 -6.392561530469852e-05 -0.001886241023181291 0.0018254629088903821 889 0.00044530508444336355 -0.00039022776526750425 -0.0013786971678025506 1595 0.0017225094972788423 -0.0002470035253970995 0.0018487516706426803 877 0.0010257289243558554 -0.0013534208536522582 0.0007276357186101995 1596 -6.808407902169928e-05 0.0007370134731172007 0.0002783837470939409 876 0.0005672653018730878 0.001220345917658305 0.0007579435430642684 1570 -0.0006292494526997914 0.00013717434589251916 -0.0022069615646091935 859 -0.0021386309847582674 0.0008834321692587782 0.0004874789665262429 1568 0.0016271259770308652 0.0012951794671701717 -0.0004645399559729071 857 -0.00024422165760382174 0.0015409903304520862 -0.0012236043362319048 1571 -0.00012178135255702107 0.0005594135750484376 -0.0012714114707530334 1569 -0.0007685725644634705 -0.0006031700401421864 -0.001606399985694842 860 0.0006452186907251216 -0.000427799484848059 -0.0002317323195154099 858 0.0003431131284724603 0.0004554795414622474 -0.0018344922458315923 911 1.4517549652594405e-05 0.0009338993757865373 0.0002039874022040102 1624 -5.8294486388632896e-05 -0.0019274647653949564 -0.00036474285504880404 1622 -3.4442421078283224e-05 0.0010508650891306766 -0.0014985881525334877 916 -0.0018953710981249564 -0.0012671033750348188 0.0011519411199067736 1627 -0.0004749097571798656 0.0005426533856295306 -0.0005015819775309164 918 0.0008233714941430235 0.0006592648388928993 0.0007276517758553062 1629 0.0005574050541568373 0.00038915390117473135 0.001262446211305558 890 -0.0018412820538319702 0.0024017227115808366 0.001479328339662925 891 -0.0004744815673030905 -0.0015285246241292013 -0.001630831198595236 1611 -0.00042141336474918055 -0.0007211240412712479 0.0003002887308529616 3074 0.0005179242889217549 0.0003663278935137022 -0.00017838752519471575 1612 0.0008199376412019418 -0.00022603012047705 -0.00043713265035903487 3793 0.0007311140733944417 0.0003927478644361374 0.0007648605705700448 1598 -0.00025802523376702185 0.0016748734580155987 4.527428961642664e-05 879 0.00025500779018482336 -0.0004514863266038533 -0.002132752418700528 878 0.0006460547563557975 -3.3056072935778134e-05 0.0021536580108569075 1597 -0.00020089156186847983 0.0012704850701800708 0.0019951693115528475 1572 -0.001970326981420017 -3.71210599029173e-05 -0.00031883157913888084 863 -0.0011467509648135194 2.0960373475609152e-05 -0.0010862895128488767 861 0.0014463015258414551 0.0008288171562587253 4.409364595112835e-05 3754 0.00045793607087503646 0.0006911856438227356 0.00012562685174866497 1574 -0.0009780140096423294 0.0009026311153137888 -0.0011887706951230776 3043 -0.00024078442032430918 -0.0003431923840382952 0.00039392014932110135 864 -0.0014459102174400286 0.001621141733895474 -0.0011023591749957603 1573 -0.0006186832909358894 -0.0014102806805584092 0.0006898134707024144 1575 -0.002103052422098772 0.0012821274345864234 7.528865349987071e-05 862 -0.000560515652783275 0.0010867001372769026 0.0010842614066003285 915 -0.001496911288862074 -7.119377038268353e-05 0.0007599019275970288 917 0.0018017291426570114 0.00072816878589845 -0.0014552626850008956 3097 0.00010206180226822914 -0.0008750003714948337 0.0002591661904700021 1628 0.002138578769551291 -0.0008920197683749539 0.0013389221260853264 1643 -0.0018800976881222765 0.0010583381470946466 -0.0014744482961090474 165 -5.499025092474278e-06 -0.0002282612187458244 -0.00029311241365849103 1641 0.0006139135331143349 0.00015366984754939725 0.00015474183250502706 167 0.0004160178399054504 0.00025693649194784025 0.000900502743471225 1634 -0.0021840882923051808 0.0006870199254475792 0.0017812937592228582 1632 -0.0018052167744065897 0.001468672884924437 0.0006832898076119955 1614 -4.914235075514136e-06 0.0023189503864491285 0.0018459721369490929 1613 0.001314292853472896 -0.0004239705936985097 -0.001743029740833474 1617 -0.001997322134353225 -0.0015626614984127322 -0.0010573445860110498 1618 -0.0008951251682058532 0.0006933808315661548 -0.0016357161157687032 1600 0.0017071398219887762 9.902204223816375e-05 4.544273847770187e-05 137 0.0012516004377855195 -0.0016566261513123973 -0.002479497082273389 1605 0.0010539817061913314 -0.0008766764602298575 0.0007942188378705945 138 -0.0006760443756840212 0.0007572613503360575 0.000215987931088916 1606 9.735555652872873e-05 -0.0010918153547112774 -8.590209363756597e-05 1601 -0.00170630929301088 0.0009415145603102856 0.0018796808107053517 1588 0.000652778440501422 -3.2568812500103185e-05 -0.00015444260023767323 1586 0.0023991759081055538 0.00031626066576892964 -0.0008053916369975314 1579 0.00021432182819600435 0.0006227402270384326 0.0006223151841344688 1577 0.0004626295309690348 -0.000972149886762938 0.0021917192550527913 113 0.0007355769775356534 -0.0014452748282988365 5.266933113027834e-05 111 0.0012916755877415153 -0.002686070030845009 0.00021054770974582066 1580 0.0011884465152633046 -0.00012714170325797323 -0.0005394781925370074 1587 -0.0008243774032455178 -0.0010319385349094824 -0.000186844999829506 1578 -0.0010714553299361559 0.0011792972683641856 -0.0012858364239315752 1589 0.0016133826127044065 0.0001469724852723918 0.0010128554929634069 1642 0.0016998570713200615 -0.0011948711252126485 -0.001810922690769551 1640 0.000741472068359741 0.0006527198668545055 -0.0007021314376746658 1646 0.002106420603652002 0.0014274235322806865 0.0009057707143375264 1636 0.00045651552221915827 -0.002138460163413005 -0.00045879095589710164 169 7.006109108870099e-05 -0.00010484012811916125 -0.0016208095926744117 1638 0.0006780088023956926 -0.0011466189551736666 -0.0003214753329049882 1645 0.0005238603455926581 -0.0018145600030312987 -0.002020313875470838 171 -4.673408563193876e-05 -0.00039328577712641774 -0.0005234912376754209 1647 -0.0005641329830096456 -0.0024632490203084782 -0.0011808369304271934 1619 0.0023008807695030307 5.9393491950850945e-05 -0.0007062567418393247 1616 -0.0004039085485635248 -0.002373648439245664 -0.0004420268415674636 3798 -0.0002963727471792961 0.0016682607026607095 -0.00047341076875624796 1615 -0.0012509092503057834 -0.0019958501667816887 -0.0014563306098428672 3803 -0.00222875230638236 0.0005932861401242739 -0.0008083991039836542 1620 0.0008485514468278418 1.3365635894136384e-05 -0.0013060099571522402 1608 -0.0016296687092322714 0.0011449485681904977 -0.0017187173306326788 1603 -0.0009355161583616517 0.0012701728196405047 -0.0014929567813002458 1602 0.000314339307405911 0.0007441431642555016 0.0006214487669410915 139 0.0004129627114290089 0.001253799601055701 -0.0008947194988979799 1607 0.00058124146590023 0.0009129938801217396 0.0006708866834644716 140 -0.0006320362018121528 0.0012001634659113908 0.0005952702433905348 3772 0.0009441982057760024 0.000971134210768672 -0.0012926363791316716 1590 -0.0007643571848154998 0.0015819091983341406 -0.00014975140656107522 3763 0.0001449977552782096 0.0005121339583139578 0.0004975045449938191 1592 -8.786280366149637e-05 0.0006088475496595785 -0.0005973005740204765 1583 0.00032788320437014077 0.0007523640207970603 0.0003326637800067332 1581 0.0007593806032935304 -0.0009502730273104494 -0.0006006044700787171 1593 -9.996469783459189e-05 0.0016115425736344256 0.0001306393781514755 1584 -0.0017908834090380498 0.001285281712652342 -0.0001468432553101036 115 0.0022516007831598667 -0.0019260354617196222 0.0025675031469101638 1591 0.0016634707640855047 0.0001644986381055879 -0.0004813954709997144 1582 -0.0018462443961021842 0.001904607109562462 0.0007926849944675565 117 -0.001871594376730231 -0.0015376593593749335 0.000506947153998153 1644 -0.0008331167815352921 -0.0008527618506840523 -0.0023415838393396286 3817 0.0014394200388767576 0.0008501706643112342 1.698556569529699e-05 1637 -0.0003078428392888163 0.0011596233682110756 -0.0004497128714944106 1635 -1.4488247096872912e-06 -0.00014919509970840567 -4.735609575608375e-06 3826 0.000592987446706371 0.0014183639492113338 0.0017926962208502993 913 -0.000912661527127597 0.0007993294408635795 -0.00033870614866191484 995 0.001185771850639427 -0.0001997671346629041 0.0006680360608140732 1704 0.0008147595941749917 -0.001018872743634001 -0.0020133261930323394 993 -9.837013233411781e-05 -0.0011256545200894552 -7.620855088864115e-05 1706 0.00013409125563996625 -0.0005789960516101474 -0.001627823634907278 969 -0.00014718330750506606 0.0023035453525525433 -0.0009245572300843323 1690 -0.0019369061047819398 -0.00010391621917108006 0.000238771078290419 970 -0.00024312357545546413 -0.0007495904135296455 -9.374904017245798e-05 1691 -0.0015396141422424005 -0.001587229161535499 0.0017527252240424687 958 -0.00021688103014579313 -0.0007041924469132347 -0.0011416339184086325 957 -0.0018760049031463927 0.0007164335572706708 -0.0007012131553309777 1676 -0.0009257639445139068 0.0016422791627580694 0.00016386078910975155 1677 0.0011353921505600393 -0.0007747913330683068 -0.0010538847375085778 938 -0.0006948475475857823 0.002475280330625876 0.0005683251242480298 1649 -0.0018348975569134002 0.0004626687888340973 0.0009688398826405316 1651 -6.078582443039903e-05 -0.002071762257905907 -0.0012757889321107357 940 0.00042791728983919094 -0.001717552807050725 0.000755236120720371 939 -0.00022191338948207811 0.0007923716864430513 0.0005413432594242048 1652 0.0007703811289151536 0.0004431404010533874 0.0002967938435184856 1650 0.0002510646587159269 -0.0019106617093009159 0.0006903430572651453 941 -0.0009497838279681059 -0.00031066168644137363 0.0010629665617994818 3808 0.001986381581884851 -0.0003116783532104502 -0.0003606927583328628 1626 0.0009665291878190277 -0.0008760130365752323 0.0005409356758972703 999 0.0006380834262532852 -0.0008559992507769852 0.0006440042400543892 1708 -0.0011650791464329225 0.00028151419258068335 0.0004493770511144477 997 -0.001000440735508117 -0.00190330898563088 0.0009501950809660621 1710 -0.0022302049893133543 -0.00018391709384904683 -0.0009044774232420652 971 0.0018581301088036574 -0.00033059708844301676 -0.00014851573911327535 3874 -0.0009495726248975071 0.0015437066332321101 -0.0019385630994566958 3155 -0.0004289644707620021 -0.000603972466755314 0.0007179450231941067 1692 0.0018786510753261501 0.001300588372298546 0.0012464363118533947 1693 -0.0001272102094691973 -0.0005016172138263052 0.0015356337966398927 972 -0.0020908459618412846 0.00019039044786216838 0.0017512066093337165 960 -0.0010176728206741324 -0.0007769242489238065 0.0018746658692861233 1679 -0.0004476252162239486 -0.0019050291689530886 0.0002212419110506351 1678 0.0007552438711052389 0.0009567401690129364 0.0023510152673032808 959 0.001839054377366198 -0.0002047681970696717 -0.0011866180673689667 1655 -0.002090056998647857 -3.7322322898438544e-05 -4.951498951477444e-05 944 -0.0005628858283416435 0.00042435254612420236 -0.0010351091317914282 942 -7.308216415775979e-05 -0.0004810610396777473 -0.0007573144237020299 1653 0.0010141806532761835 0.002361732411905709 0.0007784594232891328 3835 -0.00010815202776827816 0.0011076052636979845 0.00037835848769926603 3124 -0.0017530028685048126 0.0004135241887667639 0.0007252587481141434 943 -0.00020565464245842098 5.326221520719678e-06 0.0008191500681383496 1654 -0.001094973013963033 -0.0005723430208159873 0.0003236997187686019 945 -0.0007874600427609591 0.0007961500782399242 -0.0013557540515662773 1656 -0.0011141734288605632 -0.0011556859401075828 -0.0004768478878859722 1633 0.0003565078237273956 0.001027098819694745 -0.0002438252778671866 1631 -0.0016536637102998496 0.0007689120363568958 0.0011537017716945473 1715 0.0009078189766762142 0.0016791604970829948 0.001073330866395538 1713 -0.0003801213356776896 -2.504286723451236e-05 -0.00031477090302131356 248 0.0003262106705496082 -0.0013942347139113001 0.000723862371085436 246 -0.0018768792919500934 0.0008405664578058942 -0.0009746694712826154 1722 -0.0005390067534743507 0.0009254403453497493 -0.0019908245522676196 1724 0.0014452052785716488 -0.00045721997647292924 0.0021389319421889876 1694 -0.0002863316292856244 -0.0008950535585530003 0.0021797781399304278 1695 -0.001265851271158754 -0.00203292813802877 -0.0016910606992291313 1698 0.0010033209727441925 -0.0006838720642311164 0.0004427229271687966 1699 0.002119460413429013 0.0008200319337423876 -0.001850097856956009 219 -0.001390065325393982 0.0015828496047225712 0.0016266161177556791 1686 -0.0010442532460747103 1.8749720547773987e-05 -0.00011471371024126577 1681 0.0006257046946398087 -0.0014105600610125246 0.0013058149292323469 1682 0.0017094460556775575 -0.001374092373938114 -0.0013804751830279337 1687 -0.0020056116662361453 -0.0005712673876496568 -0.002350647877270087 218 -0.0009748396258224627 -0.0005956623698087202 -0.0013157881449500119 1667 -0.0005670665777893739 -0.0016694505614613065 -0.0015995068175423252 1658 0.0004043766919164485 -0.0014454243915178328 -0.00045518382753404916 1660 -0.0008845147936247459 0.00012899541782869723 -0.00019095231587202204 1669 0.0010441300032034996 -0.0009321508000457735 -0.001362415194197669 1661 -0.0014948871271630421 -0.0013014462480866477 0.0002707094036169407 1668 -0.0004960516730594998 -0.001200202831277736 -0.0006226340626757651 194 0.00037094839310009746 -0.00015537931105086668 -0.0006897409090466534 192 0.001025589301913846 -0.001155971302848744 0.00018937829312411399 1659 0.0006804563536000048 -0.00017377487380223849 0.0008099013002314901 1670 0.0004894702443148497 -0.00042541262494328507 0.0003658979235597105 196 -0.0010660507807464536 0.00023825860794031949 -0.001798380124767721 1674 0.0009170008721579215 -0.0002646680209883877 -0.0002345656796123041 1728 0.0012165195794013334 -0.0009353932750387599 -0.0005365360634853664 1719 0.0003751034566348225 0.0021194386760066057 -0.0006870349270280301 1726 -0.0015249493439799082 0.0010342131934946053 0.001961297279591928 252 -0.002222121511430342 -0.0012874580385338831 -0.0006842499919325957 250 0.00017052138656872265 0.00044585576900760954 0.000292782320230698 1717 0.0012513160794694867 0.00015996952343043857 0.0007255951122716008 1701 0.0013719626028587393 0.001151108089661689 -0.0021532677658472827 3884 0.00196197685626753 5.0440242716864956e-05 -0.0013718185978047108 1697 -0.000104358451117066 -0.0018350154232332663 0.0013511066915079155 1696 -0.0005102202853603981 -0.0014716454919505057 0.0013442321687173867 3879 0.0010418308499576352 -0.0005855381518277999 -0.0015180568232583654 1700 -0.00018168290683275902 0.0010977440808911353 -0.00011321562489913998 1684 0.0019299111095964858 -0.00034944328328662816 0.0005667895790907723 1683 0.002236724618565581 0.0011393116703109444 0.001588731150098121 1688 -4.707030787159082e-05 -0.0006851352362303885 -0.0015349462119165404 221 -0.0026151521120879396 0.0028130372380794984 0.0009365807460532218 1689 -0.0003099013255537654 -0.001723240988733284 -0.0016110839550114143 220 -0.0027410605111058586 0.0005302816290256606 -0.002355432823683664 1671 0.0017756246034464915 5.3175707002380175e-05 -0.0002607672622696981 1664 -0.000621287777308791 -0.0007048186353521112 0.0020125121546785262 1662 -4.8897195533225905e-05 0.0013803756167717982 0.00014647387016757335 3853 0.00035922827704273626 0.0008805396579390742 -0.00039282212028602477 1673 -0.001039462066209996 -0.00013077449706637965 -0.0010732742086900203 3844 -0.0007972563881201993 -0.0003502606048780446 -0.0005228356654837389 198 -5.1144258547709646e-05 0.0006003972648552227 0.0001742514615914487 1665 0.0001546135099242935 -0.000112358741313821 0.002637999245951085 1663 0.0010896117775962204 -0.0005671517654696934 0.00038886374391730117 1672 -0.001799042051326406 0.0009501083362444276 0.0012324772387039067 1046 -0.001037767571722789 -0.0004911510657340165 -0.00019581051546373966 1048 -0.0011530317446937807 -0.002249413354392608 -0.0015211337549935829 1757 0.0015865324218439477 0.0008735895309293316 -0.0005581675634985417 1759 -0.0024650115333258787 -0.0013094507973577818 0.001775007438654463 1049 8.34624739997048e-05 -0.0002663527899645177 -0.00018018690332538296 1047 -0.0007915655169051979 -0.0014981543006256804 0.00027549389147543983 1758 -2.9817684417321228e-05 0.0005417696120810797 -0.002546875480085194 1760 -0.0015582968135390118 -0.0003610807885491389 -0.0017799982912506992 1021 -7.46922494579169e-05 -0.0025992858084377935 -7.518535530684663e-05 1730 -0.0008954210838298265 -0.0012691105474573817 -0.00033947933760434287 1732 -0.00044022543559149737 -0.000926042685121576 3.0562352638720345e-05 1019 -0.0016176440871591186 0.00129937915033049 0.0001673870221496226 1733 -0.0023098701753838657 0.0008233189135192677 -0.00021808334586910028 1731 -0.0015272754407486934 -0.0004125532442101538 0.000405078189773167 1022 0.00031931364505714214 3.0607782510089156e-05 0.0014266350497219933 1020 0.0006371834280705531 0.0004925105226973921 -0.0007018543228288498 994 -0.0006959301984760975 0.00044597543786251885 0.0004752670763873859 1703 -0.0005569384897193338 -5.127363505143362e-05 -0.0005696593418313771 992 -0.0003475233866544357 0.0004494456511638799 0.0010810024318732713 1705 0.0008353299637606994 -7.145029518581831e-05 -0.0015491272783219054 1052 -0.0017249383428168666 -0.0012553989071832352 0.0012156229389599226 1763 -0.0007802170621584105 -0.000403019220659891 -0.0006194750327824289 3232 -3.309602099008883e-05 0.00018513983003565042 0.0016236009511910753 1761 0.0006996908357400541 -0.0009470237205369389 -4.889980337059469e-06 3943 0.0009125427592970243 -0.0016798978483804701 -0.0007770109337937057 1050 0.00041122631355365005 -0.0008689712964914961 -0.0006759159229960336 1762 -0.0007476964534514621 0.0006338276901278405 -0.0008120801904737294 1053 -0.0012388260585609076 0.00025275433942647857 -0.001037304774663004 1051 0.00011941101284097463 -5.714811160391006e-05 0.0002864238074261067 1764 0.0003856059785371296 0.0005814940225576607 0.0007036987711024538 3916 -0.0003936292742958314 0.0010280240101068188 0.00259790753664642 1023 -0.001795947899691095 -0.0017175044847358711 -0.001573226995814669 1025 0.000279908354137929 -0.0009882518982824915 -0.0005649443377759228 1736 0.001710316062592341 0.0003304833276416843 0.00035931678939851285 1734 -0.001132385103747096 0.0005520925490225591 -0.0013548965274991142 3205 -0.0010683054861055927 -0.0005380594153524129 -0.000625160127621384 1735 0.0010754354513296594 0.00027759724341948604 -0.00041586324434488963 1737 -0.00048658966514751796 0.0001481636674098884 0.0005929144081448928 1026 -0.00016971631133965944 0.0004428977367413906 -0.0007630808710109739 1024 0.0004563562034289485 -0.0015245484249592632 -0.0008129020177607759 996 0.000203439971226902 -0.0013434487321524952 0.0013671115483939891 1707 0.0019465560194597187 -0.0005667725377318451 0.00011997150454653467 3889 0.002389672508274756 -0.0009978247246773461 -0.0017456596566905562 1709 -9.766888191014298e-05 -0.0007111742963177638 0.0014419920943277624 998 0.000711975396618698 -0.0005811216664842201 -0.0006059207911173726 3178 -0.00044980634759632376 0.002033124981393684 -0.0009290313814318317 1766 -0.0006257155906193727 -0.0015108680606574208 0.0008638894465037344 1775 0.00039555926064398 5.8695369074241376e-05 0.000387379836449717 1768 0.0018645190981092037 0.0009853259441236605 0.0014196303931786963 1777 -0.0008745891062386548 2.888363089999105e-05 -0.00133410695153635 1776 -0.00044078277387419847 -0.0013132125626577357 0.0013309886107871084 1767 0.000729724971278602 0.0017894863198861372 -0.0020545779722501807 302 0.001282865702234835 0.0005755086773662251 9.999930069235505e-06 1769 -2.8970764615907172e-05 0.001118869316100717 0.0020187723927283037 300 -0.00010589719639948281 0.0009192557050491823 -0.0013807230414439758 1778 0.0007232556923750431 -0.0021206961847344964 -0.0011867970593092323 1739 -0.0005828764556874915 0.0005084808485648026 0.0006345259502525558 1750 -0.001998426051469316 -0.00020262773355491878 0.0016589405490482728 1748 0.0021508404516218144 -0.0007392531655696213 1.535109923447896e-05 1741 -0.00028658280272720823 -0.000181924762831034 0.0008196148282512258 1740 -0.001265051340252071 0.0014707312117076972 0.0024490925971634558 1749 0.0016688604453351994 -0.0004628595889854981 -0.00033820987245492364 1742 0.00019114642811425287 -0.002271114341411476 -1.2423289347815794e-05 273 0.0006814920712360729 -0.0003387784020498501 6.433086224409874e-05 275 -0.00015890971119931715 0.0004326155232779326 -0.0020640852805035277 1751 0.000259694601955464 0.0013098172075857437 0.001959807604252042 1712 -0.0003382597706098828 0.0007748238811641659 0.0011307043976306378 1714 0.001409965916555489 0.00023443841929680283 0.0005210675769154314 1721 -0.0001319761141169305 0.002302806391584441 -0.00044629765863228794 1723 -0.00180897551818031 0.0006652252890845349 0.00021678896589121595 1781 0.0008122486458815859 -0.00033052677632047344 0.0018416182526510467 3952 -0.0003331741225210934 0.0007197468611982508 0.0003703995402161513 1772 -0.001225635988681916 0.0016432867596038677 0.002660193719033149 1770 -0.001230637308780326 -0.0012911953231331335 -0.0005501313544638857 1779 -0.0007355416801067287 -0.0006322897717289768 0.0010963314673356865 3961 0.00014601732918517523 0.0010077563039214397 -8.48959747493383e-05 1782 -0.0005084547800735041 0.00020980455998895675 0.0010125071422226926 1771 0.00010928525387245928 -0.0011492373680931291 0.000644869591000279 1780 9.997080367204775e-05 0.0013798252111195005 -3.9872857961582896e-05 1773 -0.00019394505710233116 -0.0005350794457778847 -0.0010982478176811076 304 0.0004303964184488529 -0.0008700854383739587 0.0012432217009037158 306 -0.002068198096250709 -0.0006506922858106422 0.0008300697980754199 1754 -0.0015875712133984364 0.0009225995619205969 8.214658436341026e-05 1745 -0.0014906879495233927 0.000362787757498874 0.00017051774360616343 1752 -6.538235107377737e-06 0.0002736101380436968 -0.0014018462592159553 1743 0.0008086298228564549 0.0005002541558571895 0.0024662189962995837 3925 0.0012038415751756601 -0.0019904156657199615 -7.810370003720447e-05 3934 -0.0023567431879580837 0.0016339483024902183 0.00064908365019334 1755 -0.0005550037270379783 0.0010137561398863189 -8.988004128002765e-06 1753 0.00040236654933508906 -0.0007857245155149556 -0.0006610531810243434 277 0.0010039972697574102 -0.00127456589539449 -0.0008555216388393514 1746 0.0009289404332184655 -0.0012789477897976007 -0.0007097643199266862 1744 0.0005406594846624944 -0.0004111897107969304 0.0007280803921092033 279 -0.001968518413578835 0.00030953330880834247 0.001518465545699924 1727 -0.0027103576130706607 0.0014919800544098665 -0.0011327920000805502 3907 -0.001792265949386238 0.0012267067933004459 0.0016895302751865624 1716 -0.0003774241690724916 -0.0004694004292234683 0.0007755624912214676 1718 -0.0008113148240867657 -0.0011740503429478483 0.0006253856733525557 3898 -0.0025604069838022323 -0.0004884059746872709 -0.0015792762036372187 1725 -0.00022017755700133763 0.0011185267790917658 -0.0021593222957364076 1128 -0.002519297163123275 -0.0021906384458441476 -0.00010640698345295717 1130 0.0008433604054138439 0.0015524626552706473 0.0005448589734587804 1839 -0.0019890197905915244 0.0005248645486424647 -0.001453702289447736 1841 -0.0006354160045718884 0.0006223253151857291 0.0002565947862340401 1105 -0.00040853549236387874 0.0010528588313675755 -0.0002596240970745518 1104 0.0018487873063324257 -0.0008487486423809907 -0.0013679132136147742 1825 -0.0002539926403403888 -0.0008423697698169816 0.0014288450183990162 1826 -0.0006103837995585025 0.0010467800710067512 0.00048241869240421673 1092 0.0005781337387392729 0.0004277225443180897 -0.000952915203939421 1811 -0.00015608009035657352 -0.0005485110705378018 -0.0009572847669581387 1812 0.002148881182693156 -1.4357629859836378e-05 -0.0014145898516853483 1093 0.000159037746089312 -0.00048369351550380034 0.002528258547020396 1075 0.0006006381893040654 0.0012586598114204298 0.000797703784323396 1073 -0.0006606724356333472 0.0019347784146506917 -0.0006036178728410467 1786 -0.00030554634888478935 -0.0012825693810755256 0.0012831302743804393 1784 -0.0019237393582400722 0.00033334320987701827 0.0005802061751558967 1785 0.0009140516276976887 0.00019653358245185328 0.0008521806673922142 1074 0.000562132335362741 0.00028349819065395907 0.0001985691190731346 1076 -0.0015927043269321644 0.0008487885087559418 0.000882006408851493 1787 -0.00041433213189757804 0.0001679525132313995 -0.0005468987501665542 1843 0.00032920865086766055 -0.000730936574129075 0.0009573807797146122 1132 -0.0005680418067150628 -0.0011294869764816623 0.0017082470147506343 1845 -7.746656075039446e-05 0.002073335588266652 -0.0006221186921900257 1134 0.0014653385028747623 0.0023999924794268607 0.00042232135832975955 1827 -0.000662385233959421 0.0006337815668341513 0.0018345955165714049 1828 -0.0002579130941476966 0.0006309575112492183 4.5188592637253116e-05 4009 -0.0014990791852270583 0.00016183545129765087 0.0011671445239915816 1106 0.0008188357460083508 0.0005668500669362378 0.0027177734158452573 3290 0.00034212732914794654 0.001104214201180436 0.0008502368298618792 1107 0.0008179115197675896 -0.0005670319052337724 -0.001269512578275411 1813 -0.0013495210353141318 0.0003904189053857514 0.0001305469133042296 1094 -0.002042336970478548 0.00017462850078719667 -0.00047822687158049403 1095 -0.0026019306107721465 0.00026251682603566475 0.00032271826350962194 1814 -0.0017278072210583967 -0.00015307797740842866 -3.244274410274658e-05 1079 -0.0005253509949539498 -0.001303887788937197 0.00015899382903896596 3970 -0.0010776779605001362 -0.001873635979476079 0.0007436615393149096 1077 0.002299287435542349 0.000503792062888684 -0.0004860032824352925 1790 0.002257210621964515 -0.0004492735852004098 0.0012998850467318879 3259 -0.0018820065700977094 0.002121168734923236 0.0019988819192595366 1788 0.0007340415597660473 0.00041975978390149235 -0.0007824830266926894 1791 0.0011992716358675214 -0.00037642431503359707 -9.887000197643871e-05 1078 -0.0016911867628810787 9.396497553691859e-05 -0.000276079933970063 1080 0.0013139773677219603 -0.0010214154253830722 0.00015624526858217533 1789 0.0005997982080360492 -0.0009464495553075962 -0.00192660237753554 1857 7.315130305568713e-05 -0.0008019889331126527 -0.0005795900831860926 1850 -0.0009266932923176328 -0.0016198502613098053 -0.0008671111675851578 381 0.0005179902236452618 0.0012771595990033523 0.00022741931682006787 1848 0.001072318605429679 -0.0005185236481192524 -0.00033564678008109227 1859 -0.0003519107220461863 -0.00046531906886322335 -0.00035754566340328393 383 0.0006340220087293518 -0.0012471445486830234 -0.0016044322107297059 1833 -0.0005913444307101075 -0.0024198981052717767 0.0009506770769650486 1829 0.0015885175941629424 -0.0013039547185379544 -0.0011112205511396086 1830 -0.0005041996948740195 -0.0016726828455718796 0.0002509008625241558 1834 0.00013069909580770082 -0.0021254224444863744 -0.0013234192657357751 354 0.0008804326886195505 0.0004175140945121876 0.0003564905192940573 1822 0.001155300897393553 -0.001925697459483594 -0.0014309125217468965 353 0.00233856524080898 -0.0010518856367224632 -0.0007679828431494068 1817 -0.0011741808640207182 0.0013316471122946628 0.0001406962336482757 1816 0.0013767932358227924 0.001212514459022401 0.002481171028937809 1821 0.0003081102562393363 0.0026982577946750965 -0.0008884775465963746 1802 0.00023718182435479758 -0.0006508069513538146 0.000277280118976968 1793 0.0016723473603883763 0.00035345353849175595 -0.001862524895248934 1795 -0.0005604760875805385 -0.0008043666229213103 0.0004293100637620123 1804 -0.000716949845712603 0.0009661481958267038 0.001052212360470373 327 0.00014679850476741825 7.29846189869562e-05 -0.0009300091312118091 1796 -0.00047141892398157954 -0.0024308776345941573 0.0018958291874005173 329 0.0008715248659428171 0.00043280179281579567 0.001676888430030241 1794 -0.0009302011939413866 0.0012059690911297302 0.002627763625904235 1803 -0.000268384891537239 0.001293621289148503 0.0005454626786759458 1805 -0.002001549001619253 0.0007358495697022379 -0.0007347791002146309 1863 0.00023969835324033628 5.4785314645858506e-05 -0.001225890346041429 1852 0.00020621287657801666 0.002350346005880039 0.000882207838937306 385 0.0009503146460071482 0.0011223165676054238 0.0014819164134060752 1854 0.00028727316276274143 -0.0013022745693307284 0.0016649747430262448 1861 -0.0005711304631785089 -0.0010277993488657594 0.0022230610426358143 387 -0.0018120758810461009 0.001373213352004713 0.0005745768277557492 1832 -0.0010653225970907844 0.002447703057415713 6.439452898719406e-05 1836 0.0009714780891147336 -0.0019308719974463545 0.0014711141934478523 1835 0.001687911075445644 0.0008718224895023967 -0.00011120582968629066 4014 -0.0013571641308679331 0.0003293286379390864 -0.000571050400580516 4019 0.0018191517037287098 -0.0010906276414103238 4.5977568701147586e-05 1831 -0.0009958897067030605 -0.00024713873746234905 -0.0009905563715176255 1819 0.0026761533251137997 0.0012545517724132397 0.0006190945201019493 1818 0.0007677341203275339 0.0009824138316289724 -0.002397446898463078 355 -0.0013070914286546296 0.000642253793019362 -0.0010295482027651544 1823 7.959534438688285e-05 0.00018405466760154242 0.0001665278380983343 356 0.00189547718977797 0.0006637248506184818 -0.002122573170497787 1824 -0.0007792772107421183 -0.0008528184328003797 0.001000819733035683 3979 0.0004154826320255725 0.0011487842500467426 0.0026331905328138283 1797 -0.00039468186124329616 -0.00017486475851367618 -0.002756597959647287 1808 -0.00010597304690779046 -0.0008183666986498442 -0.00029628833286104994 3988 0.001189245707470646 0.001651858593746171 -0.0001524245168450216 1806 -6.905747376064484e-05 4.862125079691925e-05 -0.0003631849444448558 1799 -0.000548214685857816 0.002064191625555885 0.0011610977838342317 331 -0.0015467201715372797 -0.0006581355332690106 -0.0006718031902999792 1807 -0.0006930260100425969 -0.0011905859765265136 -0.0009483035351004588 1800 0.0005557857181526524 -0.000682485471500223 0.0018924801024521058 1798 -0.001146563046007317 0.0002773449615460662 0.0010464787693074973 1809 0.0006855860228437789 -0.00030843570580900014 -0.00015327714715389741 333 -0.0012455070373835234 0.0008558135734919616 -0.0017545508985643498 1186 -0.0007118097779713307 0.0015105046204061286 -0.0016598201780482174 1906 0.0026342740726276502 0.0025955564750990605 -0.0026523199358462154 1907 0.001491138334474076 0.0009290582908693715 -0.001251290056551789 1185 -0.002267235325036924 0.0009616165511071263 0.0012523927302270674 1174 -0.0015931190666039824 -0.0006509574795836163 0.0023586975700721317 1173 0.0008070705134392724 -0.0005647419898965513 0.0003012560334504067 1892 -0.0013657998598317533 -2.7344944875395483e-05 -0.0005866763075185479 1893 0.0002824887172684536 0.0009209145748996561 -0.0007654200210496628 1156 0.0008207626451587258 -0.0014063132454658722 0.000826400371682472 1865 -3.8437557213826835e-05 -0.0024183786346725273 -0.0005470287032584432 1867 -0.0007466355760582296 -0.0009646141699277526 0.0012416249499274613 1154 -0.0024893201385745075 -0.0009958141629773697 -0.00011247779765550256 1155 -0.0016620821882692089 -0.0006471849702275666 -0.0008034880117170681 1868 -0.0011452050192290518 0.0012723872589173867 0.001747744603809067 1866 -0.0003073564016541101 -0.0005564965491916959 0.00113339526678786 1157 0.0018668017436393016 3.5919921571848056e-06 0.0010152277473229213 1127 -0.0011050403447359497 -0.0009846087717267189 -0.00031702868323859375 1838 -0.0016797534852543326 -0.000608190972319522 -0.0005477144378218267 1840 -8.441570281101339e-05 -4.599042762790692e-06 -0.00029103486119292396 1129 -0.0022858877372576073 0.0018198304241059012 -0.002217006595788667 4090 -0.0006614739078915056 0.00015364026238366213 0.0013627264294904019 3371 -0.0016966546906382334 -0.0023600536050154258 0.0008870030978703803 1188 0.00017450657173306362 0.00041481132515031266 0.0016992131367002848 1187 0.0013592612147815281 -0.0014651476973727032 8.079668658239614e-05 1908 0.0010605559369234296 -0.0007666344287592809 0.00015611715130528752 1909 0.0005136483411849398 0.0005436078831797879 0.00020942845401537694 1895 7.685137285767894e-05 -0.00039076335125822923 0.0002276454578644773 1894 0.0004007943542434615 -0.0006360533090377834 -0.0017678251132622403 1176 0.0009839931835038025 -0.00018351324874962314 -0.0006061821216715732 1175 -0.0013981943642875961 -0.0008977624496176124 -0.0022601514559900133 1871 0.00029548349830960975 -0.0017745691420353459 0.00032867677686319207 1869 -0.0026904442203501 0.00010327125767024012 -0.00029483208960137577 4051 0.0011537687993706202 -0.0015558650005174728 -2.184780835073213e-06 3340 0.00018556864816836956 0.0009403661168153723 -0.00048810325919453035 1160 4.0627935192149526e-05 -0.0018409429206481499 0.0015578485887159201 1158 0.00087118889044388 -0.0013188599665138305 -0.0021037130220859625 1872 0.00040065472416412804 0.0001461797976380992 -0.0016415400529758018 1159 0.0010710947182190605 -0.00012355189556668348 0.0004831898867713549 1870 -0.0018967172846871974 8.883314661105527e-05 -0.0006602139858972383 1161 -0.0012900907363590285 0.0004602936382654087 -0.0015933648810110006 4024 0.00022347951060073916 0.0009801053018515455 -0.00020426382957473778 1133 -0.0006745411717205942 0.00031236666665225175 0.0012930823809663096 1844 0.00022794669334369423 -0.00026094306719531835 -0.0003416770961651313 1842 0.0001888082883347124 -0.0010794386054726844 -0.0012650350654884299 3313 0.0019055540006980578 -0.000696820529629777 -0.0011669602131136418 1131 0.0006699896472191133 -0.0008858131921976703 0.0007703663273222517 1914 -0.0011417695746906084 -0.0013792566388574257 -0.001096124324513535 1910 0.0007232856565830273 -0.00137506040092027 0.0011996323030874377 1915 -0.0009389778406345734 0.0008403571370974173 0.00021089504914057942 1911 0.0001325032266909586 -0.0006043216583786319 0.0008449960321535348 1898 0.0014073405750775517 -0.00024907912248382357 -0.0012362007133874338 435 -0.000591985075575504 0.0020271346166490962 0.0013535854312169387 1897 0.0004073586748188901 -0.002163676696999511 0.0003145848671796086 1902 0.0023915669685786586 -0.0005557963976789699 -0.0013373518209723347 434 0.0011936153106278104 0.001367954623732987 -0.0011609034767422189 1903 -0.00047953086003302183 0.001526852235470103 -0.0010256428043294605 1885 0.001236903103651276 0.0007117421342622784 -0.0002638189814265447 1874 -0.0004679808773231616 -0.00013477176761143633 -0.0007061999092825041 1883 0.0026922956216810677 0.0015116747034050232 0.001056179807556781 1876 -0.002127554078186057 0.0016577452676632665 0.0010695402986049731 1877 -0.000164356063655109 0.00022292770254943761 0.0001809355669159184 410 0.0017784977030841068 -0.0005493978724619259 -0.0020671900798208465 1884 0.0013689300470648156 0.0010210056983699172 0.0021985168436764505 408 -0.0006956731259496986 -0.0013717522068411169 -0.0013081625418929449 1875 -0.0011757955451078604 0.0001187331081847437 0.0007618886417999665 1886 -0.0005163451488799708 -0.0006570732858895783 0.002391320286696 1856 -4.7444786612983736e-05 -0.0017352795128248231 -0.00131171033929414 1849 -0.00043231079928911047 -0.0008180986367200197 0.0006024150022715837 1858 -0.0003813293539391108 -0.001236609790794709 -0.0011380186077087234 1847 0.002038339655826468 -3.489499950689756e-05 -0.0010578268722302013 4095 -0.00046423732841479595 0.0017191445624445084 0.0011649585579217635 1917 0.001511816128851947 0.00024402735230372868 -0.0009189900160010908 4100 -0.002055875894937043 0.0017731606524697572 0.0009217456257257492 1916 -0.0010043896277005082 -0.0015090279361096252 0.0009077899858697849 1912 0.0017367287783795371 0.0010812270659952882 0.00039308861012130763 1913 -0.00010311798636994168 0.00168885226004866 -0.00047954404142314393 1900 -0.0025331455560048837 0.0005256225640905627 0.00037067650777788974 1904 -0.0008744241968797798 -0.00037847705633154945 0.0002885491381906392 437 0.0008544708602272514 -0.0010139258106080223 -3.325572482008849e-05 1899 0.0009850991498509803 -0.0023540692836967023 0.0010247958357648395 1905 5.40154845635743e-05 -0.00026226253102669796 0.002242596496550044 436 -0.001984600132741913 -0.001716699188172827 0.0007169156313945311 4060 -0.0012878816999858035 -0.002523808786277474 -0.0002226880085463962 1889 0.002330659426027806 -0.001069355673593259 -0.0006958892596114058 1880 0.00039145023467894663 -0.0003195220514957244 0.00015775555020720769 1878 0.0014149521383579773 -0.0017476100917979093 0.0014999168787150964 4069 -0.001912801755530974 -0.0014723189089328134 0.0006135280406727552 1887 1.123499948884265e-05 0.00020069026076554436 -0.0008459508854433986 1890 0.0005567811752392481 -0.0008781244711871638 0.0006023694931346007 414 -0.0012075928398888394 0.00024452433350146264 -0.0006761651839919556 1881 0.000396814955689082 0.0010815979902352698 -0.0008125937719302271 1879 0.0021757513907693696 -0.0008084016953496403 0.00012541372061690122 1888 0.0007759973718950701 -0.0010435345474959215 -0.0005877146499385707 412 -0.0016380927079149366 0.0009511571759999054 0.0017811554755058864 4033 0.0002258166506985855 -0.0016937050918425388 0.0002712970378845052 1853 0.00018415230935831103 0.00045720308870059157 0.0019335044926003348 1851 0.0004529500888833084 0.000682668132475341 0.0013149358671931395 4042 -0.000507180681994196 0.0003326330092824621 -0.002151005762873586 1862 -0.0015478036497903792 -0.0015686237063192226 0.0003154757939341957 1860 -0.0008785886449655005 -0.0016640614135832806 0.001972567446834452 1263 -0.000843332796851552 -0.0005772716396417017 0.002038117955740844 1976 0.0007103258683234276 0.00022004330951724783 -0.00021442131178659569 1265 -0.0017387080930580906 -0.0011087124604333613 -7.72448536210924e-05 1974 0.0012001781950756638 0.0003666802924146271 0.0011788758285813023 1946 0.0007664979945231461 -0.0003228471723829172 -0.0004887883436569698 1948 7.09120816761066e-05 -0.00028209756054304127 -0.00011016062140569143 1235 -0.0006242849330556138 -0.0003235977589424576 7.898226776364623e-05 1237 0.0005815963387397777 -0.000382007220385699 0.0005670419489927051 1238 6.43045688468095e-05 0.0024037401231679417 -0.0007667979798013572 1949 -0.001732031150916647 0.0025660723650495995 0.0008517637101496357 1236 -0.00042215234739030475 0.0007668562140418587 0.0006872329192350595 1947 -0.001484700731474854 -0.0010599990748817606 -0.0014538360497694386 1919 9.000868442921519e-05 -0.000558675192027504 -0.0007530845094444781 1921 0.00020429845675324623 -0.0021803277615563476 -0.00026252528768939433 1210 0.0006810094199946657 0.0022718039869826985 -0.0001878898782499065 1208 -0.0005888747961817246 8.082246912429598e-05 -0.0006607551028762642 1211 0.0018355614263722473 -5.697398542729671e-05 -0.0010700098598302665 1922 -0.0003156817881534947 0.00047191512828572216 -0.0005497410535528051 1920 0.0019655937074871885 0.002086377544533567 0.001348178901325806 1209 0.0008220567722251498 -0.002418082927998838 0.0007006098298782113 1269 0.0003183306068554885 0.0001046894435905736 0.00021151921023361163 1267 -0.00015128709375957335 -0.0005875376325096425 0.0007571488125814222 1980 0.001650856537924746 0.002030874720320793 -3.146649306884613e-06 1978 -0.0008156604110377481 -0.00021064883564289808 -0.00046399038768258597 4132 -0.0007707953500118437 -0.0009098089039395567 -0.0019291808249481477 1952 0.00021376566507871447 9.488437838761285e-05 -0.0007172244207037615 1239 0.00028147994308523085 0.0006243606486601432 0.0020021747086089825 1241 0.0013897787008546837 -0.0001019568221344026 -0.0018866920548656608 3421 0.0014685655002064624 -0.001019024898243639 -7.614195398416256e-05 1950 0.000681016756448913 0.0013184846678145389 -9.567272815393687e-05 1242 0.00041831737165748915 0.0011843316464395749 -0.002276884672014761 1240 -0.00018255319212432796 0.0015507184098239475 0.0003688888697967839 1951 -0.0015602706180519491 0.0013567949698506266 0.00011986037159748245 1953 -0.0013785712334786241 -0.00037236764869933553 0.0009079393914433406 3394 -0.0017475039755543847 -0.001271969957220907 -0.0007008850756702754 1925 0.00034735731849871467 -0.0013545374424697063 -0.0015661240565228531 1214 -9.986986088979721e-05 -0.0006879955641464681 -0.001144740302939652 1212 0.00028298027682859364 0.00015319201634936622 0.0011436623094397637 4105 -0.0012359270780637885 -0.0005029907779526495 0.0013570956214556341 1923 -0.0019153135590450174 0.0009992032320654022 0.0016307656316480314 1213 -0.001385986936603315 0.00015568297710652837 -0.002095815181789784 1215 -0.0003918932019291422 -0.0022051815633389077 -0.0005420804386991266 1924 -0.00167319416327014 0.0007796371288193325 5.474424294443141e-05 1926 -0.0011869324207551503 -0.0008208876435686981 0.0006272982379694262 1994 0.0013901035596764087 0.0016598802579422252 -0.0004241210273564734 518 -0.00120023960933574 0.002002885192141402 -0.0011203258946183648 516 0.002220325671158258 0.0017330810587472966 0.0004205587946160456 1992 -0.0007986843753524564 -0.000908118404918868 2.620764211135832e-05 1985 0.00043694869878265353 -9.99963953102704e-05 -0.00027763761531095774 1983 -0.0020371824950563364 0.0005459459868664388 -0.0007551756866821877 1957 0.0012079650746100463 0.0005978587940038231 -0.00019329893195838823 1966 -0.0010890073715193911 -0.000511329557059463 0.0010878693792914233 1955 0.002303779975467075 0.0006334305630264187 0.0012570040880140688 1964 -0.0006689584086899711 -0.00076996142489197 -0.0006951367031852323 491 -0.001168307979937873 0.0019452485519940773 -0.0022199014048328546 1956 0.0003851826149164469 -0.0008697839750133377 0.0014496753317697758 489 0.0017058551654991693 0.000871540374806924 0.0008148467005597397 1965 -0.0009410336083964467 0.0014014117501568056 -0.00042857687315714014 1967 -0.0003198381078591457 0.0005383888223359717 -0.00022209150932980815 1958 0.00045730613988971547 -1.5995817480472622e-05 0.0013304995685708137 1939 -0.001723986320709567 0.0016480970374840474 0.00010671061133446231 1928 0.0018597593044485004 -1.0667883865976067e-05 0.0011391773901378913 1937 0.00030727255867266925 0.00015850621044607776 0.0018738150199973749 1930 -0.00016858438197919746 0.0003481803138800322 -0.0015322249074544785 462 -0.0010474725514528513 -0.0003145162070349579 -0.0005189625063591879 1931 -0.0015096905485022561 -0.0007157220514337902 0.001373303553894914 464 -0.0002193562959885173 -0.0017692288100410476 0.0017682056729694385 1940 -0.0011284653253279978 -0.0023363633188123586 -0.0013461800685336412 1929 -2.121676409201547e-06 -0.0010398628302098803 -0.0001788519058231264 1938 -0.0009635040565898772 0.00215548330086491 -0.0002551367147650461 1935 -0.00018096472541970416 0.00046666220389115305 -0.00038020372294308383 466 -0.0014533381669758593 0.0004021064894705165 -0.0012997140738842913 1933 0.00037811696842460826 0.0017115439932461067 -0.0010477311299619458 522 0.0001037375426700838 -0.0009652653943053663 0.0008996325382236465 1987 0.0015526814012313923 -0.0003722744220573018 0.0008403001968695834 1998 -0.0005517909402123494 -7.192397784630902e-05 -0.00255904968080985 520 -0.00034949825786120847 -0.0006421946473828061 0.00011503320749295864 1996 0.0023166025413417857 8.258233655329596e-05 -0.0005505628036634085 1989 0.001652643261634715 -0.0025859789235815377 -0.0015008892513820999 1970 -0.0016118969126049337 0.0009361738698561958 -0.00035154655392029266 4150 -0.0016743571675881448 0.0009887756349795847 0.0026385912381984384 1959 -0.0007053599084386501 -0.0005957874990169735 -0.00016384153460258146 1968 0.0022572092591051107 0.0021164215199528124 6.655172475391921e-05 1961 0.00024339240790950982 0.0006534213884378285 -0.0019119440489803023 4141 -0.001796903319285229 0.00030401848167416505 -0.0006703358119259483 495 -0.0009460757638610262 -0.0012141678729616872 7.788967756247817e-05 1969 0.0013333987530695988 2.6805018415777446e-05 -0.0002594269297967835 493 -0.0011245800609100162 0.0014437076672759832 0.001994651751038749 1960 -0.0008793323222610187 0.0013055093225306405 0.0008912267637301112 1962 0.0010686586914263419 0.0005760349606913644 -0.001373118520728269 1971 -0.00036331568357044256 -0.00020490992913698661 -0.001269686914551797 1943 -0.000891583933591797 -0.0003171238323318588 0.0002563583851287665 4123 0.001762605325308466 0.0010946907787596427 0.0010293645494638972 1934 -0.00027785006170554297 -0.0015275436636449549 -0.0015380016609632804 1941 0.0020300445096609237 0.0007750636571399798 -8.182386201415945e-05 4114 0.0011718466439486683 -0.0002490727319490148 0.0008921356558483622 1932 -0.000985176253139292 -0.0005854208612552855 -0.001184340130831028 468 -0.00016845037298108216 -5.983402109152993e-05 0.0007976412811207343 1942 0.000629048501720604 -0.0009683071175389975 -0.0005243982459862799 1944 -9.894491773283038e-05 0.0004080632963609958 0.002220405223628208 2057 -0.00046991174047333406 -0.00016119862557603394 -3.0153672130679405e-05 1346 -0.0015678742592451062 0.00014753078393454813 0.0014106549945081222 2055 -0.002632399712269572 0.0023235101720908533 0.00023325196928047367 1344 0.0011700355459951747 0.0008155497174114844 0.0020183271308233065 1318 -0.0002747428354989642 -0.0021107168684384933 -0.0007045467010714342 2029 0.00035482458529463275 0.0004795786256205298 6.327744452307063e-05 1316 -0.0021822369717023954 -0.0016422336023460902 -0.00023483255288344354 2027 -0.0007067278418181822 -0.0008296336235812996 -0.0009001487118316062 1319 0.0010709428552389574 0.00040517463105737834 -0.0009132286844872273 2030 -0.0010244914966254539 0.001295252695267841 -0.0010447189401588362 1317 -0.001446909420868053 0.0006692058108088839 0.0002553422632927315 2028 0.0009219807380518249 0.001395405830511511 -0.00024625631751646736 2002 0.001855139001116818 -0.00036941102506352855 -0.0010552983791777579 1291 -0.002280991970810001 0.000554251432702079 0.0019113241602371925 2000 0.0015141575817190186 0.0009171358318667243 -0.0019948600114890066 1289 -0.0005631302247044365 -0.0026965751916907133 0.00036327007167509854 1290 0.0016298916929838442 0.00020658368270971492 -0.0006039225949170991 1292 -0.0012514666366145826 -0.001551924626978864 0.00027419871609955554 2001 0.0016440930104709055 -0.0001919025408102928 -0.001317836332525751 2003 -0.0009754938684399905 0.00020586673597091843 -0.001371021128100677 1973 0.0020778107510389734 0.0006945462628829828 3.20438865424389e-05 1975 -1.733956433751959e-05 0.0016196057229206937 0.0008514614310197919 1262 8.986085822831674e-05 0.0001959648618513883 -0.00023283505354956173 1264 -0.002211356066396577 -0.0007853188658372961 6.085949213163028e-05 2059 -0.00029512882086935727 0.0003357497297655928 0.000528551580257228 1348 -0.0005085515449454816 0.001133877374593093 0.0007543878767020927 2061 0.00044104647278043877 -0.0009924012016103221 -0.002529077339809713 1350 0.0002129983232097279 0.000679970790515058 0.00038521790786989193 2031 0.00026622330065183167 0.00018565572485410454 -0.0019547596505221383 1322 0.0017391224702290541 -0.0020744599171791415 -0.0014324488906515501 1320 -0.0010246756338458693 -0.0018206598819001172 -0.00033153056967267754 2033 0.0011265742363487955 -0.0002657981624292912 -0.0007563955495800984 4213 0.0013793031628358922 -0.0008176947724316857 1.0987733336066143e-05 3502 0.0008359784166334914 0.001790386359234246 0.000658449619636928 1321 -0.0019435452782098346 0.000822163418316667 0.0018571960875387644 2032 -0.00013009771487296684 -1.534594298265718e-05 -0.0008514602636092829 1323 0.0010738291162233303 -0.0003234971534783813 0.0009365005993776365 2034 -0.0003925651278117114 -0.001050019295676424 0.00030973331956993754 1293 -0.0001496535004261979 -0.0003218921615451148 0.000358004216286083 4186 -0.001433563835596513 0.0009235313832230108 -0.00028852690801901555 1295 -0.0013433139366456968 0.0013203644028186522 -0.00018450954289702325 2006 0.0006120251932919822 0.0010471339078522018 -0.0011538652334646957 3475 0.0004238835921395374 0.0011609806785328977 0.0006499268964133199 2004 0.000837397642067311 0.0005535970013682012 -0.00011896777253934975 1296 0.00018166474572798457 0.0009712410866407629 -0.00041285669119341486 2005 0.001234532963760381 -1.3836672829513168e-05 -0.0014160136679903105 1294 0.0016749493827020513 -0.0019558758261562286 -0.0019757910420435914 2007 -0.0014119324599427279 0.0013482713409329675 0.00042265115458852906 4159 0.001804840225757393 0.0005732666700949086 0.0003770215880857402 1268 -0.000151312399293508 0.0019650622976720386 0.0007071136857201435 3448 0.001208910927801577 7.004179663212476e-05 -0.0009951856383064919 1977 0.0017359634415636722 -0.0010247835888743653 0.00151544256944141 1266 0.0017174031096967822 -0.001261608683882551 -0.0005417014472260006 1979 -0.0003255070111743821 0.0015097280248009069 0.0006073542227075304 597 -0.0005035647247827052 0.0014921891275265949 0.0019687272272796022 2066 0.0010411910690964787 -0.0020672266649739385 0.000625000638304295 599 -0.00044130941160103014 0.0001631507662148879 -0.0009644698635600836 2073 0.001658469744655416 0.0010886059328135671 -0.00023265960553545172 2064 0.0013262436203065758 -0.001873097332841709 0.00014908505158690562 2038 -0.00013528862578398833 0.0006650377033404842 0.001116104100646008 2036 -0.0017318478223656143 -0.0013722179767492373 -0.0005589811087849589 2047 -0.0004520169126115273 -0.0015960663866289835 0.0010754403528431388 2045 -0.001198825607789575 -0.001224158448896164 -0.001964333676838193 2037 -0.0008186514318461768 0.00035237236007317277 0.0009513296584036359 2048 1.9928146497408174e-05 7.027437835645809e-05 -0.0015195134900475014 570 0.0002567301684903867 -0.0012711546903853377 -0.0010175770679789712 2046 -0.001519999539957038 0.0017218720070346595 -0.0014143480670542367 572 0.00047844392633949984 -0.0023262893733664238 -0.0014466561467383686 2039 0.0006133386068261923 -5.105808298304197e-07 -0.00028537455257634636 2018 0.002021625523658037 -0.0021396946386234273 0.0006670817083149129 2020 -0.0007939183722659908 0.0005011083363139696 -0.00040845014322125417 2011 1.942900376921501e-05 0.0006815191022520989 0.001829892342741646 2009 -0.0025500828339505167 1.1086988051709455e-05 -9.105211501934246e-05 2021 0.0003527425877855239 0.0010215218853447778 -0.0009458610833163435 543 -0.0017549333650806282 0.0012637985794011057 -0.0016180859065029168 545 0.0013078964118121896 0.0012167844095163816 0.0022645042348025265 2010 0.002527675477972919 0.001153908187884925 0.0015534390740202535 2012 0.0003242556400012914 0.0014329031448770105 0.00019874614474562832 2019 -0.000529987318831474 0.0023410098746152437 0.00027932920832087404 1991 -0.001995463708849202 -0.0009767007606515969 -0.0011649069230446514 1982 -0.0016979649167176056 0.0006488774916846353 -0.0007311021953624905 1993 0.00020857769659564807 -0.0018154758476546492 0.0009864474733790917 1984 -0.0009560180316068871 0.0015148131351761574 0.0017048791330500138 2075 -0.0007502483006130737 0.0018082994135858537 -0.0008632263421638807 4168 0.0009412747542069892 0.0001629365337622703 -0.001018848786854259 2077 0.00012240944827784185 -4.6617159658689363e-05 -0.0012640526117827268 2079 0.00035924747010555814 -0.0008756856114788065 -0.00020308391514343603 601 -0.0002905087479404952 -0.00010199136356942289 -0.0009591267632473072 2070 -5.4071615938759785e-05 0.00026260635939532066 -0.0009751990044856952 603 0.0012024344520422609 -0.0020979281299783885 0.0020783390778845168 4222 -0.00012836741777035574 0.00017217197111125092 -0.0002357653259466415 4231 0.0019576799560266337 -0.0007781155278843631 0.0010846812833724255 2051 0.00034536630255710974 -0.0006967513366038141 -0.0005714960279437989 2042 0.0018853496182837342 -0.0005802681717389931 0.0005888867602351138 2049 -0.00016649612584273307 0.00035515493556182733 -0.00010788656656168685 2040 7.112372837904802e-05 0.0017099646367034224 -0.0018128455804599427 2050 0.00015814845355922706 0.001941701253892914 9.247751770895263e-05 2043 -0.0005020728084430009 -0.0005894649916904413 -0.00020981340293114314 2052 -0.00011954628923786488 -0.0010677272238252314 -0.00019315966614723529 574 0.0014207352014308854 -0.00010113117650588246 0.000835704880295841 2041 -0.0007167894279650159 -0.0012688959919293944 -0.0004762246139046612 576 0.0011135633444901815 -4.560148518926196e-05 -0.00111246662771435 2015 -0.0007717548742430028 0.0003241285089450595 -0.0005954664911216462 4195 0.0018064682415271421 0.0002272632553874393 -0.0024128494697794327 2022 -0.0011432488316869016 -0.00034844284325931006 0.0008387422206840201 4204 0.0010876727322968575 -0.0020297097934115116 -0.001123037137518509 2013 -0.0005696200484000213 -0.000471925288113198 0.0001134905038113986 2024 -0.002219366381033108 0.0015728257714490304 0.00022351470329376412 2016 -0.0013252023401740384 -0.0011381769157040283 0.00254922169119663 547 -0.0002819153534476365 -0.0008362992270698073 -0.0008834542863047684 549 -0.0010074760721887161 -0.0004853740706064146 0.001146788640838734 2023 0.00042033400525483136 -0.001480754134194481 -0.001487822637746776 2025 -0.0006829071916792089 -0.00041439981469765046 0.002747602765782468 2014 0.0008821492986651245 0.0004330515008841712 -0.0009317597032502606 1988 0.002034413674017082 -0.00129145470227813 0.0005182634671188081 1995 -0.0006547310796385093 -0.001375502829254654 -0.00013696210208380476 1986 -0.0005375350141875223 0.001263819123322855 -0.0006899313885097068 1997 0.000196462792929261 -0.0017869449483064953 2.7653204164165487e-06 4177 0.0008625685517497077 0.0012934002274471923 0.0010949729960875228 2068 0.0002478126022568744 -0.00029506206808291367 0.001732813024698302 1402 0.0006462715003580474 -0.0011744949477913696 0.0018111406936719987 1401 0.00047914804249167857 0.0020823643086925075 -0.00042197264508348127 2123 -0.00154121783871053 0.0008769472513096622 0.0009703605069807193 2122 -0.0005734310212755017 0.0011099785707972764 0.0006832190568252147 1390 0.0013829730447612212 0.0008084939170793703 0.0009016587958338002 2109 0.0006358071108096424 0.00037813768726144845 0.0015184006093170498 1389 0.0009618938274575117 0.0006199957069512842 -0.00036679651000693855 2108 0.002099291575577662 0.0002223291010763777 -0.002125815688298415 1372 -0.0010319835830262104 -0.00012669172770275782 -0.0004303516631207981 2081 0.0023265680293059333 0.0011593643413531176 -0.0020104710705297953 1370 -0.0008690746152958616 -0.0005887699179822337 -0.0009831852105711076 2083 0.0008045399234267534 0.0008789292507724593 0.001974658217289049 2084 0.0012124599385167573 0.0006476993245919573 -0.0004662108400974019 1373 -0.001709985664867165 5.295862939585106e-05 -0.0013912189612831285 1371 -0.0011439820766212007 4.700296768680415e-05 -0.001491471382937885 2082 -0.00040035113391516755 -0.000559761198845161 0.0002267909420118415 1345 0.0005137290375083676 -0.0010377139037841693 0.0012079840390812895 2056 -0.00024291606064867697 0.00023255176412896649 -0.0022809420637520286 1343 -0.0012975886584526398 0.0009435784331614473 0.0002657537071647318 2054 -0.000376859021141299 -0.000941691356042112 -3.959917489241779e-05 3587 -0.0015782582279054147 0.0006664174770899134 -0.0019746938538885866 1404 0.0003912904151703474 -0.0001673807664426373 -0.0004474556627417103 2125 0.00023728354952123166 -0.0003130157090365604 -0.0010922666631666066 1403 0.001073196496820917 0.000556007017374533 -0.0002876474733268053 2124 0.0005948088244524606 -0.0006741986711704233 0.0009072747656063398 1392 -0.002169825323237564 0.00029427432697616356 0.001101648658973106 2110 0.0012020377427673537 0.0012799802024938017 -0.00023655254551491808 1391 -0.0017738950104820611 -0.0018196821653545276 0.0008208014730537744 2111 0.0004060113027631643 0.002059538798975727 0.00043961571181420954 4267 6.107382267317007e-05 -0.0014351314720467663 -0.00027008736544026444 2085 -0.0008474464550092516 0.00036255562424309393 0.002372451942980087 1374 -0.0022739942504404753 0.00010740623386303137 -0.0008124381522427548 1376 0.0014907898811813123 0.0006612511052941396 0.001801402496996689 3556 0.0010622615903981125 -0.00017439701662786723 0.001961518701720782 2087 4.684573718696805e-05 0.001932756648726711 -0.0006914549815822534 1375 0.001129247632367236 0.0004977149586018398 0.0003063985334123935 2086 0.0028547798000487633 0.0008214359736061481 -0.0009129765735853041 2088 -0.0010753342381340624 0.0011657793846646888 0.002258796718843926 1377 -0.0009854647218747485 0.0010437207232481564 0.000561570842453053 2058 -0.00013268704027668643 0.000461074889579193 -9.226459213800648e-05 4240 0.00045681781226838015 -3.328806882316133e-05 0.002286671518676369 1347 -0.0005252492252747236 0.0006879184489036213 0.00015921505777725855 3529 0.0013578542039562208 -0.00017110347809634743 0.0009638820224959462 2060 0.0007102905545966214 0.00028679586310638645 -0.0008601011059815862 1349 0.0006558724608353578 0.000806820246252586 -0.0020362317770267428 4306 0.0011779743513730134 0.00071891409273799 -0.0008232489946328093 2126 0.001342234039033511 -0.000839051470548607 0.00022811471674405687 2130 0.0016813563188315653 0.0017336032180040827 6.314195808041498e-05 2127 -0.0020545183915628156 0.0015574589035418252 -0.001382737280757196 2131 0.0010132816203177472 0.00011809792602364243 0.0008417573587559104 650 -0.0012345119505497838 -0.0010451695794766892 0.0015029568133503072 2118 -4.741228698747126e-05 -0.00044511739795104763 -0.000721580998213958 651 -4.4243652348168014e-05 0.0025858923188912405 -0.0005385406212927901 2114 -0.001873522053885 0.001828047942709112 -7.771344191917159e-05 2113 0.0023767613791330078 0.00039777000127493847 -0.0019608530908482107 2119 0.001152398897656086 6.018285383963418e-07 0.0021897296180817794 2099 -0.0022637646283966842 -0.0011703414228821027 0.0017518329717721097 2092 0.0010130738489369598 -0.00022800286887846672 -0.002005575581397532 2101 1.8246026378286628e-05 -0.00015882128437303962 -0.001513523817225911 2090 0.0016555479764462056 0.0019917755664945616 0.0017797739079073983 624 0.001833734621813912 -0.0009486144401666038 -8.175245484841787e-05 2102 -2.9652574251763783e-05 -0.0007576076438289064 0.0006485912594195743 2100 0.00022819547746566536 -0.00015688037166948022 -0.001714112824206242 2093 0.002228959125489024 0.00038695114579706015 -5.123723369707426e-05 2091 -1.8449684376659102e-05 -0.0015326477096396763 -0.0007514990521144322 2063 0.0004116937962334202 0.001254503463422898 0.0024414813395580077 2065 0.0011405187289792575 -0.002728203364209658 -0.0004344574938587487 2074 -0.0017684791917259941 0.0016116237156368212 0.0007229396420291608 2072 0.00097689746811406 0.001680889873668165 0.0010147940775482056 626 3.87827115086736e-05 -0.00024336393182916582 0.00025861365291684774 4249 -0.002126898031900197 -0.00022782529087149103 -0.0010688569621313188 4258 0.0010313803766927982 -2.2433942131335708e-05 -0.0005393237649336963 628 -0.0014443439042783033 -0.0004305091055265039 0.00040655725084355826 653 -0.00010467789594868792 9.615860663092393e-05 -2.91159593428709e-05 2078 0.0008485041993938383 0.0008120692564285665 0.002260104674620721 2067 0.00019609314711377108 0.0013756659401864685 -0.0002284644375568582 2129 0.00011132800142629588 0.0005828379063801523 -0.0007745917695269239 2133 -0.0026644747261947333 -0.001379975048678815 0.001277020109771445 4316 0.0008603682466401222 -0.000612712381407907 -0.0021399428503710415 4311 0.001230998447143244 -0.001120915501322193 -0.000748741790028233 2128 -0.0016049014001864052 -0.0006848772326438084 -0.000877977130217556 2132 -0.00168673536210592 0.0014817752608416424 -0.0016744908605929797 2115 -0.0004942257865392975 0.001105019933833126 -0.0013305881176967338 652 -0.0009595469079696859 -0.0008328238043802647 0.0004997706607357035 2120 0.00040226226798566666 0.0005956587100597172 0.0003385863780498415 2076 -0.0010425994104378816 0.00031995914134237094 -0.0006845192525667178 2116 -0.0006844799813682511 0.00036372986933349725 0.0026529795697976095 2121 0.0024558516828925192 -0.0007996451821611514 0.0019263683062142808 4276 7.114710594494569e-05 -0.0001537287628850957 -0.0019052205441121 2096 0.0010597796294384019 0.001589145739038848 -0.0011987050928406462 4285 -0.0007963312246302421 0.0003192860393644941 -0.00046502096622020396 2105 0.0016546373573730687 0.0009252086579388108 -0.0017463108919272712 2103 0.0014134156830844587 0.0009036644736783994 -0.001852046660118575 2094 -0.0024549935472786824 -0.0013256320231888408 0.00019450185028965436 2069 0.0008564530973569253 8.669262705767366e-05 0.0009183785279439408 2095 -0.0007845533495547277 -9.797771361898548e-05 -0.001878698206367188 2104 -0.0011849272046678128 0.0001565444440954581 0.0021431475327188232 2106 -0.00019588104222599182 0.002528852813415435 0.0008894581546545239 630 -0.0008440669418539082 0.0009086162209821704 -0.00030260919400078756 2097 0.0007931091951822222 -0.000721146483584317 -0.0014010604887084472 4518 0.014144977970155506 0.0021536829287793677 0.0055902843381428115 4403 -0.002104031741515132 -0.001558846794642532 0.010821803587324558 4840 -0.004875459048860342 0.001840561935227743 0.004939968221684916 2172 0.00010886027019421478 0.0020687040154720947 -0.001471603895190043 1452 1.5362844060856683e-05 0.0002013095226134484 -0.0004734418862052583 4494 -0.004141208884933867 -0.0006358679414927198 -0.007384515169468845 2163 0.0006459108745215749 -0.0019505884914653958 -0.00023874777464909886 4560 -0.0008558839188711836 0.005180527101271168 -0.010809647370418965 1450 -0.0004349184909225282 0.0013241870750337042 -0.0012795522311231837 4433 0.008061927256152946 0.0033640427481153967 0.001335703430069761 4393 0.003949034801140654 0.003180525569569642 -0.0017430248019555436 4501 -0.0022676992329344796 0.0027205968251350567 0.0020093773179359394 4624 -0.004604700602580522 0.009863162849745184 0.006653993833747104 4765 -0.00667341127613778 0.006359520904462931 0.0034387284345697242 2139 -0.0016067022804125588 -0.0005828973951886554 0.00010505856464897688 4382 0.006889025036299644 -0.0063965531588589565 0.005590123127121392 2137 0.00022009896123654886 7.053820076737428e-05 -0.0004202386629383109 1426 0.0008983111635465424 -0.000773856722341092 0.0012379692107213549 2135 -0.0005285309926082709 0.00013874092934420103 -0.0009855964119606356 1424 0.0007151834739327555 -0.0014944492936852906 -0.0012204061994664415 4740 -0.00170438798210985 -0.0031271142563109398 0.007532140096865347 4480 -0.0017484045078032468 -0.004696148089307705 0.0034565782415630288 2138 0.0003862672245297557 0.001466865664478372 -0.0013834328017748396 1425 -0.0013023230530737426 -0.00028759910465905956 0.0015868464551052172 1427 0.0012320712381068393 0.0005251644317280468 0.0021222493921732506 2136 0.001532284677887835 -0.0011283405532548042 -0.00043741019501031763 4755 0.00792218313901849 -0.008569548405849923 0.00036480989732229254 4490 -0.0042254349573187695 0.005006301616871814 0.0007839105698809912 4426 0.00390632241511369 0.0006237920471193676 -0.008883397059211267 1428 -0.0015383261790899764 0.0012104747917141062 0.001460854128951977 4859 -0.002189335919827246 0.004272288458895654 -0.0027803844856111263 2167 -0.00202593798424468 6.364218963261434e-05 0.0010508040831851808 4663 -0.003562881665696392 0.0009892348349102714 0.00039932782850329624 5333 0.003577439265364925 0.0018558785053392197 -0.002103234298712969 1421 0.0021944380568757822 0.0008660745707677364 -4.3545579139500764e-05 4638 -0.003883022029267439 0.0032982589416968174 0.009034876901254403 4617 0.001034080026921765 -0.007380896853977094 -0.00019503968022933045 5045 0.00676206311637647 -0.002413023340622506 -0.009009579810621131 4606 -0.002149364117559499 0.003889377611110698 -0.0009746815236898485 4321 0.00012627850950896156 3.454935615605976e-05 0.000399004792439167 1430 -0.0016487126534215613 0.000905682656151273 -0.002622334343195571 4695 0.00545388073790062 -0.002055319964542994 0.005364643637247323 5136 -0.003806447874511752 0.0037627752011383684 -0.0070214356130797045 2141 0.00027683361384513367 0.0003773596128755272 -0.00015416985079269108 4547 -0.008526284887241864 -0.005899027063716146 0.0056138900744016566 4604 -0.00018763060623567618 0.0012192530527433908 -0.0057845511563476655 4578 0.0079007808953385 -0.0006392141660905967 -0.00020971875630957024 4623 0.0007170441936002929 0.0014583740907824255 0.007983910871112866 4775 0.003701855784037352 0.004403478817284774 -0.0030483911952695546 2142 7.009674853406325e-05 0.0009520563197120992 -9.361781699128652e-05 1431 -0.0012689425789325515 0.0013193991142561711 0.00016091586214805453 2140 0.0002971632497656507 0.0011392730317145948 0.002761634600858572 1429 -0.0001544804423716129 -0.0019894739954651143 0.0008113802910263241 4455 -0.0003638530895134449 -0.002910099006184295 -0.007306512195920593 4557 -0.0046005926397654036 -0.005205235746536302 -0.0022394453374558637 3610 0.00019198864012926658 -0.0015585005357407603 0.0007294353146416637 5513 0.00028797691269680307 -0.0023561543245104333 0.0021587303327973294 5061 -0.010991067819596365 0.0041917790540019935 0.0047056875909493815 4408 0.007786387820129456 -0.002925719464055146 -0.00024910730551989734 2181 0.0015017922180519529 0.0011308565061731199 -0.0006639370839059116 4474 -0.006516469451563298 0.004215830384630003 0.0027339139700988963 2183 5.1134226225957227e-05 -0.0013148393949585651 -0.00022070387946483976 4432 0.004542444813686845 -0.000337217742327722 -0.004150197807252872 4394 0.012887408495592906 -0.0068653495484728546 -0.004337284145839145 4580 -0.008394679371101924 -0.0017482656130686537 -0.004922813471310112 4820 0.010974145539119953 0.0008761002628694448 -0.008350559622469259 4387 -0.009263902904767024 -0.002348003210010453 -0.007280237585584227 4707 -0.006946636649798819 -0.0010651231715829504 0.001651592506180901 4795 0.002289454710643353 0.003540108368316667 -0.012594291737500766 2146 0.0009505568449773518 0.0006473158991020813 0.0011119916718521036 2157 0.0007820028094109062 -0.001319746125232957 0.0011432301603918886 2155 0.0011699550224549453 0.00022234915567058357 -9.708362895684432e-05 4704 0.0019203082967635045 0.0014713085240556593 -0.005777540891820937 2153 -0.0005892231931588175 -0.0006854803508501879 0.000742810427390457 4610 -0.0010916000138489472 -0.0003383708396111647 -0.006587647352905389 4434 -0.0013798589294468746 0.0023705894986817714 0.008474945768621726 2144 3.9231872386785076e-05 -0.002318581896007502 -0.0008336002917891348 4431 -0.0068856987357947975 -0.0038094248138858177 0.006254438221174918 2156 0.0015535194186736484 -0.0003767611913384323 0.0014303743995611779 678 0.00032086452167121124 -0.0015799212688467042 -0.0015086156577135343 2154 0.000578291575232299 0.000873525702875456 0.0008508685191289375 2145 -0.002394721915054809 0.00034078039582350933 0.0005901243076841035 2147 0.0014604517938143352 -0.001471578686897517 0.0020319549735454885 680 0.0009800333968300646 -0.0008523696937373401 0.0013902910140744058 2148 0.000692116692244811 0.0009761354663576538 -0.0026248443977520616 4517 0.001088895148405205 -0.0006053896090918962 -0.0027357407461472364 4395 -0.008647830540839263 0.0001452755318476452 0.002876522309510072 5254 -0.002484413042194851 -0.009318959409333335 -0.0007365057322773115 4729 -0.004000389252453333 0.006741614480915117 0.001030813613790458 4462 0.001058323283101699 0.0007902537324206142 -0.002782643888499856 4512 0.0038848896824303873 0.0013134054593712122 0.006172838821595705 4636 -0.00909026718671024 0.0036419790028625883 0.007279321180558373 4671 0.006157064889301931 -0.006058455439405581 -0.00130321756340374 4693 0.0024877331799044765 0.007316642514270893 0.007846050481114822 4481 -0.006183972299351606 0.004208365565074566 -0.003983615447171309 2176 -0.00022841211088717048 0.0001735806661642199 -0.0015828348783086803 2185 0.00017160975071323623 -0.0006821809111603018 -0.000295782108173928 709 0.001966425342860557 0.0007068748050124418 0.002356200217778255 5168 -0.005152449071757104 -0.01512737788013288 0.003952379066839843 4986 -0.004098846960583109 -0.0005033661099467303 0.005440866803963558 4549 0.011906099479348222 -0.007523809384556293 -0.004571255918160321 4594 0.0011176987637372285 -0.006042495635066998 0.0030862287739729546 4330 -1.6261429900472262e-05 0.001101510975523618 0.00023805842283637028 4572 -0.0014588722004420759 0.0022693282780872712 -0.0022678442290027076 4781 -0.0008218299087921344 -0.00011150084946657538 -0.005850843874553452 4760 -0.0015525793898594595 0.0001170525463570781 0.002007700975968046 2150 0.0006419453906762683 -0.00020360883257725657 -0.0012404038665948264 2159 0.0012810616950417286 0.0024837911525543406 0.0017366061886200917 4339 0.0008194261807923948 -0.00021379008147727474 -0.0003552373792146044 4605 0.0009734113949552343 -0.007382151878558768 -0.0016281299163726554 4672 0.005991493574324657 -0.008041699982340302 0.0015833375417554278 4440 -0.002582332012081428 -0.00376469675274929 -0.0005032772800074292 4583 0.0035051268976360565 -0.00200986437626163 0.0023318085557610785 4628 0.0017173175874116665 -0.009820789597274067 0.0018056519465245572 2151 0.0005450114018946412 0.0020390290473787124 -0.001279109268621621 4533 0.005675693743749668 0.004778116865468336 -0.006072932370916386 2160 0.0006825706398758708 -0.00012481266435389413 0.0010414940705321513 2149 -1.2442093421571356e-05 -0.0001498452143737037 0.001641506361635682 2158 -0.0015331125321887999 -0.0019950828550983216 0.0012471348443506805 682 -0.0012130261098981532 0.002021151301883639 0.0003130790264009261 4398 0.004643581811614014 -0.003073993876829912 0.005033429367610121 4473 0.0002805505486788763 -0.004336260670209288 -0.00011493881072884642 5012 -0.0004226211656883841 0.009551675388717278 -0.003532050867090417 4551 0.013981842701565501 -0.0020710702434657974 -0.006487520111236652 5146 -0.0023697187177598358 0.0016526371520988957 -0.0005560957405517628 4421 0.0015877082234507706 0.0021057594334506604 -0.0003965746108257589 4619 0.003151377777384727 -0.005267219648993517 0.002064937554806628 5119 0.00488164138361833 0.0028150096341877824 0.005500262730397321 5008 -0.008491750763184288 0.0005501861430535098 -0.00449462677513553 5084 0.0014603950530994493 -0.008794325513378354 0.0067526321418788565 1453 0.0005017938107108007 0.0014776840747877918 -0.0020477417594700065 1461 0.00047461194324623763 0.0015812985602322149 -0.002225387140113566 4585 -0.00671907897935731 -0.008785272610523538 -0.004053659457807467 5082 -0.001986121073641192 0.0010154500384722352 0.010382983170602086 4664 0.0058853375220426305 0.008663296587027967 0.006495282676103994 4995 -0.0025860550731950996 -0.003927972277325192 2.061974533733963e-06 5480 0.002057135027133193 -0.003253287297410609 0.004949231823522626 1451 -0.0012517380840361635 -0.0009212482466939594 -0.0005089381715436675 2164 0.0006686409298418672 -0.001249553172513256 0.0001162963651301311 1444 0.0018720600366229228 0.0002483948677048062 -0.000874536074526269 4876 -0.005002961290250114 -0.003621918699314841 0.008662297321063396 4831 0.00909003024529362 -0.0061329335390278815 -0.00861758071892834 4717 0.004954012140211987 -0.00027688449096494044 0.0006606317692155506 4940 -0.014031414049450606 0.0006839893572414548 0.007314298507488953 4615 0.0005955568556017497 0.006840179925248631 -0.011801428940546413 4469 -0.00038012420799468595 0.0007677878549144173 -0.009188004234677478 4698 0.006498319029005572 -0.0006610870992431004 -0.000893984002161665 4757 0.0010036580731023488 -0.004153379066196282 0.00044660610433223344 1442 -0.0006270101634534113 -0.000595625688082193 0.0007061434653475899 2162 -0.0008514040800758384 0.001046735815114463 0.0009248798382891814 2165 -0.0002253968727934877 -0.001804362319270998 -0.0018247291345151995 2174 -2.25384405997404e-05 -0.0018473239691467105 -0.0014410990369854684 4503 -0.0009392624841831449 0.0019139723490971875 0.00030683585402952184 4472 -0.0014185138286010794 0.009806512046232778 -0.0024108288693539337 4974 -0.003452552342941412 0.0006538974210741832 -0.0005047468114220922 4777 0.0029489279757675016 -0.0006650393987159131 -0.002401946348327677 4407 -0.006657913459443428 -0.002825935574223837 -0.004084855482963572 4737 0.0005434916785242508 -0.010218847969898715 0.00029965220990568785 4837 0.005336736524471796 -0.0013176916150107868 0.007051005744377879 4988 0.003738202220801427 -0.0025047440644886594 0.00781474005806426 5198 0.0018512800706575832 -0.0017309334351574832 0.009617438218534611 5102 -0.0048828408871048066 -0.011801885268119117 0.002562302042222491 2177 -0.0009726055636165913 0.0017350343790624092 -0.00069683767271414 4845 -0.005188607942855252 -0.004522366917070062 -0.004903422571481778 2168 0.0009883833999938707 0.0005885408857253724 -0.001732567483538854 5387 0.004892157671185697 0.0029473760721357746 0.002951350265198844 5166 -0.005646173604280553 -0.002412506446687038 -0.0010717077573517062 5122 -0.0016366527972062907 -0.0004707126352343691 -0.0009218583011051647 2169 0.0004918155934511179 -0.0013704953397758286 -0.0010687147155145377 4521 0.002694635257580896 -0.0027830761299364876 0.005067308622546267 5072 0.008381565275892481 -0.0037995393407066515 0.004408339703168838 4635 -0.004796670345016303 0.004418547293487657 0.002512078112744438 1454 0.0003294852585928395 0.0012849364477763956 -0.0005823570199023774 4749 0.007912259410382217 -0.001406559650971459 -0.0037898548297283594 4708 -0.005472987307763554 -0.006490851253430629 -0.0016287613018512797 4656 0.005418950395518024 -0.014348900901558605 -0.009296559222855497 1456 -6.18318326830211e-05 0.0016336656036974595 0.0017611265057230552 4774 0.001673716680410351 -0.005440702573191441 -0.00908764563499853 4457 0.0015880841874249198 0.005315469912623899 0.0008526725510315008 5332 -0.006034920444113037 0.0004166058300217629 -0.0029521752433518756 5473 0.0006837875654537708 0.008786479971328755 -0.0023461732184380524 4821 -0.00020987110697898035 -0.0009649140873493121 0.010893645946530042 4838 -0.00360398684177072 -0.0030418204327276733 0.0033367849682194852 4748 0.004201940431244316 -0.005776835575020054 0.005030620357502678 4625 -0.0021605465947383343 -0.0004909810165010366 -0.003554294835932182 4378 0.005226220374080763 0.008249164989977317 -0.010317904313202413 5079 0.0020817805195825503 0.0022672900145248973 0.0033937616058210833 5437 -0.008283964267202105 -0.0016199802478512359 0.011101987327636616 5307 -0.0021604401164295613 0.005194397979831299 -6.563778271621401e-05 5284 -0.008525024003367512 -0.003268116062378834 0.0017079695477912797 1477 -0.0006888379916947238 0.0001210700448279309 -0.0007259764031934172 2173 0.00025524814366818154 0.0007414483565317707 -0.000590345817432262 4869 -0.002702740115390965 0.005101792697491819 0.003767792079783536 4915 0.0013921930613931225 0.0005092835442792135 0.001758875888221125 2182 0.001198360433672138 0.00042510354332574813 0.00195678788684025 4681 0.0019507765933824749 -0.0024116516180429353 0.005965979524813568 4798 0.001558621901955872 -0.0016911945616957598 -0.005095711323508825 5023 0.0027460361913664113 -0.0012175867301269037 0.0027226726669847844 4766 -0.0031564192979561664 0.005328886841346292 0.007386552644405446 2171 -0.002245459058144775 0.0023698992974924803 -0.000594225330966704 4814 0.0016291196314498168 -0.006737957482373055 0.0007893158808995075 5229 -0.0017744426357334463 -0.0033074725569533364 -0.0006852160749875119 4488 -0.0006779154039217271 0.0042087293991884675 0.0006200253129660025 2175 -0.001956327684764975 0.0011672318626731396 -0.0013167772490573417 4789 -0.0025797374152111904 -0.002510587806213583 0.0040176518427295655 5099 0.002030538459748202 -0.0004508177431792493 -0.007779364760028472 704 -0.0010205771509614724 -1.0296584709196342e-05 -0.0003472441892120836 4483 0.003152188683722592 -4.466871267773338e-05 -0.004028863973241532 2184 0.0010181559877983325 0.00014656104606493943 0.0002564049130783753 4778 -0.0011061180274478083 0.0008501275749928817 -0.0003960852371875018 5135 0.006121453264344487 -0.0008610444563988525 -0.008377916295764 5499 0.010214655133254947 -0.009519713915148536 0.0027199833923349636 5329 0.0020747998667560996 -0.002302364357031852 0.0011207703036547312 2186 -0.0004611947831536364 0.001505149058259628 0.002702556525312938 4870 -0.0005280034843962353 0.00160332321867716 -0.002579763121795526 4832 0.0034520904759511753 0.005728896254024362 0.00010257342844403281 4651 -0.0042585530138764555 0.0012159314076178273 -0.0009015591281682792 5172 0.0051840441098884435 0.00858302020886847 -0.001884909466018295 708 0.0006731692222433109 -0.0015109393490288958 -0.00022640727956017175 2166 -0.0005279590075066671 -0.0005471176332013882 -0.0012073849473330771 4723 0.00553725999026125 0.002212286573964421 -0.0006371587996770365 4504 -0.00384564092718141 -0.001493793074088113 0.00649968188322443 4366 0.00019420690026832098 0.0011564402971149207 -0.00010973024325589302 5492 0.000917638597662792 0.0002695240489053743 0.00590649661997378 4357 -0.00152356989827095 -0.0003044209366289229 0.0019743477098352973 5031 0.0025242386712340218 -0.003087895522226265 -0.005692101516688955 2178 -0.00028529344758763064 0.0008853317152383408 0.0012247239828918873 5094 0.0065427993147888506 -0.004229515657533185 -0.006200580978277207 5222 -0.004441588239549108 -0.0004988124089617782 0.0012803001134585614 7 0.0015624548332422777 -6.813515333213777e-05 -9.387756487787453e-05 5103 -0.0007504373603534653 0.004317002977571184 -0.0005703517623996496 4850 -0.005222734350120657 0.0005406546826569759 0.009258030342077518 2187 0.0006034548155082399 0.00027986656557206914 -0.00037153749331102497 4744 -0.013699507043291976 0.001198374469149768 -0.000995664957567195 4896 -0.0013108003115611356 -0.004499599634351389 -0.0051309507505768815 5484 0.003470704413127092 -0.0018675598989664284 -0.007230891570657103 5071 -0.00034646832533898704 -0.0066391947763020185 -0.005658190843726987 5178 8.560885809749251e-05 -0.000742470233733276 0.005250459884584269 5435 -0.0037826139833734896 -0.005625745882904178 0.00786054587245939 4881 -0.0009212655180975256 0.008837415039160855 -0.004163904821663072 5494 0.003089392805039127 0.0030931282400019754 0.013721478760645674 4922 -0.00011490873727877183 0.00339569661719529 -0.006026003752415366 748 0.0013809212098786538 -0.0021006134591104106 0.0008469235615102347 1472 -0.0006794787984347908 9.203293995924111e-05 0.0022756036467654747 5157 -0.00258648244894869 0.0027599902715396323 0.0011933797634283386 5181 -0.006705543760046777 -0.008287552466540784 0.004007361042828847 1455 0.0016175180101767844 -0.00044953637160403655 0.0008408877004836769 5260 1.5742366454010704e-05 -0.0009073261983518065 -0.0019209885100311878 5359 0.0013898946049854045 0.012698006257241885 0.01018250185789645 5402 -0.002062286673222492 0.009675466641401962 -0.0015755211567488056 4445 0.005494831671344342 0.0008482550943697033 -0.003220204161266403 1463 0.0001973010584326367 -0.00021361293586357323 0.0006728343107967709 4739 -0.001641374774440334 -0.0023906360647380324 0.007934981953420071 752 0.00025360128496075074 0.0017890887149955405 -0.0004839412346592292 4751 -0.005480753249850168 0.004653490043126364 0.00463402898634928 756 -0.0012209144780695258 0.00011997399260337937 0.0019606638984989285 2198 -0.0009717466370783203 0.0006011233061041075 0.000761846353505045 5113 -0.000872989333056884 -0.0009682632898397198 -0.0029422925719289 5438 0.006200430080236703 0.004003410573340407 -0.002692056528104606 5490 0.0009138232157837139 0.005786680192531469 0.006161190053048233 5370 0.0018308171293191385 -0.0016727303295926237 -0.0029324114969947893 5502 0.008196922967633214 -0.001345518433085092 -0.002832689607649471 4586 1.7732086494465967e-05 -0.002014496949540385 -0.008675751020656841 5163 0.00867700758513313 -0.0014663868885727838 -0.0027468130040115197 5251 0.005279591992208679 0.004501982535905444 -0.008012809779277139 3637 -0.0005153788516355454 0.00034127526451625757 -0.00017442508441621726 5444 -0.004622043563930155 -0.009553924130355322 0.007040030320164455 3639 0.0010788738973804717 0.0014666861760633777 0.0009729506317641676 5486 0.00255215561344969 0.003422794412313411 -0.0037752865241369054 5488 0.0031533490376894234 0.008134084284651486 0.004200457865479781 5291 0.0031585891779195795 -0.0010082841507452452 -0.0005113082536886989 5393 0.0038861786581671047 -0.005177419177718994 -0.007673103734907047 5207 0.00989892914797107 0.003895693482822114 -0.0019897355433260455 5193 0.005411199500966722 0.0011337623166779226 -0.0019550210817274095 5334 -0.008834475522483533 0.0015982469046749875 0.011620089187672796 747 -0.0013621762085570155 -0.0015495418646136378 -0.0005773047175756957 5190 0.0010990750844741596 -0.0050519483075232964 0.010179918188180126 5303 0.010550424240997397 0.0028060694894551236 0.0012964867150815533 4498 -0.004926136716602055 0.00110648784884967 0.008462170726526557 5417 -0.0014855755070797673 0.020366440786708555 0.004842897655603623 1470 0.00041361855079718687 -0.0015810864593188674 -0.0005765443720588226 4511 -0.009196810693999946 -0.0046269762167591485 0.00988775112431625 4955 0.0018232653017268687 -0.0065627610778931115 0.002812679067195487 5018 0.0032527683909199427 -0.0028085661815863312 0.0016127773690726979 4375 -0.0011948188797868255 -0.008774840641474296 -0.006565955515383521 3 0.0013098695824069833 0.0006512444392084652 -0.0024036067760782867 1459 0.0026173725532242487 -0.0002657706703496863 -0.001889263146418964 5507 -0.005711570508546436 0.013215656586569341 -0.006706375590122021 4908 -3.993981400220192e-06 0.0008158535901004915 -0.007316318714101225 4968 0.005144069866970993 0.0009946091714326478 -0.006716397331064535 1465 -3.1856889008853595e-05 -3.6322018391944416e-05 -0.0001537541662478515 1474 -0.0016385674828541799 -0.0010864744048142533 0.0006185831026850237 5319 -0.012185773795721411 -0.0008256890865605724 0.0021976078550447514 2940 -0.0012473717670918926 0.0012439575439676686 0.0008055649341256257 5459 -0.00013689274011346317 0.0035575244427020637 -0.00042141409433928655 5511 -0.005686808207093636 0.007450412476570674 -0.010816305373896811 5365 -0.001736459086177073 -0.0029052464137702826 -0.005859845096174958 5506 -0.00654816224214712 -0.005689201848930103 0.0024457300789245216 1483 0.0013550406224204737 -0.0006845455848972365 0.0027629936202928362 5131 -0.014089383036504335 0.009917870223636337 0.008288426795565112 5481 0.005309770459759281 0.00648656885913914 -0.0059981066262268625 1476 -0.00038826788469036445 -0.0004831413447989382 -0.0018636851016644138 4716 -0.004371971569883201 -0.0027541879331888924 -0.0009108960549741626 4861 -0.002686362462140563 -0.009307580742412247 0.0038438236962106023 5271 -0.009322455871173892 -0.0013263960438980006 -0.001798146233556886 5132 0.008007729309605461 -0.0016924646750746581 -0.004000520438746747 5414 -0.009485459274470568 0.00025561918508424416 0.0014633917178141782 5407 0.0003994656003857625 -0.001983039278935542 -0.0022480923731286045 5377 0.0033830559821987076 0.0016346654412255487 -0.002568041452923181 5475 0.001783988725601569 0.005057738640660176 -0.0016570281058479268 5269 -0.0058309299412609835 0.0029436817176731874 -0.0005821956102094746 9 0.0003712971951378857 0.0016062087486324133 0.0006987781750804726 5452 0.0018090022107393618 -0.0006990556401775558 -0.007717823024407172 5065 -0.0016349138658696156 -0.006913918577796934 0.005230628966644066 4888 -0.0020732101330125066 -0.0023860063072844535 -0.0012570782885464402 5317 0.003904402215032071 0.0012598287981504654 0.0028927357384932553 5413 0.0011072741500992732 -0.00979197041272656 -0.00520234159559444 5367 0.0015399050918492795 -0.006305337247531875 -0.0008434275456817272 4642 -0.004982304024776276 -0.004673666241704479 0.0019764934163848317 2234 -0.0019728999681245447 -0.0003206101397330483 -0.00023187919427686645 2225 -9.526753773076444e-05 -0.0003451388649589279 0.0012203838417024207 2236 -0.0005815646384329861 -0.0007424773283710494 0.0009620250428222362 2227 -0.00135518091350691 -0.0005078227571247806 0.0006512453662263962 2199 0.001056368255263147 -0.0021610965849181694 -0.0010980282776420023 2201 -6.50300780225101e-05 0.0005042969459663352 0.0003338249936375927 2190 -0.0008216993369575243 0.0006115331969116453 0.0014876364401927194 2192 0.0002657830579988504 -3.942330187807399e-05 -0.0017707890953026651 46 -0.0017714942034588689 -0.0005084948513849078 -0.0004120789747093384 2229 0.0004533598009523834 0.00162944209810126 -0.0016235950384369737 2238 -0.0011748219322553182 -0.00026960481750998983 -0.00014670100210359524 2231 0.000862017645385251 -0.0012351997040631873 -0.0014847612550244634 37 0.0002648024274436443 -0.00022782146974710662 0.0005382133549341542 2240 -0.0006030874396847201 0.0017429226548948693 -0.00153912888572894 2205 0.00015457656131856044 -0.0005837839427487925 0.0005489637316251393 2196 0.0009777481965971319 -0.0009064278115931414 0.0009901865544207022 2203 -0.00020229907040777463 -0.0014919671365060038 0.00048154662507711226 2194 0.0016294215969133836 -0.0003799716155567014 -0.00026294886499985564 2945 -0.0006829510826639857 -0.000989009608569806 0.0007036410581094416 2947 -0.0024786741648850216 0.0010060206734784861 0.0005014528614788985 2956 -0.0010570494780564085 0.0002567181647383799 0.001694688636912752 2954 0.0009307306277041836 -0.00027446357645916845 -0.0014703422411929503 2919 -0.0011832045026464776 -0.0001741388953739034 -0.0015171527924743113 2921 -0.0007500618317257816 -0.0002864598200672686 -0.0007011809305413931 2210 -0.0009369130655510084 -0.0015751507842669684 -0.0005858603765311349 2208 -0.00019502231306855024 -0.0016657726238482884 -0.0004564324800971515 2930 0.0007048050460791269 0.0006708848607517148 7.862438548239287e-05 2928 0.0006610821009512427 -0.0010258939434587137 -0.0001161934980712701 2960 -0.00022628801018327073 0.0014213898822593074 0.0014895390068050184 757 -0.000993973783413846 -0.00024952433200747196 0.001206089323991873 766 0.001253772859420781 -0.0010321586909252986 0.0017002090391322628 2949 0.00015915234531136725 0.0020649611889150495 0.000645114850271454 2951 0.00022488488677526418 -0.0017220140631492061 -0.0019675095010271964 2958 0.00042268878664348077 -0.0006163946121137663 0.00022071304605584402 2214 -0.0021379543059082185 0.0009879481867933336 0.0010430996009458365 2925 -0.0001147346865062837 0.0008293561526545776 0.0003806511976047498 2934 -0.0018728334850751343 -0.00030666024577136663 0.0007876753326987763 2212 0.0005012947494432299 -0.0016265618086484203 -0.0006978814479658211 2923 0.0011493388122762165 -0.0014602796834861506 0.001727103849648343 2932 -0.00039046463601276766 -0.0006569451719983387 -0.0013326140661834313 2282 -0.0007931293487574807 0.0010697706650832429 0.000619209217759706 2280 0.0004093507557631432 0.00046731772261881946 -0.001429122964033265 2271 -0.00045760331093664796 0.0007455843983891063 -0.00011506942998974301 2273 0.00026245020612284623 7.27625571595767e-05 -0.002075626676082052 2288 -0.002124350617219041 0.0005192287847497352 0.0016171493957393126 2279 0.0017207299657103598 -2.704195387132416e-05 -0.0007307808160851093 2290 -0.0002429043886702255 0.00024576773274261467 -0.00031050141353338194 2281 -5.267483825799075e-06 0.0014208096668068505 0.0011591343529724365 2253 0.00034257814079016497 0.0008518304834088875 -0.0017036875621225282 2246 -0.0016559236063401067 -0.0012578279757965811 -0.0008184175762254031 2255 -0.001712148288101455 0.0007372157987611786 0.0008368534626436227 2244 0.001800245877257711 0.0022187059564829025 0.00019415304162788026 2261 -0.000357820810362562 0.0006392729309733546 0.0006598664961135597 2254 0.0008564152503761314 0.001529809463679952 0.0009134892500725363 2252 -0.0007000438306158137 -0.0006763129355413604 -0.000587408329785741 2263 0.0007540588555494763 -0.0013823977338939383 0.0005504204419275955 2219 -0.0001647598896645894 0.0010504822984330371 0.0009055510897456794 2228 0.0011059066041015147 0.0007688608360155486 -0.0003073593593781616 2217 0.00027799177481498496 0.002675631758140648 -0.00018121532705538687 2226 -0.00021745390749601263 -0.0005274544306617958 0.000109390804334108 2286 0.0007942682581558029 -0.00014530979153622257 0.000933356728173579 2284 0.0017456822855980967 -0.0007216027058072044 -0.0003161400731524391 2275 2.280126034426115e-05 -0.0006274101856074817 -0.0011404660839979045 2277 -0.0010140416677135008 0.0019740021718052518 -0.0021184401107146164 100 -0.001166073959821301 0.0004421563761517351 0.0015909558653250915 2294 -4.49794619274105e-05 0.002124572174891459 -0.002257743573153915 2285 -8.954306519218485e-05 0.002305742862177236 0.000386367617495411 2292 -0.0019436018266901607 0.0012120027796178432 -0.0007664842645076674 91 -0.0017766007183252991 0.001739364580295077 0.0013501440600004746 2283 0.0015134795188066735 -0.0014036186025313357 0.002048797261859028 2259 -0.00018190798844665821 -0.0011724567397670062 -0.0018609685704532135 2248 0.00045554577705782923 0.0019133278153014655 0.0003530526624617577 2257 -0.001395728886587325 0.0012495954150271238 -0.00030887379132890093 2250 0.0014703464604095028 -0.001130897748936602 -0.0008114475233195401 73 -0.00017911059441617656 0.00025958516251565675 -0.00032264760526673334 2267 0.0004975391012735169 0.0017917230070570267 0.0002812192370977736 2265 -0.0004821319087395573 -8.59985333429901e-05 0.0009168460430336485 2258 -0.00032848850712022444 -4.981027064726953e-05 -9.507555658099052e-05 2256 -0.0016102116783624871 -0.0016733268199801655 0.0006161108802414905 64 0.0007136841807185534 0.00012855875653880857 -0.0010974231156643387 2230 0.0010570187229516086 -0.00010451433028127216 -0.0003683274196966768 2221 0.0018882907895287735 0.0026298849932940875 0.0007064284087841322 2232 -0.0013422861893637758 -0.001108976472716964 -0.00017143458272119892 2223 0.0013229727560575388 -0.0005687820057657875 0.0012263344849144635 2289 -7.616967987306004e-05 -0.0010497411898234225 0.002237497645674827 2291 0.0013176892267669023 -0.001993292690281478 -0.0010415321101741298 3000 0.0001909605704872256 -0.00025405943009907056 -0.001581374915526577 3009 0.001791820748442361 -0.0003264049406949029 -0.0010369042150529756 3002 -0.0008671078082663037 0.0007498092949681857 -0.0010784914546123313 3011 -6.27856058419596e-05 0.0001110899651181334 -1.2376082581437922e-06 3001 0.0013475499780589834 -0.0005058519024500509 1.3781605901999183e-05 2999 0.00044222918254962525 -0.0015159354894419184 0.001079187720800511 3010 -0.0007833857903417128 -0.0011831201636502585 -0.0004301864904426338 3008 -0.00034539097826761763 -0.0001458714029018719 0.0021006356458567886 2984 0.0006526914178852823 -0.00021001171876540263 -3.4142681853742115e-05 2975 0.000458282245010058 -0.0013825931601090706 0.0008461629804807863 2262 0.0002574062283540375 -0.001402318149670062 -0.001110682320425951 2264 0.0015379581408608476 -6.733697854584969e-06 0.00036101013065977265 2973 -0.0017981993631365077 0.0022126435446226914 -0.000758737895713996 2983 -0.0002495580592843876 0.0013005840652422656 0.0003087023730208932 2974 -0.00012942464735966538 0.0014001034088975994 0.0018876104989457188 2972 -0.0001772796178956446 0.0016853922992004365 0.000871616229783664 2981 0.0007649995780963606 0.0003283424491086779 -0.0007398926663084037 2948 0.0002689229514629002 -0.00012764458270898837 -0.002733009462670084 2237 0.0011870463512914865 -0.0010478599892555815 -0.000856919312601947 2235 0.0016140037251740698 -0.0016012471255523284 0.0010856813128452163 2957 -0.00240047458654908 -2.837647466036398e-05 0.0008774729651834398 2946 0.0006230168785988096 -2.3889260949344193e-05 0.0006366826863048598 2955 -0.0009269718962959458 -0.0003862359451862873 -0.00059928872267592 2982 -0.0005141720058002774 -0.00035468177087144624 -0.0001934048593353482 2986 -0.0010614325045097905 0.0014653285656199885 0.0020964845369637157 3015 -0.0012406432361434573 2.243497435779713e-06 -0.001286832685226287 2952 -0.0007302820771641642 -0.0006958714957915821 -0.0011886608409347075 2293 -0.0016744469575621726 0.0007476075736573197 -0.0004722906595052358 2961 -0.0007585138738985281 0.00010491197724786907 -0.00026673749580518073 2295 -0.0005592229666530092 0.00015990374921713395 0.0005340269361452318 3013 0.002528776449871039 -0.0014436941000510084 0.0003370805684733921 3006 0.0009980870263394722 -0.0025663075039752577 -0.0011814699733541268 3004 -0.00010837955047212266 -0.0014581009806298865 9.859370766486498e-05 3003 6.166401294185582e-05 -0.00032842957906593483 -0.002437551927372295 3012 -0.00041888375502141116 -0.0007692637297630161 0.0003687677471284575 3014 0.0020127709650261975 0.00026682613594037805 -0.0005521183098249406 3005 -0.0002795054781810822 -0.00040046766785653115 -0.001253399922787078 811 -0.0015585900997215308 0.0014486009457131347 -0.0003845297668631383 820 -0.0003414126196370881 0.0008908839740761638 0.0014765641888183339 2268 -0.0005971013471753426 0.001149512249392247 -0.0013191434814712843 2266 -0.0019390356841613153 0.0013171018578442364 -0.0001480771621089074 2979 0.0006655239246436619 -0.0007475964629423105 0.001038882208724497 2977 -0.0005634930673596515 -0.0007497662486207001 0.0017307069214030865 2988 0.000824892268485858 0.0016136522971124689 0.0011502810951761267 2959 0.0012912864437861456 0.002125407629856282 -0.0005206628609293693 2985 -4.9102218470832223e-05 -0.0022914881611992414 0.0006809054461823271 2978 0.0007128718956629892 -0.001055854300405332 0.001022444811853624 784 -0.0018923344117618773 -0.001238786165233661 -0.0016770007584033463 2987 0.00038531312605414626 -5.440255416903992e-05 -0.0017608090315224703 2976 -0.0001893979557431786 -0.000802037960125256 0.0009163568199398058 793 0.00019073738253620634 0.0019067512318756842 -0.0008895513529274068 2950 -0.00026529814435371737 -0.0015163584764364747 0.002384442144658607 2241 0.0010121722452707327 -0.0011303965482637143 -0.0007627299013918296 2239 0.001330206610666973 -0.0017503490920673715 0.0005651520623013888 2354 -0.0010277134146849706 -0.0017610658628700458 0.00127519823330358 2371 -2.860237000959975e-05 0.0006339785017049377 -0.0006177005701194864 2360 0.001569740490974891 -0.001260729054043868 4.598494583771392e-05 2369 0.0011897071360944397 0.0025515235254575737 -0.00014406222000364196 2362 -0.00033099495951989066 -0.001857928550644884 -0.001703071716377687 2342 -0.0011619764716574688 0.0006692582855268198 -0.0019002916581079268 2337 0.00022527775388459182 -0.0018047636290909716 0.00017177300549183622 2336 0.0014877003119119101 -0.0007117442988081148 9.55011095647981e-05 2341 -0.0014794678968594942 0.0016157210254006357 1.0551580601035268e-05 2331 -0.0005897994984788485 0.0017979789366296289 -0.00010140262081153066 2332 0.0005906191552149862 -0.00021751335738994925 -0.0005569831553699199 2327 -0.0008333575505799257 -0.0014241071136428854 0.001676647357195076 2328 -0.0008141176015574419 0.0004937340867364162 -0.0008620793018478464 2309 0.0025003075800342964 -0.0008492184212456256 -0.0006201921003361546 2298 0.0005265095242695862 0.0002394469729254359 0.0019227235527596261 2300 -0.00022003141907710644 -0.0003649783745572166 0.00021267100684345625 2307 0.0005805690720957521 -0.001150899562894636 -0.0009801704220266405 2315 0.0012262575267094915 -0.0017273252726517402 0.0019363390770066585 2317 -0.0002498727704564594 -0.0012985248603426599 -0.00026633506904931957 2308 -0.00032602241312642394 -0.0027616005598638882 -0.0005108104450336371 2306 -0.001174184646325524 -0.0016468589906261297 0.0004896768794098629 2361 -0.0012745999230913717 -0.0012344337465472397 0.001102241145615333 2363 0.0004648809093721548 -4.714050127656907e-05 -0.0005193983593009123 2352 0.0005369868065823471 0.0027121496759594027 0.0012064447439474732 2365 -0.001869826749605191 0.0016326704167801392 0.0009131262087821409 172 -0.0006470554661141864 0.0018483482371999195 0.0015838723230744436 2373 -0.0018767104012828773 -0.0013587005142606475 0.00016031886072207034 2366 9.500560912144383e-06 0.0003541513357434894 0.0012800633269019726 2364 -0.0007720978847352599 -0.0006369434960159129 -0.0013742331153699765 181 0.00041972569879002424 -0.0003339348318361565 0.0015557803653796084 2375 0.0006514903502440867 0.0013315971703902793 0.0005039775966921235 2344 -0.001478744404637766 -0.0026954063709083787 -0.0008546530795582464 2343 -0.00025548808144204723 0.001518423285132642 0.0010354414802189959 2338 -0.0012215849294305147 0.0005540197495576946 0.0015158143028109734 2339 -0.0010998153845097217 -0.001261223915346731 3.272692389548297e-05 141 0.0012661281235705631 -0.0013704368036195607 0.0004361699194526253 2334 -0.000947124613087202 0.0018809770295012374 0.0003044963257891626 146 0.0009615018316745444 -0.002200163310122525 0.0006688813616866094 2329 0.0008896265748117565 -0.0004813625233270076 -0.0008211003408092187 2330 0.00018144935110118543 -0.001758877003411385 -0.0007001829928221519 2333 0.0009294299355669429 -0.00010286206489403514 0.0008350759572947738 2302 -9.611702007120105e-05 0.0012289155141755755 -0.0014554250575275138 2313 -0.0016705154933302304 -5.329002125519823e-05 1.1141670998986077e-05 2304 0.0016329704125770373 0.00213358994280552 -0.0010234165231595076 2311 0.0011468576291041649 -0.0005458481883126283 -0.00039247749120744057 127 0.0006073477563359807 0.0010825835006144922 0.0019414836025365674 2321 0.0006330044525681316 0.0012246027192355149 0.0017795915630982409 2319 0.001646982365608591 -0.0005560921969194668 0.000543301652083698 118 0.00029356822509615105 0.0006854346757509669 -0.0013627955684318107 2310 -0.0016270247732768069 -0.0011517933044367119 -0.001161955593366236 2312 -0.0015617466124889664 0.0006853920696393681 0.0012069974119067407 2367 0.00033417958191939357 0.0012249656696969027 0.00030108613841826285 2358 0.00033128918442902546 0.0011568377816965248 0.00013904796289953072 2356 -0.000581261987708465 0.0014460101405267592 -0.0016115633096218248 3090 -0.0011074649049862368 0.0002527711735002096 -0.00017247498867480515 3083 -0.00027625228287387216 -0.0005790234605745459 0.001101388660164663 3080 -0.0014924687523202868 0.00037978681613171853 4.247512886406714e-06 3082 0.0002703660557625453 0.0005974480718165604 -0.00045063763524622177 3089 -0.0009230160387490728 0.0004121614015666614 -0.0003322230833302255 3091 0.00105367006891485 -0.0025369535760032366 -0.00031423760165427586 2347 0.000525218551915591 -0.0021875961222685885 -0.002229350312986419 3071 4.700255928003753e-05 0.002208459225118301 0.000541249629235552 3066 0.00023313343861011693 -0.001781151103251458 -0.0003665854469385064 2346 0.0012893994789247123 0.0011924878083757503 -0.002112174131275015 3070 0.00012184331814863456 0.0012924206006304454 0.0002142692227239812 3065 -0.0009993690447622902 -0.002032187967462415 3.315286811050724e-05 3057 -0.0021687367431095722 0.0010507223313296439 0.0017245311983012652 3053 -0.00017400370077782004 0.0017083180775750329 -0.0007912660490711149 3052 0.0003933860216659193 -0.0014818006911009832 -0.0007852702608524321 3056 -0.002140518732772027 0.0025846631908673584 -2.5629426237158952e-05 2318 0.0012438082629807462 -0.000969319079641117 -0.0019240589687746458 3038 -0.00042838921817120955 0.00021265018836735643 0.0009125704718301302 3029 0.0023323257186077884 -0.001433137080424534 -0.0010835410544636815 3027 0.000143164504635694 0.0007748620562116695 -0.002367729441538278 3036 0.0016152750437373508 0.001208762725865789 0.00023066779863915713 2316 0.0006953465290446173 0.0008181606308228167 -0.0007206982037802351 3026 -5.342788775770208e-06 6.844107713245128e-05 0.001903227894827681 3037 0.0009802360937487865 -0.001511064019803006 0.000937760745989598 3028 0.0006614970421281333 6.961284603833589e-05 9.103906689955643e-06 3035 -0.0009384748886469994 0.0006087856026533115 0.0003058067763043048 3081 0.0024363087653037165 0.0001563548449962271 -3.8011477544648044e-05 2372 -0.0006785441551330648 0.0010796869750257976 -0.0006244281086600673 2370 0.0004238763149338393 0.002212507028199082 0.0004944347358641596 3092 -0.0006555730106106844 -0.0008689918057056241 -0.0006533995913526568 2376 -0.00017321992788681346 -0.00098263377370683 -0.00013204513995869927 3084 0.0002761925405037266 -0.00017720407534282988 -0.000253164559560164 3095 -0.0012480598299571218 -0.0011048832991454997 -0.001299816016172857 3093 8.68913580530776e-05 -0.0003206726662896716 0.00023898857902502268 901 -0.00023461815019093436 -0.000785666193706142 -0.0014438571267757741 892 -0.0018207140496772174 0.0016579970565569415 -0.0011091413134813228 3086 -0.0014268836518099579 -0.0008770680485498815 -0.0021942414215435036 3072 0.0002880535097205979 0.0008399671893583216 4.3416231105565856e-05 3067 0.0025748553956282446 -0.0012847246507388154 0.00015487531561477646 3073 -0.0012479965495487172 -0.000925163413334325 -0.00013602423200710298 2349 0.0021109857771628173 0.0016173367867643046 0.002169146165977332 3068 -0.0002767422583256424 0.0020019390169107175 -0.002009695522388249 2348 0.0025208760814057047 -0.0006645170317349759 0.0003101774339332613 870 6.884665037512876e-05 -0.001665760435457024 0.0001919780807520969 3058 0.00045647305668348407 0.0013801750458438326 0.0009190773860180125 3054 -0.0010143209864535874 0.00016916196390188206 -0.00019682353000059338 3059 0.00022100459752848493 -0.0023852716172326318 0.0010939944992578404 865 0.001954279228335922 -0.00018689755436029367 0.002733908427853537 3055 0.00022203104252074097 -0.002235432727882807 0.0018089828198279197 2320 -0.0019214277256771686 0.0003534293880553624 -0.0008086256299408869 3040 -0.0017397290872412537 -0.0008829480677020709 0.00015454980464226636 3042 -0.0020641158866322074 -0.0006358580264875295 -0.0008474621353237936 3031 0.0009869235133615722 -0.00015629924946443776 0.00025240969922343814 2322 3.710296572728873e-05 0.0006887699718164651 -0.00033481913261887214 3033 -0.0018575575857021293 0.00027233445193330615 -0.0017811990500537936 3039 -0.00046356128539282057 0.000278689209860235 0.0009455546139256712 3030 -0.0007299309294455832 0.00043845088565895303 1.6984778142349654e-06 3032 -0.0008265598820219113 0.0006711999583416805 0.0013146508299957033 838 -8.697307076016136e-05 -0.0017367902619766066 -0.0014183893830658593 847 0.0006264932522398541 -0.0006987752184163537 -0.0005396110176778572 3041 -0.0014976441938426082 -1.780262476463318e-05 -0.0003755578297898218 3096 0.0015987032734760106 -0.0008349259948336279 0.0005882449332813938 3087 -0.00011686978694489718 -0.0012055442508993907 0.0006915704683424391 2374 -0.0004412046203458909 0.0009071826964309863 -0.00028239973086187625 3085 -0.0003579002668711829 0.000614149108626637 0.001518143523871101 2441 -0.0002305320360187677 0.0015458712744902906 0.0001127861357406194 2450 -0.0008782235596330849 0.00041780438405733934 0.001991459012253409 2452 -0.00034704855673906346 -0.002002685285079033 0.0016601300456236072 2443 -0.0005820953989189995 0.00019941855668550394 -0.0001863589437184046 2423 -0.0002489949433006431 -0.001980465185635725 -0.0020190228314080827 2417 0.0005308407308509779 -0.0015114774585240102 -0.00019133014057062456 2418 -0.0008445480294297133 -0.0010509818036141519 -0.0007102479494169945 2422 0.0007700531940899374 -0.0006200888426414876 -9.325929012845137e-06 2412 0.0011083438326864965 -0.0004026929829600728 -0.0004493796763180263 2409 -0.0006057064006397613 -0.00048570041961664193 6.944510053416217e-05 2408 -0.0019030353429861772 -0.0006219805480424734 0.00225950126240664 2413 -7.70592293299554e-05 0.000972624826513878 0.00028316133036648355 2388 0.000530073935451787 -9.889677992337307e-05 -0.0006330588543925599 2390 0.0008959860281764051 -2.2533041731317874e-05 0.001939208171778405 2381 -0.0012555985427090723 0.0014960250600059243 -0.00044945626838611237 2379 0.0022915877209145614 0.0013164980534462816 -0.0013631639442008591 2398 -6.755158997856243e-05 0.0007692446306296098 -0.0013763945622102041 2396 0.0008261647964755644 -0.00028703720016950816 3.078691646833578e-05 2389 0.002292638208045276 -0.001744638489735397 -0.0012317164676547694 2387 0.00019773245929057643 -0.0025206288910633408 -0.0010981378912077546 253 -0.0007702509740625597 -0.0012290790669879088 -0.001418781134832675 262 -0.0007803045691352865 0.0018292047950800214 -0.0019522176378075475 2454 0.0009616206327057301 -0.0019181914767905312 -0.0006936722468987566 2445 -0.0004952452379062854 0.0010734305030258551 0.0024204707295141597 2447 0.00029075034654199323 6.990628510995757e-06 0.002303059882022663 2456 0.0001407045437966845 0.0014080919724807567 0.0014589813441504686 2419 0.0015973660504911837 -0.0012133748763147895 -0.0001216648677362488 2424 0.0012841587904422252 -0.0007856036345012697 -0.00024342989619099823 2420 -0.00015349526376377126 -0.0002601088888378683 -0.00035381634813687866 2425 -0.001277050365021482 -0.0010840961854630866 -0.0002297161828061162 227 -3.395430424243873e-05 0.0012353806893901332 -0.001826029451778308 2411 -0.0007394822828068581 0.002130236566462767 0.00026046275465687555 2410 0.00031756498894073757 -0.0014256950865740553 0.00105373284967081 222 -0.0007798221077244944 0.0009248911396395345 0.0008841171421303006 2414 0.0018294278004832333 0.0006040057458477198 1.6562665057917884e-05 2415 4.188798553158191e-05 -0.0022546236188204062 0.001845624547312158 2394 0.0005114841724686028 -0.00121800075492273 -0.00034062892480960037 2385 0.002036659160905916 0.0014707529552528513 -0.0018935905885109601 2383 0.0005930602961599119 -0.0011478845706987648 0.0007596093779602477 2392 0.0008479372723784824 -0.0008707926070397067 0.0005835985466718472 2391 0.0018957996142903982 -0.00020814487349419858 -0.00016762489812156833 2400 0.0021726637741294407 0.0006397320401903476 -0.0021487665844326397 2393 -8.693309767328957e-05 0.0004726828805111671 0.0005890163418168341 208 0.00025641717625810414 -0.0005706727535819737 0.0005512998878680023 199 -0.0014385096709186318 -0.00021728156202375582 -0.0009676029043159653 2402 0.0001443993719010962 0.002569772002609431 -0.0009132902995598964 3172 -0.002125174503525746 -0.0003249791430755271 0.0010563983714742065 3163 7.503664089414906e-05 -0.0014517796782614295 0.0021161728751860416 3161 -0.0002428550631489038 -0.0015197793246863188 -0.00039958644077578583 3170 0.00037868990475667234 0.0012179732986806848 0.0008806100830006493 2427 0.0008978063983993497 -0.0012572713692635589 -0.001150789677690837 3147 0.00054856716850678 0.0010300502985606196 0.0009311048782284993 2428 -0.00035591004944456604 -0.0015699499160697176 0.0005725661676871971 3151 -0.0018275660742051083 0.0008635239413403549 0.0001697629546785922 3146 -0.0006630538440086245 -2.376886325954281e-05 0.0013619882259861425 3152 -0.0014779451032578385 0.00018427939999043474 -0.0005726437803295799 3134 -0.0005095368909725306 -0.002570221741282565 0.0004831241639354606 3138 0.0007484414150202452 0.0022380187149264098 -0.0009348844658984147 3137 -0.00022214690588791687 -0.0015405650441765416 0.00028643218573419044 3133 0.0006973294363734625 0.0002887520071111944 -0.0002578126243292549 2399 0.002095604229904083 0.0010417228203099752 0.0011688221895107005 2397 0.000775641328861541 0.001663892548722236 0.0013913287460952009 3110 -0.002398650574658196 5.02634757676302e-05 -0.0018285612462185551 3119 0.001824878161336955 0.0010540214434505187 0.0015343109682226079 3108 -0.0008821527582496148 0.0017521369530402123 0.000471800395807063 3117 0.0006418618654146088 0.0008768172487868244 0.0009407151227353206 3109 0.00038607771258734793 -0.0004342910799560503 -0.0010909503804239244 3118 0.000850542322813926 -0.0001236679107065894 4.536373583701619e-05 3107 -0.0021637887717315465 0.0004014156497576108 0.0016187678956878725 3116 -0.0013023219827893058 -0.000649956460971833 -0.0005055041884451454 3094 -0.00160807321522564 0.0009334622285581658 -0.00044254840407087145 3153 0.001757832612163025 -0.00035466149902593834 0.0005260791441809025 3174 -0.0007448110864823072 0.002265044169476889 0.0001488201076379641 973 0.0009235004096288658 -0.002245032739853145 0.0006651688814500055 982 -0.000405607293109884 0.002101860709835242 0.00197437495334825 3167 0.0015506534124594459 -0.0017937356219322558 0.001347670794820756 3165 -0.0007813825892485734 -0.00035912847635502575 -0.0024099586195511324 3176 -2.5969331900105254e-05 -0.001172269684135638 0.0016955128526696698 3154 -0.0010876355687885499 -0.0015250501105898778 -0.00014290075349794595 2429 0.0002470033582265209 -0.0005888902531390254 -0.0008292424310545848 3113 -0.00032675848529653616 -0.0006914793070029007 -0.0023586358584006765 2430 -0.000386357275060798 0.0003133131761221302 -0.0004363420830504521 3148 -0.00039692762939112173 0.0013939305774676905 0.0010425412584586407 3149 -0.000601896452811348 0.0006990462258846476 0.00011570515070949807 3135 -0.0009637172465995995 0.0006720081334052103 -0.0008090403428903894 951 0.0020019128985176993 -0.00038522564221259853 -0.0005387201833227037 946 -0.001037445465527437 0.0012053484794812062 0.0012858200145793677 3136 -0.0011452189134901862 -0.0017471633056462704 0.0017677168933549205 3140 0.0012218953696942294 0.0021801523712106246 -0.00021975312163408848 3139 -0.00035948087873627485 7.268794689770401e-05 -5.449857161851299e-06 3123 -0.0009831612892916026 0.0004266428213891148 -0.0009281692104346553 2403 0.00012292340653977172 0.0005369933640033762 0.0015402968525335809 3121 0.0016208035177887386 0.00019116903238525869 -0.00024522842366693845 3112 -0.00043063262462572725 -6.562998004658381e-05 -0.0019239157641269752 3114 0.002033870414331159 -0.00030929181176034027 -0.000533094106543528 2401 -0.0015201901222841412 0.00014594785062748187 0.0007251770313482862 928 0.0009394095023544402 -0.00224786318637731 0.00040864549784833505 3122 -0.0007250519658853864 -0.0001027913114211177 -0.00030418482986325807 3111 0.0019293552558823836 0.0018161835995687563 8.753179674974285e-05 3120 0.0026035709838091803 0.00042140720335154095 -0.0012545673011445904 919 -0.0012160275004824814 -0.001156387784240818 0.0012162110175934382 2489 -0.0003197993606481437 0.001100574709907035 0.002134116317540309 2496 0.00039485042442002926 -0.00031344823304468904 -0.0009929861448894884 2487 -0.0009304869230348439 -0.00040668296953670744 0.0014444411529158444 2498 0.00044787493025579407 0.00020457653672453573 8.178914362739565e-05 2495 -0.0003704408129825195 -0.0011451427165755726 -0.0005911038911177401 2497 -0.0008794988663784601 -0.0022976044022476024 -0.0002372734165627881 2506 -0.0007832885699263146 3.737256496979223e-05 0.00022864837904858736 2504 0.00017151480551664535 -0.0005759999404575296 0.0006332428810010793 2460 -0.0006672855087071694 0.0005473838670396979 -0.0013260185189995141 2462 8.032335593116202e-05 0.00013014408374147513 4.9936147680192285e-05 2469 0.0015052115955203355 0.00021199469723277582 -0.0007189146444814764 2471 -0.000934952416346956 -0.0001840483737188083 0.0004978775591458137 2479 0.0012103078087771892 0.00013496417732073655 -0.0006745054680158974 2468 -0.0010074792103243041 0.0013270071318191036 -0.0004782949824721015 2477 -0.0010849729814894462 -0.0013797525625192566 -0.0002360578078332375 2470 0.001366983761845053 -9.090873654607067e-05 0.00028399625898009855 2442 -0.0015500815751538896 -0.001116178232001471 0.0014283334497354047 2435 -0.00026935513700820923 0.0017147067580146566 0.00015589209376047283 2433 -0.0010604856554346808 -0.0002853128901243035 0.0006032877743383045 2444 0.0005832067808939516 0.0015561650562663002 0.0006831769580917684 2493 0.001502173812418071 9.593045836192257e-05 0.0026277685604287173 2502 0.0012526724571460684 0.0005525430026471018 0.001047946036970256 2491 0.0005711121611668759 0.0008328039015241843 0.00034384617244611823 2500 -0.0011870580768231504 -0.00014869740691055358 0.0011827304359691526 2510 -0.001360730644946495 0.0004814997362655054 -0.0021575366039960106 2508 0.0012127265081550021 0.0013137658181058712 -0.0004906232740115716 307 -0.0020907434661935403 -0.0008411856130459562 -0.0011557795578340628 316 -0.00041360305677350226 -0.0001666372701892916 -0.0015524410083893132 2501 -0.0011737262088013507 0.00027444708087255885 -0.001240618953794724 2499 -0.0010736768741070597 0.0005738410504405175 0.0010925264754107068 2466 -5.886732820053857e-07 -0.0005441776084907656 -0.0007502871147680875 2475 -0.0003483468509252953 -0.0022637985945403415 0.0011316542252322187 2464 -0.0010728374104185597 -0.0013919423792828893 0.002236229539159115 2473 0.0005258931430073555 0.0012596014692509707 0.0007101458147221211 280 0.0013791841945131726 0.0002716855296555486 0.0019349967433264098 289 0.00035785969413326517 0.00016130139168806716 -0.00041136117881894886 2483 0.0014865942525233125 0.0006387414853390525 0.0012406301045514451 2472 -0.00248448335028453 -0.0013142261589098208 0.00011693047612002742 2474 -0.0015973049833771379 0.00015133694502834655 0.0020534186628411786 2481 0.001735180100057976 -0.00010423718180155436 0.00043928244322273026 2437 0.001352798080157081 0.0009344965391886772 -0.0015061136550717647 2439 0.0002086093451081637 -0.0007307248276338376 -0.000846076094488964 2446 0.0012868988475055476 0.0014197865937841017 -0.0005746085777102662 2448 0.000559525665199226 0.00031119437976745846 0.0001329231989631041 3227 -0.0005959833201160676 0.0019286071291277338 0.0012170697754515843 2507 0.0021201301289564198 7.39336450004257e-05 0.00035212167198801466 3225 -5.514850014600803e-05 0.0020166754750058817 0.0021502864331045535 3216 0.0010704142626922182 0.0004727678900139584 0.0009165645268269284 3218 -0.0008518935919786604 -0.0011332995443157933 0.0002847911652445945 2505 0.0015182144015489407 0.0006949444164569372 -0.002316067593846979 3226 0.0019022726253102537 -0.0006809388494768713 0.0022250367434070335 3224 -0.0008011665462649303 -0.0007646349889296304 -0.00045124162825488 3217 -0.0005359950380612955 0.0012253505264373061 0.002347429075363656 3215 -0.00023280508284239504 -0.002053711604671067 -0.001021877562508006 3189 0.0010011079871239657 0.00044167613541944617 0.0006825561217557613 3198 0.0006863225296404496 -0.0008822602155359049 0.0007159920078919236 3191 0.0008236533197161113 0.00013898851012978655 -0.0014429863512738614 3200 -0.0011161010979264456 -0.00011503613839869051 -0.00034299830338171814 2478 -0.0013208956410325433 0.00036428871528287844 -0.001988872906333917 2480 -0.0007919501088856204 -4.384025546078606e-05 0.0014449674629792232 3199 0.0015034008371658132 -0.0004977038208506578 0.0009765436655281162 3190 0.0007002071190511483 0.00028647997956731275 -0.001177494695975842 3188 -0.0007560631925867707 0.0007182756172310957 -0.00035573228603951595 3197 -0.0008932916352333601 0.0004768627688336053 1.3066843389044204e-05 3164 4.604749952759834e-05 -0.0005059437124685186 0.0006407199635477749 3171 -0.000892699365708387 -0.0022862935317093406 0.0007952814915567001 3173 4.434772280157372e-05 -0.0007171982498759286 -0.0009936512167872805 2453 -0.002412059456707051 -0.0008802547273724239 0.00038395168271610934 3162 0.0021521197229501035 -0.00014289513505909898 -0.0010340257713104413 2451 0.00033073345076079647 0.0003604030242554435 0.0007334052546361412 3222 0.0007748691579595661 0.0008460419430937441 0.0009988639533271687 3229 -0.00034684690441453875 -0.0017480980556587775 0.0004234760938495406 3231 0.0010253436447619194 0.0020514299183982928 -2.9447378869010537e-05 2511 -0.00026360604515340846 -0.0001797836818889665 -0.00047532662795396474 3220 -0.00034484872712000703 -0.0025663697093355983 0.0006360468933502533 2509 0.0012321022254595413 -0.0001277215704727707 0.001000174071611548 3228 0.0020449136649369373 -0.0003523821472213482 -0.001187917735990427 3230 0.0014149152401947594 -0.0026712736489637023 0.0008192964655186488 1027 -0.0005401451151700458 6.172925945340576e-05 0.000687077539438612 3219 -0.0010449317470378916 -0.0001541885121190957 -0.0001820428866320641 1036 -0.0013288178477476277 0.0023630164723295963 -0.0014810983293960845 3221 -0.00024144851672076037 0.0005367245821570139 0.002271443013727424 3202 0.00020933514619286006 -8.939126364833599e-06 -0.0020506190168359797 3204 -2.6798062011299494e-05 -0.0015354805423708434 0.0003446840004560146 3195 0.0006020301452805753 0.00025117995049567634 -0.00079850574339185 3193 -0.0001262275771874296 -0.0007227633571478973 -0.0003760507363261799 2484 -4.444065834654284e-06 0.00011355365462972734 0.0011412111550876492 2482 -5.0870174277254905e-05 -0.0006961139676620273 -0.0016216408269478467 1009 -8.97399467431842e-05 0.0009860823526952516 -0.0005601335229308891 3192 0.001898803009165275 0.001331886921951755 0.0013950205562863966 3201 -4.5914465949075094e-05 -0.0022247761616117972 -0.000743694079434345 3203 0.0006122852670009779 0.0006497623958485047 -0.0006707048588239721 1000 -0.0005682041668949559 0.0012325880329779161 -0.0027062719288450466 3194 0.00041087087750975824 0.00017122217003486461 0.0016464593878663678 3177 -0.0021876889596211258 -0.00037251775628600154 -0.0010855974547825163 3168 0.00022989896255261056 -0.00014820640805728456 0.0019229952775245026 3175 0.000526738889120116 0.0009677814568552748 -0.00042266521182601747 3166 0.0002761400649146194 0.001255013136437617 0.0013921354084485864 2457 -0.00029417338287826816 -0.0006873900810721776 0.002099551729905922 2455 0.00010649471317396341 0.00013660980391196748 0.00025434407049842447 2585 -0.0011685938135894453 0.0007472596155499289 0.0010227134333193316 2576 0.001398458852652417 -0.001136739177380628 7.297241962497542e-05 2587 -0.0011481310350415072 0.0014077289920694722 -0.0002519100196291739 2578 -0.00046377126021106664 0.0018677088776183402 -0.0016025227610940334 2552 -1.886176450809898e-06 0.0007376912796544189 -4.1994719244340794e-05 2553 0.0014802696255952989 -0.0007655549340311128 -0.0003700356993932422 2557 0.0007681307878020854 -0.0018292210902026102 -0.000739540798566807 2558 0.0007799699138143723 0.0006828464419195962 0.0004935494931429376 2547 0.0007458339988985572 0.0004588848791553166 0.0005989712152721909 2548 0.0011029254369181295 -0.0018488617334275386 -0.00040956784106844796 2543 -0.0007046613996451135 0.0003868965455042923 -0.0022123521423049316 2544 0.002463278406543967 0.001315274390488254 0.001755142867627843 2516 0.0010075336834181078 -0.0006694503151870321 -0.0013279851068843658 2523 0.0015597997039774642 4.346068447892202e-05 -0.0006447573951971158 2525 -0.0018246878634272027 -0.0007723724110447255 -0.0005411880696478167 2514 0.0010550428275697336 -0.0005797422347719793 0.001290098473568291 2524 -0.0015027075826746705 -0.0020753997902971913 -0.00028400727323723836 2531 0.00010685570587980976 0.00030848911192988063 -0.0017025890470965682 2533 -0.00014857640464480235 9.565036199908877e-05 0.0002258032985810914 2522 0.0007533211791631333 -0.0004186933956582045 0.0013823745651282287 397 -0.00047270198344321777 -0.001801953970790037 0.00042717756790019903 2582 0.001817171086637201 -0.0001438920191217431 -0.0010242929322174747 2589 0.0026782927322040514 -0.0008022874006511687 -0.0006700211614319933 388 0.0011135731970186356 -0.0017362443059569647 -0.0012439535134407605 2591 5.8036715311066914e-05 -0.0015187826587286664 0.0006921049475623056 2580 -0.0021963006080591052 -0.0003947794549260601 -0.0012317376143739394 2560 -0.0015932128453292728 0.0017151855233467884 -0.0014854264262725105 2554 0.0003883992947971615 0.0020625848070055927 -0.00036957863590456747 2555 0.0010140534274090008 -0.0007786619837697802 0.001301972648234037 2559 0.001055992370706229 -0.001598565898481294 -0.001044371869414667 2545 0.0012082415800636157 0.0005053400595275898 0.0009570351410778195 357 -0.0004036364264128299 -0.001413083446127142 -0.000964203943213611 2546 -0.002501448901520473 0.0006337353472391206 0.0004047550950226921 2549 -0.00044298095948329744 0.0002703006133929139 0.0002443975954033394 362 -0.0006395048867826956 0.0007758407347765125 -0.0003067811412856495 2550 -0.0005232702296633775 0.00041182548236979406 0.00035138508539333656 2518 -0.00034813371490621824 -0.0008706124246692687 0.0002587492119135379 2527 -0.00034147493088725186 -0.0022220244934511 0.001228404643882505 2520 0.0023334220474977253 -0.0012460320881755047 0.00128428804525467 2529 0.0006163402657826582 0.0009071537482298558 -0.0015904646576506652 334 0.0009542064162080093 0.0007404554324298401 -0.00024536820843082597 2526 0.00018724038142836814 -0.001568292627627467 0.0004339490936039628 2537 0.00017425813668817017 0.00043004184430854895 0.0010006589948302093 2535 0.0025463041147642607 0.0010248729285295501 -0.00017931635253223735 343 0.0007899063231067005 0.0020902702267486467 9.778179724819432e-05 2528 6.779539944918233e-05 -0.0014706317201976702 0.0005672665174464978 3305 -9.065264901275509e-05 0.00032237864137136575 -0.0015284372051488585 3298 -0.0009003989097103823 0.0009303832931573076 -0.001962143343058949 3296 8.355921135437766e-05 -0.0010448870316826216 0.0003223168842584512 3307 -0.001980295950331811 0.0017643502303658022 -0.0007987262304578083 2563 0.0003865705811063893 0.0013606338162206 0.0010683187573975654 2562 0.0011509775054633154 -0.0011505816949449708 -0.001655960880537228 3287 -0.0004661094649354232 -0.0008798814360462671 0.0012688060324141399 3286 0.0006814782948744204 -0.0013723345420426838 -0.001191905436958264 3281 0.0018302607310540175 -0.001702048854439814 0.0014455169066592759 3282 0.0003223374248477067 0.0006008617313485647 -0.0005064289022288196 3268 -0.00024851435226354063 0.0023672231724849975 0.0014526132965996764 3272 -0.001689105020068038 0.0003248909112383003 -0.0019530009604056867 3273 -0.0006553597163179603 -0.0003379226323615078 -5.543162178780147e-05 3269 0.00011657348164747467 5.853031818729281e-05 1.9253055494576708e-05 2534 -0.00043762409864585685 -0.00011029198765528936 0.0004193251040557778 2532 -0.0016792842823082745 -0.00044178399317177665 -6.541293285612995e-05 3254 7.552705024304403e-05 0.001585316860606096 0.001055700029867084 3252 0.00012470611358487375 0.0017101670888083045 0.0011912132660964834 3243 -0.00089837943061634 -0.0006910188948898591 -0.0007724112967958205 3245 -0.0013882088792383943 -0.0017962951517815932 0.0011353358333877745 3253 -0.0008053207996671953 -0.002169673092423698 -1.7564796313761753e-05 3242 0.0014314044366776644 0.0010450193518379627 -2.6215614311165744e-05 3244 0.002647822285038908 -0.00035028673718635753 -0.0016647423755707085 3251 0.0007971076180710574 -0.0003600045374603626 -6.960451739059458e-05 3311 0.00021960181094669666 0.001120154118112065 0.00011097828753487383 1117 6.845498288632042e-06 0.001763016995729889 0.0011581378644352895 1108 0.0005169385021484192 -0.0012924561646864526 -0.0019639299351372932 3309 -0.0005948109444113153 0.0010600651444644027 -0.00043888570852677997 3302 0.002256109856221681 2.5639636442893656e-05 0.0006105889507563796 3300 0.00014882302430435437 -0.00161757372067236 -0.0004225310186188752 3288 -0.0013603711740478037 -8.91229514981477e-05 -0.002102040599250786 3284 0.000457359999529847 -0.0012779736062975859 0.0005307064392343362 3283 -0.0019205411403092208 0.00039555109157146423 -0.0012795295808166291 3289 -0.0005660571028774894 6.67268245827554e-05 0.00015807750801962004 2564 -0.0026604148418254837 0.00037570115931979736 0.0015160109269707 2565 -0.00038602885202195295 0.0017225300586955574 -0.0023343388096214853 3275 0.000748843654755336 -7.426968222836925e-05 -0.0015493022366600577 3274 0.0013530058807199837 0.00010794615920264742 0.001110551965457363 1081 0.0018362172564685545 0.0010983096622734366 -0.0008160284623909564 1086 0.0013059721929425893 -0.00028177092335043255 -0.00026430067817266264 3271 8.207544129282089e-06 0.0016186173129812906 -0.00030926248025827784 3270 0.0006649297299034186 0.0009134869378210554 5.9196614726260205e-05 3256 -0.0010134257212916905 0.0006228152353089569 0.0014052644503221878 3249 -0.0003315822036934666 -0.0003084280430542541 -0.002647132470822207 3258 -0.00023229654613365967 0.0001763687304866964 0.00031851291290008513 2538 0.00030261331074194885 8.822313051456141e-05 0.0013922369983661192 3247 0.00017895662823595607 0.00026732731863725843 -0.0013771401231133585 2536 0.00149610747680073 4.248946545407561e-05 -0.00033676420987023504 3248 0.002568121124137306 0.0008930596876660496 0.0010983273392444195 3257 -0.00041735683589831435 -0.0009015956349733908 -0.00037918802388162484 3255 -0.00039261537910775714 -0.0012649888450473566 -0.0012690121132793147 1054 -0.0019350334341862827 0.0013602663291594906 -0.0003053048080832484 3246 0.0014652845075908945 -0.0009917991518924353 0.0010416054089423977 1063 0.0012461489301199963 -0.0022511021123307064 -0.0006303665696723005 2638 0.00040078811600716396 -0.00018205643178075036 0.0022754818934732834 2633 -0.00014970879881985653 0.0021195145732207017 -0.0003607871391161071 2634 -0.00044676199613256115 -0.0027687818491148835 -0.0010673748405007292 2639 0.0008530176366417276 -0.0007509122942232227 0.00016764421585495565 2628 -0.0006426369104559253 3.11645837391219e-05 -0.0002676949317744063 2629 0.0012198224660516573 0.0014046154325287462 0.00028551630865776643 2624 0.0008359103915237614 -0.00029068947061471127 -0.001886422133953359 2625 0.00036029223527511565 -0.0002294814123771117 0.00044999975655131636 2595 0.0012983115801002854 0.0005198653522862496 -0.0003453424128635007 2597 -0.00134436002035537 0.0018307562508035002 -4.561829757332111e-05 2606 0.00044121206326249015 0.0012266087144939502 0.00040071275070197314 2604 -0.0013174255242731677 -0.00013097703737013867 -0.0008263350001410943 2612 0.0008003948473667894 0.0006162612824235703 -0.0004106258430677616 2605 -0.0007697510505409481 0.0007294735136721849 0.0004913382884226456 2603 0.00011710356534673136 0.0021501140182414043 -0.0007336800184296888 2614 -0.0012003866572045665 -0.0005703395552329417 -0.0015409231146714187 2568 -0.0012847635774864662 0.001146793951675869 -0.0007255411494621858 2579 0.000711434824034247 0.000525937910533558 0.0006368911650454398 2577 -0.0002688700779090382 0.0012796663006240019 -0.0009423156297349627 2570 -0.00023503179469967815 0.001166357559516777 -0.00021442654376715325 2636 -0.0011701343459843885 0.0018056105838130175 -0.0005523490641400825 2640 -0.0009207533823447187 0.0017381572345548876 0.0011531778211400492 2641 -0.0012598504318375007 0.00043178644802202484 0.00041216858185589563 2635 0.0014468619953700126 -0.00022101194486692528 -0.000891677728408166 438 0.00015352891259423325 0.0011760918100538053 -0.00023179571425250515 2631 -0.0006301236167699498 -0.0010639024526702188 0.00017976059916157653 2627 -0.0017914632636026643 0.0017972865243726344 0.0022865228318780105 443 -0.00011930580429281063 -0.0005822486526780669 0.0006001135005403212 2626 0.0023489256085515785 0.00013894441899692527 0.001252284305986234 2630 -0.001925579633337365 0.00034260621714053826 -0.0014974939917971617 2610 0.0003551836880936626 0.0016994312363411567 -0.001282606439499898 2601 -0.0011279835971226815 0.0022469597340697687 0.00011579790342867047 2608 -0.0019805171568684195 -0.0006336532564016176 -0.0008406733466741452 2599 0.0008943551355171917 -0.0005407690596137001 -0.0013410970147845949 415 0.0006842502612195568 0.0019212876219897757 1.2186978453481833e-05 2616 0.0004446387302534172 0.0010044605437459744 0.0004311418083952144 2618 -0.0012122670346539858 0.0009946596455322949 0.0003077849231399204 2609 0.001532293004112754 -0.0007630225562612878 0.0015837723796244595 424 -0.00011054249517597264 0.00039718517524073077 0.000819280596306335 2607 0.0001428468739231236 0.0013740029318046302 -0.0005255377470476823 2572 0.0001692833140941809 -0.0014677020464575604 -0.0006139745826296344 2574 -0.0008136898013967988 -0.0004591644033600335 -0.00022922605263679192 2583 0.0003568332178400524 3.9824657023619935e-05 -0.000288343479668918 2581 0.0007437272451651679 0.00036965429428731204 0.0015593972912071007 2643 0.001629602186678042 -0.0011404498216131536 -0.0007785147437196154 2644 0.0015838837715574138 -0.00024021226104198405 0.00010919144158382725 3362 -0.0007439170744692031 0.0007438793549090398 0.0002646946253394996 3367 -0.001191689022551856 -0.0011961802619009415 -0.0002298759048287211 3363 -0.0026504524499790976 -0.0003695459713960362 -0.0005965901179951353 3368 -0.0008441969832234737 -0.00023956522593386514 -0.0011441425403516346 3350 -0.0005419147280527007 -0.00016815813166870313 0.0002937802415580433 3349 -0.00014642143879993507 -0.0008360813952195551 -0.0005488352873041859 3353 0.0008395326170591139 0.0022534324147347393 -0.001056964232910104 3354 -0.001360317446554827 -0.001697069724900451 0.0009306687400888796 2613 0.0020237367253873473 -0.00029076000764250353 6.596026104873547e-05 2615 -0.0003782864368099263 0.0003510599119774568 0.0009171211670355421 3324 -0.002386812667821039 0.000308163039088092 0.00074522389789931 3326 -6.18300428118898e-05 0.000556624135412532 0.00048664772573065145 3335 -8.405311192132784e-05 0.0007498685578949149 -0.002703758576053674 3333 -5.001209443526787e-05 0.0006400574989876856 0.00024612014752636076 3334 -0.0013973981200864724 -0.0004930660766409216 0.0008225950546594497 3325 0.0011050046727039183 9.048446398868281e-05 0.0015856028370300433 3323 -0.00013623356137900484 -0.00048407008691166815 0.0002518589426150175 3332 -0.0015413697169979763 -0.00032921852505679843 0.00047829849596244466 2588 -0.0015596087782844261 -0.000613245788690325 -0.00223883910309023 3308 -0.0009911352205574525 -1.5262025169190642e-05 0.0008338537487991131 2586 0.0002371841326308077 0.0011976992836752348 0.0016487329501779675 3299 -6.112991697512261e-07 0.000250847336799419 -0.0025580367604383066 3306 0.0002442320020511603 0.0005567283377686679 -0.00034534930702037506 3297 -0.0007330136325322523 -0.0005175500440007758 0.00031329373595503094 3364 -0.00010071601516805739 4.61805760115213e-05 0.0006852451531942048 2646 -0.00028753529877340554 0.0007311470495045293 0.00046376916374144027 2645 0.0008185532660319552 -0.0006281488245605611 0.0016610075297475969 3370 -0.001644549986218867 -0.0017389450592706658 0.0004739559435299463 3365 -0.0006444198909333215 -0.001546862850272068 9.21108034122398e-06 3369 -0.0014358012326525797 0.0013546562842968839 -0.0005375445364088323 3351 -0.000998737509449235 0.0008035623702541642 -0.00032710869883140724 3352 0.0005012146700888482 -0.0012045856694841211 -0.0009861249283689183 3355 0.0008872810546471 -0.0005542853468863214 0.0008139234725084968 1167 8.113466490270262e-05 -0.0019919588402953423 -0.0013545724365017625 3356 -0.0003254501719330441 -0.0002967782108856125 0.0009244019654061375 1162 0.0009031017091194577 0.000215339800339707 -2.0372427113925988e-05 3339 -0.0001487578977609448 0.0020543174745208813 -0.0005348962899153424 2619 -0.0006383756826149035 0.00023535138203316548 -0.000275419011500331 3330 0.00021335192887440564 0.0014127832283998241 -0.0024474354805364557 2617 0.0008153057665696505 0.0012941883156715583 -0.001018389309134001 3328 2.3871598100165927e-05 0.0008340673873073194 0.00031796217888991154 3337 0.0007933689016030777 0.00113354554597674 -0.00010920724418890879 1144 -0.0006269118307637574 -0.002463886663261038 -0.00024567941660541244 1135 0.0009554692950959455 0.001428737256349846 0.00028545578993614167 3336 -0.0020330377360470438 -0.000793826043843592 0.0019255014844067422 3338 4.596215570808627e-05 -0.00046112700235696746 -0.0011478137571703285 3327 0.0011807275484892823 -0.00015330848831381538 0.0006421542334719864 3329 0.0018776177506008866 -0.00030875938210944785 -0.001715402866002494 3312 -0.0002631092581728806 -0.00031218864861897334 0.0023235549019972107 3301 0.0022559131457494173 -0.0009166806506964087 -0.001678451641173187 3303 0.0011585406813803259 -0.0013677487796363564 -0.0015231818261692983 2592 0.0013987227248834552 -0.0012464436879161642 1.6254582112878242e-05 2590 0.0001303540574929137 0.001755329650703275 0.0008832226200888738 3310 0.0016484857473604607 -0.0013506038322670573 0.0022254007207592927 2711 -0.002142512859228544 -3.710177993430019e-05 0.001102774077453753 2720 -0.0004666204627340817 0.0006021731610552368 0.0005061626180697671 2713 6.956576353299135e-05 5.34539821394355e-05 0.000650484739521366 2722 -0.001327519825471511 0.0015882328050837913 0.0014402293745358747 2685 -0.00016591544655692142 -0.0007947329047705119 -0.000942705023757921 2676 -0.0003228634540826244 0.0017402325729435656 -0.0011834641910836612 2678 0.0008741696350454469 0.002684324892756839 -0.0006723134136771714 2687 0.0007329886517641977 0.001597364958066976 -0.0014505989124733406 2686 0.00202685191666597 0.001133485032035938 -0.0013803490308241005 2684 -6.825498079706662e-05 0.0017187906584957106 0.0006341684242692886 2693 -9.50327018738738e-05 0.0015479897199144532 -0.000806152283691826 2695 -0.001035900475807938 -0.0012921543236238617 -0.0018552482118497017 2651 8.833187151587063e-05 -3.744026566686841e-05 -0.00036994417748521493 2649 -0.0018894088900886028 0.0007524958088555546 -0.0006638987469789657 2660 0.0006829815241500329 0.00034942026035199997 -0.0005067994178349052 2658 0.0013174430893628845 0.001441080684123696 0.0021660139469209284 2657 -0.0019605387507309812 -0.0009188733393337371 7.223109896060584e-05 2666 -0.0004310419036580981 -0.0019841613880859964 0.0013572250099720285 2659 -0.002366136940579323 0.00025395510367834476 0.001188067147261281 2668 0.0026087310463001143 -0.0020995040101945417 -0.002164847364623282 523 -0.0021889271562263663 0.0008533300374830952 -7.761779391897991e-05 2715 -0.0001680251548249155 -0.0009445614975894052 0.0016151776116505152 2717 0.0006235149674863416 0.0011060739373143988 -0.00027139782331068085 532 0.00026953095124292344 -0.0015678598017896152 0.0006120353253679846 2726 -0.0017361375624407658 -0.002232858801226461 0.0005711173535510265 2724 -0.00020991147629259815 0.001121055232503872 0.0024468326846704127 2680 0.0017168628830644102 -0.00012599889586745877 -0.0010745680269926613 2689 -0.00028446587317753377 -0.001632031183523978 -0.0003716814326352167 2682 -0.0009678051778541097 0.0005211577053863619 -0.00016047459600063217 2691 -0.0023122785206656994 0.0005041566729321093 -0.00040582669738154853 505 -0.0008452120760965877 0.0007971890002721581 -0.0005454016385697396 2697 0.001219421885858603 0.0016398721954660415 -0.0007566549499980037 2699 0.0026062763611350436 -0.0013187789250994485 -0.0018637535523662744 2690 -8.973978413024484e-05 0.0005262958206100894 -0.00021527538530430345 2688 -0.000980498453430381 0.0001786056696502753 0.0005372090378986317 496 0.000256356155361762 0.0014883361349307931 0.0013164062646645964 2653 0.0018521814212725319 -0.0014744119410164884 0.0021426302899897674 2655 -0.0004570141101464969 -0.0011002475232557238 0.0017036530110335062 2664 0.0006145080667378732 -0.0020623471920055156 -0.001768268036475527 2662 -0.0017490782989188056 0.0007397467991964116 -0.0009187860986773127 478 0.0008463150890118123 0.0011851513310121467 0.0010163754260235744 2670 0.0014357764331804006 0.0008850758250435729 -0.001711044427373105 469 -0.002194373127745484 -0.0006765863447007561 0.0003096397180938963 2672 -9.076679641324627e-05 0.0004856317185129353 0.0006416486149661556 2661 -0.0019700677073557203 -0.0008880682859508291 0.002302875025608102 2663 -0.0003686871345866486 -0.0002953492674860284 0.0016914440678498406 3431 0.00013510589417455824 7.537285908633742e-05 -0.0003279356684269281 3440 0.0010094153322926357 3.878545116452322e-06 -0.0008068401429360359 3433 -0.0005539727217707504 -0.0014294980548790628 0.0022594119460530096 3442 0.001274500237217993 0.00037660712209583187 -0.0018767535907982117 3405 -0.0014715950692626044 0.00061839705514739 -0.001182575259483249 3414 0.0006278215232201415 -0.0014431104726329244 -0.0004796290990644953 2694 0.0015487206711885548 0.0018256828032271514 -0.0012352956943807326 2696 -0.002055652742959284 -0.0010193089855010163 -5.484066802946856e-05 3407 -0.00021794624406446894 0.0008372399666724337 0.0008191824692579909 3416 -0.0010436428151454743 -0.0017526804927560987 -0.0013930148823475198 3404 0.00040523025799840424 0.0006590496834070259 0.0006692484681483509 3406 0.0019017244567214057 0.0009563987940499812 0.0023989470851509495 3415 0.002162845254772382 0.002227723684625174 -0.001962609304752129 3413 -0.00047591155106118006 0.000915928515067983 -0.0014865681996280944 3378 -0.002360882942814532 -0.002368486011076953 -0.0017128084016820705 2667 -7.994855585258861e-05 0.0009442964634422082 -0.000319164896423353 2669 0.002500748835067489 0.000971676264641819 0.0014313769938002225 3387 0.0005291483900448902 0.0018267182928465714 -0.0006430189140624646 3389 0.00029145072978341746 -0.0003598081629620246 0.0002689064080580914 3380 -0.0004545569604090824 1.966799189753298e-05 0.0005112330932681628 3379 0.0013251113307967293 -0.0018079535758960255 -0.001366261904086475 3377 -0.00021417060752692793 -0.0009758564275283528 6.239788232235781e-05 3388 -0.0016400691639413456 -0.0004475072666284966 0.00036921410185356256 3386 0.0010776639896379627 -0.001839890006646919 -0.0013795675014261714 3434 -0.00029898213005770825 -0.00019352262743645133 0.0021809886545357633 3392 0.00023149928701139428 -7.274549773679854e-05 -0.0012418788174597822 3390 0.0009079011195058668 -0.0015428721334083144 -0.0001679890840443803 3437 -0.0005142026271255701 0.0011116732578677565 -0.0001286534522621707 1252 0.0007960024486993089 0.0016940594660452564 -0.00032216518416792344 1243 0.0022432555746977998 0.0022636495924304835 0.0019696742269814287 3444 -0.00021998301168676878 -0.0006875066776077887 -0.0004244679319089751 3435 -0.0010851417307030686 -0.0008196643465263541 0.0013377524499442375 3446 -0.0008662140336940065 0.0009539206840040891 -0.000529525954706879 2700 0.0005784477836855304 0.0004352583246708434 0.0012771053520255144 3411 -0.0004190109308563209 -0.00036775874494351387 -0.001998160606175408 3420 0.00036074262849597667 0.0018851460833138535 0.0013583566759447598 3418 -0.0021946535448217975 -0.0017502601751594841 -0.0015319967963340622 2698 5.267559258862083e-06 0.0009394718422883492 0.00020219684785690445 3409 -0.0015958742424397544 -0.0014154828597289799 -0.0002291197359165862 1225 -0.0015095199505839462 0.0022281602139715994 0.0021582266005695577 1216 0.00037292361485923974 -9.122491193295666e-05 0.0008841610688968481 3410 -4.973756249893567e-08 -0.0015886670329121253 -7.824001490865551e-05 3408 0.0007791398039419036 -0.0006347862815564198 -0.00011570380878015915 3419 -0.0009746122387368781 -0.0017405190981097517 0.0012201844975818247 3417 -0.001491211784305467 -0.0018173813996316794 0.00010321849787323916 2673 0.0002082823454667113 -0.0015631752057085758 0.0011603738324634768 2671 -0.0009234858447995371 -0.0007607292254907965 -0.000515570249111569 3384 0.0005624479544059961 0.0016135045915382407 -0.0005765487258499841 3391 0.002057825055345508 -0.0022254794072728715 -0.00036228021834003614 3393 0.0017211216069815808 -0.0025118947141432586 0.0001644988818835716 3382 0.0016375190082598486 -0.0013816415143991549 0.0006639883111899628 1189 1.2817835897496223e-06 -0.000502531175668839 0.0014452903116401066 1198 -0.00024101434191742792 -0.0008549051485110305 -0.0001254186932230384 3383 -0.000707207237731982 0.0015794699196123015 8.646354390918999e-05 3381 -0.0011358484779908857 -0.0023344530578558926 0.001364379536593731 3432 -0.0011395247345989993 -0.0003772938227384129 0.0003299095946344324 2801 -0.0019144995409906159 -0.001213686220719073 0.00037858903993775615 2792 0.001493633515508741 0.000931468416305144 -0.0002990943084697358 2794 0.00043743286300590716 0.0014059838922895705 0.0012038838315745104 2766 0.001233816064640616 -0.0023133617099994354 0.0002943745055937518 2757 -0.0016733016023868315 -0.0004496554724421132 0.0019492681925430556 2768 -0.0001650130140494595 -0.0003887239455540915 0.0008061512122537347 2759 0.0006521793463708475 -0.0017320225804569505 -0.00016936077493765757 2774 -0.0004098482108669376 -0.0018590808465454118 -0.0007476689954421605 2765 0.0008513783744504256 0.000541409414424278 0.0019738977342584406 2767 -0.002116106033144344 0.0010628377926512416 -0.00031928736192835477 2776 0.001065412613939604 0.0013409687828260834 -0.000475998246911593 2730 -0.0014439920853057888 0.001200822726941178 -0.0014188970777781315 2739 -0.0008326535042759935 3.398164906822602e-05 0.0004820187904255341 2732 0.0007538604187921374 -0.0005878095077130644 0.0011685816115617363 2741 0.0004268854522827523 -0.001792211408423582 -0.0008529831388945248 2738 -0.00044237205137690383 0.00045229700949699493 -6.203659433341377e-05 2747 -0.0016217359579271775 -0.00028660536643279757 0.0012552441649203636 2749 0.0019647454911022625 -0.000156036243687795 0.0007529846075005554 2740 0.0023648313710142527 0.0008628921190840719 -0.0024244794014135532 2714 0.00044734162486266527 -0.0010125051739373844 -0.0014937109880906988 2703 -0.0013646914409377905 -0.002307673981477787 0.0027125474874181363 2705 -0.0025435525793365416 0.00023592084316850304 -0.0002318374893183605 2712 -3.3951350142320466e-05 0.0007811361064123546 0.0004476811192142087 2803 -0.0017009451028161086 0.0012229915841777284 0.0001499495217340079 2798 -0.002593741489466007 -0.00043219224897330755 -0.0010224201521363413 604 0.0017633643569541077 0.002243372487303823 -0.001026758903299065 613 0.0003304065113672386 0.0002386429698227602 -0.00014465785662320756 2807 -0.0002335742588328866 0.002193054885043 -0.0014551407190919775 2805 -0.0010893496996434511 0.002073368926218174 -6.823677019154092e-05 2796 -0.0014725752619199036 -0.0011798584125245642 0.0005761667207924985 2772 0.0010175066214322239 0.000649640519403727 0.0006005566976981956 2763 0.000466049274133224 -0.0006457552406517342 0.000502802249680338 2761 0.001194892193138253 0.0009419433884814422 0.0017888513773663126 2770 9.370037128360865e-05 -2.5305967115098334e-05 -0.00036442059631839425 586 0.0001909527906457612 0.000726506912597518 0.0024849051935217164 2769 -0.000932063057365607 -0.0004387272681092184 0.002070168416544479 577 0.0016366872473041775 -0.0011275071649837812 0.0003599434418068471 2771 -0.0017444642493237108 -0.001110449349567388 -0.0011060021755675198 2780 -0.00015916436466517376 -0.00024084080243563354 0.0007814100503405865 2778 0.0017475383310113558 0.000949197970768714 -0.0014140889319573852 2736 0.0008328915529892786 0.0018049164105249649 -0.00045021333018784374 2745 0.0003319967927282385 -0.0007357968139060722 0.0023342588365075252 2734 0.0006821306212817062 -9.51050584645482e-06 0.0017514285658204096 2743 0.001941459077846462 0.0009876087345666068 -0.0003870935497066866 2744 0.0013270271529555275 0.0017641747674827062 0.0025938910193761587 550 -0.0005463119053865017 -0.0010085830328443962 -0.0015414216591035676 559 0.0005401249415013478 -0.0008661831650083451 -0.00020187918253504597 2753 -0.0018593688909672276 0.0009903107582198362 0.00011654739593291129 2742 -0.0014560249968291936 -0.0009355143533909477 0.00014599177419861564 2751 0.00048411660060863806 -0.001836351438021798 0.000420241696551996 2716 0.00017914480184250993 0.002275529756871353 0.0001408601577617013 2709 -0.0027675200171505803 -0.001038329472100975 -0.0006918818716969372 2707 -0.0021705239982951676 -0.0012027506212008042 0.00018936021598855133 2718 0.0010373107686234779 0.0018140424351351086 -0.0003058409492428774 3521 -0.0011034125867743255 -0.00024292572658355836 -0.0010234768617549492 3514 -0.0006171658545821685 -0.0005861022088198612 0.0012183224010849886 3512 0.00015170754467103056 0.0005641140576682596 -0.0027405111603559114 3523 3.77592477257202e-06 0.0011693730096889391 0.0007573760719805378 2777 -0.0011726868914438307 -0.00014459733666048378 0.0005171379789584416 3488 0.001287845635795373 -0.002289654244544624 -0.0011482895995550144 2775 -0.0025341993033694246 -4.575656253020459e-05 0.00044784854636103284 3486 0.0012460045241173975 0.00034330359658680935 -0.0002842834204295901 3495 -0.0017054380944894656 -0.0002568430372848305 -0.001226197563248384 3497 -3.1699275924316865e-05 0.0014305583944866308 -0.0013588174978242116 3487 -0.001248764648564289 -0.0016700606279526034 -9.109037110094755e-05 3485 0.0014484008931850022 0.001469946480796764 -0.0010600942823573406 3496 0.0008929035563451706 -0.001725566721476822 -0.0003859224920937589 3494 -0.0005483184824790035 0.0009419768659160955 -0.001095301659057075 3459 0.001074052874174889 0.0021353880296379533 -0.0003104273375951906 2750 -0.00019469823246478086 -0.0006154663774277681 -0.0010208734821277768 2748 -0.001967524113053064 -0.0005593837064950577 0.0008723078083428048 3461 0.0002454435412549572 0.0012933454906169659 -0.00033697831140714306 3470 0.0020410440858146047 0.0021112154963578034 0.0004737042079812509 3468 -0.0006430513633091399 -0.0015335636927157623 0.001088677104139046 3458 -0.00016141571212549945 -0.0007483135496101107 0.0011167946587489694 3469 -0.0002893701808716607 2.388374152185622e-05 0.00012814976853579114 3460 -0.00030776879249670003 0.0013160807501973303 0.0011607617424247625 3467 -0.0002439613396227622 -0.0009806116772880609 -0.00018845005042371452 3443 -0.0007989100304991984 -0.0004834530952309824 -0.00018258947223055906 3441 0.0009547352170739759 0.0007565839661773792 0.00033812257119515427 2723 0.0018102543179575785 0.0005172013465615344 0.00104057753782292 2721 3.4138811492585765e-05 -0.0013638440870017024 0.00044785765308808965 1351 0.00026086085076435905 0.0014234059493850653 -0.0007475149994533353 2727 -0.0025547709374249172 -0.00011783914973648776 0.00013382947412207666 3516 -0.0015370959446256063 0.00047593195026775556 0.0014480909778734185 3518 0.001036724301891619 -0.0007196118082295412 0.0009049226135150889 3525 -7.351370213974054e-05 -0.0015456792537000994 -0.0009882456751335587 1324 -0.0016599885773852167 -4.3322790282744345e-05 -0.00030129447391240814 3527 -0.00012013525505310608 -0.0007707944639974524 0.0015077749824479116 3490 -0.001511453630411941 0.0007845026552994593 -0.0015808442236401143 3499 -0.0005271612432045504 0.00044328714148556035 0.0017333800962423128 2781 -0.0022759188792787588 -0.0004535783095975382 0.0007697015332170285 3501 -3.582663635058039e-05 -0.0003050013128056274 8.12710889557095e-05 3492 0.0005695284117636185 -0.0001105191936078085 -0.001920862116026387 2779 -0.0008990180540268133 -0.0021899150726025643 0.0016151815513101415 1297 -0.0008109107056827132 0.0009014239015463523 0.0011553349474585212 3489 -0.0013738027607334545 0.00020995420331702689 -0.002106681073720733 1306 0.00013172009479408176 -0.002728791821013419 -0.0006992765824859037 3498 5.727576645657125e-05 0.00026280854813370987 0.00031771439378606016 3491 0.001279625532449434 0.0015491384480606607 0.0005390649386079975 3500 0.001171912952200915 0.0008238681356792616 0.0012174986208803576 2752 0.00019685384820893504 0.0021288706992936726 1.3874408527709148e-05 3465 0.0005622820214505062 0.00045980625790780416 0.00036758664577293647 2754 0.0023824055187962705 -0.0011890747274196757 0.00210962012821547 3463 -0.00019987112877793223 -0.0003730780075030535 0.0012345077628547624 3474 -0.0015485576479971185 0.0012589581931941299 0.001961453413913329 3472 -0.0017820709111762893 0.0006959099331563931 -0.0002429787183762447 3464 0.0008824060781232339 -0.002290312574747673 4.9765000130202796e-05 3462 0.0004904637578008863 -0.0001384660509630548 -0.0008966545935517685 3471 0.0008321925712774572 -0.0009832902892265678 -0.0020610989494169968 1270 0.00033629296437715926 0.0023146182243813525 0.00040219663363005604 3473 -0.0002147142115388629 -0.001833546851184646 0.0002496105528953542 1279 0.0005240646170893906 -0.00018784535360175623 -0.0025375271033970847 3438 0.00015752353543004466 0.0018391648038554279 0.00033738769264191493 2725 -0.00020506604643940381 -5.8690854023490946e-05 -0.0022958040073966287 3447 -0.002429709044827265 -0.0015033664068380556 0.0019917588360967085 3445 -0.000979381397011447 -8.270296777461677e-05 0.0010305655562846115 3436 -0.00010418138141918536 -0.0004350534764035593 -0.0014283256049998768 2854 -0.0012654207145991504 -0.0021302748829831954 -0.0005534890796408374 2855 0.0021918207864671997 -0.0009306379171605983 0.0011195424738493327 2850 -0.0010188403877671108 -0.0020953847235983224 0.0009179602965478213 2849 0.0004107166877819525 0.0009852218280326716 -0.0008146256427317635 2845 7.0570953351039e-05 -0.0003268103716889941 -0.0017494812157968524 2844 0.001898500097692298 -0.0016828711332120539 -0.0006260424933922775 2840 0.0006489471967476305 0.0007141480847310902 -0.001172677540612767 2841 -0.0005299832832530813 -0.0004330364147453144 -0.001920121114175058 2813 0.001832444790439717 -0.0012781737094017902 -0.00051781117451128 2820 0.00036165236773723206 -0.0005189127752066288 -0.0001012795000720104 2822 0.0010048244265157041 0.0014307389953921502 0.0008986764063943949 2811 0.0010743518470066732 -0.0017765140817903912 -0.00081439742616957 2821 -0.0016678330803022875 0.00186017646150103 -0.00022080080950861395 2828 -0.0009997563979188945 0.000717333886496903 0.00042824970363563507 2819 0.002503600065200034 -0.00039910543612883733 -0.0020409793399785202 2830 4.2587349297471986e-05 -0.0007348412016879945 0.00228565338130789 2786 -0.0008886515040324598 0.0001653582614908194 -0.0011933252302105035 2795 0.00010030130335184225 0.0015995331929617462 0.002671579882479392 2784 0.002125270863530107 0.0023226654743104913 0.000551517290126328 2793 0.0009957889855490374 -0.0017175071110413524 5.013623565230187e-06 2856 -0.00033445869434890914 -0.0006836687628379017 0.0011613143838196986 2857 -0.0010687490117633543 -0.0005752696055386357 -0.0007650299297522113 2852 0.001230493373359471 -0.0015238157182781724 -0.0004316674284291944 2851 -0.0005678620348833424 0.00020106921588215732 9.409802602967834e-05 2842 0.002586940039408449 9.508268801705958e-05 0.002061562941021801 2843 -0.0021726951221862417 -6.3718076123966e-05 -0.00034007389410948587 2846 0.002311608092224463 0.00021624681439284425 0.0020447856014903917 659 -0.0001960505747685493 0.0010770992881831397 0.001001358207906824 2847 -0.0020909232003173024 -0.0015566547177300076 0.0002908067876197082 654 -0.0017143195617848501 0.0005702483380059492 0.0001250150399885404 2824 5.822467786504676e-05 -0.000468745239020089 0.0014005595184149286 2815 -0.0002076525471487933 0.0015650362629258021 -0.0009440148417595675 2817 0.00011462490205160845 -0.00044643943712946075 -0.0014006874790103282 2826 0.0006998784672973746 0.00026525329219736875 -0.0012713765272003349 2825 0.0005866924439412659 0.0002713952934322781 0.0019142607581031004 2834 -0.0005836260254883785 0.001134303170993638 -0.0005022776084606185 2823 -0.0012414701553940415 0.00020258540545535443 -0.0002703764341633766 631 0.0013063262112050745 0.0011200933952270624 0.0010866089639534997 2832 0.0011533563947551835 0.0008560751421385264 -0.0019943044227931587 640 -0.0010585520604772204 -0.0011640071056350403 -0.0002765488215356928 2790 -1.4953639739016377e-05 0.0010782080158079216 0.0009921903894140075 2797 0.0016247737680220745 -7.38170215553112e-05 -0.00015590160787362682 2788 0.001614661675407899 0.0006681064896914225 -0.0023763616150476144 2799 0.0015886470011752508 0.0021165200861398845 -0.00010186951034305762 2860 0.0014340054015665863 0.0005981550037337823 -0.00029169520499759417 3579 0.0013834396462244648 0.0005509096440145261 0.0005126648983216583 3583 -0.00044709139488855235 -0.00025854190149203786 0.0009047161533668384 2859 0.002553901324137869 0.00013166080587511918 -0.0002848746861061459 3578 0.0008550997210750529 0.0004426164059367216 -0.0016160025629316194 3569 -0.0004047561998232561 0.0008885059184112704 -0.0005950629149209955 3565 -0.0007502582812586936 -0.0014392960786550062 0.00046179632224028014 3566 -0.0018572313716615622 3.509230680572538e-05 6.477471291388794e-07 3570 -0.001930946543909006 -0.0008299642072354695 -0.0013786541053154829 3542 0.001331454590523784 -0.00027217661433634596 0.00013650578987670905 2829 -0.0012881158224689038 -3.0119907960641894e-05 0.0020021525929634345 2831 -0.0015229120371792757 0.0017486764764683977 0.0002751405715346113 3551 -0.0015815527344759505 -0.0014606924946276051 -0.0012512440136632163 3549 0.001294279298584011 -0.000449243513004348 0.00015481279323071619 3540 0.0009324144063984656 -3.8617092499055846e-05 0.0009785813827195822 3539 0.0012972006235338165 -0.0007239137746830486 -0.000541415766731563 3541 0.0008110438114381003 -0.0008510184198682361 0.0008540126954887698 3548 -0.0003035278100232923 0.000906237451493317 -0.0016446011707916593 3550 -6.874687973807531e-05 0.0004699664251657143 -0.0002541103024192232 3515 0.00046842351446360576 0.00035643533442766785 -0.0003144659220844973 2802 -0.00010738724177403354 -0.0006247990313278664 0.0009687716746774953 2804 -0.0015984260645592763 0.0018192085754470406 -0.0008538258505061602 3522 0.0009386805157813234 -0.0007015135230007503 0.00018908748104326826 3513 0.0005287348422083611 0.0005316261935511893 0.0017589501132098538 3524 0.0001864867749614323 -0.001787818126033275 -0.0012958724854570036 3584 0.00015659206976582094 -0.0004863757513340957 -0.0020691495660831206 3554 0.00015744542383422854 -0.0006414849567694121 0.0014255113067575993 3552 -0.00020919919513426397 -0.0007289116278855635 6.817719381412826e-05 3543 -0.000915752780026826 0.0006766297609272763 -0.0014135936638341017 1333 0.002173751165728785 -0.0008587838943520539 0.0007717817356049102 1360 -0.0002561911162820324 0.0014017742296758638 0.0009106653676615661 3517 0.0001379604395501044 -0.0012861496719736441 0.0002062409903938042 3526 0.0003069574834371387 0.0009814390558102134 -0.00020465079450686353 2808 -0.00017627420155499982 -0.00015268472338626857 0.0007599896384788659 2806 0.00020672974692687344 -0.0010072214347410981 0.0005454428207689224 3580 0.0003357833295437435 0.0008145190462772666 -0.0024028649032296597 3519 -0.0015996427723239874 -9.553037051879742e-05 -0.002172528556303178 3585 -0.0009837669686045699 -0.002078938646663087 -7.288097067713111e-05 3528 -0.00025783618628728643 -0.0001868775060202203 0.0007692760495854376 2861 0.0007410297698967553 -0.0004892602101298766 -0.0025609063880939814 3586 -0.000669524220357792 0.00011330645169637386 0.0021443353439856852 2862 -0.00048340610061406084 0.00038358209143437736 0.0017398985674029882 3581 -0.00011981238375781324 -0.0002890538481722624 -0.0007910104093501156 1383 0.0008794027145385794 -0.0008522622387470711 0.0006264125422040992 3571 0.0017146784669436752 -0.00045220501922305263 -0.0013826084519704858 1378 -0.0009774491186438417 -0.0002064613400434897 0.0018816181216216492 3567 -0.00022932585999399274 -0.0004010615251650151 -0.001270668413558287 3572 -0.0011735000347227224 0.00023118268937959065 -7.641102722399289e-05 3568 -0.0012498792356908978 0.0008712386323285967 -6.088460909658153e-05 3555 -0.0013725020933591167 5.415434364974608e-05 -1.978910278525219e-05 3553 8.538044277360524e-05 -0.00013177223073278298 -0.0006645460763636718 2835 -0.00076798366303876 -0.0009792195074327524 -0.0005703272320727567 3546 0.001171100146313422 0.0001900135143594894 -0.0019845142866869443 3544 -0.0016403370763304677 0.001652159937329275 -0.00042972200261399084 2833 0.0005964481913798229 -0.0019765561920027327 0.0005939570125081594 3545 0.00010943455678611054 -0.0005961309968803322 0.00022091596338937763 4460 0.0031093671220032803 0.0021186187400236045 -0.0015961012596608162 2902 0.000903477073601015 -0.0006807963710349717 -0.00011769365029270303 5112 -0.002600546561556667 0.0024678894133830123 0.002599536948969996 4537 -0.004618631790978801 -0.0052173431326763735 0.0014444284011391464 4385 -0.0005810865427363153 0.009043281120721235 -0.00045159135751681085 5143 -0.007578440162019693 0.005888466837445537 -0.004616206005763968 4969 -0.0023112717369795713 -0.012286617697846097 0.00046142687661615794 4599 -0.002931943267534274 -0.004390028036657728 -0.001404767834405334 2876 -0.0011752708554029164 -0.00034863425500869364 -0.0017472965580891502 2874 0.000496376409751405 0.0011476500804402968 0.0023453185916042455 2865 0.0006711976991799163 0.0020261380610938295 0.0011110178538112764 2867 0.0003114701553805786 0.0015208631237415414 0.0020268175324478313 4791 -0.009292746019096224 -0.0011148400574788452 -0.004019459478553555 4655 0.005118758761306564 -0.002674171077298067 -0.001752188667873616 4542 0.008132160841691284 -0.0008524117574890631 -0.004217589455548675 4613 -0.0034151584261141294 -0.0005397798302950238 -0.005652810092919474 4785 0.006494793672075749 0.00527080754910626 0.0008424840720692121 4862 0.003534839815850071 0.002595353176813464 -0.0030524325104291893 2884 -0.0002500505005622164 0.000985838256126473 2.407555094617001e-05 2873 1.6753840461906228e-05 -0.002035206773496308 0.00014504299956778874 2875 -0.0015053051966802445 -0.0014504230218656132 -0.0006961604868239671 4758 0.0013707958852870901 0.010109786991231183 -0.0030075778533958392 2882 0.00041174826542101283 -0.0015987811127605458 2.3000810977317652e-05 4893 -0.006826522487501714 -0.010159318942093888 0.001913243617068047 4939 -0.007498570437296238 0.0016621195515504929 -0.0042301577923032204 2913 -0.0004735022927897361 -0.0014383882563691207 -0.0008894165322452679 4612 0.002558585041042729 0.00254330757926244 0.001908166077690303 4574 -0.0006606671502614517 -0.0020008157763125034 -0.000918421507004798 4561 -0.004639808257075401 -0.0026403945171451144 0.004606664253423493 5053 -0.00291390962049612 -0.00696799505487578 -0.000997005985278451 4452 0.0028190415715873703 0.0026217254200372954 -0.004068230833462447 5239 -0.003133501220567084 0.003345871899746099 0.009873349879814038 2915 -0.0014499662217652665 0.0005155530646618999 -0.0007374508188404548 2904 0.001304127239200196 -0.0014188028973820255 0.001768729933992918 721 -0.001231819208216392 -0.0008270459486409496 0.00021054930037688448 4571 0.0021487763658998467 -0.003953900526304371 0.0051106496094878 4989 0.006736430384150675 0.005208927860816708 0.004032575150350428 4745 -0.009866357145705773 -0.003556396295430376 0.00558506329471997 2906 0.0010036956892309767 0.0015863781166829808 0.00047567638883832045 4662 -0.005154433453932508 -0.007814369662104418 -0.004465191388646689 4562 0.0024600585245418997 0.008525594924303596 -0.0030053281606858794 4937 0.004574717371975695 -0.0029512569273459407 0.0027894296744030763 4928 0.00037648561595186175 -0.0003277646907176357 -0.0007440276232654366 4541 -0.0032779873002497404 0.0034904979148257373 -0.006123476440752062 4399 -0.009742800309257525 0.0027990131341612875 0.008717139654513033 4388 0.009553954349206875 0.0038317630952510217 0.004488409740373564 2878 0.0006482030604324466 0.0003447656733642783 0.0011834577316122558 2880 -0.00029658931408536545 -0.0005181286486268775 -0.0011387459423278907 4467 -0.000956583520645023 0.0011366155206685472 -0.011497103648039051 4680 -0.001381033940367039 -0.004212065191146634 0.0021259778323569505 2869 0.0005519011349892921 0.00020110774747840638 0.0005691288480510794 4475 -0.00011942576133131536 0.0025097211153348345 -0.003216931636766502 2871 0.0001263657413470593 -0.0004208719461638957 -0.0008497657651410839 4570 -0.002176783931422596 0.00046204856816413695 -0.0051841836412178975 2886 -0.0006780360888569551 -3.831622774352249e-05 -0.0004919623985704622 2888 0.001360192706013609 0.0005882283504250996 -0.0013070514375157253 2877 0.0021139432183025046 -0.00012149121570440968 0.0012901867078841645 694 -0.00021658506152472134 0.0006615263135315117 -0.0007713693773289051 4647 0.002629365511325775 -0.009644186533776035 -0.004984980418587854 2879 -0.0007485229486150444 -0.0009619197030009048 -0.002094709871553567 685 0.00020234611453660194 0.002229070481886639 -0.0016307136955348357 4415 0.00331208439793172 -0.003923979121637172 -0.003363538365457253 712 0.0019311792542193076 0.0007454768007279749 0.0010328654713112797 4489 0.0007307593447647971 0.0027035354105028023 -0.006418215464487958 5287 -0.006887117253667227 0.000906835903394325 0.0030547703329158616 4701 -0.0008774561589686094 0.00022705682416644457 0.00033592708581459997 4386 0.0015795861502156342 -0.004326181020357591 -0.0035350334774884155 2883 0.0013755551567982281 -0.00018207056605461518 -0.0012258058979522772 4800 0.00019118506663236387 0.002657623018357348 0.008920562820088096 4442 -0.004410245650157382 -0.0015185630401590264 -0.0023924829717714897 3605 0.00011283211883030063 -0.0007212474497007208 3.104375475596359e-05 5130 -0.0005660520476164555 0.004279936001474033 0.002708667406251237 4667 0.000604624887055263 -0.0038097187832857103 0.008745356638079176 3603 0.0005335157696736942 0.0002871258036868543 0.0005584943680725059 4447 -0.004785872466554791 0.0019361223951298585 0.001242738441920308 5199 0.0012957222769713103 0.006324788743519453 0.006208343806768563 5206 -0.00559093446765469 0.00453908497024576 -0.001978968263841567 3594 -0.0024043228669993616 -0.0008192027622966952 -0.001786585194453599 2885 -0.0006052233640121312 -0.00038461368707616485 -0.0003793610897400196 3596 -0.0008871143426694168 0.001546627203296675 -0.0007646227738489185 5010 0.0020275924431974405 -0.005300513754314517 -0.0018456581561639208 4546 -0.0005243044893506734 0.010543320052123306 -0.001420563423943076 4833 0.0014338126071812597 -0.004657825704859629 -0.0021007392163689565 4639 0.005306428783360349 -0.004609144817241811 0.006021871673400078 4535 -0.0016731328959865067 0.0003562366528732583 -0.0034715750270383856 5015 0.003972631664877 0.004581399852412429 0.00556229457180649 4523 -0.0046137652110331195 -0.0061417956395140505 0.001021984945387288 3593 0.001838900189383452 -0.0005500669867596715 -0.00202557060531043 3602 0.0013229906554285606 0.0007049117108475151 0.00033634574808213795 3595 0.0005752693561632799 -0.0004978568058556275 -0.0015562108317604515 3604 5.177114037778865e-05 -7.232850332175567e-05 -0.0012873742193092123 5160 0.002542580144661585 0.004176174115076473 0.003934305542946601 4669 1.9830460461642375e-05 0.0016128082718693784 0.0010724020713368141 4839 0.0003357448876773116 -0.0033651225971793168 0.0024477051449473806 4611 0.009496781623597217 0.005005700485143074 -0.0028091520821997553 4761 -0.0007964482050568317 0.004962116892899511 0.0029785429899260325 4690 0.003200281091512026 0.0026662520543919684 0.0025403387559241298 3622 -0.0010100508545917175 -0.0018697291176837524 0.0017507803748847545 741 0.00020109384161436355 0.0008679730810172271 5.241221822461237e-05 5139 -0.004690715469029224 0.0035450168668419834 -0.0018154581284597923 5002 0.009193696397882112 -0.0012114363936653477 0.006839166759802828 4943 -0.0071288959519084545 -0.0029129100729213034 0.003824465545098233 5037 -0.0009192059691152572 -0.002416123738239238 0.00036512917430739063 5088 -0.0034094126281497246 0.007197166470593366 0.0047693078144932025 3626 -0.0013631210154186313 0.00024316951917966638 0.00038105161817095267 4414 0.001918663473103701 0.0015915815203958053 0.002397679022008023 4401 -0.006929000494738469 -0.0047235837744539965 0.007761548671898809 3635 -0.0014819506161692629 0.0013651791692620946 -0.0012430075920903173 4966 -0.0010851570811685508 0.01217981684592151 0.005826370311289273 5221 0.007157724142176858 -0.005437335970665536 -0.00034709442908385866 5109 0.0030602916892424076 0.0023412638250618362 0.005704500925463296 4659 -0.0008105603093335177 -0.002408416369699426 0.011689616061398274 2889 -0.0018972139876775526 0.00010079886474529353 -0.001940645977824906 2887 6.475366761739005e-05 0.0011394800024357543 -0.0012324878833237806 3598 0.00046238479441580434 0.00034241381093340454 -0.0012963655697411358 3600 -0.0007461764338012363 -0.002057627876970977 0.001163135736603701 4515 0.0053347181351251 0.002213467658486584 0.003425445556899473 4397 -0.003147479211456634 0.0044079637779691145 -0.005100458825342468 4428 0.012511420097596497 -0.006186293718970554 -0.0024505959618989705 4687 -0.002448342385818439 0.006250406230600526 -0.005025046138403218 4727 0.00023226681860930734 -0.0032257200921640213 -0.002661181232297316 4726 -0.014473636248236565 -0.0051012310063899636 0.003458526852144081 4646 0.00027450194327469893 -0.0011076420706898015 -0.016379793850360234 4485 0.0007922022143478102 -0.0031974749891676597 -0.0034975724068290106 3597 0.0016950159240325532 -0.0015180828807460824 -0.0014104529067810604 3599 -0.0012650802754465772 -0.0007400702495998706 0.0006024364369194231 3606 -0.00032857235391570106 0.0003547374962364013 -0.0007022862438083935 3608 0.00015675218695146887 0.0010607296980166391 -0.0006393752561214907 1414 -0.0010299240762962178 -0.0004262811223481309 -0.00024215204534735438 1405 -0.0024489922632810854 0.00017261407947249778 -0.0006558380900814455 4720 -0.012355696427085595 -0.002164795770346627 0.003234771441328835 4746 0.004069949014859204 -0.0017010201263637777 -0.002147888459807291 5009 0.0015293143338142258 -0.0069155595565551006 0.0010635476342083909 5192 -0.0036582102584372285 0.0010441411765344981 0.0032538244117084167 4502 -0.004528645969531925 0.001439804430740429 0.008762716619475242 4926 0.0003815398618758132 -0.011978454165058145 -0.004911525639312282 2900 0.0014123322358939713 0.0006159769789196687 -0.000255731807881256 5380 -0.003502448994083618 0.0022788833592630865 -0.003539897201126737 4660 0.013438581728930062 -0.005226590739931374 0.005692537167271791 2189 -0.00024303740277359067 0.0004223692903331437 -7.418818013507027e-05 2193 2.2614778372028084e-05 -0.0023264981480294344 -0.0006980496492756894 5468 0.0013346915379807707 -0.0016776449170344027 0.005514251219034585 4916 0.010853557410678498 -0.0011787143419249245 0.007965076149225163 5382 0.0005946999149061329 -0.0007760713664646126 -0.002485168904964388 4951 0.0007224795537626133 0.00863498477293983 -0.0016675649502398537 2892 -0.0016584337498493874 -0.0014019222688032185 0.0007314950230042593 4856 0.00844220481740698 -0.003430975532993511 0.0020222258658205553 4654 0.004953790470735484 -0.0015923592794173074 0.0038533625144109903 4390 -0.0024219816850647074 -0.0029793799349135653 -0.0028705688909924877 4608 0.007707243855747189 0.005128505597058206 -0.005128646101014529 4492 -0.0025156558020791096 0.0017271890144078155 -0.001232801904979602 4805 -0.005142976125139664 0.0010780999022077474 0.005086392355428174 4668 0.005036336775195274 -0.002516922854354809 -0.004187036236042818 4849 -0.0030630768165917184 0.004671441719420323 0.004030880036799532 5047 0.0023922949167254964 0.005222695641328048 -0.0004108615930885263 2903 0.0012681279002116138 -0.0019180388120331755 0.0012363932462732593 4630 0.005843168419016494 0.004197880669106296 -0.011246512812583391 2891 -0.0011605715956473017 -0.0008491313160478924 -0.001816629787393395 2911 0.0025903243736309176 0.0013429602184177323 -0.0011020428305047359 2894 -0.0013500209048513683 0.0012952709027779675 0.0006263858465068064 5267 0.001560841913755569 -0.0055018733254781835 0.0001656604853692165 5498 -0.004672169105057726 0.005761300917294482 0.007769941272796242 4972 0.0007747222110773571 -0.005735761748234884 0.0027760217342802434 4982 0.0021229259034101556 0.0046771689331502435 -0.0037855148584693735 5234 0.0004334803091775298 0.0001517137122787433 0.006016434134028225 5098 0.007080930565778671 -0.001985829856626058 0.003922438468410602 4459 -0.0023159423952683823 -0.010120122297764657 -0.003856768419736302 4686 -0.000874773489177536 -0.0007815858261247358 -0.0017791213120748573 5347 0.0008434661491849394 0.008045667031331931 -0.00416252756342471 4732 -0.0021363391787679853 0.005098955191764998 -0.010643598238446492 4733 -0.0010350671115482712 -0.009981359714841554 -0.007512677292543203 2907 0.0024975155167194316 -0.0007238106188601919 -0.0008903730452834148 5204 0.004147358169417416 0.0032152523071820147 -0.002043313069287985 4544 -0.0036041251218053745 0.008317899794054368 0.00278437410434899 2916 -0.0016775525435667312 -0.001298567877858189 -0.0001867945742926871 4402 -0.0029035166399598825 -0.001912580796051222 -0.009208437164588622 4436 0.007299514008456513 -0.006831677391160646 0.007313690658842673 2180 0.00025192081876212606 0.0004971379959039567 0.000854674317369799 2896 -0.0011407645166341127 -0.000931753301375945 -0.0013933929421024002 4384 -0.0009537624613117066 0.0007845568973658285 -0.001081717109470479 4554 -0.0005471416774549203 -0.0026926778420137978 0.0031486032765888753 5186 -0.0027674820413941363 -0.003117966419910302 -0.0016690336010958453 4454 0.002626287714457185 -0.0032497446441030337 0.009272597549260669 2905 -0.0023679345687359983 0.0006395849069371421 -0.0022300881499722636 4823 -0.0013017977456446827 0.0038349780466731495 -0.001410135832274497 713 -0.002132203841400679 0.002147566226270753 -0.00019389839644263747 2898 -0.0014370051819248117 0.00023241324367080868 0.0012569153901510733 4468 -0.004653868808380946 0.0004071502866537283 -0.0011341096332147234 4904 0.003957039926148036 -0.0015211233889987864 0.0003955522310664304 5052 -0.0024588681360373415 -0.0068433652015116725 -0.010040866206251888 4787 0.00011629328268624052 -0.013357129684455136 0.0006604140822223174 4981 -0.005890581255931267 -0.00303626038295558 0.006099088074645994 4923 -0.003486563182687729 0.005039819661576893 -0.004716639289451275 3623 -0.0009088582365643801 -0.0003505260542832156 0.0015328383950056488 5295 0.004988820639344284 0.0030261709459982952 0.0007823602045842611 5483 0.0007089993734736535 -0.0016806476576556764 -0.006646450296452411 3628 -2.237963681915719e-06 0.0003683169360219273 -0.0003481651335470596 5350 0.0069903311253914835 -0.0011983042276414494 0.002387078115604279 5363 -0.002320954559257913 -0.008661468310087092 -0.005571448406153139 5220 -0.0036953154116702654 -0.005189703228418377 -0.0014814873268646377 5230 -0.0012585264298398435 0.005134007491238431 0.008926477308296005 1448 -0.00044197406120088543 -0.0003847038304366781 -0.0016111259665598956 2901 0.00033889498810861767 0.0007457907900596348 -0.0003418020123806156 4804 -0.006601235225316301 -0.008986722571019243 -0.00019508072315868423 4834 -0.0032354494435607247 0.0010229373000880102 0.007116750126923718 5462 0.004040717113218529 0.0014308447582052652 -0.006064638521171226 4793 0.00013702677194672597 0.004491811264393889 -0.0156737602582164 3621 0.0015140560670097224 -0.002428523574172653 0.0005062426351140717 3631 0.0005101861647882058 0.0011997133677134936 0.0010185170354477698 5013 -0.00020353632554783002 -0.0027504953192140904 0.0003445075729859552 5228 0.003883849670536981 0.0022112878714071636 0.0023034271331095883 5408 -0.003441247121813933 -0.004989012339938367 -0.005417088465710687 4710 -0.012733491648878987 0.001409875109721056 0.0038171180742805552 5159 -0.005768420038545581 0.0016641907342633956 0.0030478818904055706 3620 0.0009725618837202201 0.0013939318053507745 0.0008293488236735234 5162 -0.0041152791501827095 -0.00011074969299174108 0.0024770339983500003 2909 -0.00013406614902959142 0.0013389984970952526 0.001115161035366459 4803 -0.0012984353625518155 -0.0008523582001235361 -0.0036987926803155676 5268 0.0022429418209001534 -0.009530975732341202 0.0051360463338954105 5493 0.001753286257204765 0.001620630427621786 -0.01520995076568167 4603 0.0010835025589014593 -0.004315900271895433 -0.0002640080410709537 4742 -0.00171191394121569 -0.005562918853788106 0.0011746689094675725 5040 0.001662186323794693 -0.007941244391184234 -0.00011317388644647357 5282 0.002720593540214568 -0.0065147018580045315 -0.005057745415890685 3625 -0.0003092542232278172 0.0014771619579675853 -0.001017243447478995 4674 -0.008026828151323172 -0.002002193250605599 0.010298420268654377 5170 0.00047204163502817715 0.0010826880075391406 -0.0004556703204561003 5191 0.0008955475199008956 -0.008937550270967237 -0.004153957517143972 3627 0.002076692270124046 -0.0006165515840102546 -0.0014950891050936098 4810 -0.004536660701709307 0.0018672715891664502 0.0029984639712618186 3629 0.0006319922797194985 0.0020704305655940207 -0.000499183360296097 5210 -0.007242818098507245 -0.0004718616911520204 -0.0031525382194581746 5406 0.001346330427795371 -0.004849518333343236 0.00047967993897639935 5214 0.0015761299581923422 0.0030377869553190736 0.005051442271584819 5272 -0.008837975756932698 -0.0036262728935532442 0.004522786057274166 4539 -0.00123219093921796 -0.006084839716667127 0.002015239343247716 5296 0.0010548555227671394 0.011974223717256299 -0.001586218833665223 3624 -0.0011468820021460742 -0.0012053176634283763 -0.0007111359842306908 2914 0.00045270384861174906 0.0002640997677497064 -0.0016012938434266598 4792 0.009134112581049587 0.0032206476396852745 -0.00361215370816218 5369 -0.0044891028993333925 0.0024315937651614972 0.0007866201081262276 4418 -0.00021645904799233142 -0.00040823019331331304 0.007014985509141236 5371 0.0050944779634101225 0.004677691234166572 -0.0009561459693364302 4577 0.005834157956534962 0.00562325919878773 0.008868116094544944 4555 0.002381652901915005 0.0017360738062811346 -0.006315034242810638 5443 0.0034954662605060152 0.004523551694827655 -0.01090807620108831 5173 0.003932371956993409 0.0007830310375557853 -0.0020396985096508176 4731 0.002148826302161521 0.0011565569668685702 -0.007678155845711747 2908 0.0013968621908613497 -7.536468165661559e-05 0.0019603087623436873 5227 0.0017580887278104862 0.003331447208114806 -0.002205623796144875 5322 -0.0040491570018303166 -0.002569422575715531 0.003001809536045363 5308 -0.001957185274208884 0.009659112870363175 -0.0015730806056723221 5453 -0.004845030522138459 -0.003415701001255168 0.0013712864399540647 2910 0.0008471814089413682 -8.343540949107059e-05 -0.0006979326348970353 4790 -0.009969878171354706 0.00213722631767539 0.00014448394984336433 5390 0.0027354896986460223 0.0022318993402065143 -0.010055356591723418 18 -0.001351834598295971 -0.0015497113195297762 -0.0005683137787988442 5449 0.00025887125938847986 0.001354057775168754 -0.009295328656015364 4471 -0.0063980541961533265 0.0017554795302216512 -0.004473137143723613 4684 -0.0025334680977606053 -0.0052097618778772364 -0.0025012973382536 5469 0.0032666012029158122 0.0009092298544931165 -0.00741034919067018 3665 0.0007815740514951015 -0.0018340381609960007 -0.0005255148621149048 5457 -0.006313891393147134 0.00019654344607871518 0.005441788374485607 5355 -0.0033687472654803235 -0.002766529008395955 -0.005637527834864258 5429 0.008167320646207392 -0.004070636854475446 0.004987484930050607 5111 -0.010064994096509624 0.003099250707510186 -0.0012442925731715672 5225 0.0037965258644362923 0.007170965415516894 -0.004769772141420866 5209 0.002802903164523658 0.002595847393369376 0.005131292451179304 2211 -0.0002533823828299248 0.0013045988630683105 -0.000550582140797327 3630 0.001437792897715078 0.0014153551674126624 -0.00071547941257797 4990 0.01454897933026532 -0.01282885102875987 -0.006469469704499095 5373 0.0005086712147403107 0.000812186755417235 -0.007579810034575243 5415 0.000849196397118789 0.007903384975787109 -0.001759198840337865 2912 0.0011282873280598629 0.0003976022039039607 0.0010526357796580915 5034 0.003957989086318805 -0.009622330372490268 0.0020475794781394147 5054 0.0007243059052918705 0.0013454916518081004 -0.01507635059385685 10 0.00010863810258848945 -0.0019171593232382522 -0.0006121380986696999 5180 -0.0021995532000912334 -0.0035548003587047286 0.005224656022905716 4553 -0.000901082687416505 -0.0011943599121032912 -0.002130394524501884 4824 0.0006996701511886392 9.033971710022077e-05 0.011622129801999403 5337 0.0026946390347061967 -0.005871885384164756 -0.0018671453383859102 4743 -0.0050453551687894265 -0.0003779619269540914 -0.013188930524230839 2200 -3.9211206930168246e-05 0.0008099721284408797 0.0013025090440512187 2202 0.00032379254852966466 -3.266502200072706e-05 0.0008943220902099718 5215 -0.00303491269140401 -0.0003582827913123454 -0.006035991915841128 2209 0.0014856136206711176 -0.0016281589700877955 -0.0018592631963391564 5033 0.0007373802918565864 -0.008731173546035038 0.0030374468875380193 4954 -0.0020783048448716544 -0.0017926936465257402 -0.0014740872090115045 5147 0.001469044187785328 0.006629699257487277 0.0008191135931737583 5150 0.001430410624803337 -0.00783750905197286 -0.005868905551208842 5441 -0.0036297497463623606 -0.0022883220507762384 0.0027546777153692596 5419 -0.0037573842678129926 -0.006287538077577927 -0.0017236329277852042 1439 0.0005106753398002207 0.0007078427258319486 -0.0027143363568053348 5183 0.00484011854213876 -0.011632284000260529 0.0014874923815789021 5471 -0.002939889561079508 0.005740093375665455 -0.0017700485597382325 5496 -0.0022331373324752262 0.008470548097439867 -0.001114578222213749 1440 0.00014567316700021403 -0.000786467769186208 -0.0005574187063093431 2922 0.0012742940396407332 0.0011251590371016617 0.0010488020479658133 5487 -0.007264931156316367 -0.0020542768781422103 0.009672629768795075 5288 0.0037693283195642325 -0.0020782837031472295 0.00787990010658242 4905 0.013302781033156009 -0.006491637919660879 -0.006264236173879346 5500 0.011360056225225318 -0.008020609346583127 0.00020575964938822865 2924 -0.002473553931017975 0.0018538533603861583 -0.0005135817940095744 5232 0.010349939135400048 -0.0017513159493255613 0.0035130117229332652 5450 -0.004973839024472746 -0.0019560073613172626 0.013354090825092492 5478 0.001524474492897119 0.0038801667833994365 -0.0061975732039210585 5311 -0.00594193282446729 -0.0059964887151737175 0.0037892332950643067 2920 0.000791382340556533 0.0012841292310456038 0.0003922799338581572 4640 0.008330559765317262 -0.006975427259474992 0.003912977238168384 4965 0.0005584489609827244 -0.013596576587563532 0.013073779450419938 5508 0.007455182457441788 -0.001989220287726551 0.0035534186989004705 5446 -0.001543965953008612 -0.0007408311827247238 0.005334501320455677 730 0.0008794887498682463 -0.00010414267252700668 0.0013198725652143768 4634 -0.006078270074611333 0.0022427457314465053 0.0050613007921229015 5244 -0.0066120027755054815 -0.0031551722620891043 -0.008644767401285468 5510 0.005439733516952669 -0.005303073412864835 0.0002441740526804084 4597 -0.001731219527496684 -5.813441770105473e-05 0.004400716209436023 5104 0.00386137185067643 0.0060708885906445645 0.007864406470586918 5442 0.004465710521890847 -0.003731438991055871 -0.006769476861430029 5383 -0.005796770965153017 -0.004409658064229335 -0.00901233204540475 4818 -0.005525187557622948 0.0034181098743130724 0.002212534107223102 4853 -0.001918288197970098 0.005782781212028616 -0.0021388306165034876 5318 -0.008612672622040985 0.01261775886016993 0.004378366495330664 2927 -0.0008989498654192799 -0.00015782925010007992 -0.0009717633215463601 5197 0.0010391326167102331 0.004424525158931243 -0.008681680242580314 5397 -0.0004770196935560204 0.006484811087091628 0.0004119781214222463 4950 -0.001750970135340474 0.0017831120646833796 0.0030656548030864937 4935 0.0012792702891787251 -0.005067309186952525 0.0007151805844818598 5176 -0.01723122147279219 -0.009912791163336944 0.008600666659990605 5358 0.0020856803379270777 -0.004491063894869417 -0.002148818794143455 3674 0.001109952281195128 0.0006967853561458657 -0.0007141249776473511 2963 0.0006431590956690789 -0.0013549469966195869 0.0012897129184939315 2965 0.0007291312292074042 0.0005232725684262865 -0.0009019081581639496 3676 0.0014868623203468684 -0.0006829072984872861 0.0014370516039802451 3648 0.00013392260143044648 -0.00011189918042019131 0.0007916420689773099 3650 -0.0016093763549200211 0.0013368385232296453 0.0004601891808199024 2937 -0.0009428197254276645 -0.0009088237272515027 0.001102245058116146 2939 -0.0005390580871421415 0.0001351674009511649 0.0006629921947425448 2967 0.0004330784431577161 -0.0010619559883017142 0.0006458051419726315 1486 -0.000870433249781734 -0.0013069906930952787 -0.0024627959734116003 2969 0.0006331750631145728 -0.0007277503636394523 -0.0011564420521580588 775 0.0005269250499780728 0.0016714994669187984 0.0003338700831826266 3680 0.000986016406893469 -0.0008813485220235254 -0.0013726365319923482 3678 -0.0015339879562836156 0.0008755781238524738 -0.0006251530233021083 3654 -0.0012288008271655157 0.002237946453820071 -0.0004949165728925217 2943 -0.0011032621389288275 0.0020646895305746937 0.00020279851088851565 3652 -0.000495573175184918 -0.0006019888230869516 0.00017401629627585404 2941 -0.0021262144438548725 0.002132053266447533 0.00022792905835962484 3683 -0.001833771092718049 0.0005437818145298547 -0.000685849994389558 3692 -0.0007287198636225073 0.00023254306530687665 0.001163735951716773 3685 -0.000999300427735178 0.0019893180398294786 0.0002753525636433776 3694 0.001092344028599351 -0.0009428071301077205 0.0007864450404775412 2218 0.00020712945857322227 -0.0018033986408544454 0.00019933061838523826 2216 -0.001978556799350216 0.0003474281309405044 -0.0001530961350447431 3657 -0.0005064588801434331 0.0005861823653000857 -0.0009697693822270162 3659 -0.001487676928162805 -0.0019347956731792402 -0.0022140931995021456 3666 -0.0006116788095386187 -3.1786874815393964e-05 -0.001959011650865103 3668 -0.0020350557504215296 9.745015260469766e-05 0.0007564097309688282 3687 0.0012381057747694072 0.0013751409378748533 -0.002410511294175028 3689 0.0013235070605637418 -0.000874679857688142 0.0015381648227970968 3698 -0.0012123281804648019 0.0007917588765322394 -0.00202496689065206 1504 0.0014088480236494052 -0.0012848019727767146 0.0018286888183105593 2222 -0.00011761862786678536 0.002035411233364152 -0.0002992835298058173 1495 0.0014208380539216833 -0.0012199086782768481 0.00014733523913838505 2220 0.002009263532828175 0.0017272085644388943 -0.0010834315442357638 3696 0.00046220471450337305 -0.0012767224610979776 0.0006675676011119241 28 0.00016464895971531952 -0.0010084117633344203 -0.0011097305988201737 3661 0.0007773097453334012 0.00035769844986415986 -0.0007522374419330236 3663 -0.0017440187246344717 0.0002029411241149374 0.0021836125865497564 3670 0.0006473693548080803 0.0013707863553543186 -4.533476396692418e-05 3672 0.002239333116671611 0.0010226563186656666 -0.00037917057758681417 1 0.0010726158643061508 0.0001318683513314399 -0.000559789209519522 3018 -0.0025218290406432255 0.00011236114894202533 -0.001742510317267239 3731 -0.0004127977751519666 0.001670470065500434 -0.000751741648710049 3020 -0.0012567064828186694 0.001686274455352351 0.0012017197315789614 3729 -0.0014873457931960752 0.00122618769593823 0.0005607437775712258 3730 1.7117275266993097e-05 -0.0018833227602541238 -0.0006679821308625249 3019 -0.0002626410990435431 -1.2417875041290972e-06 0.0002558471333904207 3017 -0.0009011479621789788 -0.0013848986129901494 0.002118190640938814 3728 -0.001970707420902296 0.001999196339684248 0.0012338975846226511 2991 0.000641580965490208 0.00048051388944039884 0.0013298531225989466 3702 0.00021598436895349635 -0.0016696402053675075 0.0003667816532281859 3704 -0.000418132074730548 0.0010212941049352808 0.0016255694490682172 2993 -0.0012890744399642615 -0.00047552847201432933 0.001962743487863688 2990 -0.0006840552068960442 0.0020555960808624103 -0.0006395389765855964 3701 0.001719460241731305 -0.000876081720607358 -0.0011507996937062544 2992 0.0007990214422050305 0.00020389346272246356 0.001753828964553822 3703 0.00043748439800573213 0.0016351799253110553 -0.00027360322590202026 3675 -0.001246678699280821 -0.0001377929861553968 -0.0001281179661325421 2964 0.0017440575254943132 0.0020079398531502395 0.00033568035093628837 3677 -0.0008169511071633939 -0.0017650920849952888 0.0017009748095042055 2966 -0.0017282717689424934 -0.0009526157108629236 0.0015852524685213403 3733 -0.000926576433320836 0.0008151705006499667 0.0004630127651957562 3735 -0.0017492379481240006 -2.724270207046754e-05 -0.0006972799546465169 3022 -0.0006067361874461778 -0.0007678881887734634 0.0015767577864551508 3024 0.001532009056506699 0.000295398721390735 0.000174704251044647 3021 0.0018560612264583486 0.00022205945337068044 -9.554415823060389e-06 3734 0.0007270044362375279 -0.0003089642193361842 -0.0010267438551992622 1540 0.001947635964110012 -1.7606712143849405e-05 0.0006836128156654498 3023 -0.0015563457065324146 0.0016497879019411643 0.0010730048764828759 829 -0.0021918407222078075 0.002076290349241512 -0.00034038636606002824 3732 -0.00023788573971812547 -0.0011129480462524145 -0.001321398055726585 2997 0.00033900038356869883 -0.0011181519284726251 0.0005945972037190448 3708 -0.0014400540822052973 0.0009465648718311711 6.534626093283261e-05 2995 -0.0015230206553988232 0.0003688399475766473 -0.002346740478760815 3706 0.0010770446206155397 -0.0005638800451666316 -0.0009031711864695589 2996 -0.0007944206997025275 -0.00030328991505168676 -0.0003293432108267709 3705 -3.534127278819127e-05 -0.0011531547550935406 0.0015562391528122555 2994 -0.0002377356729791637 0.00013455662719496787 0.0015437407673013137 1513 0.0023991081487793626 0.001501914095104999 -0.0018831013644758858 3707 0.00041326099652876135 -0.0013708330622834034 -0.0016270734506191088 802 -0.0008193210027270378 0.002059195431068167 -0.000396705955081294 2968 0.0014421371980053227 0.001370139196144894 -0.0017494868439060355 2970 1.4966359513559268e-05 0.0001927323903942892 -0.000708176008022106 3681 0.00010329119079002086 -0.00033937425356108937 0.0015791996791861321 3679 0.0007649099691115542 0.0014686372414468229 0.0017984819327908157 3749 0.0005613196459243281 0.0022024409851141044 -0.0005887972971084286 3747 -0.0008467968286904374 0.0006923678036849759 0.0007281662434907774 3740 -0.00010211264725534406 -2.6497788007093497e-05 -0.0006832023239713673 3738 -0.0005430728338320723 0.0004115520073539752 -5.059448874264829e-05 3737 0.002636681477547983 -0.0006021345797999919 0.000880527141200289 2272 0.0012299398551269746 0.0016549253259751837 -0.0008998393044174957 3739 0.002123626247899081 -0.0021995395253042445 0.0018308291640248258 3746 0.000508711726296903 -0.00022463068212627384 0.00047620333093565363 3748 -0.0018020042742699469 0.0010280946865870114 -0.002344342231106152 2270 -0.0009747223257669412 -7.376736782400174e-05 0.002161214652881169 3720 -0.0007436443980925793 -0.0014975374667132114 0.0005569037800238639 3722 0.0009887277397639604 -0.0008645329459800494 -0.002420138413323688 3713 -0.002562863923123113 0.00021664543569660218 -0.0016704343517098057 3711 0.001455029855079434 -0.0009100576446379738 -0.001472516001562705 3710 0.00012564926924341243 0.0019396549431041782 0.0003161507417440686 3721 0.0007903774680338149 0.0014568057587925314 0.00017276893448799503 3719 0.0018211301398263365 0.0008189013361069861 -0.0012899609519643484 3712 -0.0011693644222737594 0.00012420117123555178 0.000696118089365541 2243 -0.0012986668058157637 0.0008914129378950437 -0.0016203898259372807 2245 -0.0006716147377459706 6.090967040363478e-05 -0.0002199231624774613 3684 2.963297552646834e-05 0.00020270841378757523 -0.0004481620563802817 3686 -0.0005672332482577875 0.000636434969241628 -0.0005090357751060372 3693 0.0011973682435616581 0.00014042934909585646 -0.000918179933455876 3695 0.001928129430636057 -0.0007292468814923605 -0.00030450851639908234 55 -0.0009986493081212198 0.002098622384247538 -4.964557392844217e-05 2249 0.0023703344516016697 0.0011001313861507599 -0.0010847928561772456 3723 0.00039964581433268984 -0.0010685089689433493 -0.0017989009254870648 3688 -0.001194910313894977 0.0004279983380453558 -0.0005370673968415453 82 -0.00045510380009684956 0.002701840808481212 -0.000999679637965043 3697 0.00040450409735089826 -0.00015312634721055497 0.002192480078764901 3699 1.920525732367249e-05 -1.0723768129965042e-05 0.002274991043218715 3742 -0.0018381247983412195 0.0025219400740000195 0.0007407883928334465 3751 0.0010051171111099266 -0.0017376103787641436 0.0007371448817467166 3744 -0.0010950550728182492 -0.0005614133115661487 -0.0011199645133363346 3753 0.0016982342704098168 0.0004921852166487289 -0.0002500393914181984 3741 0.002406702006750028 0.0019772647393696014 -0.0008275052176320021 2276 0.0017944280745509976 -0.0002578045944222726 0.001282445760476144 2274 0.001077586599837601 -0.00016426486351501558 0.0006901071579485324 3750 0.00012396695740761595 0.0013024706017216094 0.0004870514561574628 3743 0.0013488639486829985 -0.000483213121120873 -0.0005970470220181268 3752 -0.0015861487873487304 -0.000793420325618108 -0.000641109834538968 1558 0.0008747235033846842 -0.0007340417574897415 0.00035567513699990693 1549 -0.0021366273304370817 -0.0010409298924837712 -0.00014453859225910509 3690 -0.0014955819899882337 0.001376078110689598 0.0025078310018069546 3717 -0.000285059884741915 -0.001194005500274465 -0.0010536242469126778 3715 -0.0002867682821651833 -0.0017794894632774856 -0.0008651352683920609 3724 0.0013419746645591203 0.00017504199863599586 -0.001027819563221297 3726 4.9193400285650656e-05 -0.0004485118480142986 -0.001427548345750809 3714 -8.581144807484706e-06 -0.00024128636631940347 0.0004956357123818604 1522 0.0016065180787698146 -0.0025382124653875217 -0.000789097024583891 3716 0.0015276506910727764 0.0012300199356064675 0.00031241632741193896 1531 -0.0014442571755797036 0.0012521982291580304 0.0014654080577308653 3725 -0.00048530169298728696 0.0011933787645866266 7.705891532594619e-05 2247 0.001637364585129442 0.00022168360229411982 0.00036927527398923003 3810 0.0005985889030578665 0.0005238152448167688 -0.00018183314912221995 3099 0.00045763739021749026 0.001335930376723731 -0.00035791675968183936 3811 0.0002396405794984379 -0.0018950869307739835 0.0006974982490634516 3100 0.0012308663862593645 0.0020788208612849655 -3.440838965014406e-05 3098 0.0006056598493392727 0.0010808539669016457 0.0017131639427915308 3809 0.0001644411899470147 -0.0013534628586101098 0.0008214579402176427 3795 0.00016915350449526437 0.0008199074132451529 -0.001938810861686911 3076 0.0016604829030833147 -0.00026482470148807063 -0.001866646363953632 3075 0.0006188230485532204 0.0002734937213530167 -0.0013470946814927885 3794 -0.0013463404651508028 0.0009969196828372182 -0.0007953103967636122 3061 0.0022012638978300457 0.002093672469373314 0.000413092285602257 3781 -0.0012395375492673666 0.0005330531101514779 -0.00012956576659327134 3782 0.0010423863579893727 0.0007931743337699162 2.0932921343666056e-05 3060 0.001010738195498611 -0.0003712516638065647 -0.0010105599505948009 3758 0.001113791933506152 -0.00044287639841816655 -0.0002817722483525717 3047 -0.0022917230927537056 0.0021691777230575596 0.0003676258429667625 3756 0.00018001452992908546 -0.0007526152339885346 -0.002124161293805974 3045 4.102616181480428e-06 -4.418736072253886e-06 0.0006751227787210148 3757 -0.0008464321037114418 -0.0009231490537426963 -0.0023580801053429733 3046 0.0011704437183325373 -0.001665190408036902 -0.0006522686451736627 3044 -0.0005969282502922244 0.00101675250363438 -5.783546838012332e-05 3755 -0.001110155511253905 0.0009196151826224332 -0.0017697595983661323 3101 -0.0008827340671276394 -5.599751786912336e-05 -0.001264280785082453 3812 0.00032117113682081973 0.0018544091857298172 -0.0022340462608892294 3813 0.0010592810120938056 -0.0003657801868046811 0.0004222305935976101 1621 0.0007835089681217607 0.0002705874792426014 -0.0006978461796140144 910 0.0006912546820983974 0.0013922042842014059 0.00034875591730168325 3815 0.0014205198416518776 -0.001056511848472189 -0.00027429261163353015 3104 0.00020896931088894874 -0.0006710037682790472 -0.0011285076772689887 3102 -0.0002348272069530518 0.0010036298225841555 -0.0011051225496183416 3797 -0.0004885054193219476 0.00019580287391928185 0.001637657300745454 3796 0.0017426817640455615 -0.000382011588387008 -0.0009918586176567285 3078 -0.0010556219652769576 0.0018521267952681855 -0.0013688626294464992 3077 -0.0004860336838037535 -0.0008602851051541553 0.0009088158570494855 3062 0.0002372717290343324 -0.0008646146070700267 -0.002016585581282514 3783 -0.00020061205041294638 -0.0012142605219599748 -0.0016401380213141058 875 -0.0013997752441795154 -0.0003783122126449119 0.0007282070601643329 3063 -0.00028275122884954145 4.3029198455171985e-05 -0.000716669173864135 1594 0.00029113017658607726 -0.0009996892542897358 0.0014237332429076792 3784 0.0007350336559062285 -0.0006829977223526394 0.00043157532604114765 3051 0.0005088459417601475 -0.0014007844673344955 0.00012941061523139984 3762 0.0005221758920928076 0.0023780394599731917 0.00034869606929574987 3760 -0.0019521729969789246 0.0001612891393351903 -0.0024728666034912142 3049 -0.0014488114562339885 -0.000559890290342479 0.001393506150164509 3759 0.002478884791952609 0.0008092411350744494 0.0013473175031717037 3048 -0.001829375866249721 0.00010296360443653747 0.0023923774508190837 856 -0.00040569154130235116 -0.00027312702667014457 -0.0016418080567480644 1567 -0.0019452580642245808 0.0005381914637217604 -0.0020627939548006203 3761 -0.0002675066928403036 -0.0010091988368637103 -0.001499176936397401 3050 0.0016942558600192702 -0.0008883878770120408 -0.0008243230508999691 3814 0.00026900857359328403 9.390614261863537e-05 0.0013970933565793423 3103 -0.0004651782873316653 0.0018275993563648452 0.0002472280827495949 3816 0.0005765824930814833 0.001279925893139526 -0.001065898059072578 3105 -8.230604965968325e-05 -0.0005198568665542797 0.0010764071640642825 3819 -0.0001508074546528838 -0.0003937596549000667 0.0011039346040903042 3827 -0.0013849943237142386 -0.0011438091749870994 0.002279196880642652 3829 0.0011917262067854813 -0.0004983050898729901 -0.0017687700379041653 3820 0.0016157668355089828 0.0015699495729902696 0.002265192914495003 3818 0.001338275095817775 9.946302813554331e-05 0.00027893158196647615 2351 1.3640943626993477e-05 0.001431641631394934 0.0021189756524254595 3804 -0.0004607919287876831 0.0022320343484898107 0.0010930705385771254 3800 -0.0007852126309024556 0.00020333875034428167 -0.0002046734340409033 3799 -0.0007281004648263035 0.0001225920895869387 -0.000407590604123161 3805 0.00025308678831825217 -0.0006022662549290767 -0.0006273838706076948 3786 -0.0024387476732955905 0.0005859966425473934 -0.001293514346017586 3790 -0.0007616417910354758 0.00019969381947919167 -0.001884772138890301 3789 -0.0006445119558391743 0.0009386922697495057 -0.0010697114988294622 3785 0.0016336968504933594 -0.0008155182093363314 -0.0009911496808666636 2324 0.000687892425301263 0.0007293358229554994 -0.0020534879244092 2323 -0.00020846238627909462 -0.0001485431560195882 0.0025609168988652243 3776 0.0018853736991809047 -0.0017961780348363537 -0.0013008225664750328 3765 -0.0021225191973221554 5.629446493026196e-06 -0.0004893019007240002 3774 0.0021851232069524814 0.0010166386026395082 -0.0006894002564620356 3767 -0.0016628675939621253 0.0003770301117071936 -0.0002572851000357271 3773 -0.00030209581514653474 -0.0020365387339594996 -0.0001426764768361398 3766 -0.0012313465592560485 -0.0007182482729582247 -0.0009597301924782512 3764 -0.0027101633677856485 4.884531613444723e-05 0.00020350413415003632 2299 -0.0005685910883979368 2.560807796799479e-07 0.000719936881554876 3775 0.0002467541882314072 -0.00036466030542615555 -0.0004884838915901798 2297 -0.0009376919641372987 0.0014747156808547226 0.0006658379993756244 2353 -0.001155682574018255 0.00029125888950330627 -0.0003534934339331744 3830 -0.000547953988042524 0.00038522145715926166 -0.00020176186403020563 3828 -0.0023387812804776635 0.0021167410999721886 -0.0007255836637227534 2355 0.0005107090448537015 -0.00039465431088417895 0.000585818670550412 1639 -0.0003786182455244193 -0.0023074723376450925 -0.0012347223666246804 3831 -0.0008477373761868047 0.0016113014058063149 -0.0010889117542416675 3822 0.00144019848278601 -0.0006094633195140938 -0.0009250925435709716 3833 -0.0007032685842679675 -0.0005169675682510876 -0.0006862685042278065 1630 -0.0023234166367627845 -0.0014441359695553618 -0.0012833846394984187 3824 0.00060353888371667 -0.0013438235903624092 -0.0015961435545866261 2357 -0.0007316641614210197 -0.0015349679784881776 -0.0021450253326303205 163 -0.0004544197357536668 0.0003417678289704298 -0.00034885730404767305 3806 0.00012955074133179172 0.0022026293219236342 0.002250604502175225 3802 0.00011876847128939965 0.0020822310058084014 -2.6192841247871246e-05 3801 -0.0018618122510717964 0.0011387696807603164 -0.002156102214155333 3807 0.0007769429709168389 0.0003431653258302018 -0.00181093478090456 1604 0.00030047619618957244 0.0016125865254924667 0.0013107263297813885 3787 -0.0005108360160008675 -0.0009713285756963253 3.9172351433599314e-05 3791 0.00027692384544523454 0.001098503122379579 -0.00013159684445017558 1599 -0.0007544713253963818 0.0005905287175274066 0.0007142106734248103 3792 0.0013669379004314524 -0.0009663711512737539 -0.0010537240826346793 2326 0.0008813729066385631 0.00015500312065251827 -0.002053484206482677 3788 0.0014447970341340984 -0.00026415180816773435 -0.0005253920024695245 2325 -0.0007829860869143889 -0.0009559261783008228 0.0007700388306191441 136 -0.0008072887379358847 -0.0002211088647073794 0.00043960185424061593 3771 0.00022459073555306463 -0.0011733361242649031 0.0010709882184426049 3780 0.0001441368734532946 0.0002534941160254171 0.0005639420025679465 3778 3.816163325624626e-05 0.0002028419109601021 0.0009086907624494866 3769 -0.0005429805977021065 -0.002293165184847512 -0.0008221249990926504 3768 -0.001137605766054881 -0.0002321156014919194 0.0014043096706436383 3779 -0.00034048527377231826 0.00045192194933938617 0.0023150357573472153 1585 -0.0014266483629314932 0.00011383457677972353 -0.0005055618603867757 3770 0.002191826964685066 0.0007909531486460462 -0.0013445951478396037 2303 -0.0002132981796256619 0.0011793030162888895 0.0020815816866003025 1576 0.001504320832139391 0.002126976588507624 0.0018286756711082216 2301 0.0001645378583189864 0.0006702508408423554 0.0016039649966182257 109 -0.00018272420164890915 -0.00011087729338868087 0.0012682172463196265 3777 0.00010821974994586333 0.00020461343897414585 0.0021730409455267092 3834 -0.00018894859890524135 -0.0009735012977737101 0.0016372037741004453 3832 -0.0002611487778921201 -0.001542784405066801 -0.00020215864273475238 3179 -0.00026489177382613355 -0.00025257929712604985 -0.001153407717331991 3181 0.0003929267919021782 -0.0016233078098380287 3.6953800004956103e-05 3892 0.0005782299538211819 -0.000511037866321869 -0.0007473249488771298 3890 -0.0016705713239520646 -0.0016069659718295378 0.001065209503728186 3156 -0.0010603404644802718 0.0008280852974851052 -0.001405616529550618 3876 0.0018845741710028787 -0.0009072440934231027 0.0010008476653345214 3157 -0.0025831622759957297 0.0005952524576052721 -0.0004901351818426725 3875 -0.0021498073307040133 0.00044179231046969866 -0.0016935429693262455 3141 -8.569036948772343e-05 -0.0011260967782928243 0.0007455747433111173 3862 -0.0002159543580809969 0.0012834270970237419 0.0009368203243907576 3142 0.000564125194441067 -0.0009407173098720883 0.0011596156401047413 3863 -0.0002662039842456055 -0.0012297854138933891 0.0008467431315821437 3839 0.0019388519260411562 -0.0012283870742542257 0.0001972514845599337 3126 -0.0006990287565599108 -0.0007054864202825824 -0.0012850885278145596 3128 -0.00024685120637075965 3.989282825327643e-05 0.001255514723828518 3837 -5.3755177530605616e-05 0.00045772734077481657 -0.0006522076824515443 3125 0.00044302321760076625 0.0014708331850635317 -0.00019953951210966955 3836 -0.0017932795541790506 0.00023935181408772004 -0.00030885065446529646 3127 0.0004335014119118347 -0.0004464305265350091 -0.001333471930540496 3838 -0.00011403518400871816 9.426484442206346e-05 0.0011084844500118588 1702 -0.0003222185309085879 -0.0007921691074598376 0.000679839994185848 991 -0.0006585203600039873 0.00019713013571178621 0.0017044945276151176 3896 -0.0012664294918170603 0.0005661872478273375 0.0018117473259061413 3183 -0.0004507091212307831 0.0015575909417119974 -0.0012419879941298546 3894 -0.0013685980660243884 0.0010920673055263958 -4.521375477062155e-05 3185 -0.0005168323331024371 -3.05670852360127e-05 -4.347511479353824e-05 3159 -0.0009306959583137923 0.0006175260400152697 0.0020442022082131604 3877 0.00046334601190335103 0.0003502253201384381 -0.0006440154577292201 3158 0.001689930545512441 0.0005301904312795447 0.0008380303973762643 3878 -0.0016421301734983055 0.0007086625097180548 0.0014653913978791562 3864 -0.000944799853925059 0.0018803863361313603 -7.303968113569548e-05 956 0.0007773649038247048 0.002036317270404696 0.0018505871401404768 3144 -0.0013693381524155447 0.00024140874006708902 0.0013583147286253137 3865 0.00033462931349247864 -0.00010169648729236366 -0.0009053755041468719 3143 -1.5997513176593467e-05 0.001140539899275894 -0.00026058061655794234 1675 -0.000625030988951234 0.001457467876486138 -0.0005130376188030616 3843 -0.00032191360954801537 -0.0004739462440755786 -0.001596147294998257 3132 -0.00039376703992188367 -0.0017003002263465351 0.002481428412823456 3130 -0.00015747799896570318 0.0018485113478094312 0.00010865397071605182 3841 0.0020463371705399026 0.0014706016010694253 -0.00234438645337568 3131 0.0006315378467231338 -0.00032457648775044944 -0.002340511409881995 937 -0.0010915888915745625 0.0003535239837196881 -0.001974883236841805 1648 0.002072304003344876 0.0003906921032950266 -0.001189501441906054 3840 -0.0018410362115805436 0.0005421421651113467 0.0010683513066728528 3842 0.0011129157443796353 -0.0005171087163507015 -0.00038857663745376194 3129 3.676291873562043e-05 -0.0022599871446166908 0.0016189619710299489 3821 0.0013712738139651493 9.440095576869327e-06 -0.0009040583019815913 3908 -2.7182683251753188e-05 0.0013264348068061436 -6.419267382559539e-05 3910 9.911198141656415e-05 -0.0005836393100219551 -0.000986900528739901 3899 -0.0003021164330502548 0.001538737333299689 -0.0007220459801661927 2432 -0.0005765468198738516 0.0005190563787973382 0.00031500457500476897 2434 0.0018887649117795364 -0.0018243326043271167 0.00012209070985507624 3901 -0.0003549492778471884 -0.0006816393365258719 0.0009190740843779031 3886 0.0009468874943917391 0.0010528851726321017 0.0005155952165796947 3885 -0.0005063348390856008 -0.0005033469859555257 0.0006266951966982198 3881 0.0015914912575065747 0.0005741855262939416 -0.000535948389834706 3880 -0.0012197605607233636 0.0007295992706716349 -0.0007971127081234542 3866 -0.0019270680087926345 -0.0014551540860931382 -0.00019312040269583042 3871 -0.0013668909231961625 -0.0009860305655104702 0.0016882777694032104 3867 -0.0002459073337749469 -0.0013023431149569436 0.001557525302193934 2404 -0.0003347436123476576 5.689088311162027e-05 -0.0022011526563884692 3870 0.000643142157666803 -0.00030496510927325703 -0.0008249151769539409 2405 0.000925301816410272 -0.0008561749637491252 -0.0002264905000510318 3848 0.0008256927671365674 -0.001037836681885778 0.0011573886303196123 3857 0.0007285970216494076 1.0647673366944582e-06 -0.0009342314689666202 3855 0.0009705776853803345 -0.00040050251763668304 -0.0021819523435181562 3846 -0.001292991119188975 0.000407953404045308 -0.0004462442003612564 3845 0.0014993050537231096 0.001566814200732285 -0.0006492792825385288 2378 -0.0016543231939923138 0.0005053917899882646 0.0018223102655624338 3854 -0.0013783658969899037 -0.0006223383395613769 0.0007419072154226885 3856 0.0008071414440955983 -0.000930957136256036 0.0008676928646033056 3847 0.0007862249207682038 0.0021297630825255235 0.00044949522115490266 2380 -0.0005703808327322593 0.00025729850091393835 -0.000459206143587452 3825 -0.0015705764610413028 0.0011295063053339232 0.001788854183316592 3823 -0.0018377862953732763 0.0008736810873714047 -0.000384504469404134 1666 0.0009870888060028353 -0.0019973618056175146 0.0011463083117888811 2384 -0.0004228867123645518 0.0006076153327021687 0.0006290723048183145 3860 0.002412521750647116 0.000941453059265173 -0.0008499094827102832 2382 0.0009802901526649833 0.0002581009208689679 0.0009495558821022028 244 0.0007637746993868468 0.002008494982467349 0.001897468699865163 3903 0.0006453649260865617 0.0025779538667295107 0.0002373388424916959 1720 0.0024523539907967276 0.0016773042997289813 0.0015235053800256488 2436 -0.0009468170412040405 0.0004494630849725171 0.00012533557260626868 3914 0.0007298712899505818 0.0012081873695291153 0.0008376239256547212 1711 -0.002111326904994995 0.00031323593835651167 -0.001069144603025872 2438 0.0012186952297188794 0.0011492295994573961 0.0021381579545970307 3905 -4.685427777405423e-05 0.0017314688283137291 -0.0015910762666162793 3912 -0.0021141403699358524 0.0005054560407361651 -0.0008340169415152415 3882 0.0016923561193528905 -0.0004569498807069904 8.550675466206846e-05 3888 0.002100203791588534 0.0015467318390052045 0.0010399378142318084 3887 0.002228542388055826 -0.0005047611763634185 -0.00034040097905903874 3883 0.0006852017088904986 -0.0007324659167095773 0.0003789256038917569 3868 0.0007745351786140923 -0.0005889719949837504 -0.0004165827954477908 217 -0.00032110228621511387 0.0009538699909869889 -3.1692831158133036e-05 1685 -0.0013535836466869156 -0.00046894894551832884 -0.0020074160381339276 1680 -0.0015162831071695942 -0.00027341177453833287 0.0018811911108136928 3872 -0.0012737242352122698 -0.0019177768478747497 0.0017499942827113543 3873 1.7086978540472968e-05 -0.00021926983054589184 0.0015484370330755698 3869 -3.152261777424363e-05 -0.0019445200823375388 0.0006411314881515878 2407 6.12725985151396e-05 0.0010150324348143808 -0.0025399660621533357 2406 0.0014420384524277102 0.0008080146858461519 0.0003453015573553079 3859 0.00021709270699333183 0.0022193399531900576 -0.0002707029430843729 3850 5.0241368816614506e-05 -0.0015968294602875602 0.000996035462349352 3852 -0.0007946957762675121 0.0002751498752849809 -0.001667129723109644 3861 -0.0008066245357477395 -0.00041772573634139083 0.001054692936722349 1657 0.001421298401167375 -0.0008820704338700006 0.00031397826075929753 190 0.00026816255666598974 0.0006938066899441995 0.0011151585918995983 3849 -3.202652780926883e-05 -0.0011225418134874247 0.00045335761989254305 3851 0.0022460586474191318 0.000644650891659868 -0.0002851073648708455 3858 0.0010089532307919046 -0.001237687096188303 6.795534441026135e-05 3236 0.0022406419146431262 -0.0023430561888894493 0.0005163215899566735 3947 0.0007950390802574363 0.0019346052485068258 0.00028540833404420876 3945 0.0003948503108445081 -0.0012492879505843829 -0.001303632660762761 3234 0.0006481774395638389 0.0014573169941175406 -0.002598092953449149 3235 -0.000794277797593528 0.0009407535450449335 -7.610793338663476e-05 3944 -0.0004043771279490145 0.0008149485607104165 0.0007662631191032786 3946 0.0007527744756272352 0.0012144452411004738 0.0019901382533947147 3233 0.0009164604885431548 0.0014177521267410699 -0.0020163787542783937 3209 0.002543437323697945 0.0008331301778284892 -0.0013858353665967649 3918 0.0001805045233146652 0.0004133812657926921 0.0020975091600100373 3207 0.0006196574723294163 0.0017031157946657072 0.0005769543304584361 3920 -0.0008490219402081233 -7.651494156432972e-05 -0.001328460982793164 3206 -0.0016335240427097885 0.0019988434567309588 0.002078913559486308 3919 -0.0015758143712548635 0.00016449255486033544 -0.0005027931420296845 3917 0.0001483999606400894 0.002064262758205 0.0008137492062749885 3208 -0.0006362614257711631 0.002477681371740553 -0.0010076927427709087 3893 0.0022025475774496628 -0.001626526940252345 -0.0001678189879214245 3891 -0.0002752581193166241 -0.0009339606958718093 -1.482704693867552e-05 3182 -0.0007428141020319465 -0.0006308002493117179 0.0013879217919048911 3180 -0.00043135429994573286 0.0005066748646868123 0.001855629395392893 3240 -0.002461205754151981 -0.0018973559144586896 -0.0014648677385137076 3951 -0.0009342592871225117 -0.00037117363781784897 -0.0006747572669168324 3238 -0.0002638263291877325 0.001334189595894119 0.0003138681785375024 3949 -0.001326233597775252 -0.001524378831498707 0.000906761820108451 3237 0.0002705360383135571 0.0017330246346316013 0.0006293552024883394 1756 0.0005845986812330864 -0.0004461578010426389 0.00016013311595970301 1045 -0.0010708654242615149 0.0017886950707444915 0.0002608132366116755 3239 -0.00037522281790063733 3.050617725091319e-05 -0.0019362010496240055 3950 0.00037047588993199517 0.001925511537656944 0.0012721640065048636 3948 -0.0015851229297599424 -0.0006066339345252904 -0.0007253799965502013 3211 -0.002479774157070021 -0.0016338744220687914 0.0010115456989111613 3924 -0.000523716612300551 -0.0005453524590079634 -0.0014607045374865745 3922 -0.0016461920971929385 0.001147959846455167 -0.00035635089771437166 3213 -0.00110364230297433 0.00023044942633256807 -0.0007691526877769868 3210 0.0017198004289986112 0.0018375861571077548 0.0003964832316346509 1729 0.0007562493743223544 0.0008964448201529387 -0.00023895052233721963 3212 -0.0016565323087136853 -0.001900913970140864 0.0016719607309305692 3923 -0.000953581709210124 0.0011355121455262347 -0.0019629120228029187 3921 0.0011473385352505213 0.0005660164623640758 -3.6238235752042306e-05 1018 0.0009050080258921427 0.0008826835679320436 0.0017990949590436674 3895 0.0009430700226566975 0.0014587318395296548 -0.00047325236959778593 3186 0.0016710025400762162 0.0021575100535667744 -0.000409616370071609 3897 -0.00048737097034114206 -0.002111429457928273 -0.0003621625515841005 3184 -0.0015018868784926202 0.0025586676246969696 -0.0009667299952697658 3954 -0.0017407863468946847 -0.0007675532078365572 0.0006547853048311126 3963 -0.0020986887281895634 -0.0003051116265201468 -0.00024456885744667613 3965 0.0013504660621593335 0.0016109225291842824 0.0016050063838599343 3956 0.0014443837423306278 1.8328416448551714e-05 -0.0008657382582493718 3962 0.0010825213805832718 -0.000997934722143047 0.0010006014513465908 2488 -0.00106015865670976 -0.0007358202036217227 0.0019207212759854784 2486 -0.0013604795142945379 -0.002237926157357621 -0.0004655530042222613 3955 -0.0007687906974381739 0.002512599166138274 -0.0007126412043705573 3964 0.0011603460293471762 -0.0010675051787251092 -0.0010416385803930614 3953 -0.0007636967390756829 0.0011512420562569267 -0.0002502583242806949 3936 0.0002936617791323205 -0.0007892867733444409 0.0011823229890993439 3938 0.0008171342935162892 -0.0021790380705219467 0.0017369467065753617 3927 0.0009202830795519612 0.0011632709308638622 0.0022545732508562847 3929 -0.0005867634541109907 -0.0011979574165176697 0.0004165294980645498 3935 0.000878920396583943 0.0007886726599240234 0.0015076280282513553 2461 0.0005304186334603384 -0.001108467538968073 -3.878862753517649e-05 3928 -0.0001892155591549469 -0.001285779592196726 0.00030451458183579534 3926 -0.00027157409317802423 0.00035951390736272564 -0.0006942701813037076 2459 -0.000713806761987294 -0.0002546363133227342 0.0006156973749088992 3937 0.001069593706947259 0.0015960985795159623 0.0013461902878704045 3911 -0.00021067231071170188 -0.0024931019355599435 -0.0014349367875922084 3902 -0.0008677988756768486 -0.0008137309279395942 -0.001882013518853153 3909 0.000342783066245429 -0.0002105868471528958 -0.0013680026375587182 3900 0.0006465281103856281 0.0004447853553882987 0.002113359535698059 3969 0.0007090211033719616 -0.00033650915041478493 0.00040457082153991675 3967 0.00047073534904746076 0.0003373503262458185 -0.0012287036583536039 3960 -0.0007674954431945836 0.0010256447371838548 0.001884638090309725 3958 0.001097013095891391 0.00016425125956438715 0.0010525318014374732 3968 -0.0005334819308278544 0.0005598942302700496 -0.0009552952920219836 2490 -0.0002276142163768649 0.001174410666151731 0.0005922646826555043 1765 0.00019254505080947741 -0.0006790355951230533 0.00045319788512507774 2492 0.0006628743706331599 -0.0011944505191902072 -0.001375013601232619 3966 9.61058311253057e-05 0.0016954807532073317 -0.002117733549473772 3957 -0.00027929653690426026 9.619784202666423e-05 -0.00019654304514239642 3959 0.0005259912216129007 -0.0006609908645722165 0.0004109725250544072 1774 -0.001256963119254515 -0.000599485892782614 -0.00024071410191200428 3940 0.0015409167432137228 0.0004402416953430255 0.002625166773443552 3933 0.0009684634869477056 -0.000259923828607231 -0.0010804779129090724 3942 -0.0008480543690319881 0.002488540882382557 0.00035463180980061746 3931 0.0005872124830349184 -0.0010799561753700561 0.000614391182975815 2463 -0.000683778074879767 -0.00045149727086807746 0.000547924101402048 271 0.000736158837637623 0.0014804502336686455 -0.0007953367134874283 2465 0.00023640109959673571 0.0024485368461746853 -0.0016511665815370125 1738 -0.0012679286442602682 -0.0006918154929099378 4.942473594295258e-06 3939 0.0017326281862053757 0.00030928403930059376 0.0005705195585158653 1747 0.000617146132840684 0.001576741413459295 -0.00033125189623546547 3930 -0.0002416220040036745 -0.0006087986384908314 0.0016668823451979156 3941 0.0002719851894310249 0.0001659753377567983 0.0017501780649074356 3932 0.0014248342159172262 -0.0006712199849103749 -0.001291771685225335 3913 -0.00010001677142875472 -0.001352957165167648 -0.001660052507720122 3906 -0.0004895840651315143 0.0009296034276299956 -0.0004558105446113704 3904 0.0013966090416502983 0.00135964262223786 0.0007609228214085144 3915 9.535641879096664e-06 0.0003092991235096399 -4.69712424843009e-05 298 -0.00017421942474660267 0.0007955610635175459 -0.00105338752847317 3316 0.00020101357154131546 0.0015023067684200018 5.675970674868082e-05 3314 -0.0002381225441064633 0.00011892451983218705 -0.0005990141341018034 4025 0.0007224157246721451 0.0009746762701804731 0.001581484754502859 4027 -0.000828323296548856 -0.0006655470224273745 -0.00038918459155595883 3291 -0.0009104112124487801 -0.0006142941319621886 -0.0006237181127037189 4010 0.00036140989739964833 0.0014023723292864566 0.0007168038211024458 3292 0.0002661268563149662 -0.0003625043774848763 0.0008485012731041893 4011 -0.002135758147985406 -0.00010536807344376908 -0.0004639376730537347 3276 0.002510229648939486 -0.0010689596602569385 -0.0014990849620627317 3997 0.00010368757353974595 0.0027665914063519947 0.0008955013671961191 3998 0.0006220989787868636 -0.002071745458089532 -0.001657116676017177 3277 -0.0012947972575108138 -0.000999795152863233 0.0005195720854042753 3972 0.00040153048672647075 0.00048522003698414423 -0.00023233682186459014 3261 -0.0007098356653534497 -4.2946465172210516e-05 -0.00027007791699411744 3263 -0.0006879140818195316 0.0006578280455492283 0.001998795916863805 3974 -0.0012410322236085895 -0.0005295101877365194 -0.002062961942747413 3262 -0.0011608102338280485 0.0005397547804746431 -0.0014596804276591417 3971 -0.000550475193155959 0.00013365947200393111 -7.440984255771641e-05 3260 -0.0014886228542861967 0.0006617687966295153 -0.0017963357111665757 3973 -0.0012790473686200398 -0.0005154614562631178 0.0003810923809180603 1126 -0.0008897805644259393 0.00011442856650070807 -0.001763883887762584 1837 -0.00017411976339829264 -0.000201366467952577 -0.0003215138307260015 3318 -0.00022199337353615099 0.0009869094309151512 -0.0022688057980066794 4031 0.000738152943962087 0.0004662257790862352 -0.0009005597169909182 3320 0.0002675960816300101 0.002268979684568907 -0.0009568823402237262 4029 0.0014628252558340393 0.0013110510147601477 -0.00028544190166382454 4012 -0.0013710171636815813 3.106242780942319e-05 -0.0007314394178342334 4013 0.00045903111557397415 -0.0004413023415764372 9.482338825353583e-05 3294 -0.0013633669001133848 -0.0010186282905716058 -0.002666084153408081 3293 1.7527089864193164e-05 0.0023010478903514016 -0.001123431470443619 4000 0.00017457386360582067 0.0014025259384144167 0.0005175670187811928 1091 -0.0015597634903729667 -0.0002028692324291419 -0.00035615320088204245 3278 0.0015572965262269861 -0.0003233892888852832 -0.0019807550783222743 3279 -0.0008270689011500836 0.0001876147397292657 0.0007063297123893269 3999 -0.0004554334400415183 0.0009894716302212376 -0.0005551508216127695 1810 0.0015134404948302547 -0.00032560031145478416 1.356434899275892e-06 3976 -0.0023106853829653394 -0.00017333961872693747 0.0014905017839882888 3265 -0.0005638197325045619 0.001563816201035657 0.00030922199738908336 3978 0.0010591824351351615 0.001245755867590619 -0.00015998138433252502 3267 -0.0005897255011892018 -0.0012510847115741938 -0.0008489338307811757 3264 -0.0011826970906067338 -0.0007156087354086016 0.0017205393095879001 3977 -0.00017206029469594639 -7.973518443394451e-05 0.00023074097861582998 3975 0.0002819685898915226 0.0012351101260065472 0.0013067764849937725 3266 -0.0004503079919468232 -0.0013018954997059602 -0.0024942586496785476 1783 0.0005501307477903893 -0.0008388968155555181 0.0013466032340062359 1072 0.001455780277545346 -0.0007606355213485609 0.0011470091157794117 4043 -0.001295580807028325 -0.00015590236916380442 0.000758055265027533 4034 0.001208318797261868 -0.0016100500211114798 -0.002706540863800998 2567 0.00034063009432826 0.0016804097641293422 -0.0012569279212895168 4045 0.0013731067885334428 0.0019130590268641168 -0.001951243188362276 4036 0.0008187459937442497 -2.7853490414686283e-05 0.0013935846505293717 4020 -0.0010315474988129786 -0.0011238637546468716 -0.0003186355775704377 4021 -0.00045949021657455615 0.0006303920650909439 -0.0017672259040996932 4015 -0.0010800996471903768 -0.0006551928880601583 -0.001076383168312389 4016 0.0003939678673186191 0.0011044395963690202 0.0003820791601548781 4001 -0.00047686724809259124 0.0008319517137164131 -0.0019157494065849122 2540 0.0020632122184873363 -0.00043542605343276065 0.0020248875494283465 4006 0.0011272505336522376 -0.0007150270750679017 0.0009574069954831257 4005 0.0013286147317319668 -2.8772682908419472e-05 -0.0005324441266064783 2539 0.0010677992851047537 -0.0021939584949218945 -0.00036677784548061666 4002 8.2419093435273e-05 -0.0021003158884605974 -0.0010293327268844636 3992 5.184313581903721e-05 -0.0024017171467970557 0.001025201270197626 3981 -0.00025059429874119913 -0.0018951511041206094 -0.001774873486534117 3983 0.00013098840722919813 -0.000503438394622184 0.00018751862158638633 3990 0.001968677714260757 0.00044049927769258855 -0.001274980394463498 3982 -0.0017670988975686571 -0.0016554393244890963 -9.35773029746771e-05 3989 -0.0018248134314821358 0.0011235851939920918 -0.0006699629262909078 3980 -0.0006828537826042263 -0.002145780945181976 -0.0009878841018979212 2515 4.689280706670577e-06 -0.0008141157550291651 -0.0004435274808466336 3991 0.00045247144347503314 0.0025157841079662415 -0.0008729935705343423 2513 0.0017729294565597311 -0.00020839088219286209 -0.0021097892329063907 2569 0.001506748495302057 0.0001443073870204246 -0.0018738834781803992 3993 0.00016226329502578348 -0.0007785284374491325 0.0015581898186628519 325 0.002195427644182555 -0.001241964883348124 0.001429862491445224 4049 -0.00038509263118075845 5.006961122044418e-05 4.438040031622462e-05 1855 0.0010255135311616802 0.0004401954486850986 0.0010189861793519482 1846 0.00010997953248422822 -1.2512946397940598e-05 -0.0004690474376617085 2571 0.0005154737966095117 0.0002810957107142755 -0.0005522927464969556 2573 0.0012378151827812946 4.364166608461593e-06 -0.0003359893760926545 4038 0.0021391696740629823 0.0003628082739697974 -0.0001451508489696161 4040 0.0002815701976131798 -0.0015956208620389132 7.187483219706081e-06 379 -0.0002163432123950582 -0.0015676130383786536 0.0006869138578137113 4047 0.0014945466016929088 -0.0002926358661104293 0.0006050427955052444 4018 -0.0002719918837065065 0.0008805851512244413 0.0009622906546446208 4023 -0.0019169459302532514 0.00107093816741115 0.0022149198635585026 4017 -0.0015564510014972825 0.001353516194192018 0.0014299340417122332 4022 -0.0002004693471204344 0.00155255491460656 0.0015246208600535683 4004 -0.0014224999810080216 0.0004381265236013225 -0.0009414838064739635 4008 0.0009213489485571246 -0.0008790904886169688 2.088851949603055e-05 2542 -0.0022946753169823747 0.0006098369259460649 -0.0012201347142578901 352 -0.002173451104939844 0.0025452295117500386 0.00143931521777409 1820 0.00022379076618274542 0.0006393485458152307 0.001176913777082096 4003 9.078797445171479e-05 -0.0011129656043123296 -6.977042213862097e-05 1815 -0.00011835399308977044 -0.0003330747312829604 0.0017464757374836492 2541 0.00010886745794701398 0.0003101798122950301 0.001070759794526178 4007 0.001089698654698541 -0.0002550119237416282 0.0006123968276012643 3996 -0.0010119416348940246 0.0004990304296340524 -0.0013700316012592293 3987 -0.001665509124337612 0.0014950945451141994 -0.0013736277517629705 3985 -5.2620088583168085e-06 0.0015754551228934046 0.00017756169639049075 3994 -0.0008102816083452044 0.0007090728499438202 -0.0019168885922192112 3986 -0.0014565371385124675 0.0020072521725882785 -7.171147916806083e-05 1801 0.0009007235427650137 -0.00017355505068264226 -0.0001415411954063827 2519 0.00016600502802190413 -0.0005895055556529649 -0.0005309264357240264 1792 -0.0015699240207886485 0.00015703939323049904 0.00039568764651472157 3995 0.0008802253440895753 0.00013953290773034135 0.002526180406406538 3984 0.0006719019792049896 -0.002040890751947461 -0.0008824634588881291 2517 0.0014556602904003046 -0.0019980201683703074 0.00013639180581775912 3372 -0.001288951681523332 9.13495536148533e-05 -0.00026715892648026315 4091 -0.002275227818883883 -0.0015191222719336892 -0.0007839181441063052 4092 0.0002824783876125887 0.0023325967654605124 -0.0004063723355830038 3373 7.640570380889342e-05 0.0018000756368456074 0.0018928906505722987 4078 -0.0015199308397790359 -0.0008913010866357586 -0.0012087438939819156 3357 0.0007189085310032087 0.0006468323592655745 0.0010794772810181253 4079 -0.0006390815454035539 -0.0015600299005516325 -0.00019409306878833375 3358 0.00030790109171085264 0.000925923682371276 0.00049587509931629 4055 -0.0012309916784063427 -0.0005753477642701033 0.0003934874174484997 4053 4.4383111686839734e-07 -0.0011026706582395478 -0.001229648498846079 3342 0.00048403835875256975 -0.0008145962206635284 -6.398758746264889e-05 3344 2.2302108543370124e-05 -0.0004821005742265909 -0.00046492554535054915 4052 -0.0014338390777861249 -0.000425888550508516 7.036012361927605e-05 3343 -0.0010818792731323308 -0.0009152840323808669 0.0003829802155198565 3341 -0.00015644267648727745 0.00046576186405385806 -0.0011457157660430422 4054 0.0004347687731118212 9.659051446569305e-05 0.0001886975962155646 4028 0.0014391673826257881 0.0021746341255577083 0.00033312075507922626 3315 -0.0019524133269851539 0.0006583819613788762 -0.0012673008362832138 4026 -0.0007011800476186991 -0.001067324884166367 0.002519280280630559 3317 -0.0008241638471208988 -0.0004472074884425868 -0.0011209016384703748 3374 -0.00022959620392362526 -0.0007907439827408373 0.0008791653599292124 3375 -0.0013735713968405425 -0.0013511592860866067 -0.00168453678138965 4093 0.00266510347662265 -0.0011031320107456255 -0.00018546200062255177 4094 0.0002449534801841703 0.0014217708201094388 -0.002100999212336725 4081 -3.4756090160458896e-06 -0.001204928832191867 0.0005769030461231783 3359 -0.0005994751792710622 0.002008665229953083 -0.00021348749926910322 1172 -0.0018776370942655684 -0.0010333716030150781 -0.0017291655688477185 1891 0.001334058311170408 1.5082314717804147e-05 0.001367364664601707 4080 0.00011731624927572296 -0.00022198288636949269 0.0009646752233737668 3360 -2.7096613842259466e-05 0.001070124152958134 0.0017238946791689744 4057 -0.0017368326669795339 0.00025382097037420404 0.0017853352073346367 4059 -0.0002100108376761993 0.00200620359306806 -0.000981617668685834 3346 -0.0018915385383464398 0.001476383343147482 0.00016419540051856374 3348 -0.002000535189490264 0.00237474060022947 0.001839994378504838 1153 -0.0008392865437070287 -0.001315441005030917 -0.0016001067603508136 3347 -0.0009821507873729132 0.0005490482815227358 -0.0027147574127721497 3345 0.0011830937785740994 0.0006515745103788353 0.00032224814815823375 4058 0.0014705545264142908 -0.0005581641584122326 -0.00023979569375457105 1864 -0.0001755671081506088 -0.0008971575213017452 0.0023580701548648244 4056 -0.0009976597057670062 -0.0004487536730015703 0.0015771779032409982 4030 -0.0009143507485757321 -0.0010877383020611523 -0.001393166754919126 3321 -0.00011364219589319853 0.00014078981585564617 5.4279804771033844e-05 4032 -0.0011183736548218766 0.0009326449380429406 -0.00044889003892182775 3319 -0.0019129397522872505 0.00036573411836094295 0.0009266156598242056 4096 -8.35971511650305e-05 2.8630065901847756e-05 0.001314687852493385 4101 0.0014933297492008449 0.0005539395456184585 -0.0021915287210806152 4102 0.0009429963387690718 -0.0011235564353768643 -0.0004003100592148926 4097 -0.0005432016899484366 -0.0014992757283746885 0.0011693527256041965 4086 -0.00012883183453949614 2.135481658873707e-06 0.00011349556533856386 4083 0.0008632189790372842 0.001825615555399567 -0.0017933448165283312 4082 -0.0006845233064039185 0.002021200460756812 -0.0007418675496006224 2621 -0.0006513667751765597 -0.0011640865198433916 -0.0007485300262677931 2620 -9.63303933591167e-05 -0.002466110298905208 -0.0003076217683657339 4087 -0.0007144437040268303 0.0005165206153047561 -0.0011979400364570973 4062 -0.000341410807730532 -0.0013844755702285827 -0.00013514093635296403 4064 0.0015262528969556036 -0.0012835637355244598 -0.001613650243050534 4071 0.0001446540299402839 5.899747513503774e-05 -0.0015619894975160379 4073 -0.0002767446309584724 0.0003546469024434296 -0.0009969982730071855 4070 0.0023951968218187385 -0.0013289969277520148 -0.0004899565622679268 4061 0.002714144810556613 -0.00039012160635409215 0.0009264427456188263 2594 -0.0016602296771244629 0.0014515547863663712 -0.0010463430797720942 4063 0.0015257386861258998 -0.002417783222506161 -0.001669281961524399 2596 -0.0012412429902616423 -0.0015787031745736733 -0.0002655425136880174 4072 0.0002998323652565689 0.0003182567895003782 0.0002695963926415677 4044 0.00017905241258096274 0.0007572313815137255 -0.00019975590487408086 4035 0.0002876541598602242 0.0017230734969547132 -0.001054348080589356 4046 -0.0006550935629353887 -0.0007580999671805522 -0.0011181012374130586 4037 -0.000563630365853985 -0.00010293002032876752 -0.00016945367089269184 4104 0.0007592769894466107 0.0010084192084765047 -0.0013850231827274113 4103 0.00040090632659349826 -0.0006877388798141278 -0.0009397338651244294 4099 -0.001141811965127165 0.0017179359980948768 -0.000588440651203152 4098 -0.0007529789834716213 0.0011192893500175704 -0.0018285529999290356 433 0.0003286669618547197 -0.001318307714739932 0.0002554895687908478 2622 -0.0006986745565974136 -0.002147845733317985 -0.000597707556269629 4084 -0.0014326847399524696 -9.86495097302023e-05 -0.0010481900474634733 2623 0.00019490834269714858 0.0008444952845436574 -0.0020230581485637346 4089 0.0008057183352798123 -0.0019835105733163132 0.0006689120728715519 1896 -0.0015887008452533534 -0.0015443649609489024 0.0004792639467660801 1901 -0.0002217062013244466 -0.0006021439166587441 3.715178618930899e-06 4085 -0.0004182525850026504 -0.0010527795064591851 -0.0028069054698186967 4088 0.0007775361965676334 0.00018864889025766124 0.0004358895933872578 4077 0.0003542646816673649 -0.0018663411404386137 0.0011763955403432404 4066 0.00026089401667595273 0.002133894744894473 0.0017757441198488584 4068 -0.0005390664682948834 0.0009523117602431913 -0.0013245036725792348 4075 -0.000274693101969536 -0.0012857711912949528 0.0003223647273892775 2600 0.0002083458556066145 0.0009694293398011481 0.00010951918719435787 1882 -0.00023607295113846935 -0.00023087200729634194 -0.0014929986265092635 1873 -0.0004868854067567699 0.0008414869393447749 0.0007828155943957865 406 -0.00043260311434516804 -0.0017276963215949051 -0.0012592061422502137 2598 0.0003609775976524908 0.0019110308972544808 0.0016155015599732796 4076 0.0005118426961157325 -0.0013809063963704693 -0.0008347339759114829 4065 -0.0009470394441408352 -0.0004120528833291321 -0.0010758912292564828 4067 -0.0028306881873549914 -0.0005394461097632017 -0.0006620123892772066 4074 0.0002878912427194565 0.0008002408832016967 -0.000164536990998975 4041 -0.00021785818447718795 -0.0016387194823375157 0.00015053625852029206 4050 7.303427098043691e-05 0.0013945032082455372 -0.00032659648869210324 4048 -0.0005326211137107989 0.001099850276931897 -0.0004454018477861538 4039 -0.0013679403873551985 0.0016744974463261848 -0.001445628419421301 4160 0.0002480163059278642 0.0019205112419246398 -0.0012262671264035986 3449 -0.0007965462618776506 -0.001963038167807943 -0.0021572647052221644 4162 0.001493386142614869 0.0007429499847873196 0.0009414978896089714 3451 -0.0005413710322811299 1.613978386761283e-05 0.0010680607179946145 4134 0.0006293570697427516 -0.0003579407918478537 2.7462008636814587e-05 3423 -0.0006906759226039542 -0.0006639569435119691 0.0011602861986714462 3425 -0.00017044377791812656 0.0012607571088874712 0.0002892212375976422 4136 -0.001110916054603601 -0.0009032477411865439 -0.001576977428757772 3424 -0.00018873638583377086 0.0002049772333939646 0.00022980872216109462 4135 -0.0008626210361771885 0.0012947064235676574 0.0004727393166801939 4133 0.0010571886820136451 0.000610928438212978 0.0007403566989649032 3422 -0.0013615132289582393 9.999906177204953e-05 0.00022703731938131114 3396 0.0015835470089378058 -0.00101177645469933 0.0013526435718639541 4109 -0.0020640751767957463 -0.0017775659837811664 -7.38389851833133e-05 4107 0.002255485283475579 -0.0006925995815462157 0.00029297066615092574 3398 0.0008483975831976029 0.0014630501822595742 -0.0014354171812044052 3395 -0.0007323500837191827 0.0007944251812304405 0.000651640266969031 3397 -0.0015854531349416506 0.0002984506837193494 -0.0004306786719643586 4108 -0.0016261823595916873 -0.0009348854649331239 0.0012658250445980346 4106 -0.0015242272542023217 -0.00245640011239291 -0.0017091338934392118 4164 -0.0018164653117008934 0.0010023270994360713 -0.0011603514922017305 3453 -0.0004302736133315838 -0.0020564424163078032 0.0016572523664439684 4166 -0.0021755532635947803 -0.0022041979545712864 -0.001069208038455079 1972 -0.002216849630675802 0.001749590816057042 0.0006034315154675449 3455 -0.0021474816395872344 -0.0009562623594399893 0.0008560867562718918 1261 0.001659885008221879 -0.0014058930698526016 0.0007470360473588976 4138 -0.0006862501062529949 -0.0004366088142392034 -0.0011227499639384596 4140 -0.0022855879597923024 -0.0002705061684895138 0.0001340406752894722 3429 0.0011676517018907348 0.0018067890496015746 -0.0019896715128826415 3427 0.0007127816620861231 -0.00023970702743016255 0.0015148573356939723 3428 -0.0005900384216813756 -0.00011942527203450667 0.0006024273058196159 3426 -0.0011609997854317325 0.0005073011952955515 -0.00017295490303399481 1234 -0.0014630191968198452 0.0016024784031215733 0.0022399106695576735 4139 -0.00022587295861277337 1.2871902733749534e-05 0.0002229095680519387 1945 0.0010250245447595528 0.000389863158465278 0.0005290513806541686 4137 0.0004044383664064677 0.0004507193653826954 -0.0012082460591038586 4113 -0.0011247331922736863 0.0011424654745116653 0.0006587484843747734 3402 -0.0006378892302463879 -0.0018450765264007589 -0.0012880523397748745 3400 0.0013995112521874343 0.0007584111173974117 -0.0014489353395892575 4111 -0.000775978824713279 -0.0002893832103052819 0.0007338993575799541 3401 -0.0001454604289649799 0.0020058750719525818 0.00042099218286470366 1918 0.0021640784174651647 0.0004306670815604512 -0.0011942717913348848 1207 0.0021997146012671825 0.0009359773796621652 -0.001975215278747105 4112 -0.0007360183395299256 -0.00040862289020209843 0.00018702853477228516 3399 -0.00037364963304476785 0.00048523460561885104 0.0001656842418902441 4110 0.0015731950575409972 0.0013359518985899428 -0.00156551884781834 2704 -6.91420740294834e-06 -0.0007045072796824929 0.0005549425052456834 4169 0.0012125640996195068 0.002106497511231512 8.100274787784445e-05 4178 -0.001919894031910611 -0.00016227484682823905 -0.0021388618941859676 4180 -0.0024843145100009634 -0.0014184817338482518 -0.0005362741692559307 2702 -0.002096550844337494 0.001566462505127475 0.0011270864730411044 4171 0.0010400028038240483 0.0014816548764899594 0.0019503572777029765 4143 0.0006761928538530196 -0.0008478531584032461 0.0006598345870487557 4154 -0.0023791076378301824 -0.0006878862547580958 0.00033470723691743603 4152 -0.0003231977098369199 0.0011024238268555072 0.0001646354077784499 4145 0.0017359886197860976 0.002167235200934844 0.000554361775653271 2675 0.0006011697711275027 0.0007225376979926509 -0.0012175784810619858 2677 -0.0011662156258895376 7.162809280101645e-05 0.0013364448379547195 4151 -0.0003631769744617936 -0.00010710632581254474 -0.0008757242143343008 4144 9.03471313747344e-05 -0.0001964290665356491 0.0006722189270625034 4153 0.0010732295127106435 0.000879894620935499 0.0004269593579020413 4142 0.0007963167780252634 0.002436657163242993 -0.0012079062658086927 4125 0.00032660278715319847 -0.0024594802587953658 0.0001805290779461862 4127 -0.0008735359408394497 0.0014691676074958687 0.0014098296466051726 4116 0.0006971370486357452 0.0002935456497997521 -0.0008542831018072473 4118 0.00015154863765514098 0.0018977459010311641 -6.956148462059246e-05 2648 -0.0016304417403686822 -0.0015441813044398437 -0.0008472846880644461 4126 0.0017977175709951148 0.0014453580973917332 8.2342541173975e-05 4124 0.001079087733594811 -0.0003108309676175076 0.0004689206736513173 2650 -0.0014599012370789832 0.002472771742496013 -0.0011208159781060311 4115 -0.0017287693416901764 -0.0019326989313296226 -0.0007878219006510168 4117 -0.000772789801506777 -0.0001829550610124586 0.0006400350485564015 4121 0.0009093624263799892 0.0010932937073639822 0.0008971975899503158 4128 0.0003770232199572362 -0.001114749105317656 4.9758173886723604e-05 2706 -0.0008398650012629053 -6.0019891871116154e-05 -0.001422247460827203 514 0.0018541413417379757 0.0003167364542083998 -0.0013499697511766221 4173 -0.0020168639819461457 -0.0017302658276463917 0.001042619604918259 4182 0.0019944989695710943 0.00010691399319524364 -0.0010645739518280422 4175 -0.0011115757211925482 0.0006062805417074735 0.000878258571040216 1990 -0.0019909252115908735 -9.732701666767031e-05 -0.0002111924496582653 2708 -0.000696080251426289 -0.0010950334546200207 0.0011925610373210885 4184 -0.0004435052309006973 -0.0007893582898459398 -0.0011576841870037018 1981 -0.0006324626746314179 -7.132630599644902e-05 -0.00034990002215510197 4147 0.001591927685587379 -0.0018451399211653896 -0.001394205748449132 4158 -0.00062688920750596 -0.0007772605430389266 -0.0007478526224007995 4156 -0.0014810112196906413 0.00012055960253736474 0.00013151957292000454 4149 -0.0024664651314070295 -0.0017990846857647582 -0.001834896835372357 2679 -0.0022520607481446354 -0.0013406374493320653 0.0017794403927974933 1963 -0.0009410850643782522 0.0007341156736177853 0.00165185234076822 2681 -0.0003458976574336613 0.0006036813278618915 -0.0016741311589798325 4155 -0.00065806933757496 -0.0015501984330460058 0.0013770514374049126 4146 -0.0019808434349468306 -0.0009629534746539825 -0.0008404181415142139 4157 0.001431505726483392 -0.0009670276121601228 -0.001075689427771955 1954 0.0005280490269612191 0.00017755971022414126 -0.001052399780600199 4148 0.0016727989997541493 0.0007191058560598775 9.71864397827138e-05 487 0.001755126592040397 0.0004680434664722842 -0.00014853952006769385 4122 5.9811014657107885e-05 0.0004926274754770625 -0.0001050604077259876 4129 0.0009773818663933427 -0.0017844815059226073 -0.00024135630077198162 4131 0.0007992477325845591 0.0008837049969537113 0.0005025827073057612 4120 -0.0020023333089543463 0.0016317943737177035 -4.462032034083306e-05 460 0.0004518415890680978 0.00022332773597531688 -0.0019836930824837186 2654 0.0003187311404086288 0.0019719898242222316 -0.00019819900541081018 1936 -0.0006655298575157378 0.00034686079923715443 -0.00026161600292584435 2652 0.0012153791449221838 0.0005990521356229744 0.0009485308546236814 4130 -7.822299131359347e-05 0.0003296423773967384 -0.0012837098333800766 1927 0.0011789577971410355 0.0012834841112027203 0.000246658438579623 4119 -0.000455629251744843 -0.00041275526428117843 0.0007903487750270043 4241 0.0010601729830826273 0.0016921946621314275 0.002438216327996756 4243 3.274818551312784e-05 7.667690631443574e-06 -0.0010724630401551867 3530 0.0019694883104005912 -0.0010491779921729995 -0.0004316410145356461 3532 -0.0024720813867692643 0.0021352006508315864 0.0015704369051794528 3504 0.001131998505189462 7.005226532443975e-05 0.0006255002827412733 4217 -0.0006760850464261536 -0.0017992534878563753 -0.002159443986458465 3506 0.0023415806652289034 -0.0017257967015911837 0.00021862648582789677 4215 0.0005901849396404805 0.0022640931046289383 0.0010830820494787416 4214 0.0018638286896041781 -0.002017913596564504 3.0308244023830597e-05 3505 0.0016576591848845188 -0.000602645676619576 -0.001695700554488008 3503 0.0005666955049326178 -0.002062384357612672 -0.0004953966210857627 4216 0.0017690287796238023 0.0004296133843221207 0.00037334398934577777 4188 -0.0004932714678340753 0.001682668064162448 -0.0004133911801843359 3477 -0.0013993661874965276 0.0003500617872485795 -0.002392298112416065 3479 0.00015004573536997337 0.0005258954159784593 0.00016642467217168212 4190 3.645675054280177e-05 0.001617625160873823 -0.0007666260812988442 4187 -0.0008347068038253543 -0.0004343195584560147 0.0009927532369480433 4189 0.001392978470616342 -0.0008785434207724942 0.0006390355484566647 3478 0.0006144084358880829 0.00013754588910508533 -0.0005593774825322826 3476 -0.00219212211036003 -7.714603167515918e-05 0.0017794166926683392 4161 0.0018319852952359108 -0.0001538780800765438 0.00039280855247691483 3452 0.0024626001289388085 0.0003438468950067576 0.00018667317770670096 4163 -0.0010585779011438765 0.001524951938952167 0.00027541611415818194 3450 -0.0017466505078814558 0.00114786312831589 0.0007156802165486678 4247 0.0009150468294530471 -0.0002615986465434369 0.0018672058445483347 3536 -9.746503842878894e-05 0.0013642884205819711 0.002309531299189965 3534 0.00037877539452355427 0.00168174410025477 0.0003166543679134885 1342 0.0009947534529861015 -0.0003166963218846973 0.0007506425607983964 4245 0.000911817144975367 0.0013276781126332813 -0.0006429288624812844 2053 -0.0007975905098739429 0.0007761481321944604 0.0027898852646713224 3508 0.00022008392110849746 0.0023795342263924595 0.0015964954495237965 4219 -1.1685445550073663e-05 0.0007373907239353998 0.0008093561287486678 4221 -0.00036570353460320957 0.0001046035420240606 0.0007126750934722859 3510 0.002288880332109964 -1.7427254897977706e-05 -0.0018810128437809197 4218 -0.001181574143812411 -0.0012459524200242507 -0.001278846126310677 3507 0.0017797750122525364 0.0006359567454162864 -9.40631058494951e-05 3509 0.0012018960892976787 -0.000925494440267534 -0.00027889273251861086 4220 -0.0008753847029577824 -0.000982478379320904 -0.0009790027226270277 1315 0.0005780693479030222 0.0003964583088451024 -0.0020312617790002587 2026 -0.0005796881319352017 -0.0008523395995156488 -0.00020812626241493667 3481 -0.0016034436559302328 0.00020380377111556193 -0.00011441626988294867 4192 -0.0015529519132157943 0.000508489739765104 0.0015878621547930388 4194 -0.0008661242794792152 0.00032855155705735647 -0.0026392003043594256 3483 -0.0001871764044990594 0.001363454213364681 -0.0008165200913374778 3482 9.481922000107454e-05 -0.00156183165563629 -0.00048159025281550405 4191 0.0021053510393290887 0.0008765339736501647 -0.00035511287960002485 3480 -0.0007070517351510052 -7.073487256756446e-05 0.0007810323596615673 4193 -0.0011189626338985574 0.0005221918109745546 0.0012406422145532618 1999 0.0021090137012407945 -0.0009795095639352769 -0.000854234462400166 1288 -0.0012699729669157123 0.0019256107687918628 0.0019184020332125827 4167 0.001681908817069569 -0.001225278939307915 0.0003473274625415256 4165 0.0006202375974131554 -0.00016805889219311605 0.0020905480297717894 3456 -0.0005483924580265787 0.0001248265252498616 -0.0004275075833174266 3454 -0.0005598068134476254 8.908818074260033e-05 0.0006668242742809536 2783 0.000556059748761824 0.0005931224715463937 -0.0007535032740772923 4252 -0.00023652812323079878 0.0018260389736759377 -0.0021319662435539924 4259 0.0003616822514692459 0.0013796043930374116 -0.0016072767722766859 4261 0.0007504123478454109 0.0007337702128558188 -0.0017767098743708596 2785 0.0007307665341918092 -0.0003535547685571208 0.00011147471176678556 4224 -0.002419557639297957 -0.0017975106964352961 -0.0005794309822300345 4233 0.0007117991318556108 0.00022387595842530365 0.00043773404378633107 4235 -0.0016214442348847164 0.0009165255836508108 0.0007340986954898483 4226 -0.0008543349329691452 0.00016959699992981911 -0.00010319739391867564 2756 -0.0015237245835890974 0.0017611675741463315 -9.595515424536821e-05 2758 -0.00012921990518455 0.0006139286158032711 -0.0024963388415412003 4232 -0.001972204470452076 -0.0006724541592145999 0.0008339313260391296 4234 -0.001732298791308168 -0.0004977954178906612 0.00023488867978119536 4223 0.00039385838088703195 0.002089798632325435 0.0008581606146376415 4225 0.00044310388370222666 0.0014540539567806973 0.0016144043185939033 4206 -0.0004916463283245621 -0.00037594595149252554 -0.001153456417140834 4197 -0.0017138082739348855 0.0018175939278916712 0.00023679573332877125 4199 0.0018859044388463554 0.0007270163978283424 4.9319421681539655e-05 4208 0.0024332349670740656 0.001177189860020732 8.702839056343018e-05 2731 -0.001776108627943199 0.0012635698294768969 -0.0023963386043216873 4198 -0.00020355406318158398 -0.00047415534420539073 -0.00045734434751133594 4196 0.0020311812576200667 0.0007519497804963364 -0.0006983636355102996 2729 0.0021252509924827795 -0.0014524861307132215 0.0009639190965462995 4207 0.0014396216110881064 -0.00034184769196010916 0.0002980153102383929 4205 -0.001309321028045165 -0.000737136572625182 0.0006939811836803073 4181 -0.0010159187784830866 -0.0013104673121584717 -3.7098273617317446e-05 4172 0.0025499839776966606 1.787573760173456e-05 0.0005095309472502274 4170 0.0008938727176156867 -0.0004081741394045815 0.0012928014088134465 4250 -0.0007886700822775491 -1.9199612392798923e-05 0.0003081412928274002 4179 -0.0007220655894100093 0.0006286988176833577 0.0005898052585426566 2062 -0.0011847443669885998 -0.0013592806800675516 -0.00026498502701668134 4263 -0.00029549246869675205 -0.0003563713557266303 -2.0443124599006006e-05 4254 0.0006878768190758066 -0.0012816903527655022 -0.00010358500887266628 2789 -0.0016278839873149142 -0.0006825887892971878 -0.0012498331409478585 595 -0.00015509047886992525 0.0009448354789961745 -0.0016542130890038682 4256 0.0022013687248742656 -0.0019411367578856629 -0.0008042203199590484 4265 -0.0018131447527869765 0.0007837777128083788 -0.0017586984326157856 2787 0.0015290643933986792 -0.0015726453953451938 -0.0016356559661907574 4239 -0.0011460225734032236 0.0012404763228950763 -0.0012171288806209755 4237 0.000844779574965059 0.0006353740567132917 -0.0003371299111626883 4230 0.00021461782454294722 -5.0021213566102006e-05 0.0007320817549977747 4228 -0.000851639946229221 0.0005310908475877122 -0.00032117787452434895 4227 0.0004977502333212544 0.00020659332176125404 0.00027467964108465184 2044 -0.0008308392598098433 -0.0014875203583392164 -0.0015394206742152365 2035 -0.0016946755281006453 0.00020192860497712448 0.0017869874564492212 4238 -0.0015757264162905439 7.472283098534189e-05 0.0011589409928603443 568 -0.0013410011162462913 -0.0007122884436179674 0.0019180388522060247 4229 -6.997691426887851e-05 -0.002187126007844042 0.00018662251962518357 2762 -0.0012625841644445474 0.0010016891636431382 -0.001296925551167794 4236 -0.0008327811257738869 -0.001681257552805336 -0.0007156051845637571 2760 -0.0008838493030949293 0.0014450052506623228 0.0009397008600099302 4203 -0.0010634050876182602 -2.8365349033732286e-05 -0.0008130103675405395 4212 -0.00023691939074579514 0.00022570439151739638 0.0006445812318819752 4201 -0.00041809226605471527 -0.0007631416336900223 0.00037312097682256316 4210 2.3034264953939333e-05 0.00036542082629550596 -0.0006687058588186055 2733 -0.001073075515744903 -2.3570311298096383e-05 -0.0007904308651728695 2017 0.00012133258906978626 -0.0003549458469180786 -0.0012260359713700951 4211 -0.00036471286950921517 0.002583609228008015 -0.00046755019705740377 541 0.002529467213815253 0.0012724151035106081 -0.0009206502635433642 4200 0.0007592415692634258 -0.0013952324892596464 0.002085891240415901 4202 0.00026744965375412083 -0.0012345629348596103 0.0011343958075243435 4209 0.0014871386728507957 -0.0021472119587897724 -0.0005625496754740244 2735 0.0011013438038553205 -0.001915010956162067 -0.001538774461529751 2008 -0.0012549934166134486 -0.0020808580049095065 0.00010081741035963376 4174 0.001183915698494399 -0.0007312244733678587 0.0016046287964355862 4176 -6.749028666635766e-05 0.0007802154713054414 -0.0004277765679046441 4183 0.0020143724954637845 -0.0010449956084934051 0.000538508698064619 2071 -0.0003786459691752183 0.0010521576178633332 0.00021264985020205896 4185 0.0003313739024941539 0.0016803938208425394 0.0013791207633905892 4307 0.0014442368775854646 -6.245738325827768e-06 0.001604003864869199 3589 0.0025490726714707565 -0.0007338584960041247 0.0006944505680477572 4308 -0.0001556616000000442 0.0002968847509120134 0.00040710853160597386 4294 0.0016695281670057946 -0.00012113653805105465 0.0007000333580241306 3573 0.0022230797786201356 0.0006300948159668829 0.001466621367627282 3574 -6.450990623791623e-05 0.001266197695797427 -0.0012626294025123155 4295 0.0002017385720022324 0.0008518909358194195 0.00046157565589423734 4269 0.001767312527859896 0.0005877239684287876 0.000587156761501407 4271 -0.0004974076127768874 -0.0010721669888042631 -0.0013465756313395425 3560 0.0004730486656109962 0.0019919889522298883 0.00038410335262131713 3558 0.0025758283282985794 -0.0009937253525027358 -0.0002473025919160983 4268 -0.0009919645613889138 -0.001383607942390377 -0.000813184368685484 3559 0.0014519262440190982 0.0020242344242865236 -0.00043108588772589333 4270 0.0011237971316001398 0.00021160116454062218 -0.0006346709928751499 3557 0.00017517201741851013 -0.00021414917561858073 -0.00030978473572953547 4242 -5.1887408779555236e-05 -0.0009636803810200026 0.001218923626810129 3533 5.6796154278346625e-05 0.00034101310823481936 0.002294702317321611 3531 0.001653055929714044 0.0003431660720700019 0.0008966804833846647 4244 0.0011772935652585863 -0.0011867564523549037 -0.0003368882196800871 3588 -0.00025192169711266144 0.0010544188747786086 0.000387707373786748 3591 0.00041561929942467174 -0.0005729413909813632 -0.0018226016109760958 3590 -0.0017001099816293442 0.0016946863919595737 -0.00039385881152054865 4309 0.0006311765411641108 -0.00040168388041087686 -0.0004889849788212921 4310 0.0005003955600725947 -0.0021637712702565854 0.001474180382577713 3575 -0.0008316844637335638 2.057625648692763e-06 -3.65824710806921e-05 2107 0.00048593981623157464 -0.00044502177904946077 -0.0009230972349256951 1388 -0.001097629086813893 -6.528335845857247e-05 -0.00044197472269305637 4296 -0.00027047455084415516 0.00032134778243968535 -0.00108926139602702 4297 0.0017070025810404005 0.0010901898568055164 0.0010238368913664565 3576 -0.0004654311080670927 0.0011121724279071399 -0.00012307166304011108 4273 -0.0017793097415298924 -0.0014029225781619478 0.0005044439400082829 3562 -0.0005474558831368838 0.00016613913000751305 -0.0003010645706219466 3564 -0.0010438129364025608 -0.0017549319061514624 0.0016044298533206033 4275 0.001869045430195817 0.0007485440153388717 0.000172822366757393 4272 0.0003039930169664247 -0.0010059801365821445 0.0013093774287041423 4274 -0.0022602715359953795 0.0008463759274078598 -0.0010347687784791801 1369 -0.001143995551065034 -0.001767676275884699 -0.00030568963938764466 2080 0.00037461198269385723 0.0005815042523235302 -0.0008852085112263076 3561 0.001841008952678895 -0.0002718379215127923 -0.0014787993053264241 3563 0.0009608951424599909 -0.0002691781781945146 -0.0018285738966325785 3535 -0.0004724695765152443 -0.0006126111097701515 -3.152181535398275e-05 4246 -0.0016960134094955415 -0.0005804942061833733 0.0016921124725809453 4248 0.0008292375810101902 -0.0008432913562054919 0.0014176740626784324 3537 -7.528731906392963e-05 -0.00038532547823362105 -0.0014814736644085307 4313 0.0014027107972617758 -0.001222488554440855 -0.0002710168826007386 4317 -0.0002860721089969536 -0.0004947896921993646 -0.0010427182095120269 4318 -0.0015069498319137083 0.0017820926521922536 7.930465126881068e-05 4312 -0.00017131830510710077 0.00039900232227035957 0.0007721847400879395 4302 0.0018376179239854517 0.00023902548623264087 -0.0011316326565741933 2836 0.0007392293893740338 0.0020752936953759905 0.0017136398345799797 4298 -0.00044429852756534523 0.0007594958301951117 -0.00020054659588500216 4303 -0.0011055078478765235 0.0018058719211071082 -0.000568320907535218 4299 0.00026051702279647503 -0.0012783551119776293 0.0009802031726180525 2837 0.00035973650876940707 -0.0008288903231142444 2.2958886360419312e-05 4280 -0.0009541085487295578 0.0002754237690540723 -7.904355350519436e-05 4278 -0.00032539277878433246 0.0003021897388777937 -0.0008614402674341694 4289 -0.00036866154424400766 0.00018021467405438126 0.00135046117622387 4287 0.0015412524102867823 -0.0015151206607361988 -0.0009784178066537296 4277 0.0014165471536381874 0.0004495116302281429 -0.0019894427525486494 4279 -0.0009761972889894871 -0.0021982208212519496 -0.00045707559827157154 2810 -0.0011177428650374383 5.7339828492736005e-05 0.00237831077334584 2812 0.0014410512786490078 -0.0016346033167851182 0.0008056963177734877 4286 0.0001603654126782609 -0.0019391924848937894 0.0005518322480747939 4288 -0.0013548757981436492 -0.0011833115982739558 -8.853568037368365e-05 4251 -5.991634020822982e-05 0.000119543024967388 -0.0018055321364395382 4262 -0.0005163147777068713 0.0012050850090653575 8.231359567550359e-05 4253 -0.0005020194760732317 -0.001146250230042009 0.0012243481802892272 4260 8.499651172403028e-06 0.0013360152577271602 2.1477217848658598e-05 4292 0.000616357900653036 0.0004330482965671233 -0.0008929655340066632 2089 0.0007069651479417057 -0.000618371803456674 -0.0011296059500967928 622 -0.0009766173306206987 -0.00019666824375077357 0.0012948393456107868 2814 0.0006492681416259388 -0.0012666351800755763 0.0006128731361260565 2098 -0.0002234693899138833 0.0012100316419143109 0.0011225183462595183 4266 -0.0006711780380285025 -0.0006697464380622158 0.0006738290686855648 4264 0.0018169709356158277 0.0005273473211270677 -0.0024637274938799237 4257 -0.000554552650259004 0.0005057052466024825 0.0018006212786721878 4255 -0.0009045740026933451 -1.0875614980161447e-05 0.001154166476596548 4314 -0.0003868112124630859 -5.768440705432288e-05 -6.939806318345871e-05 4319 0.00038982447905354964 -0.001621145204474148 -0.0002067049285629219 4315 0.00021447586645499585 -0.00015098155086199242 -0.0013480254865365947 4320 -9.5219711830435e-05 -0.0006911178218209535 -0.002103270155750759 4300 0.0019301246902852863 -0.0002043424131981126 -0.000520701047492194 4301 0.002342018263672944 -0.001027189200426091 -0.001957515316574754 4304 0.0005153303730223858 -0.0020125837004171918 0.0007804496395630526 4305 1.6255677955288005e-05 0.0003311590960583088 0.0002329686130547611 2839 -0.0017677419461439344 -0.0013316990400351455 0.0003062102611170875 649 -0.0011145061673922697 -0.0005637321432007511 -0.0009190084038261776 2117 -0.0016046851831776794 -0.00015060431785031045 0.0018647365213871792 2838 -0.0007604904658689818 0.001992708880767136 -0.0005740563029771569 2112 -7.69276417684232e-05 -0.0010453072839039749 4.3727827839206226e-05 4291 -0.00022930452378599182 -0.0005297406952724402 -0.0005279148932254969 4282 0.0011914376897023942 -0.00027921642790597724 -0.0003027318586659284 4284 -5.846376264681584e-05 0.0012037149308318487 -0.00040638545431669385 4293 0.0016264529484433868 0.0010005225396428835 0.0015077308460356717 2816 0.0011399066781044049 -0.00015618229924455182 0.0005270103393571549 4283 -0.0021864968044739566 0.0009348956334386741 0.0008765653233808739 4281 0.0009996820735811878 0.00046645118657481386 -0.001306157193467211 4290 -0.0020568129024764524 -0.0016428240991774228 0.00019594274932252433 5388 0.0036156297861416912 -0.00434124265491062 0.00019800483319891166 4871 -0.0016742817745364466 -1.9652958802436664e-05 -0.004181638655330349 4569 0.0008374322253910226 -6.866511312574232e-05 0.0029897645166754123 5120 0.006963021659487718 0.001435518375377477 0.0016329560939089415 4477 0.003042924145060499 0.0022969315494523438 -0.006218433990710153 4924 0.007275527009239949 -0.010604908445856615 0.0023057470976847756 5155 -0.004053928957529615 -0.0033747753412663242 -0.0038826513127018154 4323 -0.0003939539224953651 -0.0012750178134390724 -2.179899510594465e-05 4325 0.00046637781837508734 0.0003266785833655483 -0.0004995670897992832 3612 -0.0012405756807789465 -0.0013180361150400303 -0.0007798198767471421 3614 -0.0002997921892335467 0.0006028971078935588 -0.00232862810525451 4722 -0.0038120813868923586 -0.004223472868791655 -0.0056919961465015856 4487 0.0009767358393113032 -0.0053981639913463185 0.009434303073312616 4863 -0.0017438959699816556 0.005349948924091254 0.001164204265296045 4441 -0.008273414558263572 -0.0006795634191957689 0.004893508553733468 4380 -9.118147613266978e-05 -0.0038227466743806704 0.005169062361127087 4322 -0.0024172010116713734 -0.0002852613739759873 0.0004600984268659518 3613 0.0023776350361070955 -0.0009349623673197362 0.0018764493822195612 4324 -0.0007503247614457599 0.001597455954535226 0.0018923070529761874 3611 -0.00034956866012952025 -0.0010122984632205537 -0.001888835182298383 4963 0.004765855731003656 -0.003055179935705221 0.0025921414284146346 4422 0.0011637425202373364 0.0007961845851551337 0.00664749468167568 4588 -0.003072365629199555 -0.0069251121858644755 0.0068193567611751415 4844 0.0032143345420490416 0.0009139522550595409 0.00487944075732803 4565 -0.0016835387304077031 -0.0024529733736668637 0.0029959493787582855 4734 -0.004260872454486022 -0.005382463645724322 -0.009681149691246036 4653 -0.0019453766908781318 0.0008492500966863565 0.005806276963915917 5171 0.000878268478389622 0.008372123600100395 -0.0029291126554022388 5167 -0.003319637779540601 -0.0028362704253498804 0.004098773775472144 4688 -0.0023112908539205798 0.0017547340192774936 -0.0018055558516122052 4349 0.0014900382930131068 0.0011026161691567648 -0.0006680848398156361 4358 9.70868857490181e-05 0.000336481320889043 0.0010117405592390042 4736 -0.003513299665491223 -0.007704163756533798 -0.004357935301296263 4786 0.0010648533988830602 -0.0032062170193175453 -0.0001744823730640836 4362 7.439377777291358e-05 -7.393203164596631e-05 -0.0002510761011526039 3644 0.0005176939942784409 -0.0015331109338017554 0.0009651319033118341 4508 0.00947002695048651 -0.0027168410805877433 -0.008670973560364724 4478 -0.002845406443961852 -0.0016871151455402523 0.003717003187032641 4355 0.0016268683118500972 -0.00039908230061633503 -0.0013069386366709 4752 0.003411161801832109 0.005217037666769349 -0.004273555920437835 5224 0.001293643582755603 -0.004913804926393577 0.011304715872636904 4780 0.006735876620511652 0.0006009714646883827 -0.003944626679264985 4413 -0.0025459494021547176 -0.0007646471793792412 -0.0005626747151055785 3607 -0.0014055937675163917 -0.002176403525066492 0.0001487234146796761 4945 -0.00903221760353188 -0.007451450634770143 0.0023183183448407534 4592 0.0023129875521110815 -0.002657467919466921 -0.007960226632165727 4679 0.0011009748097645566 0.004997347433596053 -0.0008929040927579987 3616 -0.0009518363329581649 -0.0008811407810642646 -0.002004078203905268 4463 0.0054566296785059564 -0.0022892736105939587 0.00568780495083326 4526 -0.0003678292035887447 -0.0032404173513443818 0.015220344070965714 4486 -0.00048098814405453784 0.004144870952778846 0.002744757037063097 4329 -0.0009391815598765292 -0.00012641504252730465 -0.0010091577285611683 4582 0.0062145494912969 0.0017872142517065558 -0.008813087120218796 3618 0.001425974007610994 -0.0020667254943609933 -6.370091124952102e-07 4449 0.00015502331126818135 0.0012123370766683116 0.0069948062693008526 3617 -0.00021292615754939915 -0.00015850824011791006 1.9342601802123914e-05 4326 -0.00019831307247864883 -0.0009041061071035376 0.00046922124677276154 3615 -0.0011556245658358335 -0.001583769284681368 -0.0014555627931108427 1423 0.0016502280651273014 -0.00035198288829845154 0.0013531765312758592 2134 0.0009483688434408636 0.0004883808998330575 0.0003306876791955639 4328 -0.0013800935937858657 0.0019105757178014156 -0.0024516549989784947 3609 0.0008461321595306923 0.0022178915883032777 0.00033357786972062825 5145 0.008156286807296801 0.0018249718867857216 -0.005157185531344832 2161 -0.002099488359526765 0.0015633847753162315 -0.0003272649294875972 4909 -0.004045663003736826 0.005391609716187094 0.001907829137078751 2893 -0.0017629932420924407 0.0003543601818526295 0.00224604783891828 4369 0.0013618170381355765 -0.0012380292939459115 0.0019466525340603223 4437 -0.001954650110837397 9.423613369469321e-05 -0.00558147332065401 4500 -0.006676927690687244 0.00011098131019873169 0.006068066661874915 4573 -0.0036400942435177845 0.0039035523089365255 0.005509489544306837 4626 0.0024172027003907534 0.0025094562639815603 0.0027753039360542387 4545 0.000840640418672988 0.007459133952854675 0.003913701015091403 4587 -0.003483877539238241 -0.00068300768927171 0.007734818149802215 4341 6.702653235067199e-05 0.0012166680579772178 -0.000361835200338242 4528 0.0036573184065271922 0.006291038458411425 0.00464841795273821 4332 0.0015151791456784057 -0.00027544885906250513 -0.0015695966281429588 4343 -0.0007861490968216589 -0.0003702699784915778 0.00045565473906091425 4334 0.0010417537508727905 0.00038024354286379054 -0.0014967654554735197 4427 -0.0067608135030885665 -0.0059545580531911325 -0.0017838285413731415 4899 -0.00439524212943274 -0.008913276430586172 -0.004692440426171404 2866 -0.0012622708379253966 -4.942330556938408e-05 0.0006398842598888981 4333 -0.0016928989726851358 0.0006227684160388938 -0.0004817977297489267 4331 -0.0005905031575452093 -0.000822170949560516 0.0003209275267972325 4340 0.0014213837997354897 0.001934452022859409 -0.0018518325396349147 4342 0.0006285028166551703 -8.995879406975115e-06 -0.0002885694753211476 4980 0.002346716333421166 -0.0006182410622574978 -0.0026428695797495456 5327 0.009036534784061077 -0.0024975474921446967 0.01126848614668884 2864 0.0007243927423693549 0.0012553879981985375 -0.0014980807231802758 4676 -0.0014806179477172751 0.0027197041856743677 0.005399012815822769 4813 0.0013833001002119096 0.003332374590383737 0.0029744732246975636 4425 0.0031312621724750313 0.0039688602334541 0.00019860449919832223 2895 -0.00042031578089036636 -0.0017777646468293642 0.00013114227276445452 4596 -0.00033018182001406937 1.8206958463630343e-05 0.00445398285493843 703 -0.00114702374300944 -0.002406957913376381 0.0014583688057045491 4645 0.00017576427313846683 0.00536351030316613 0.002054907622467022 4591 0.002209353542784859 -0.005843166046748877 -0.002222373420633036 4405 0.004216622235921963 0.0022850766426238266 -0.005845655197268035 4373 0.0023885164686440904 -0.0012518694445563467 0.002218657190518946 2897 0.00019783163464809188 3.184315723949848e-05 -0.0014209272734760968 2179 -0.0010838189751245545 -0.00014321826992181154 0.0019149404338660197 5320 0.0070563226444250865 -0.001776590247629484 -0.0006252498028962703 4371 -0.0009014256816384632 -0.0005293293782169506 0.0014719380525079588 4327 -0.0021524534200204042 0.0013981023259237477 0.0003853639465452585 4880 -0.007992862398657338 -0.001143668424772888 0.000330629884969255 4514 -0.0036096531463082585 0.007072240431474356 -0.003609679771714524 4409 -0.006904247311857874 0.011279574810956709 -0.002604924312615231 4506 -0.002543572376097326 0.0020811910106740437 0.0029734014942970977 4622 0.0001992594103024388 0.0008041407355077082 0.005965583929825907 4336 -5.474057101276567e-05 0.0005408783068859995 9.00120136790492e-05 4345 0.00043933786459208796 -0.0004072048924823532 0.0023948194891005928 4338 -0.0005492821911355216 -0.001813482683335791 0.0013209555569143184 4347 -0.0011376053319997353 -0.0007877620221639998 -0.0003230324039532441 4335 0.00033802947276520643 0.0011728161451323832 0.0010939232022073404 4344 -0.0013186476421664605 -0.0007618921522920526 0.001073391563633783 4337 1.0516573813176356e-06 0.00024257078660708085 0.0016705246961866132 2868 0.0018082705383270065 -9.131164657498144e-06 0.0009655188359840767 2870 0.0005558515874932673 -0.0005211972771918282 0.000936783556956159 676 -0.0003981091580565983 -0.0016784773382122137 -0.0013634710378427127 2152 0.0019325696641173866 -0.0009298546902629392 0.0003212741680952457 2143 -0.0009587689538485265 0.0016409735951426476 0.000432501972257288 4346 0.00048315707637700575 0.0015335143447141725 -0.00045658467136976393 4629 -0.006567474418665077 8.348331289829454e-06 0.006419961219960442 4348 0.00019989741491438398 -0.0004249898862115878 -0.0013455683706584183 5470 0.005820078048862129 -0.001583017501844391 -0.006638060874799401 4352 -0.00028929221759874536 0.0013095119411696454 0.0010306417725450931 5242 -0.007406793098142835 -0.006989825877456485 -0.009389793281524433 5081 -0.006279320154075358 0.0048951366217670255 6.158834684651419e-05 5179 0.008336800288461507 0.010886317527814104 -0.0016711770606116286 4691 -0.003124591326577805 0.0005583081437312507 0.0034267163791371503 4696 0.002438861455702329 0.0050535839163742486 0.00473652487645244 1458 -8.407772670450571e-05 -4.105355442564351e-05 0.0009443151705636455 4359 0.0016638380968229962 -0.0001360606677000281 -0.0012182417554758278 4351 0.001069547373307422 0.001248680922187589 0.00022768919802336896 5301 -0.00970548145398091 0.0055452412143713594 0.0002596308421367351 5184 -0.006624712825453184 0.0004169524942020764 0.0030025853795525247 4530 0.000271154369238125 0.003155945106004835 -0.003974504382735383 5019 -0.001971995235799412 -0.00010644820275193499 -0.0038007658955005546 5108 0.007996055226161668 -0.005468325401535076 -0.005927791438299352 4607 0.0030007445747321742 -0.006615498090333201 0.0021761773648307503 5312 0.00482547033003785 -0.0004037544694578855 -0.006351605268172168 4360 0.00042525861455068863 -0.00023417092612626445 -0.002083414409751731 3640 -0.0007297891594545569 0.0002002498938696386 5.128923656948941e-05 5364 -0.0025162302588211502 -0.0010424635697142812 -0.002541931468465798 5428 -0.0001208958904300858 -0.0016359512434790157 -0.001152343341265813 5512 -0.004252224527170162 -0.0004557885847033211 -0.0005697097849755805 5509 -0.0018193105370155585 0.0024850081827183543 0.008922806599506788 4419 -0.0004410739845750536 -0.0013297886250677785 3.102336315760558e-06 5185 -0.0038370134917527316 0.0028213694928031995 -0.004961503605589581 4983 0.008768760605318584 0.003245764024363278 -0.0037165343894504186 5455 -0.007608430328708779 -0.0031644719305060926 -0.0037900596873824658 3642 -0.0013016119827773769 0.0001349685049247438 0.0018112065695125516 5335 -0.005506104984006167 0.003492308134706522 0.007215591544681789 5495 0.0022138595936107993 -0.0042562054432455 0.00669064511079561 4650 0.0016142451444338122 0.008970111370401188 0.005703771481655541 5041 -0.010435570321591673 -0.010777974895737463 0.006593561155215357 4712 0.00627745021839501 -0.0007246178034069838 0.0003635549154546038 1468 -5.0175881915990716e-05 -0.00031729397602305465 -0.0020283928349623063 5075 -0.008242519361145166 -0.0075428321006997005 -0.0008885535126647667 5058 -0.0006730389872108849 -0.006654267065975112 0.0060511787724795655 3634 0.0004357644285438848 -0.0014781381828265073 -6.3245552140001e-05 5049 -0.00017296805019272597 -0.001715409260386807 0.003645726278616777 5243 -0.003930888313572979 -0.001813888080940322 -0.0008697530220927186 4353 0.0013956705014857686 -0.00023227116656270876 -0.0017987230889344916 4936 -0.00776350362335371 -0.005730262904622355 0.0034305044545275424 5175 0.00030719562074237446 0.006203718468557554 -0.003453842086897532 4772 0.0007593827273060811 -0.008485827488520904 0.007978099516326375 4809 -0.0017133488330598635 -0.005314169887893193 0.004877301032718317 4356 -0.0002127608680618089 0.0010181799230399005 -0.00020484015662165138 5042 -0.005994594390012583 -0.0013854565244359332 -0.006192117268138971 4767 0.010530435887741423 0.007432428471722414 -0.0030028580729523067 4507 0.004525240125797943 -0.0020276826659420656 0.0058264661250065335 4665 -0.007089534129255148 0.0031594201534698675 -0.007691686687035599 4675 0.0009276214880623427 -0.0010252474107772325 0.003508696183706507 4621 0.0028210547112347086 -0.0014802374433305248 0.0039394601612896185 3633 0.001298739203876172 0.0005317668860191242 -0.0005731191511916471 5044 0.0014272994178493692 -0.0018479831648839855 -0.002071963722460108 750 0.0016655060368857787 4.69622056342709e-05 0.0007473323977169271 5336 0.006053336949953842 0.0039799239658700435 -0.0016890851891985202 4920 0.0019206427413651144 -0.001759567104281292 0.0002447520862245584 5290 -0.0026847653068796406 0.0029739139519070774 -0.005312279998804003 5188 0.006002535308651335 -0.00806492096086921 -0.007021575378387081 4873 0.002276682978055095 0.0015174180507066966 0.010277127453100728 4782 0.004447377627580349 -0.0040960176728287905 -0.005344741331632121 4952 -0.004343053332104134 -0.006079554195778141 0.00343574049445946 4996 0.0006756070973272534 0.0007627448103343012 0.0017177028642215825 5497 0.011073194420298797 0.021203225041964358 0.01250408455067252 1485 0.0006292412892619508 0.0006075421277937272 0.0004675219080248577 5305 0.002045333309384442 -0.006414962966128415 -0.002782436203760846 4410 -0.003693150746698119 0.0018426555233070118 0.0030303108849100853 5235 0.0002637758930111485 0.005994881209462526 -0.0006920924430615298 3667 -0.0017808706931921375 0.0015382399665851937 -0.0003534757261731158 4368 0.00022387506226264568 0.0010638779689905254 -0.002008570962235704 5247 -0.0029603795158726545 0.008626874314754554 0.0015926160299194869 4788 -0.0038401765809316897 0.004980285029188315 0.00499963912276068 4361 -0.0013136929593452825 8.465647402646327e-05 -0.0019743717616147257 5089 -0.0009412814554432573 -0.003524586965565955 0.012313837967542903 4367 0.000653423162368195 0.0011175153146737616 -0.000357373163831868 5087 -0.007694339941990377 0.0027290410406681544 0.003751890675078039 4370 0.00041419402556330375 2.3139531478576572e-05 0.0020004543801595887 4550 -0.0038402526165118795 -3.8937794435708634e-05 -0.0025517747544998564 4806 -0.005755518599845106 0.0041447065762464635 0.0018581667406660741 5165 0.003648637469438588 0.0026822881969738453 -0.0034922520523182708 4631 -0.002974885650003171 -0.010664261200521347 0.0037056878613083285 4411 0.005578180500773225 -0.001211191092058537 -0.0008076546286388136 4830 -0.006041211597112787 -0.003923801129318923 -0.0031055983870597933 3671 -0.0010164909966105036 0.000745330393682072 -0.0014665982815206305 4802 -0.005079190018048532 -0.0004572783189947108 -0.0035643921257521188 4559 0.0015321486019714051 0.009912580400599731 -0.005695501923589299 4543 -0.006011576483317406 -0.016048710083284224 0.0068802296938140954 3662 -0.0007196574086152439 -0.0021670936708332463 -0.0017446502500430105 2170 0.002094134444216267 0.001021065191474464 -0.0005412990166953305 4372 0.0011207630336918586 -0.0004877993502033723 0.0009286230915408139 5028 0.0027499730115804876 -0.002691810796005416 0.006401417797676024 4812 -0.0039430436598409885 0.004423248358332508 -0.0009251410907835393 4404 0.0014121385803637766 -0.011290218528978555 -0.0009618243876255988 4363 -0.0017646103063040206 3.161152841638765e-05 2.7256572079875467e-06 4601 -0.007794167232939926 0.002825374160508325 0.0004788957268947664 4633 -0.00497782558302659 -0.003069408948986474 -0.0028112416501270806 4406 -0.0019257915365219528 -0.0034233910138496072 8.997281160370152e-05 4522 0.005910964168993482 0.003097596234785654 -0.0024696057035957343 4412 0.0061046848186219116 0.0037643233644504967 -0.010159135170084776 4505 -0.003657946993497244 0.0006157200682024486 -0.005521785022515998 4377 0.002881022478444892 0.01042819936118293 0.0035995546270790675 5021 0.0024357219809910966 0.005330031387687368 -0.00014521939479580828 4600 -0.006382702090006115 0.001419829998390335 0.001220749339503903 4702 -0.0017908594602698271 0.0061950392231029505 0.004642471009812611 4354 -0.0012518249399730793 0.0003723092294193467 0.0002453859915613754 2195 0.0010402894733817147 0.0005975390808881087 0.00033559981489727575 4808 0.010493789826496895 0.004259506098516973 -0.008352724089327381 5476 0.004543139760293917 0.0004143511872373092 -0.00333106564566476 4364 -0.0020838561437015357 -0.0012201524381783035 0.0008378915815989727 4913 0.0005626634063109275 -0.002222781807305236 0.0097450008410744 4877 0.008469437332591706 -0.003572955289840708 -0.008661046869470152 4957 0.0008846465859530789 -0.0008611703442250824 0.0013472133163439479 4374 -0.0015678587731647532 0.0012636606495923979 -0.0011849691574958299 4365 -0.001017342646298519 -0.0010058485703908385 9.82249590211547e-05 4641 -0.00044803237932344604 0.0030290554134097827 3.6306903747898404e-05 5420 -0.002881116562847543 0.0003146594079574185 0.005881625512906256 4540 0.003320089374540509 -0.00035114909125879103 0.0027450877989133823 4376 -0.004657395951448723 0.002835701733924688 0.010793591773182008 5007 -0.0004658280508269165 -0.004059800306877475 -0.0003835743946641515 5418 -0.001692472243633331 0.0025564788849253934 -0.004361427269292039 5391 0.003958053398212772 0.0031435884615153664 -0.001051853045595765 3649 0.0010244277769678723 -0.00020395520253939782 0.0020368504022507204 5294 -0.003235890780396386 -0.006751090304681071 -0.00695767792302014 3638 0.0018374087195952055 0.0009091119143638249 -0.001255372444110704 5404 0.005460831370182553 0.0053120136760110605 0.005534848804535966 5285 0.0040099442746622605 0.00680206403847591 -0.006976926328827213 5422 0.00341307098705211 0.011186299376427072 0.0030279099703025706 5466 0.010023579491111916 0.006246635953388697 -0.001006461850012488 5241 -0.0027599006615241957 -0.0034735605306137275 0.0028249605445011413 5463 -0.0026914204503347082 0.002767007381052299 -0.0053138373332598235 5375 -0.0008333279536646072 0.004836931812782849 0.003279027024069646 5374 0.0012817653128977871 0.000635535314972582 -0.012302236615468254 4350 0.0018783034567098366 0.0006856890270642972 -0.0009006006623114099 5454 -0.01824554077698814 -0.001623696535514257 -0.0026845692153465365 5141 0.0029259990004015172 -0.0061135080008405986 0.0019509457868298991 5086 -0.0044295995703933074 0.005764140523240263 0.003784363643839634 4962 0.0008666840588545089 -0.008496031947321854 -0.000808858012907942 5360 0.004915069775231659 0.009535467292719885 -0.00034307623666572694 3632 -0.0013580477875887195 0.0006713101854559141 0.0009665457041091833 2931 0.0008822280680799079 1.5911794085223538e-05 0.0005295994491270484 5213 -0.0007051513333826112 0.007423160477438682 -0.0021910076750838625 4718 -0.0008406284770221195 -0.0014669580095589172 -0.004604881690851752 5279 0.007498968300572563 -0.004551633986051595 0.0005782483281362575 4959 -0.005062009856407242 -0.0038141621568594224 -0.007881026224094584 5323 -0.001504964507179479 0.002844784673140444 0.006469993144280003 3636 0.0007972984835985092 -8.553947499691326e-05 -0.0008219605940591586 3651 -0.0003202054412106993 0.0008716345836770183 0.000286863828904113 4960 -0.005691172713079257 -0.0008475811188077519 0.00994142966663552 4466 0.011107614043344097 -0.003643607938175942 0.005015607683386408 3641 -0.0005264777170806392 0.002454863535621209 -0.00021440094721479207 5035 -0.00019065491107913586 -0.005787164536751416 0.0011802194469045309 4783 -0.0029496094095010396 -0.002457666104640643 -0.003564618628647014 3643 0.0017592024712101198 1.1145488938924398e-05 0.001509313041465339 5346 0.0011213143112464958 0.0017154962767877266 -0.001402698465196949 4379 0.006192554730978887 -0.0031653441184367427 -0.009264818453442073 4991 -0.0034727684186087225 0.00672229248829055 0.0013722853006075157 3658 5.6074783171299546e-05 0.0008119983329096899 -0.0003793522110341408 5252 0.012993009485654105 0.002685864407586545 -0.0012816003129057366 4444 0.0030205402705040236 0.005137069087953436 0.00014687770242463542 5144 -0.005396622733770205 0.003660610148429856 -0.002018991892263014 4567 -0.0036520253755931292 0.0034896773694168283 -0.011926076343317757 4493 -0.0067067189294307975 0.004569558787147976 -0.005166789928956357 5074 0.0061519292358068545 0.0009719004009631318 0.010130426520864691 5151 0.004467825617466709 0.008116726726466371 0.002667161439428115 4947 -0.002231298450094783 0.004670102353903666 -9.356596186622164e-05 4999 -0.0018469853689665958 0.013798372585239348 -0.0006199388162862486 2191 -0.0007718589032305589 0.0002709302580555929 0.0005343127686148741 5134 -0.0005046467685735445 -0.0028831644029650378 -0.004016897828029244 5237 -0.0060364856540282156 0.010697978144057168 0.006869050890425202 3656 0.0008888611723960474 0.0015282150698481037 0.0008511372902008904 5504 -0.006062064685112767 -0.0020226882431636337 -0.006243387444576912 4848 0.004622862120521225 -0.003277154887646844 0.013046694967644778 5297 -0.00542704229172029 -0.007009520396200526 -0.001566802981113773 5448 0.0016588528717784122 -0.001577790499957438 -0.0025913807183658086 5240 0.011873264074232235 -0.0006620288332559309 0.004623202391972939 5036 0.004903274535237999 -0.0011662871251320393 0.0010745784591280189 5503 -0.00864275159149699 0.0004293688842270091 -0.0024576432322724493 5253 0.0010831544882335758 -0.0035124637264090644 0.0010164806895098125 5357 -0.008696610059905291 0.005344228734804203 0.005351706381920343 5456 -0.0019781670032787504 -0.0036287213317525123 -0.007620236673815719 3660 0.0010820982483153805 3.4484783343071714e-05 0.0002694202710196809 5501 0.0017609279469793094 0.0009699944990514128 0.006645072180108897 4589 -0.0031421710023484327 -0.005717254151019924 -0.004052201676217882 5026 0.00547998394226404 -0.0023103616566170406 -0.0015598970235844467 5299 -0.00039213471491286863 -0.0019533961388979748 -0.00037784231174913885 5125 -0.0010384942412040943 -0.00768518581432446 0.00011631531150690705 3669 0.00015188771355047052 0.0015008258579510161 -0.0020955896193764305 4865 -0.005698053882283504 -0.0013615522130349714 0.003440402706159248 5325 -0.0016502826775400838 0.00502828043837159 0.00607284402812715 2942 0.0009632425914094488 0.0002631574817799458 -0.0014926813331258577 5250 -0.004300307884040767 0.00387137989120598 0.009309568880608502 5148 0.004693892647740833 -0.004801427670736562 -0.01060860812668008 4807 -0.005212127264641987 -0.004630459123674449 0.004911749358471558 4816 0.0019094024534407686 -0.0012389718667968356 0.008379806989290748 4992 -0.0026373426523017586 -0.0008182508735214333 0.008058817420102914 4590 0.001251485709891068 0.001733120751326324 0.0005611031955100694 5427 0.022772314897277636 0.015456881761188337 -0.0008437176200292384 5278 0.0032370237372933105 0.0043587205874862055 0.004403834880583032 5432 0.011580828187204599 -0.0015806968980338874 0.0016160055532757423 738 -0.0005263532041428218 0.0016583116246963584 -0.001714895737775772 5458 -0.006266051774230881 0.0050129331332673735 -0.0033844618648230236 5025 0.005393264631535685 -0.0030230697436701304 -0.0026972428562209902 5126 0.002908445710516358 0.0007984503899666853 -0.005444175300215663 5482 -0.000408207353848063 -0.006321020061624531 -0.0019595865835997754 728 0.0014711177592886793 -0.0005334161630389846 0.00020594794838352162 5140 0.011943364685204039 0.002626952157630311 0.0020390483456438208